专利摘要:
The present invention discloses a method for manufacturing a fringe field switching mode liquid crystal display device. Here, a gate bus line has a double layer structure of an ITO layer and an opaque metal layer, and thus the gate bus line and a counter electrode region where a counter electrode is formed are formed at the same time. In addition, a data bus line has a double layer structure of the ITO layer and the opaque metal layer, and thus the data bus line and a pixel electrode region where a pixel electrode is formed are formed at the same time. A polyimide layer is employed as an electrode insulating layer formed between the pixel electrode and the counter electrode.
公开号:US20010005238A1
申请号:US09/738,157
申请日:2000-12-15
公开日:2001-06-28
发明作者:Suk Yun;Seong Park;Young Kwon
申请人:Hynix Semiconductor Inc;
IPC主号:G02F1-134363
专利说明:
[0001] 1. Field of the Invention [0001]
[0002] The present invention relates to a liquid crystal display device, and in particular to a fringe field switching mode liquid crystal display device including a pixel electrode and a counter electrode of a transparent material which generate a fringe field having homogeneous elements in parallel to a surface of a rear substrate in a liquid crystal cell. [0002]
[0003] 2. Description of the Background Art [0003]
[0004] A homogeneous alignment mode liquid crystal display device developed by Hitachi company in Japan is an in-plane switching mode liquid crystal display device, and has a better field angle property than a twisted nematic mode liquid crystal display device. However, the homogeneous alignment mode liquid crystal display device has a poor opening ratio and transmissibility. In order to overcome such a disadvantage, there has been suggested a fringe field switching mode liquid crystal display device. [0004]
[0005] In the fringe field switching mode liquid crystal display device, a counter electrode and a pixel electrode consist of a transparent conductive material on a rear substrate. An interval between the counter electrode and the pixel electrode is larger than an interval between a front substrate and the rear substrate. Accordingly, when a picture voltage is applied between the counter electrode and the pixel electrode, a fringe field is generated in a liquid crystal cell, thereby re-aligning liquid crystal molecules. [0005]
[0006] A method for manufacturing the fringe field switching mode liquid crystal display device will now be described with reference to FIG. 1. [0006]
[0007] An indium tin oxide(ITO) layer is formed at the upper portion of the rear substrate [0007] 1 according to a sputtering method, by using Ar gas, O2 gas and ITO target. The ITO layer is patterned according to a first mask process, thereby forming a counter electrode 2 in a comb or plate shape.
[0008] Thereafter, an opaque metal layer for a gate bus line is formed according to the sputtering method at the upper portion of the rear substrate [0008] 1 where the counter electrode 2 has been formed. The opaque metal layer for the gate bus line is patterned according to a second mask process, thereby forming a gate bus line 3, a gate pad and a common electrode line(not shown).
[0009] A gate insulating layer [0009] 4, an amorphous silicon layer 5 and a doped amorphous silicon layer 6 are sequentially stacked at the upper portion of the rear substrate 1 where the gate bus line 3, common electrode line and gate pad have been formed. The amorphous silicon layer 5 and the doped amorphous silicon layer 6 are patterned according to a third mask process, thereby forming a channel and an ohmic contact portion of a thin film transistor.
[0010] An ITO layer is formed according to the sputtering method at the upper portion of the rear substrate [0010] 1 where the channel and ohmic contact portion of the thin film transistor have been formed. The ITO layer is patterned according to a fourth mask process, thereby forming a comb-shaped pixel electrode 7.
[0011] Thereafter, the gate insulating layer [0011] 4 is removed according to a fifth mask process, thereby opening the gate pad.
[0012] An opaque metal layer for a data bus line is formed according to the sputtering method at the upper portion of the rear substrate where the pixel electrode [0012] 7 has been formed and the gate pad has been opened. The opaque metal layer for the data bus line is patterned according to a sixth mask process, thereby forming a source electrode 8 a, a drain electrode 8 b and a data bus line (not shown). Here, a contact portion of the gate pad is formed at the same time.
[0013] At last, a protective layer (not shown) is deposited at the upper portion of the rear substrate [0013] 1 where the source and drain electrodes 8 a, 8 b and the data bus line have been formed. The protective layer is patterned according to a seventh mask process, thereby opening the pixel electrode 7 and the contact portion of the gate pad.
[0014] However, the conventional method for manufacturing the fringe field switching mode liquid crystal display device has a disadvantage in that a manufacturing time and cost are increased and a yield is reduced due to many mask processes. [0014] SUMMARY OF THE INVENTION
[0015] Accordingly, an object of the present invention is to provide a method for manufacturing a fringe field switching mode liquid crystal display device which can decrease a number of mask processes. [0015]
[0016] In order to achieve the above-described object of the present invention, a method for manufacturing a fringe field switching mode liquid crystal display device is applied to a fringe field switching mode liquid crystal display device including a pixel electrode and a counter electrode formed on a rear substrate to generate a fringe field in a liquid crystal cell; a thin film transistor consisting of a gate electrode, a source electrode, a drain electrode and a channel, and applying a picture signal between the pixel electrode and the counter electrode; and a gate pad formed at the edge of the rear substrate. Firstly, a transparent conductive layer for a counter electrode and an opaque metal layer for a gate bus line are sequentially stacked on the surface of the rear substrate. The transparent conductive layer for the counter electrode and the opaque metal layer for the gate bus line are patterned in an identical shape, thereby forming a gate bus line connected to the gate electrode, a counter electrode region for forming the counter electrode, and a gate pad region for forming the gate pad. Thereafter, a gate insulating layer, an amorphous silicon layer and a doped amorphous silicon layer are sequentially stacked on the rear substrate where the gate bus line and the counter electrode region have been formed. The gate insulating layer, the amorphous silicon layer and the doped amorphous silicon layer are patterned in an identical shape, thereby forming an active region overlapped with the whole region of the gate bus line. The opaque metal layer for the gate bus line in the counter electrode region and gate pad region is removed, thereby forming the counter electrode and the gate pad. An electrode insulating layer is deposited on the rear substrate where the active region, counter electrode and gate pad have been formed. The electrode insulating layer is patterned, thereby opening a part of the active region and the gate pad. A transparent conductive layer for a pixel electrode and an opaque metal layer for a data bus line are deposited on the rear substrate where the active region and gate pad region have been opened. The transparent conductive layer for the pixel electrode and the opaque metal layer for the data bus line are patterned in an identical shape, thereby forming a data bus line crossing the gate bus line, a source electrode and a drain electrode respectively electrically connected to the active region, the channel of the thin film transistor being positioned therebetween, a pixel electrode region for forming the pixel electrode to be overlapped with the counter electrode, and a contact portion of the gate pad. Thereafter, a protective layer is deposited on the rear substrate where the data bus line, source electrode, drain electrode, pixel electrode region and gate pad have been formed. The deposited protective film is patterned, thereby opening the pixel electrode region and the contact portion of the gate pad. Thereafter, the opaque metal layer for the data bus line in the opened pixel electrode region is removed, thereby forming the pixel electrode. [0016] BRIEF DESCRIPTION OF THE DRAWINGS
[0017] The present invention will become better understood with reference to the accompanying drawings which are given only by way of illustration and thus are not limitative of the present invention, wherein: [0017]
[0018] FIG. 1 is a cross-sectional view illustrating a major portion of a conventional fringe field switching mode liquid crystal display device; [0018]
[0019] FIGS. 2A through 2E are plan views illustrating sequential steps of a method for manufacturing a fringe field switching mode liquid crystal display device in accordance with a preferred embodiment of the present invention; and [0019]
[0020] FIGS. 3A through 3E are cross-sectional views illustrating the sequential steps of the method for manufacturing the fringe field switching mode liquid crystal display device in accordance with the preferred embodiment of the present invention. [0020] DETAILED DESCRIPTION OF THE PREFERRED EMBODIMENTS
[0021] A method for manufacturing a fringe field switching mode liquid crystal display device in accordance with a preferred embodiment of the present invention will now be described with reference to the accompanying drawings. [0021]
[0022] FIGS. 2A through 2E are plan views respectively illustrating sequential steps of the method for manufacturing the fringe field switching mode liquid crystal display device, and FIGS. 3A through 3E are cross-sectional views respectively illustrating the sequential steps of the method for manufacturing the fringe field switching mode liquid crystal display device. [0022]
[0023] Referring to FIGS. 2A and 3A, an indium tin oxide (ITO) layer [0023] 10 which is a transparent conductive layer and an opaque metal layer 11 for a gate bus line such as Mo, Cr, Al and MoW are sequentially stacked on a rear substrate 100. The opaque metal layer 11 for the gate bus line and the ITO layer 10 are patterned according to a first mask process, thereby forming a gate bus line 11 a and a counter electrode region 11 b for forming a counter electrode. The gate bus line 11 a has a double layer structure of the ITO layer 10 and the opaque metal layer 11 for the gate bus line. Here, the counter electrode region 11 b is formed in a plate shape, but may be formed in a comb shape.
[0024] On the other hand, in the first mask process, a gate pad region (not shown) for forming a gate pad is formed at the edge of the rear substrate [0024] 100.
[0025] As shown in FIGS. 2B and 3B, a gate insulating layer [0025] 13 a, an amorphous silicon layer 13 b and a doped amorphous silicon layer 13 c are sequentially formed at the upper portion of the rear substrate 100 where the gate bus line 11 a and the counter electrode region 11 have been formed. The gate insulating layer 13 a, the amorphous silicon layer 13 b and the doped amorphous silicon layer 13 c are patterned in an identical shape according to a second mask process, thereby forming an active region 13 overlapped with the whole region of the gate bus line 11 a. Here, a channel and an ohmic contact portion of a thin film transistor are formed, and the counter electrode region 11 b is opened.
[0026] On the other hand, in the second mask process, the opaque metal layer [0026] 11 for the gate bus line in the gate pad region is removed. Even if the gate pad consists of the ITO layer 10 for the counter electrode, a signal transmission function is not so damaged.
[0027] Thereafter, the opaque metal layer [0027] 11 for the gate bus line in the opened counter electrode region is removed, thereby forming the counter electrode 12. The counter electrode 12 has a single layer structure of the ITO layer 10 for the counter electrode.
[0028] An electrode insulating layer [0028] 15 is deposited on the rear substrate 100 where the counter electrode 12 has been formed. Preferably, the electrode insulating layer 15 consists of an insulating layer having a dielectric constant from 2 to 4 such as a polyimide layer, in order to prevent excessive increase of an auxiliary capacitance between the counter electrode 12 and a pixel electrode which will be formed in a succeeding process. As illustrated in FIGS. 2C and 3C, the electrode insulating layer 15 is patterned according to a third mask process, thereby opening a part(H) of the active region 3 and the gate pad. Here, the active region 3 is partially opened to form the thin film transistor. When the electrode insulating layer 15 is a polyimide layer, it can be patterned in accordance with exposure, developing and hardening processes.
[0029] As depicted in FIGS. 2D and 3D, an ITO layer [0029] 16 for a pixel electrode and an opaque metal layer 17 for a data bus line such as Mo, Al and Mo/Al/Mo are deposited at the upper portion of the rear substrate 100 where the part(H) of the active region 3 and the gate pad have been opened. Here, the gate pad is electrically connected to the opaque metal layer 17 for the data bus line. Thereafter, the ITO layer 16 for the pixel electrode and the opaque metal layer 17 for the data bus line are patterned according to a fourth mask process, thereby forming a data bus line 17 a crossing the gate bus line 11 a, a source electrode 17 s and a drain electrode 17 d extended from the data bus line 17 a and electrically connected to the active region, the channel of the thin film transistor being positioned therebetween, and a pixel electrode region 17 b overlapped with the counter electrode 12. The data bus line 17 a, source electrode 17 s and the drain electrode 17 b have a double layer structure of the ITO layer 16 for the pixel electrode and the opaque metal layer 17 for the data bus line. Here, a contact portion of the gate pad is formed at the same time.
[0030] As illustrated in FIGS. 2E and 3E, a protective layer [0030] 18 is deposited at the upper portion of the rear substrate 100 where the data bus line 17 a, source electrode 17 s, drain electrode 17 d and pixel electrode region 17 b have been formed. The deposited protective film 18 is patterned according to a fifth mask process, thereby opening the pixel electrode region 17 b and the contact portion of the gate pad.
[0031] Finally, the pixel electrode [0031] 19 is formed by removing the opaque metal layer 17 for the data bus line in the opened pixel electrode region 18. The pixel electrode 19 has a single layer structure of the ITO layer 16 for the pixel electrode.
[0032] As discussed earlier, in the method for manufacturing the fringe field switching mode liquid crystal display device in accordance with the present invention, the gate bus line has a double layer structure of the ITO layer and the opaque metal layer, and thus the gate bus line and the counter electrode region where the counter electrode is formed are formed at the same time. In addition, the data bus line has a double layer structure of the ITO layer and the opaque metal layer, and thus the data bus line and the pixel electrode region where the pixel electrode is formed are formed at the same time. [0032]
[0033] As a result, a manufacturing time and cost are reduced and a yield is increased due to a decreased number of the mask processes. [0033]
[0034] On the other hand, it should be recognized that the present invention can also be implemented in different embodiments. For example, an oxide or nitride layer may be employed as the electrode insulating layer. [0034]
[0035] As the present invention may be embodied in several forms without departing from the spirit or essential characteristics thereof, it should also be understood that the above-described embodiments are not limited by any of the details of the foregoing description, unless otherwise specified, but rather should be construed broadly within its spirit and scope as defined in the appended claims, and therefore all changes and modifications that fall within the meets and bounds of the claims, or equivalences of such meets and bounds are therefore intended to be embraced by the appended claims. [0035]
权利要求:
Claims (8)
[1" id="US-20010005238-A1-CLM-00001] 1. In a method for manufacturing a fringe field switching mode liquid crystal display device including a pixel electrode and a counter electrode formed on a rear substrate to generate a fringe field in a liquid crystal cell; a thin film transistor consisting of a gate electrode, a source electrode, a drain electrode and a channel, and applying a picture signal between the pixel electrode and the counter electrode; and a gate pad formed at the edge of the rear substrate, a method for manufacturing a fringe field switching mode liquid crystal display device, comprising the steps of:
sequentially stacking a transparent conductive layer for a counter electrode and an opaque metal layer for a gate bus line on the surface of the rear substrate;
forming a gate bus line connected to the gate electrode, a counter electrode region for forming the counter electrode, and a gate pad region for forming the gate pad, by pattering the transparent conductive layer for the counter electrode and the opaque metal layer for the gate bus line in an identical shape;
sequentially stacking a gate insulating layer, an amorphous silicon layer and a doped amorphous silicon layer on the rear substrate where the gate bus line and the counter electrode region have been formed;
forming an active region overlapped with the whole region of the gate bus line, by patterning the gate insulating layer, the amorphous silicon layer and the doped amorphous silicon layer in an identical shape;
forming the counter electrode and the gate pad, by removing the opaque metal layer for the gate bus line in the counter electrode region and gate pad region;
depositing an electrode insulating layer on the rear substrate where the active region, counter electrode and gate pad have been formed;
opening a part of the active region and the gate pad, by patterning the electrode insulating layer;
depositing a transparent conductive layer for a pixel electrode and an opaque metal layer for a data bus line on the rear substrate where the active region and gate pad region have been opened;
forming a data bus line crossing the gate bus line, a source electrode and a drain electrode respectively electrically connected to the active region, the channel of the thin film transistor being positioned therebetween, a pixel electrode region for forming the pixel electrode to be overlapped with the counter electrode, and a contact portion of the gate pad, by patterning the transparent conductive layer for the pixel electrode and the opaque metal layer for the data bus line in an identical shape;
depositing a protective layer on the rear substrate where the data bus line, source electrode, drain electrode, pixel electrode region and gate pad have been formed;
opening the pixel electrode region and the contact portion of the gate pad, by pattering the deposited protective film; and
forming the pixel electrode by removing the opaque metal layer for the data bus line in the opened pixel electrode region.
[2" id="US-20010005238-A1-CLM-00002] 2. The method according to
claim 1 , wherein the transparent conductive layer for the counter electrode and the transparent conductive layer for the pixel electrode are indium tin oxide (ITO) layers.
[3" id="US-20010005238-A1-CLM-00003] 3. The method according to
claim 1 , wherein the opaque metal layer for the gate bus line consists of one of Mo, Cr, Al and MoW.
[4" id="US-20010005238-A1-CLM-00004] 4. The method according to
claim 1 , wherein the opaque metal layer for the data bus line consists of one of Mo, Al and Mo/AL/Mo.
[5" id="US-20010005238-A1-CLM-00005] 5. The method according to
claim 1 , wherein a dielectric constant of the electrode insulating layer ranges from 2 to 4.
[6" id="US-20010005238-A1-CLM-00006] 6. The method according to
claim 5 , wherein the electrode insulating layer is a polyimide layer.
[7" id="US-20010005238-A1-CLM-00007] 7. The method according to
claim 6 , wherein the step for pattering the electrode insulating layer comprises the steps of:
exposing the electrode insulating layer; and
developing the exposed electrode insulating layer.
[8" id="US-20010005238-A1-CLM-00008] 8. The method according to
claim 7 , further comprising a step for hardening the developed electrode insulating layer between the step for developing the exposed electrode insulating layer and the step for patterning the transparent conductive layer for the pixel electrode and the opaque metal layer for the data bus line.
类似技术:
公开号 | 公开日 | 专利标题
US6486934B2|2002-11-26|Method for manufacturing fringe field switching mode liquid crystal display device
US6362032B1|2002-03-26|Method for manufacturing fringe field switching mode liquid crystal display
US6281953B1|2001-08-28|Liquid crystal display having high aperture ratio and high transmittance and method of manufacturing the same
US7265799B2|2007-09-04|Thin film transistor array panel and manufacturing method thereof
JP3740513B2|2006-02-01|Fringe field drive liquid crystal display device and manufacturing method thereof
US6916675B2|2005-07-12|Method of fabricating array substrate for use in an in-plane switching mode liquid crystal display device
US6862051B2|2005-03-01|Liquid crystal display device and method of manufacturing the same
US7477350B2|2009-01-13|Thin film array panel
JP2001056474A|2001-02-27|Fringe field driven liquid crystal display device and its manufacture
US6970209B2|2005-11-29|Thin film transistor array substrate for a liquid crystal display and method for fabricating the same
US20080299712A1|2008-12-04|Manufacturing method of a thin film transistor array panel
US6335148B2|2002-01-01|Method for manufacturing TFT LCD device
US6309903B2|2001-10-30|Method for manufacturing fringe field switching mode liquid crystal display device
KR20010038386A|2001-05-15|Liquid crystal display and method for fabricating the same
US6362858B1|2002-03-26|Method of manufacturing liquid crystal display device
KR100632216B1|2006-10-09|Array substrate for liquid crystal display device and manufacturing method thereof
US7116389B2|2006-10-03|Liquid crystal display device and method of manufacturing the same
US20020047948A1|2002-04-25|Array substrate for a liquid crystal display and method for fabricating thereof
JP2947299B2|1999-09-13|Matrix display device
US11221532B2|2022-01-11|Display substrate, method of manufacturing the same, display panel and display device
KR100697368B1|2007-03-20|Method of manufacturing tft-lcd
JPH0850303A|1996-02-20|Array substrate for liquid crystal display device
JPH09185083A|1997-07-15|Liquid crystal display device and its production
同族专利:
公开号 | 公开日
US6486934B2|2002-11-26|
KR20010058193A|2001-07-05|
KR100322970B1|2002-02-02|
引用文献:
公开号 | 申请日 | 公开日 | 申请人 | 专利标题
US20050017247A1|2003-07-25|2005-01-27|Jae-Bon Koo|Flat panel display|
US20060139504A1|2004-12-24|2006-06-29|Ahn Byung C|Liquid crystal display device and fabricating method thereof|
US20060146256A1|2004-12-31|2006-07-06|Ahn Byung C|Liquid crystal display device and fabricating method thereof|
US20060146245A1|2004-12-31|2006-07-06|Ahn Byung C|Liquid crystal display device and fabricating method thereof|
US20060273315A1|2005-05-20|2006-12-07|Lg.Philips Lcd Co., Ltd.|Liquid crystal display device and fabrication method thereof|
US20070205422A1|2004-12-24|2007-09-06|Ahn Byung C|Liquid crystal display device and fabricating method thereof|
CN100376934C|2004-02-14|2008-03-26|鸿富锦精密工业(深圳)有限公司|Liquid crystal display device|
JP2010055119A|2003-09-26|2010-03-11|Hydis Technology Co Ltd|Fringe field switching liquid crystal display device|
US7679699B2|2004-12-31|2010-03-16|Lg Display Co., Ltd.|Liquid crystal display device and fabricating method thereof|
US20100141885A1|2008-12-08|2010-06-10|Sanghun Han|Liquid crystal display of fringe field switching type|
US20110063556A1|2004-12-24|2011-03-17|Byung Chul Ahn|Liquid crystal display device and fabricating method thereof|
CN108027541A|2015-09-11|2018-05-11|三菱电机株式会社|Thin film transistor base plate and its manufacture method|JPH10221704A|1997-02-07|1998-08-21|Sharp Corp|Reflection type liquid crystal display device and its manufacture|
US20010055074A1|1997-07-22|2001-12-27|Hiroshi Komatsu|In-plane switching mode lcd with specific arrangement of common bus line, data electrode, and common electrode|
KR20000039794A|1998-12-16|2000-07-05|김영환|Method for manufacturing liquid crystal display device with high aperture rate and high transparency|KR100500684B1|1999-12-29|2005-07-12|비오이 하이디스 테크놀로지 주식회사|Method for fabricating liquid crystal display using 4-mask process|
TW498178B|2000-05-02|2002-08-11|Hannstar Display Corp|Manufacturing method and structure for in-plane switching mode liquid crystal display unit|
KR100587217B1|2000-12-29|2006-06-08|엘지.필립스 엘시디 주식회사|A substrate for IPS mode Liquid crystal display device and method for fabricating the same|
KR100507276B1|2001-05-07|2005-08-09|비오이 하이디스 테크놀로지 주식회사|Fringe field switching mode lcd device|
KR20060038079A|2004-10-29|2006-05-03|삼성전자주식회사|Multi domain liquid crystal display|
KR101137861B1|2005-06-20|2012-04-20|엘지디스플레이 주식회사|Thin film transister of fringe field switching type and fabricating method thereof|
TWI280666B|2005-08-24|2007-05-01|Chunghwa Picture Tubes Ltd|Thin film transistor array substrate and repairing method thereof|
US20110085121A1|2009-10-08|2011-04-14|Hydis Technologies Co., Ltd.|Fringe Field Switching Mode Liquid Crystal Display Device and Method of Fabricating the Same|
法律状态:
2000-12-15| AS| Assignment|Owner name: HYUNDAI ELECTRONICS INDUSTRIES CO., LTD., KOREA, R Free format text: ASSIGNMENT OF ASSIGNORS INTEREST;ASSIGNORS:YUN, SUK SHIN;PARK, SEONG YIK;KWON, YOUNG TAE;REEL/FRAME:011376/0743 Effective date: 20001211 |
2001-11-16| AS| Assignment|Owner name: HYNIX SEMICONDUCTOR INC., KOREA, REPUBLIC OF Free format text: CHANGE OF NAME;ASSIGNOR:HYUNDAI ELECTRONICS INDUSTRIES CO., LTD.;REEL/FRAME:012280/0141 Effective date: 20010329 Owner name: HYUNDAI DISPLAY TECHNOLOGY INC., KOREA, REPUBLIC O Free format text: ASSIGNMENT OF ASSIGNORS INTEREST;ASSIGNOR:HYNIX SEMICONDUCTOR INC.;REEL/FRAME:012287/0925 Effective date: 20011023 |
2002-11-07| STCF| Information on status: patent grant|Free format text: PATENTED CASE |
2003-03-10| AS| Assignment|Owner name: BOE-HYDIS TECHNOLOGY CO., LTD., KOREA, REPUBLIC OF Free format text: ASSIGNMENT OF ASSIGNORS INTEREST;ASSIGNOR:HYUNDAI DISPLAY TECHNOLOGY, INC.;REEL/FRAME:013879/0345 Effective date: 20030303 |
2006-04-28| FPAY| Fee payment|Year of fee payment: 4 |
2010-03-31| FPAY| Fee payment|Year of fee payment: 8 |
2014-04-25| FPAY| Fee payment|Year of fee payment: 12 |
优先权:
申请号 | 申请日 | 专利标题
KR1019990061704A|KR100322970B1|1999-12-24|1999-12-24|Method for manufacturing fringe field switching mode lcd|
KR99-61704||1999-12-24||