A bipolar electrochemical cell plate (1) having a first and a second conductive sheet (10, 20), wherein at least a first distribution channel (Cal) of a first conductive sheet (10) is provided. and a second distribution channel (Cc1) of a second conductive sheet (20) each comprise: at least one superimposed said portion (Sal, Sc1), at which they are superimposed on one another and in contact mutually by their respective bottom wall (14-1, 24-1), and - at least a so-called reinforcement portion (Ral, Rcl), at which they are in contact, by their bottom wall (14-1, 24-1) respectively, with a separation rib (Nal, Nc2) of the opposite conductive sheet.
公开号:FR3049392A1
申请号:FR1652545
申请日:2016-03-24
公开日:2017-09-29
发明作者:Jean-Philippe Poirot-Crouvezier
申请人:Commissariat a lEnergie Atomique CEA;Commissariat a lEnergie Atomique et aux Energies Alternatives CEA;
IPC主号:
专利说明:

BIPOLAR PLATE OF ELECTROCHEMICAL CELL WITH IMPROVED MECHANICAL STRENGTH TECHNICAL FIELD
[001] The field of the invention is that of electrochemical reactors comprising a stack of electrochemical cells, such as fuel cells and electrolysers, and more particularly bipolar plates, of the conductive sheet type, located between the electrodes of adjacent electrochemical cells.
STATE OF THE PRIOR ART
An electrochemical reactor, such as a fuel cell or an electrolyzer, usually comprises a stack of electrochemical cells, each of which comprises an anode and a cathode separated electrically from each other by an electrolyte, the cells being the instead of an electrochemical reaction between two reactants introduced continuously.
[003] Generally, in the case of a fuel cell, the fuel (for example hydrogen) is brought to the anode while the oxidant (for example oxygen) is brought to the cathode. The electrochemical reaction is subdivided into two half-reactions, an oxidation reaction and a reduction reaction, which take place respectively at the anode / electrolyte interface and at the cathode / electrolyte interface. To take place, the electrochemical reaction requires the presence of an ionic conductor between the two electrodes, namely the electrolyte for example contained in a polymer membrane, and an electronic conductor formed by the external electrical circuit. The stack of cells is thus the place of the electrochemical reaction: the reagents must be brought there, the products and the non-reactive species must be removed, just like the heat produced during the reaction.
[004] The electrochemical cells are usually separated from each other by bipolar plates which provide the electrical interconnection of the cells. The bipolar plates usually comprise an anode face at which a fuel distribution circuit is formed, and a cathodic face, opposite to the anode face, at which an oxidant distribution circuit is formed. Each distribution circuit takes the form of a network of channels arranged for example in parallel or presenting undulations, or transverse shifts, in the plane (X, Y) of the bipolar plate, to bring the reactive species homogeneously to the corresponding electrode. Bipolar plates may also include a cooling circuit formed by an internal duct network that ensures the flow of a heat transfer fluid to evacuate the heat produced locally during the reaction by the cell.
Each bipolar plate may be formed of two electrically conductive sheets contiguous to each other in the stacking direction of the electrochemical cells. They have reliefs, or bosses, forming both the channels of the distribution circuits on the outer faces of the sheets, and the channels of the cooling circuit between the inner faces of the sheets. The conductive sheets may be made of metal and the reliefs may be formed by stamping.
[006] The bipolar plates also have a mechanical function insofar as they ensure the transmission of a clamping force within the stack of electrochemical cells, this mechanical effort contributing to improve the quality of the electrical contact between the electrodes and bipolar plates of electrochemical cells. There is then a need for bipolar plates with conductive sheets having improved mechanical strength.
STATEMENT OF THE INVENTION
The invention aims to remedy at least in part the disadvantages of the prior art, and more particularly to provide a bipolar electrochemical cell plate with improved mechanical strength. For this, the object of the invention is a bipolar electrochemical cell plate, comprising a first and a second conductive sheet, each having an inner face and an opposite outer face, contiguous to each other at the faces. internal, and each having relief forming, at the outer faces, distribution channels for distributing reactive gases.
[008] The distribution channels of the same conductive sheet are separated in pairs by a separation rib intended to be in contact with an electrode of an electrochemical cell, and each distribution channel comprises a bottom wall connected to the adjacent separation ribs.
[009] According to the invention, at least one first distribution channel of the first conductive sheet and a second distribution channel of the second conductive sheet each comprise: at least one superimposed portion, at which they are superimposed to each other and in mutual contact by their respective bottom wall, and - at least a so-called reinforcement portion, at which they are in contact, by their respective bottom wall, with a separation rib of the opposite conductive sheet.
Some preferred but non-limiting aspects of this bipolar plate are the following: [0011] A first reinforcing portion of the first distribution channel may be juxtaposed transversely to a second reinforcing portion of the second distribution channel, the first reinforcing portion being in contact with a separation rib which borders the second distribution channel, and the second reinforcing portion being in contact with a separating rib which borders the first distribution channel.
The first distribution channel and / or the second distribution channel may each comprise, between a superimposed portion and a reinforcing portion, an area at which it is not in contact with the opposite conductive sheet, allowing thus a local fluidic communication between adjacent cooling channels.
Each of said distribution channels may comprise a plurality of superimposed portions and reinforcing portions, arranged longitudinally alternately.
Reinforcement portions of a distribution channel may be disposed longitudinally offset vis-à-vis reinforcing portions of an adjacent distribution channel.
A conductive sheet may comprise distribution channels each having superimposed portions and reinforcing portions, said distribution channels having a substantially straight longitudinal axis or transverse corrugations.
The opposite conductive sheet may comprise distribution channels each comprising superimposed portions and reinforcing portions, some of which have a substantially straight longitudinal axis and others have a longitudinal axis with transverse corrugations vis-à-vis a rectilinear longitudinal axis.
Distribution channels of the first conductive sheet may have a longitudinal axis with transverse corrugations in a first direction, and distribution channels of the second conductive sheet may have a longitudinal axis with transverse corrugations in a second direction opposite to the first direction.
The first conductive sheet may comprise a number of distribution channels less than the number of distribution channels of the second conductive sheet, at least one separation rib of the first conductive sheet having a transverse dimension which varies longitudinally.
The second conductive sheet may be intended to contact a cathode of an electrochemical cell while the first conductive sheet may be intended to contact an anode of an adjacent electrochemical cell.
A reinforcing portion may have a form of outgrowth of the distribution channel towards the opposite conductive sheet, said distribution channel having a local depth greater than a local depth at a superimposed portion.
The invention also relates to an electrochemical cell, comprising: a bipolar plate according to any one of the preceding characteristics; a membrane / electrode assembly, one of said electrodes is in contact with the first or the second conductive sheet of the bipolar plate.
BRIEF DESCRIPTION OF THE DRAWINGS
Other aspects, objects, advantages and features of the invention will appear better on reading the following detailed description of preferred embodiments thereof, given by way of non-limiting example, and made by reference. in the accompanying drawings in which:
FIGS. 1A and 1B are cross-sectional views which schematically illustrate a bipolar plate according to a first embodiment, situated between two membrane / electrode assemblies, whose anode and cathode distribution channels have superposed portions (FIG. ) and reinforcing portions (fig.lB); Figure 2 is a perspective and exploded view of a portion of the bipolar plate according to the first embodiment; Figs. 3A-3G are cross-sectional views of the bipolar plate portion illustrated in Fig. 2, showing the alternation of superimposed portions and reinforcing portions of the anode and cathode distribution channels; FIG. 4 is a perspective and exploded view of a bipolar plate portion according to a second embodiment, in which the anode distribution channels extend along a rectilinear longitudinal axis for some and along a longitudinal axis with transverse corrugations for others; Figs. 5A-51 are cross-sectional views of the bipolar plate portion shown in Fig. 4, showing the alternation of superimposed portions and reinforcing portions of the anode and cathode distribution channels; FIG. 6 is a perspective and exploded view of a bipolar plate portion according to a third embodiment in which the anode distribution channels extend along a longitudinal axis with transverse corrugations and the cathodic distribution channels extend along a rectilinear longitudinal axis; Figs. 7A to 7Q are cross-sectional views of the bipolar plate portion shown in Fig. 6, showing alternating superimposed portions and reinforcing portions of the anode and cathode distribution channels.
DETAILED PRESENTATION OF PARTICULAR EMBODIMENTS
In the figures and in the following description, the same references represent identical or similar elements. In addition, the various elements are not represented on the scale so as to favor the clarity of the figures. Moreover, the various embodiments and variants are not exclusive of each other and can be combined with each other.
Various embodiments and variants will be described with reference to a fuel cell, and in particular to a PEM (Proton Exchange Membrane) type fuel cell, the cathode of which is supplied with oxygen and the anode. in hydrogen. The invention is however applicable to any type of fuel cell, in particular to those operating at low temperature, that is to say at a temperature below 200 ° C, as well as to electrochemical electrolyzers.
Figures 1A and 1B illustrate partially and schematically an example of a bipolar plate 1 of electrochemical cell according to a first embodiment. Electrochemical cells here belong to a stack of cells of a fuel cell. Each electrochemical cell comprises a membrane / electrode assembly 2 formed of an anode 3 and a cathode 4 separated from each other by an electrolyte 5 comprising here a polymer membrane. The membrane / electrode assemblies 2 of the electrochemical cells are arranged between bipolar plates 1 adapted to bring reactive species to the electrodes and to evacuate the heat produced during the electrochemical reaction.
We define here and for the rest of the description a direct orthonormal reference (Χ, Υ, Ζ) where the Z axis is oriented along the thickness of the bipolar plate and therefore along the axis stacking cells electrochemical, and where the X and Y axes define a plane parallel to the plane of the bipolar plates.
In a manner known per se, each electrode 3,4 comprises a diffusion layer (GDL, for Gas Diffusion Rent, in English), disposed in contact with a bipolar plate 1, and an active layer located between the membrane 5 and the diffusion layer. Active layers are the locus of electrochemical reactions. They comprise materials allowing the oxidation and reduction reactions at the respective interfaces of the anode and the cathode with the membrane. The diffusion layers are made of porous material permitting the diffusion of the reactive species from distribution circuit bipolar plates 1 to the active layers, and the diffusion of products from the electrochemical reaction to the same distribution circuit.
Each bipolar plate 1 is formed of two conductive sheets 10, 20 contiguous and assembled to one another, these conductive sheets being stamped so as to form reactive gas distribution circuits at the level of the electrodes 3,4. each of the electrochemical cells, and a cooling circuit located between the conductive plates 10, 20. Thus, a first conductive sheet 10, called anodic, is intended to be in contact with the anode 3 of a membrane / electrode assembly 2 of an electrochemical cell, while the second conductive sheet 20, said cathode, is intended to be in contact with the cathode 4 of a membrane / electrode assembly 2 of an adjacent electrochemical cell.
Each conductive sheet 10, 20 has an outer face 11, 21 and an inner face 12, 22 opposite, the conductive sheets 10,20 being contiguous to each other at the inner faces 12, 22. A outer face 11, 21 is said to be anodic when it is intended to be in contact with the anode 3 of an electrochemical cell, or cathode when it is intended to be in contact with the cathode 4 of the adjacent electrochemical cell. The anode face of a conductive sheet 10, 20 comprises the distribution circuit of a reactive gas, for example hydrogen, and the cathodic face of the other conductive sheet comprises a distribution circuit of a reactive gas, for example air or oxygen.
The conductive sheets 10, 20 are in the form of sheets, or elementary plates of small thickness, made of an electrically conductive material, for example a metal or a composite material for example loaded graphite. The thickness can be of the order of a few tens of microns to a few hundred microns, for example from 50pm to 200pm approximately in the case of metal sheets.
The conductive sheets comprise reliefs, or bosses, obtained for example by stamping or forming in press, whose shape on one side is complementary to the shape on the opposite face. These reliefs form, at the outer faces 11, 21, the reactive gas distribution circuits, and, at the internal faces 12, 22, a cooling circuit comprising channels in which a heat transfer fluid is intended to flow. .
Each distribution channel Cal, Ccl ... is formed of side walls 13-1, 23-1 ... which extend substantially in the Z axis of the thickness of the bipolar plate 1, these walls. 13-1, 23-1 ... being interconnected by a bottom wall 14-1, 24-1 .... Each distribution channel Cal, Ccl ... is separated from the neighboring channels of the same circuit. distribution by a so-called separation rib wall Nal, Ncl ..., which connects the adjacent side walls of two adjacent distribution channels, this separation rib being intended to come into contact with the corresponding electrode. In other words, the anode channels Cal, Ca2 ..., resp. cathodes Ccl, Cc2 ..., distribution are separated in pairs by an anode rib Nal, Na2 ... resp. Ncl cathode, Nc2 ..., separation. The separation rib is a wall whose surface is preferably substantially flat.
[0033] A local distribution channel depth may be defined as being the dimension along the Z axis between the bottom wall of the channel and a plane passing through the adjacent separation ribs. It is also possible to define a local separation rib width as being the dimension of the rib in a cross section. Furthermore, adjacent or adjacent transversely means juxtaposed along an axis transverse to the longitudinal axis of a distribution channel.
According to the invention, at least one first distribution channel of the first conductive sheet and a second distribution channel of the second conductive sheet each comprise: at least one so-called superimposed portion, at which they are superimposed on each other; one to the other and in mutual contact by their respective bottom wall, and at least a so-called reinforcement portion, at which they are in contact, by their respective bottom wall, with a separating rib of the conductive sheet opposite.
As shown in FIG. 1A, which represents a first cross section of the bipolar plate 1, at least one anodic distribution channel Cal and a cathode channel.
Distribution Ccl are superimposed on each other and in mutual contact by their bottom wall 14-1, 24-1 respectively, this at a portion said superimposed portion Sal, Sel respective. By superimposed portion, it is meant that the distribution channel considered is placed facing or at the right, that is to say perpendicular, a distribution channel of the opposite conductive sheet, along the Z axis of thickness of the bipolar plate 1. In this configuration, each distribution channel Cal, Ccl has, in its superimposed portion Sal, Salt, a so-called nominal depth.
In this example, all the cathode channels are not superimposed and in contact with anode channels. This is the case here of the cathode channel Cc2, located between the cathode channels Cc1 and Cc3, which is not superimposed on an anode channel. This absence of anode channels facing certain cathode channels results in the presence of anodic separation ribs of different widths. Thus, the anode ribs Nal and Na3 are said to be narrow and have a first width, insofar as they separate each of the anode channels whose superimposed portion is in contact with adjacent cathode channels. On the other hand, the anode rib Na2 is said to be wide and has a second width greater than the first width, insofar as it separates two anodic channels Cal, Ca2 with superimposed portions in contact with non-adjacent cathode channels Ccl, Cc3, c '. that is to say, not juxtaposed transversely. Thus, the width of the broad anode rib Na2 is substantially equal to the sum of the widths of the cathode ribs Nc2 and Nc3 and the width of the cathode channel Cc2.
This configuration is advantageous insofar as the cooling channel Cr2 delimited in particular by the broad anode rib Na2 has a large flow section, greater than that of the cooling channels Cri, Cr3 located at the narrow anode ribs Nal , Na3. This configuration is said to have a preferred flow, since this large flow section results in a reduction of the local pressure drop in the cooling channel Cr2, which contributes to locally improving the flow of the coolant and thus the evacuation of the heat produced by the electrochemical cells in operation.
As illustrated in FIG. 1B, which represents a second cross-section of the bipolar plate 1, the anodic distribution channels Cal and cathode Ccl further comprise a reinforcement portion Ral, Rc1, distinct from the superimposed portion.
Sal, Salt, at which they are each in contact, by their bottom wall 14-1, 24-1 respectively, with a separation rib of the opposite conductive sheet, here the ribs Nal and Nc2.
In this example, the anode channel Cal is in contact, at the bottom wall 14-1 of the reinforcing portion R1, with a cathodic separation rib, here the rib Nc2 located between the cathode channels Ccl and Cc2. It is thus offset transversely with respect to the longitudinal axis of the cathode channel Ccl, to be facing and in contact with the cathode rib Nc2. Similarly, the cathode channel Ccl is in contact, at the bottom wall 24-1 of the reinforcing portion Rc1, with an anode separation rib, here the rib Nal located between the cathode channels CaO, Cal.
The reinforcement portions Ral, Rc1 are a protrusion of the channel in the direction of the opposite conductive sheet to come into contact with a separation rib. The distribution channels then have a maximum local depth.
Preferably, the reinforcement portions R1, Rc1 of the anode channels Cc and cathode Ccl are adjacent to each other, that is to say directly adjacent, or juxtaposed, one of the other in a transverse direction. In this situation, a side wall 13-1 of the anodic reinforcement portion Ral is located adjacent, possibly with mechanical contact, with a side wall 23-1 of the cathode reinforcing portion Rc1. In other words, a reinforcement portion Ral of the anode channel Cal is adjacent to a reinforcing portion Rc1 of the cathode channel Cc1, the anodic reinforcing portion Ral being in contact with a cathodic separation rib Nc2 which borders the cathode channel distribution Ccl, and the cathodic reinforcing portion Rcl being in contact with a separating rib Nal bordering the anodic channel distribution Cal.
This configuration results in a local mechanical reinforcement of the bipolar plate to the extent that the side walls of each reinforcing portion here provide the transmission of mechanical clamping forces directly from a membrane / electrode assembly of a cell to the membrane / electrode assembly of the neighboring cell. At a constant clamping force, there is therefore a reduction in the mechanical stresses experienced by the conductive sheets with respect to the configuration of FIG. 1A since, in a plane (X, Y), four lateral walls transmit the clamping force to instead of two. In addition, the transmission of mechanical forces is improved to the extent that the mechanical forces are directly transmitted from a bottom wall of a conductive sheet to a separating rib of the opposite conductive sheet. It is then possible, with equivalent mechanical strength, to reduce the thickness of the conductive sheets, for example from 75 μm to 50 μm, which results in a decrease in the total thickness of the bipolar plate and therefore an increase in the compactness of the stacking of electrochemical cells.
It is preferred that a plurality of distribution channels of the distribution circuits comprises superimposed portions and reinforcement portions disposed alternately along the longitudinal axis of the channels. By alternating, it is understood that the superimposed portions and the reinforcing portions succeed each other, repeatedly, periodically or not, along the longitudinal axis of the channel.
Thus, in that the anodic and cathodic distribution channels comprise superimposed portions in mutual contact in a first zone and reinforcing portions in a second zone, the mechanical strength of the bipolar plate is thus improved while maintaining areas of privileged flow. Moreover, as will be explained later, the alternation of superimposed portions and reinforcing portions along the longitudinal axis of the distribution channel may result in local fluid communication between adjacent cooling channels, which allows a transverse mixing of the heat transfer fluid flow along its longitudinal axis, thus improving the evacuation of the heat produced by the electrochemical cells in operation.
FIG. 2 is a perspective and exploded view of a bipolar plate portion 1 according to the first embodiment illustrated in FIGS. 1A and 1B.
The anodic distribution channel Cal alternates longitudinally between a superimposed portion Sal where it is superimposed and in contact with the superimposed portion Salt of the cathode distribution channel Ccl, and a reinforcement portion Ral where it is in contact with a rib of separation of the cathode conductive sheet 20, here the cathode rib Nc2. The cathodic distribution channel Ccl alternates longitudinally between a superimposed portion Salt which is superimposed and in contact with the superimposed portion Sal of the anode channel Cal, and a reinforcing portion Rc1 which is in contact with a separation rib of the anodic conductive sheet 10 , here the anodic rib Nal.
In this example, the anodic reinforcement portion Ral is in contact with the cathode rib Nc2, but, alternatively, it could be in contact with another cathodic rib, for example the rib Nc3. Similarly, the cathodic reinforcing portion Rc1 is in contact with the anode rib Nal, but it could alternatively be in contact with another anode rib.
The passage between the superimposed portions Sal and the reinforcement portions Ral is effected here by a transverse corrugation, or transverse offset, of the anodic channel Cal with respect to a principal axis passing here by the superimposed portions Sal, this axis being here parallel to the rectilinear longitudinal axis of the cathode distribution channel Ccl against which the superimposed portions Sal are in contact. By transverse ripple is meant that the distribution channel locally has a transverse offset, in the plane (X, Y), with respect to a main axis along which the channel extends.
Alternatively, the anode channel Cal may not comprise corrugations, and the cathode channel Ccl may then include a transverse corrugation so that the reinforcing portion Rc1 comes into contact with an anodic separation rib. As a variant, the anodic channels C 1 and C 1 may have transverse corrugations so that the respective reinforcing portions R 1 and R 1 1 are facing each other and in contact with an opposite separating rib.
Moreover, the length of the superimposed portions and reinforcement portions of the distribution channels results from an optimization between the mechanical reinforcement of the bipolar plate by the spatial distribution of the reinforcement portions on the one hand, and the spatial distribution. preferred flow sections located at the superimposed portions on the other hand.
Figures 3A to 3G are several cross-sectional views of the bipolar plate shown in Figure 2, illustrating an alternation between the superimposed portions and the reinforcing portions of the distribution channels.
FIG. 3A represents the anodic channels Cal and cathodic Ccl superimposed on each other at their superposed portions Sal and Salt which are in mutual contact at their respective bottom wall. The channels Cal and Ccl have their nominal depth. The separation rib Na2 has a width greater than those of the separation ribs Nc2 and Nc3 opposite, insofar as there is no anode channel opposite the cathode channel Cc2. The cooling channel Cr2 located at the anode rib Na2 then has a large flow section, which results in a decreased local pressure drop which improves the quality of the flow and therefore the local heat dissipation. This configuration is called privileged flow.
FIGS. 3B and 3C show the anode channel Cal in an intermediate portion which operates a transition, in the form of a corrugation or transverse shift, between the superimposed portion Sal (FIG. 3A) and the reinforcement portion Ral (FIG. .3D). In this intermediate portion, the anode channel Cal shifts transversely to the longitudinal axis of the cathode channel Ccl to come progressively opposite a cathodic separation rib, here the rib Nc2. In this intermediate portion, it has its nominal depth. Moreover, the intermediate portion includes a zone, illustrated in FIG. 3C, in which the channels Cal and Ccl are no longer in contact with each other, which results in fluidic communication between the cooling channels C 1 and Cr 2. This fluidic communication results in a large reduction in the local pressure drop and allows transverse mixing of the heat transfer fluid flow between the cooling channels, which improves the homogenization of the heat removal produced by the cells. electrochemical in operation.
3D represents the anode channel Cal at its reinforcing portion RL, that is to say in its portion where the bottom wall is in contact with an opposite cathodic rib, here the rib Nc2. The cathode channel Ccl also has a reinforcing portion Rc1 coming into direct contact with the opposite anode rib Nal. The reinforcement portions R1, R1c are in the form of a protrusion of the channel in the direction of the opposite conductive sheet, with a maximum depth greater than the nominal value. The anode channel Cal is then no longer superimposed, in the direction of stacking direction Z, with the cathode channel Ccl. Thus, by the support of the distribution channels Cal and Ccl directly on an opposite separation rib, the mechanical stresses on the bipolar plate are locally reduced and the transmission of the forces is improved, which contributes to reinforcing the mechanical strength of the bipolar plate.
FIGS. 3E and 3F represent the anodic channel Cal in the intermediate portion which operates a transition, here in the form of a corrugation or transverse shift, between the reinforcement portion Ral (FIG. 3D) and the superimposed portion Sal downstream (fig.3G). This portion is thus similar to that shown in Figures 3B and 3C. The anode channel Cal shifts transversely to the longitudinal axis of the cathode channel Ccl to come gradually opposite a cathode channel, here the channel Ccl. In this intermediate portion, it again presents its nominal depth as the cathode channel Ccl. The intermediate portion here also comprises a zone, illustrated in FIG. 3E, in which the channels Cal and Ccl are no longer in contact with each other, which results in a fluidic communication between the cooling channels C 1 and Cr 2 which allows a mixing of the flow between these cooling channels and results in a reduction in the local pressure drop, which improves the homogenization of the heat dissipation by the coolant.
[0056] Figure 3G shows the anode channel Cal at a new superimposed portion Sal in which it is superimposed and in contact with the cathode channel Ccl in its superimposed portion Salt. This configuration is here identical to that illustrated in FIG. 3A.
Advantageously, a plurality of distribution channels alternate longitudinally between superimposed portions and reinforcing portions. This alternation may be periodic or not, and the lengths of the reinforcing portions and superimposed portions may be identical or different, depending on the desired distribution of mechanical stresses and the distribution of areas with low local pressure drop within the circuits. distribution and cooling circuit.
Figure 4 is an exploded view in perspective of a bipolar plate portion 1 according to a second embodiment. This embodiment differs essentially from the first embodiment in that the cathodic distribution channels extend along a longitudinal axis with transverse corrugations, and in that the anodic distribution channels extend for some along a rectilinear longitudinal axis. and for others along a longitudinal axis with transverse corrugations.
The anode channel Ca2 here comprises a longitudinal alternation between superimposed portions Sa2 and reinforcing portions Ra2, here along a substantially rectilinear axis. The superimposed portions Sa2 are superimposed and in contact with the cathodic channel Cc3 opposite at its superimposed portions Sc3; and the reinforcing portions Ra2 are in contact with a cathodic separation rib, here the rib Nc4.
In addition, the anode channels Cal and Ca3 adjacent to the Ca2 channel here comprise transverse corrugations, that is to say transverse offsets here along the -Y direction, between two successive reinforcement portions. Thus, the separation ribs located between the undulating channels and the rectilinear channels, for example the anode ribs Na2 and Na3, have a width that varies longitudinally between a minimum value and a maximum value.
The cathode channel Cc3 also comprises an alternation between superimposed portions Sc3 and reinforcing portions Rc3, here along a longitudinal axis that ripples with respect to the rectilinear longitudinal axis of the Ca2 channel. The superimposed portions Sc3 are in contact with the anode channel Ca2 opposite at the bottom wall of the latter, and the reinforcing portions Rc3 are in contact with an anode rib, here the rib Na2.
Moreover, the cathodic distribution channels here all have transverse corrugations parallel to each other. Thus, insofar as the cathode channels here are undulating and parallel to each other, the cathodic separation ribs have a substantially constant width along the longitudinal axis. In this example, the corrugations of the cathode channels are made in a + Y direction, in phase opposition with the corrugations in the direction Y of the undulating anode channels. As explained below, these undulations of the cathode channels and some anode channels result in the formation of localized areas where the conductive sheets are not in contact with each other, which results in the fluidic communication between these cooling channels and therefore the mixing of the heat transfer fluid, as well as a reduction in the local pressure drop, which improves the homogenization of the heat dissipation by the heat transfer fluid.
FIGS. 5A to 51 are cross-sectional views of the bipolar plate portion illustrated in FIG. 4, which show an alternating sequence between superposed portions and reinforcement portions of distribution channels.
FIG. 5A illustrates a cross section in which the anode channel Ca2 has a superposed portion Sa2 in contact with the superimposed portion Sc3 of the cathode channel Cc3, that is to say that the bottom wall of the anode channel Ca2 is superimposed and in contact with the bottom wall of the cathode channel Cc3. Furthermore, the anode channel Ca 2 is close to two channels Cal and Ca 3 which here have reinforcing portions Ra and Ra 3, that is to say that the bottom wall of these channels Cal, Ca 3 is in contact, respectively, with an opposite cathodic separation rib. In addition, cathode channels, here the channels Cc1 and Cc4, also have reinforcing portions Rc1 and Rc4, that is to say that the bottom wall of these channels Cc1, Cc4 is in contact, respectively, with a anodic separation rib opposite.
FIGS. 5B, 5C and 5D illustrate a wave sequence in which the Ca2 and Cc3 channels pass from their superposed portion Sa2 and Sc3 (FIG. 5A) to their reinforcement portion Ra2 and Rc3 (FIG. 5E). Thus, FIG. 5B shows the decrease in the depth of the anode channels Cal, Ca3 and of the cathode channels Ccl, Cc4, from a maximum value to a nominal value. Then Figures 5C and 5D show the transverse undulation of the cathode channels in the + Y direction, and some anode channels in the opposite -Y direction. Thus, the anode channel Ca2 remains rectilinear while the opposite cathode channel Cc3 shifts transversely along the + Y direction. In addition, the anode channels Cal and Ca3 are shifted transversely along the -Y direction while all the cathode channels are shifted transversely along the + Y direction. The waviness terminates when the anode channel Ca2 is opposite the cathode rib Nc4 and the cathode channel Cc3 opposite the anode rib Na2.
During this wave sequence, the anode and cathode channels have areas in which the conductive sheets are locally no longer in mutual contact, which allows fluid communication between cooling channels. This is the case in FIG. 5B, where the reduction in the depth of the anode channels Cal and Ca3 and the cathode channels Ccl and Cc4 allows fluid communication between the cooling channels C 1 and Cr 2 on the one hand, and between the cooling channels C 1 and C 2 Cr3 and Cr4 cooling on the other hand. This is also the case in FIG. 5D where the transverse corrugation locally causes the fluidic communication between all the cooling channels Cr1, Cr2, Cr3, Cr4. These fluidic communications between the cooling channels result in a reduction of the local pressure drop, and allow a mixing of the heat transfer fluid, which results in a homogenization of the heat evacuation produced by the electrochemical cells in operation.
FIG. 5E illustrates a cross section where the anode channel Ca2 has a reinforcing portion Ra2, and where the cathode channel Cc3 also has a reinforcing portion Rc3. Thus, the bottom wall of the channels Ca 2, Cc 3 is in contact, respectively, with the separation rib Nc 4, Na 2. In this example, the anode channels Cal, Ca3 have their nominal depth, but they could alternatively have a portion of reinforcement. This is also the case of the cathode channels Ccl, Cc2, Cc4, Cc5.
FIGS. 5F, 5G and 5H illustrate another wave sequence in which the anode channel Ca2 and the cathode channel Cc3 pass from their reinforcing portion Ra2, Rc3 (FIG. 5E) to their superimposed portion Sa2, Sc3 (FIG. fig.5l). There is thus a phase of decreasing the depth of the channels (FIG. 5F), which results in the fluidic communication of the cooling channels, and then a transverse wave phase (FIG. 5G and 5H) according to FIG. -Y direction for the cathode channels and in the opposite direction + Y for the anode channels Cal, Ca3, until the channels Ca2 and Cc3 are superimposed on each other in their respective superimposed portion Sa2, Sc3.
FIG. 51 illustrates a cross section in which the Ca2 and Cc3 channels are superimposed and in mutual contact at their respective superimposed portions Sa2, Sc3; and in which the anode channels Cal, Ca3 as well as the cathode channels Ccl have a reinforcing portion. This section is identical to that of Figure 5A and is not further detailed.
Figure 6 is an exploded and perspective view of a bipolar plate portion according to a third embodiment. In this example, the number of anode distribution channels is substantially equal to the number of distribution cathode channels. The anodic and cathodic separation ribs have a width substantially equal to each other, this width being substantially constant along the longitudinal axis of the channels.
The cathode channels Cc1, Cc2 ... here each have an alternation of superposed portions Salt, Sc2 ... and reinforcing portions Rc1, Rc2 ... along a substantially straight longitudinal axis. The superimposed portions Sel, Sc2 ... are thus in contact with superposed portions Sal, Sa2... Of the opposite anode channels Cal, Ca2.... The reinforcing portions Rc1, Rc2... Are in contact with the ribs. Nal, Na2 ....
Anodic channels Cal, Ca2 ... here each have an alternation of superimposed portions Sal, Sa2 ... and reinforcement portions Ral, Ra2 ... along a longitudinal axis which has transverse corrugations, here parallel between they. However, to allow the flow of heat transfer fluid between the conductive sheets, the reinforcing portions of neighboring anode channels are longitudinally offset in pairs. Thus, when an anode channel has a reinforcing portion, the adjacent anode channels have a depth less than the maximum depth, thereby forming a cooling channel between the two conductive sheets. In this example, the reinforcing portions of two adjacent anode channels have a longitudinal offset of half a waving period. This arrangement thus increases the flow mixing of the heat transfer fluid, as explained with reference to FIGS. 7A to 7Q.
Figures 7A to 7Q are cross-sectional views of the bipolar plate portion shown in Figure 6, showing an alternating sequence between superimposed portions and reinforcing portions.
FIG. 7A illustrates a cross-section with reinforcing portions in a first configuration of mechanical reinforcement, in which the cathode channels all have reinforcement portions on the one hand, and in which a first set of anode channels has portions reinforcement while a second set of anode channels do not have portions of reinforcement. The cathode channels Cc1, Cc2 ... thus comprise reinforcing portions Rc1, Rc2 ... so that there is contact between the bottom wall of each cathode channel with an opposite anode separation rib Nal, Na2. .. An anode channel in two comprises here a reinforcing portion. Thus, the anode channels Ca 2 and Ca 4 comprise reinforcing portions Ra 2 and Ra 4 and thus have a maximum depth for coming into contact with the opposite cathodic ribs. On the other hand, the anode channels Cal, Ca3 do not comprise a reinforcing portion and have a minimum depth so as to thus form cooling channels with the opposite cathodic ribs.
FIG. 7E illustrates an intermediate cross section with superimposed portions in a preferred flow configuration, where the anode and cathode channels have superimposed portions. It is located between the sections with reinforcing portions of Figures 7A, 71 and 7Q. In this section, the cathode channels Ccl, Cc2 ... each have a portion Salt, Sc2 ... superimposed and in contact with a superimposed portion Sal, Sa2 ... anode channels Cal, Ca2 ....
FIG. 71 illustrates a cross-section with reinforcing portions according to a second configuration of mechanical reinforcement, in which the cathode channels have reinforcing portions, and in which the first set of anode channels does not have reinforcing portions, whereas that the second set of anode channels presents. It corresponds to a half-wave period between the reinforcing portions of the anode channels. The cathode channels have a configuration identical to that of FIGS. 7A and 7Q. Moreover, the anode channels Ca 2, Ca 4 of the first set do not comprise a reinforcing portion and have a minimum depth so as to form cooling channels with the opposite cathodic ribs. On the other hand, the anode channels Cal, Ca3 of the second set comprise reinforcement portions Ral, Ra3 and thus have a maximum depth for coming into contact with the opposite cathodic ribs.
FIG. 7M illustrates a cross section with superimposed portions, similar to that of FIG. 7E, where the anode and cathode channels have superposed portions.
Finally, FIG. 7Q illustrates a cross section with reinforcement portions identical to that illustrated in FIG. 7A. These two sections correspond to a period of waving between the reinforcing portions of the anode channels.
Between the sections described above is a transverse wave sequence in which the anode channels undulate transversely to the rectilinear longitudinal axis of the cathode channels facing.
FIGS. 7B, 7C, 7D thus illustrate a transverse wave sequence between FIG. 7A with reinforcement portions in a first configuration and FIG. 7E with superimposed portions. The channels whose depth was maximum at the reinforcement portions decrease their depth (Fig.7B and 7C), then the anode channels are shifted transversely, here along the + Y direction, to come opposite the cathode channels (fig.7C and 7D), and finally the anodic channels of minimum depth increase their depth to come into contact with the cathode channels (Fig.7D and 7E). Thus, an extended communication between the cooling channels is carried out in the section of FIG. 7C which ensures an extensive mixing of the heat transfer fluid flow, and then a local communication between two adjacent adjacent cooling channels is carried out in the section. of fig.7D.
FIGS. 7F, 7G, 7H also illustrate a transverse wave sequence between FIG. 7E with superimposed portions and FIG. 71 with reinforcement portions according to the second configuration. The anode channels of the first set of channels decrease their depth from the nominal value to a minimum value, which ensures local communication between adjacent cooling channels in pairs. Then, the anode channels are shifted transversely vis-à-vis the cathode channels, here along the -Y direction, to come opposite the cathodic separation ribs (Fig.7G). Fluidic communication between the cooling channels is performed in this section of Fig.7G, which ensures extensive mixing of the flow of heat transfer fluid. Finally, the anode channels of the second set of channels increase their depth from the nominal value Pnom to the maximum value Pmax to form reinforcing portions coming into contact with the opposite cathodic ribs.
Transverse corrugation sequences take place between the sections of Fig.7l and 7M (Fig.7J to 7L, similar to those of Fig.7B to 7D) and between the sections of Fig.7M and 7Q (Fig. 7N to 7P, similar to those of Fig.7F to 7H), and are not described in more detail here.
Thus, the bipolar plate has a mechanical strength enhanced by the presence of anodic and cathodic reinforcing portions, while having preferred flow zones by the presence of anodic and cathodic superimposed portions. In addition, it has areas of extended or local fluidic communication between the cooling channels which ensures a mixing of the coolant and improves the evacuation of the heat produced by the electrochemical cells in operation.
Specific embodiments have just been described. Various variations and modifications will occur to those skilled in the art.
Thus, the transverse corrugations can be non-periodic. In addition, two successive reinforcement portions of the same distribution channel may not be in contact with the same separation rib of the opposite conductive sheet, but be in contact with different separation ribs. Similarly, two successive superimposed portions of the same distribution channel may not be in contact with the same distribution channel of the opposite conductive sheet, but be in contact with different distribution channels.
These different variants, combined or not with each other, and applied to the anodic distribution circuit and / or cathodic distribution circuit, can optimize both the mechanical strength of the bipolar plate, the spatial distribution of the zones. with preferential flow at the superimposed portions, and the mixing of the flow of the coolant and the cooling circuit.
权利要求:
Claims (12)
[1" id="c-fr-0001]
Electrochemical cell bipolar plate (1) having a first and a second conductive plate (10, 20), each having an inner face (12, 22) and an opposite outer face (11, 21), contiguous thereto. one to the other at the inner faces (12, 22), and - each having reliefs forming, at the outer faces (11, 21), distribution channels (Ca, Ce) for distributing reactive gases , where the distribution channels (Ca, Ce) of the same conductive sheet (10, 20) are separated in pairs by a separation rib (Na, Ne) intended to be in contact with an electrode (3, 4). ) of an electrochemical cell, and o each distribution channel (Ca, Ce) having a bottom wall (14, 24) connected to the adjacent separation ribs (Na, Ne), characterized in that at least one first channel of distribution (Cal) of the first conductive sheet (10) and a second distribution channel (Ccl) of the second conductive sheet (20) each comprise: - at least one said superimposed portion (Sal, Salt), at which they are superimposed on one another and in mutual contact with their bottom wall (14-1, 24-1 ), and - at least a so-called reinforcement portion (Ral, Rcl), at which they are in contact, by their respective bottom wall (14-1, 24-1), with a separation rib (Nal). , Nc2) of the opposite conductive sheet (10, 20).
[2" id="c-fr-0002]
2. bipolar plate (1) according to claim 1, wherein a first reinforcing portion (Ral) of the first distribution channel (Cal) is juxtaposed transversely to a second reinforcing portion (Rcl) of the second distribution channel (Ccl) , the first reinforcing portion (Ral) being in contact with a separation rib (Nc2) which borders the second distribution channel (Ccl), and the second reinforcing portion (Rc1) being in contact with a separation rib (Nal) which borders the first distribution channel (Cal).
[3" id="c-fr-0003]
3. Bipolar plate (1) according to claim 1 or 2, wherein the first distribution channel (Cal) and / or the second distribution channel (Ccl) each comprise, between a superimposed portion (Cal, Ccl) and a portion reinforcement (Ral, Rcl), an area at which it is not in contact with the opposite conductive sheet (10,20), thereby allowing local fluid communication between adjacent cooling channels (C 1, Cr 2).
[4" id="c-fr-0004]
4. Bipolar plate (1) according to any one of claims 1 to 3, wherein each of said distribution channels (Cal, Ccl) comprises a plurality of superimposed portions (Sal, Salt) and reinforcing portions (Ral, Rcl ), arranged longitudinally alternately.
[5" id="c-fr-0005]
Bipolar plate (1) according to claim 4, wherein reinforcing portions (Ral) of a distribution channel (Cal) are arranged longitudinally offset with respect to reinforcement portions (Ra2) of an adjacent distribution channel (Ca2).
[6" id="c-fr-0006]
6. bipolar plate (1) according to any one of claims 1 to 5, wherein a conductive sheet (20) has distribution channels (Ccl, Cc2) each having superimposed portions (Salt, Sc2) and portions of reinforcement (Rc1, Rc2), said distribution channels (Cc1, Cc2) having a substantially rectilinear longitudinal axis or with transverse corrugations.
[7" id="c-fr-0007]
7. bipolar plate (1) according to claim 6, wherein the opposite conductive sheet (10) comprises distribution channels (Cal, Ca2) each having superimposed portions (Sal, Sa2) and reinforcing portions (Ral, Ra2 ), some of which have a substantially straight longitudinal axis and others have a longitudinal axis with transverse corrugations vis-à-vis a rectilinear longitudinal axis.
[8" id="c-fr-0008]
8. bipolar plate (1) according to claim 6 or 7, wherein distribution channels (Cal, Ca2) of the first conductive sheet (10) have a longitudinal axis with transverse corrugations in a first direction, and distribution channels. (Cc1, Cc2) of the second conductive sheet (20) have a longitudinal axis with transverse corrugations in a second direction opposite to the first direction.
[9" id="c-fr-0009]
9. bipolar plate (1) according to any one of claims 1 to 8, wherein the first conductive sheet (10) has a number of distribution channels (Cal, Ca2) less than the number of distribution channels (Ccl, Cc2 ) of the second conductive sheet (20), at least one separation rib (Nal, Na2) of the first conductive sheet (10) having a transverse dimension which varies longitudinally.
[10" id="c-fr-0010]
10. bipolar plate (1) according to any one of claims 1 to 9, wherein the second conductive sheet (20) is intended to contact a cathode (4) of an electrochemical cell while the first conductive sheet (10). is intended to contact an anode (3) of an adjacent electrochemical cell.
[11" id="c-fr-0011]
11. bipolar plate (1) according to any one of claims 1 to 10, wherein a reinforcing portion (Ral, Rcl) has a form of outgrowth of the distribution channel (Cal, Ccl) towards the conductive sheet opposed (10, 20), said distribution channel (Cal, Ccl) having a local depth greater than a local depth at a superimposed portion (Sal, Salt).
[12" id="c-fr-0012]
An electrochemical cell, comprising: - a bipolar plate (1) according to any one of the preceding claims; - A membrane / electrode assembly (2), one of said electrodes (3, 4) is in contact with the first (10) or second (20) conductive sheet of the bipolar plate (1).
类似技术:
公开号 | 公开日 | 专利标题
EP3223352B1|2018-12-19|Bipolar plate of fuel cell with improved mechanical strength
EP3223351B1|2018-12-19|Bipolar plate of a thin fuel cell
KR102123785B1|2020-06-18|Design of bipolar plates for use in electrochemical cells
EP2771934B1|2017-01-18|High-temperature or fuel-cell electrochemical system having improved thermal management
EP1356536A1|2003-10-29|Method for making an assembly of base elements for a fuel cell substrate
EP1749323B1|2009-01-14|Solid electrolyte fuel cell
EP2351136A1|2011-08-03|Electrolyte with reduced rigidity, and electrochemical system including such an electrolyte
FR3014246A1|2015-06-05|SEAL FOR ELECTROCHEMICAL DEVICE, METHOD FOR MANUFACTURING AND ASSEMBLING JOINT, AND DEVICE.
WO2011110677A1|2011-09-15|High-temperature electrolyser architecture, having high target production by an electrolysis cell and a limited cell degradation rate
EP1220346A1|2002-07-03|Composite basic element and seal thereof for a fuel cell and method for fabricating of said assembly
EP3171441B1|2018-04-18|Bipolar plates for limiting the bypass of flow channels by the reagents
WO2015101924A1|2015-07-09|Electric and fluid interconnector for an hte electrolyser or sofc fuel cell
EP3175502B1|2018-08-15|Electrochemical reactor balancing the charge loss of the homogenising zones of the cathode and the anode
EP3092671B1|2017-10-18|Flow-guiding plate for a fuel cell
FR3043845A1|2017-05-19|BIPOLAR PLATES TO LIMIT THE OPERATION OF FLOW CHANNELS BY REAGENTS
FR3043846A1|2017-05-19|BIPOLAR PLATES TO LIMIT THE OPERATION OF FLOW CHANNELS BY REAGENTS
WO2016142619A1|2016-09-15|Fuel-cell stack having a reinforced structure
FR3035543A1|2016-10-28|ENHANCED BIPOLAR FUEL CELL PLATE PROVIDING HOMOGENEOUS FLUID DISTRIBUTION
EP3621137B1|2021-02-17|Separator for fuel cell having homogenized gas distribution
EP3678243A1|2020-07-08|Electrochemical cell holding plate comprising an optimised fluid distribution network
EP2301101B1|2012-11-07|Fuel cell having a membrane/electrode stack perpendicular to the support substrate, and production process
EP3514875B1|2020-03-25|Cellular assembly for adapting the power of electrochemical reactors
EP3136492B1|2018-10-17|Stack of electrochemical cells distributed into separate groups comprising a homogenisation compartment
EP2873107B1|2017-05-17|Fuel cell having improved electric insulation
EP3195392A1|2017-07-26|Fluid flow guide plate for electrochemical reactor, and assembly comprising said plate
同族专利:
公开号 | 公开日
EP3223352A1|2017-09-27|
JP2017201618A|2017-11-09|
US20170279131A1|2017-09-28|
JP6920844B2|2021-08-18|
FR3049392B1|2018-04-20|
EP3223352B1|2018-12-19|
引用文献:
公开号 | 申请日 | 公开日 | 申请人 | 专利标题
US20050058864A1|2003-09-12|2005-03-17|Goebel Steven G.|Nested bipolar plate for fuel cell and method|
JP2006228580A|2005-02-17|2006-08-31|Nissan Motor Co Ltd|Fuel cell stack|
JP2007200700A|2006-01-26|2007-08-09|Honda Motor Co Ltd|Fuel cell and its manufacturing method|
US20110212385A1|2009-01-22|2011-09-01|Toyota Jidosha Kabushiki Kaisha|Fuel cell separator and fuel cell|
US7029784B2|2002-05-30|2006-04-18|Plug Power Inc.|Nested fuel cell field plate|
JP2008243499A|2007-03-27|2008-10-09|Toyota Motor Corp|Fuel cell|
US8802326B2|2010-11-23|2014-08-12|GM Global Technology Operations LLC|Fuel cell separator plate|
KR20150017402A|2013-06-10|2015-02-17|현대하이스코 주식회사|Fuel cell stack with excellent circulating performance|US10854892B2|2018-02-08|2020-12-01|Toyota Jidosha Kabushiki Kaisha|Fuel cell stack having improved joining strength between separators|
FR3092202B1|2019-01-24|2021-01-08|Commissariat Energie Atomique|BIPOLAR PLATE FOR HOMOGENIZING THE COOLANT TEMPERATURES|
DE102020205871A1|2020-05-11|2021-11-11|Siemens Aktiengesellschaft|Fuel cell cooling|
DE102020114399A1|2020-05-28|2021-12-02|Ekpo Fuel Cell Technologies Gmbh|Flow element, use of a flow element, bipolar plate and method for producing a flow element|
法律状态:
2017-03-31| PLFP| Fee payment|Year of fee payment: 2 |
2017-09-29| PLSC| Search report ready|Effective date: 20170929 |
2018-03-29| PLFP| Fee payment|Year of fee payment: 3 |
2019-03-29| PLFP| Fee payment|Year of fee payment: 4 |
2020-12-18| ST| Notification of lapse|Effective date: 20201110 |
优先权:
申请号 | 申请日 | 专利标题
FR1652545A|FR3049392B1|2016-03-24|2016-03-24|BIPOLAR PLATE OF ELECTROCHEMICAL CELL WITH IMPROVED MECHANICAL STRENGTH|
FR1652545|2016-03-24|FR1652545A| FR3049392B1|2016-03-24|2016-03-24|BIPOLAR PLATE OF ELECTROCHEMICAL CELL WITH IMPROVED MECHANICAL STRENGTH|
EP17162346.5A| EP3223352B1|2016-03-24|2017-03-22|Bipolar plate of fuel cell with improved mechanical strength|
JP2017055450A| JP6920844B2|2016-03-24|2017-03-22|Bipolar plate of electrochemical cell with improved mechanical strength|
US15/467,320| US20170279131A1|2016-03-24|2017-03-23|Bipolar plate of an electrochemical cell with improved mechanical strength|
[返回顶部]