![]() METHOD FOR SELECTIVELY ENGRAVING LAYER OR LAYER STACK ON GLASS SUBSTRATE
专利摘要:
The invention relates to a method for depositing on a glass substrate functional mineral layer (s), comprising the steps of: depositing on the substrate an organic coating on a part but not on its entire surface , in accordance with a pattern, depositing on the substrate thus coated one or more functional mineral layer (s), to subject the assembly to a heat treatment so as to effect the combustion of the organic coating, and then - removing it and the functional mineral layer (s) covering it (s) by wiping such as cloth and / or gaseous and / or washing, so as to obtain the functional mineral layer (s) in a pattern corresponding to the negative of that produced with the organic coating; an intermediate product of this process and the application of the glazing obtained by this method to let the radio frequencies pass. 公开号:FR3048244A1 申请号:FR1651629 申请日:2016-02-26 公开日:2017-09-01 发明作者:Barbara Brudieu;Vincent Rachet;Francois Guillemot;Nicolas Nadaud 申请人:Saint Gobain Glass France SAS; IPC主号:
专利说明:
The invention relates to a glazing unit on which it has been deposited by a physical vapor deposition (PVD) process under vacuum, mainly magnetron-assisted cathodic sputtering, plasma enhanced chemical vapor deposition (PECVD) or evaporation or liquid deposition process of one or more thin layers with spatial structuring at scales that may vary from several cm to less than 10pm. The targeted products are varied: silver layers (solar control, low-emissive, electromagnetic shielding, heating), layers modifying the level of reflection in the visible (anti-reflection or mirror layers), layers transparent or non-transparent electrodes, layers electrochromic, electroluminescent, anti-irritation, antifouling, anti-scratch, magnetic, colored or absorbent layers to modify the transmittance in the visible for aesthetic purposes. The targeted products are in particular the stacks deposited by magnetron sputtering. We will think, but not exclusively, of glazing having both a reflective character of near and / or far IR waves as is usual in thermally controlled glazing. The function provided is in this case, either the drastic reduction of the emissivity of the surface of the glazing (thermal insulation), or a significant decrease in the amount of solar energy passing through the entire glazing (solar control). Similarly, glazing covered with a conductive layer providing an electrode function - for example for a heating function (eglass for building, windscreen or side heating applications for automotive or aeronautical applications) - will be considered. can be used as an antenna to capture electromagnetic waves. A particular case concerns the microwave band around GHz (100pm <1m) which finds applications for radio transmissions (GSM, Satellite, Radar ...). Indeed, the possibility of structuring the layer at a scale smaller than that of the wavelength gives access to the range of metamaterials where the electromagnetic transmission can be modulated. For these different functions (antenna, heating, thermal control), the highly conductive layer and without grounding, causes a significant attenuation of the high frequency electromagnetic waves and it is difficult to ensure the compromise between thermal control (above the case of the reduction of heating in a vehicle) and the good reception of the communication signals. The conventional attenuation on a windshield of a thermal control layer may for example be -30 to -45dB between 1 and 5 GHz. This compatibility of thermal functions with transparency to communication waves (eg 2G / 3G / 4G) is strongly demanded for automotive applications and increasingly for buildings without relays. There are currently two solutions to overcome this difficulty: the thermal control function can be provided not by a conductive thin layer but not a polyvinyl butyral (PVB) interlayer or other containing nanoparticles of a conductive compound such as indium doped with tin (ITO for indium tin oxide) for example. In this case, the thermal control is ensured by absorption and not reflection of the energy portion of the spectrum. This solution is only possible for solar control, and inefficient compared to the solution in reflection and requires a laminated glazing. The second solution consists in etching the silver layer after deposition so as to selectively remove the silver on sufficiently fine strips (100 μm) so as to be difficult to perceive by the eye and separated from each other by a few mm according to the wavelengths which we wish to promote the transmission. Complex patterns can be used for this application in the face. Representatives of this technique are in particular the documents WO9954961 A1 and WO2014033007 A1. In addition, the heating efficiency of a conductive layer depends on its resistance square R2, the voltage between the electrodes but also the distance between the electrodes. For building applications, this dependency is a problem because, at the same power source, an electrical resistance of the glazing is required for each heating zone size. One solution may be to burn one more time for example a base layer Ag so as to modulate its resistance by global square to enable it to be compatible with the distance between electrodes and the desired surface heating power. Finally, a silver-based glazing can be functionalized in the form of an antenna provided the electromagnetic decoupling of the layer with the frame of the car for example. This operation is also ensured by an engraving. Alternative selective etching methods are mainly from the microelectronics industry. Some use temporary layers, others consist of direct engraving. In the microelectronics industry, photolithography: uses temporary layers to mask selective acid attacks. The photo lithography allows very fine engravings (45-90 nm today industrially) but remains limited to the size of the masks today limited by the size of the optics. The laser etching of the conductive layer is provided by a point-etch laser which will sublimate the thin-film stack by scanning the beam. This operation has a low productivity on large glazings and requires a significant investment compared to the treated surfaces. Impact etching of ions or electrons has the same limitations as laser etching in terms of productivity. Other engraving methods come from traditional printing. To date, inkjet printing techniques are still limited for sizes greater than 10 m 2 at printing times greater than one minute. Screen printing may be preferred over other techniques when a scale of resolution smaller than 50 μm is desired: this method provides relatively poor edge qualities at these small scales. The purpose of the invention is therefore to provide functional glazings that allow radiofrequency to pass through. The term "functional glazing" is intended to mean an antenna glazing, heating, thermally controlled, or the like, a glazing with electroconductive layer (s) or not, as well as all the other glazings mentioned above. Radio frequencies are high frequency electromagnetic waves, around the GHz, and find applications in radio transmissions (GSM, satellite, radar ...), communication (for example 2G / 3G / 4G). For this purpose, the subject of the invention is a process for depositing on a glass substrate a layer or stack of essentially mineral functional layers, characterized in that it comprises the steps consisting in depositing on the substrate an essentially organic coating on a part but not all of its surface, in accordance with a pattern, depositing on the substrate thus coated a layer or a stack of layers essentially mineral functional (s), subjecting the assembly to a thermal treatment so as to effect the combustion of the essentially organic coating and then to eliminate it and the layer or stack of essentially mineral functional layers which covers it by wiping such as rags and / or gaseous and / or washing, so as to obtain the layer or stack of essentially mineral layers functional (s) in a pattern corresponding to n of the one made with the essentially organic coating. The product of the combustion of the organic coating is a powder which does not adhere to the substrate, so that it can then be removed with the mineral layer (s) which covers it (s) without exerting a mechanical action of the type brushing, friction or any abrasion likely to deteriorate the substrate and especially the quality of the edges of areas not printed by the organic coating and covered with the mineral layer (s) (sharpness, resolution). The method makes it possible to produce on an industrial production line, on a large surface substrate, a substantially organic coating pattern with a surface area of dimensions ranging from 1 m to 10 μm. The reduced cycle time makes it possible to validate the industrially applicable character. Preferably, the pattern-based deposition of the essentially organic coating is carried out by a liquid, direct or indirect engraved roll method such as offset, flexography, inkjet printing, masking, lithography or screen printing. . A roll with a width of at least 3210mm (Full Float Width - PLF) can be used, the engraving of which will reproduce the desired pattern. In this case it is a repetitive pattern but it remains compatible for example with the improvement of electromagnetic transmission. Preferably, the essentially organic coating is chosen from a monomer and / or oligomer acrylate, epoxy acrylate, polyester acrylate, polyurethane acrylate, polyvinylpyrrolidone + EDTA composition, polyamide, polyvinyl butyral, positive photosensitive resin diazonaphthoquinone-novolac, any organic material crosslinked under radiation ultraviolet or infrared, single or in a mixture of several of them. Preferably, the substantially organic coating has a thickness of at most 30, and in order of increasing preference, at most 20 and 10 μm, and particularly preferably approximately 5 μm. However, thicknesses of 1 μm or even a few hundred nm are not excluded from the invention. Apart from the printed areas of this organic coating corresponding to patterns ranging from 1m to 10pm of surface dimensions, it is necessary to have less than 100nm (or not at all) of temporary organic coating thickness in order not to degrade the functional mineral stack in these areas believed to have an intact mineral stack after quenching. Preferably, prior to the deposition of the essentially mineral-functional layer (s), the development of the essentially organic coating comprises a crosslinking by heat treatment and / or under radiation such as ultraviolet (UV) and / or drying, then the whole is washed. The essentially organic coating may be advantageously crosslinked under UV to limit the space required for drying. However, it will be ensured that the creep of the essentially organic coating (varnish, resin, etc.) before crosslinking is limited in order to avoid the loss of accuracy of the pattern. The varnish or resin will be properly dried before going under a conventional washing machine of layer deposition device (in English: coater) and then the operation of depositing the layer or layers (thin) essentially functional thin (s) (s) ) for example conductor (s) is performed. One could also consider washing the glass before the partial deposition (printing) of the organic coating, then perform this printing optionally followed by crosslinking, then enter directly into the layer deposition device (coater) (without prior washing). Preferably, the layer or stack of essentially mineral functional layers is formed by a method of physical vapor deposition (PVD for PhysiCai Vapor Deposition) under vacuum such as cathodic sputtering assisted by magnetron, evaporation or plasma enhanced chemical vapor deposition (PECVD for Plasma Enhanced Chemical Vapor Deposition) or liquid. Preferably, the layer or stack of essentially mineral functional layers is composed of Ag, transparent conductive oxide (TCO) such as indium oxide doped with tin (ITO). , zinc doped indium oxide (IZO), ZnO: Al, Ga, cadmium stannate, Al, Nb, Cu, Au, Si and N compound such as S13N4, afferent dielectric stack, alone or in combination of several 'between them. The glass can not be cut once soaked, it can be, in some applications, for example building, stored and cut, started etc. before quenching. This glazing can be sold as such, mainly in this case with a layer then removed by quenching at a transformer. Preferably, the heat treatment is part of a thermal tempering of the glass substrate. During quenching, the varnish or the resin disappears by combustion and effectively eliminates the layer or stack of essentially mineral layers (s) functional (s), possibly conductive at the locations of the patterns, which causes the desired selective etching. In a particular embodiment, the heat treatment is part of a bending of the glass substrate, in particular a bending by pressing. In this case, a preliminary heat treatment causes the disappearance of the varnish or the resin. If pressing tools are used to bend, it will be ensured that the combustion of the essentially organic coating takes place before this pressing phase. According to a variant of the process, after the deposition of the layer or the stack of essentially mineral layers (s) functional (s), is deposited again at least one essentially organic coating sequence - layer or stack of layers essentially mineral (s) Function (s). This deposition is preferably carried out before the heat treatment for the eombustion of the substantially organic coating closest to the substrate, and a subsequent heat treatment will produce the combustion of several superimposed organic coatings as well as the subsequent removal of several layers or layers of layers. essentially mineral functional covering them. However, the deposition of essentially organic layer-layer or stack layers of essentially mineral layers (s) sequence, from the second sequence, after the combustion heat treatment of the first substantially organic coating and wiping or gaseous blast removal of Its organic residues and mineral residues covering them, is also part of the invention. The glass substrate obtained by the process of the invention is also capable of being integrated in a laminated glazing unit or other laminated composite product, and / or in a multiple glazing unit. Other objects of the invention consist of a glass substrate coated with at least one sequence consisting of an essentially organic coating which is not easily removable by washing with water (optionally acidified or based on) or organic solvent, on a part of but not all of its surface, in accordance with a pattern, covered with a layer or a stack of essentially mineral layers functional (s); it is therefore an intermediate product (for routine commercialization) of the process of the invention - the application of a glazing obtained by a method as previously described as functional glazing allowing radio frequencies to pass; it can be a thermal control glazing or heating and transparent (applications automotive, transport and building), a heating glaze with resistance by adapted square (automobile, transport and building), of a conducting glass already structured in antenna (automobile and transport), a solar control glazing of constant selectivity at least equal to 1.6 and very high TL light transmission, low-cost masking glazing (alternative to grinding by grinding) , of a Day Lighting type glazing with TL modulated according to the height, a negative index glazing in the field of microwaves (GHz) for anti-radar application, GSM ..,., a large glazing as a substrate with structured electrodes. The invention will be better understood in light of the following examples. Example 1 Referring to Figure 1, the method of the invention can be represented in four views corresponding to three successive main steps, from left to right in the Figure. A UV crosslinkable acrylate lacquer having the following formulation is used, in which the proportions are by weight: 57% of aliphatic urethane hexaacrylate oligomer (CN9276 manufactured by Sartomer), 38% of monomers and more exactly 19% of tricyclodecanedimethanol diacrylate (TCDDMDA or SR833S from Sartomer) as well as 19% of trimethylolpropane triacrylate (TMPTA or SR351 from Sartomer) and finally 5% of ketone-type photoinitiator is more precisely a mixture of benzophenone and methanone (Speedcure 500 or Irgacure 500 BASF). This varnish is prepared by mechanically mixing all these compounds (resins and photoinitiator) using a blade. After several hours of agitation, the varnish can be stored for several months if it is protected from light and strong temperature variations. To carry out the deposition, a certain quantity of this varnish is applied to the clean and brightened glass according to the indirect roll etching method as shown in step 1 of FIG. 1. After rolling, the deposited substrate + varnish is UV exposed (mercury lamp). The thickness of the lacquer pattern coating is 5 μm. After an intermediate washing step, a stack of thin layers is deposited in a conformal manner by sputtering in step 2 on the glass + vemis acrylate system. This stack of thin layers has the following constitution, in which the thicknesses are in nm: SnO2 17 / ZnO 17 / Ag 9 / Ti 1 / ZnO 11 / Si3N4 55 / ZnO 20 / Ag 9 / Ti 1 / ZnO 10 / S13N4 25. ZnO showers are non-porous. This stack with thermal control function is frempable. During a quenching step (3 in FIG. 1 generally in a convection oven at 730 ° C. for 35 seconds per mm of glass (140 seconds for a 4 mm thick glass), the organic layer is degraded which results in separation. magnetron layers in the areas where it is present.The final system consists of the stack of thin layers described above, structured in a pattern corresponding to the negative of that made with the resin, excellent results were also obtained in applying the varnish by inkjet printing. Example 2 This example differs from the previous one by the essentially organic coating. This is an ink jet deposit of an ink marketed by the Marabu Company in the Ultra-Jet DUV A range, especially in cyan or magenta color. A thickness of a few hundred nm to a few μm is obtained. The ink (patterns) is cross-linked under ultraviolet light.
权利要求:
Claims (13) [1" id="c-fr-0001] 1. Method of depositing on a glass substrate a layer or a stack of essentially mineral functional layers, characterized in that it comprises the steps of depositing on the substrate a substantially organic coating on a part but not all of its surface, according to a pattern, to deposit on the substrate and coated with a layer or a stack of essentially mineral layers (s) functional (s), to submit the assembly to a thermal treatment of to carry out the combustion of the essentially organic coating, then to eliminate it and the layer or stack of essentially mineral layers functional (s) covering it by wiping such as the cloth and / or gaseous and / / or washing, so as to obtain the layer or stack of essentially mineral layers functional (s) in a pattern corresponding to the negative of that made with the coating e essentially organic. [2" id="c-fr-0002] 2. Method according to claim 1, characterized in that the deposition according to a pattern of the essentially organic coating is carried out by a liquid process, direct or indirect engraved roll such as offset, flexography, jet printing. ink, masking, lithography or screen printing. [3" id="c-fr-0003] 3. Method according to claim 2, characterized in that the essentially organic coating is selected from a monomer and / or oligomer acrylate, epoxy acrylate, polyester acrylate, polyurethane acrylate, composition polyvinylpyrrolidone + EDTA, polyamide, polyvinyl butyral, positive photosensitive resin type diazonaphthoquinone -novolaque, any organic material crosslinked under ultraviolet or infrared radiation, alone or in a mixture of several of them. [4" id="c-fr-0004] 4. Method according to one of the preceding claims, characterized in that the substantially organic coating has a thickness at most equal to 30, and in order of increasing preference, at most equal to 20 and 10 pm, and particularly preferably approximately 5 μm. [5" id="c-fr-0005] 5. Method according to one of the preceding claims, characterized in that prior to the deposition of the layer or the stack of essentially mineral layers (s) functional (s), the development of substantially organic coating comprises a crosslinking treatment thermal and / or radiation such as ultraviolet and / or drying, then the whole is washed. [6" id="c-fr-0006] 6. Method according to one of the preceding claims, characterized in that the layer or the stack of essentially mineral layers (s) functional (s) is formed (e) by a physical vapor deposition process (PVD for Physical Vacuum Vapor Deposition) such as cathodic assisted sputtering assisted by magnetron, evaporation or plasma enhanced chemical vapor deposition (PECVD for Plasma Enhanced Chemical Vapor Deposition) or liquid. [7" id="c-fr-0007] 7. Method according to claim 6, characterized in that the layer or stack of essentially mineral layers functional (s) consists of Ag, transparent conductive oxide (TCO) such as oxide of tin doped indium (ITO), zinc doped indium oxide (IZO), ZnO: Al, Ga, cadmium stannate, Al, Nb, Cu, Au, Si and N compound such as S13N4, dielectric stack afferent, alone or in combination of several of them. [8" id="c-fr-0008] 8. Method according to one of the preceding claims, characterized in that the heat treatment is part of a thermal quenching of the glass substrate. [9" id="c-fr-0009] 9. Method according to one of the preceding claims, characterized in that the heat treatment is part of a bending of the glass substrate. [10" id="c-fr-0010] 10. The method of claim 9, characterized in that the bending is performed by pressing. [11" id="c-fr-0011] 11. Method according to one of the preceding claims, characterized in that after the deposition of the layer or the stack of essentially mineral layers (s) functional (s), is deposited again at least one essentially organic coating sequence - layer or stack of layers essentially mineral functional (s). [12" id="c-fr-0012] 12. Glass substrate coated with at least one sequence consisting of an essentially organic coating which is not easily removable by washing with water (optionally acidified or based) or organic solvent, on a part but not on its entire surface, in accordance with a pattern, covered with a layer or stack of essentially mineral layers functional (s). [13" id="c-fr-0013] 13. Application of a glazing obtained by a method according to one of claims 1 to 11 as a functional glazing letting radio frequencies pass.
类似技术:
公开号 | 公开日 | 专利标题 EP3419944A1|2019-01-02|Method for the selective etching of a layer or a stack of layers on a glass substrate EP0937691A1|1999-08-25|Process for etching a conductive layer CA2762312C|2019-02-26|Method for depositing a thin film, and resulting material KR20170076787A|2017-07-04|Process for forming optically clear conductive metal or metal alloy thin films and films made therefrom FR2936360A1|2010-03-26|PROCESS FOR MANUFACTURING A MASK WITH SUBMILLIMETRIC OPENINGS FOR SUBMILLIMETRIC ELECTROCONDUCTIVE GRID, MASK AND SUBMILLIMETRIC ELECTROCONDUCTIVE GRID. EP2381744A1|2011-10-26|Substrate for organic electroluminescent device, use and method for manufacturing said substrate, as well as an organic electroluminescent device EP0611213A1|1994-08-17|Glass substrates coated with a stack of thin layers, application to glass sheets with infra-red radiation reflective properties and/or with solar radiation properties EP1641720A2|2006-04-05|Dielectric-layer-coated substrate and installation for production thereof WO2009071822A2|2009-06-11|Substrate carrying an electrode, organic electroluminescent device comprising said substrate, and production thereof FR2695117A1|1994-03-04|Process for treating thin layers with electrical conduction and / or reflection properties in the infrared. FR3021310A1|2015-11-27|SUBSTRATE WITH PARTIALLY METALLIC LAYER STACK, GLAZING AND METHOD. EP3419945A1|2019-01-02|Method for the selective etching of a layer or a stack of layers on a glass substrate WO2020099729A1|2020-05-22|Method for the selective etching of a layer or a stack of layers on a glass substrate JP5732832B2|2015-06-10|Method for manufacturing window glass for vehicle JP2012124076A|2012-06-28|Method for forming transparent conductive film JPH08175848A|1996-07-09|Method for dividing film on film-coated glass WO2015177481A1|2015-11-26|Substrate equipped with a multilayer comprising partial metal films, glazing unit, use and process FR3021311A1|2015-11-27|SUBSTRATE WITH PARTIALLY METALLIC LAYER STACK, GLAZING AND METHOD. WO2020234126A1|2020-11-26|Laminated composite for layer elements that have thermal properties and are transparent to radio frequencies FR3019709A1|2015-10-09|METHOD FOR MANUFACTURING TRANSPARENT FLAT ANTENNA JPH09143710A|1997-06-03|Radio wave transmission type heat insulating glass and its production
同族专利:
公开号 | 公开日 EP3419944A1|2019-01-02| KR20180115702A|2018-10-23| CN108698921A|2018-10-23| MX2018010130A|2019-01-21| WO2017144823A1|2017-08-31| FR3048244B1|2018-03-16|
引用文献:
公开号 | 申请日 | 公开日 | 申请人 | 专利标题 US20080213482A1|2007-03-01|2008-09-04|Stephan Lvovich Logunov|Method of making a mask for sealing a glass package|WO2020216514A1|2019-04-25|2020-10-29|Saint-Gobain Glass France|Method for producing a pane having a structured coating|FR2548962B1|1983-07-13|1987-06-05|Saint Gobain Desjonqueres|DECORATION OF OBJECTS SUCH AS GLASS BOTTLES| US5891520A|1997-06-30|1999-04-06|Avery Dennison Corporation|Method for screen printing glass articles| FR2946335B1|2009-06-05|2011-09-02|Saint Gobain|THIN LAYER DEPOSITION METHOD AND PRODUCT OBTAINED| FR2972447B1|2011-03-08|2019-06-07|Saint-Gobain Glass France|PROCESS FOR OBTAINING A SUBSTRATE WITH A COATING| CN102976624B|2012-12-07|2015-07-15|天津耀皮工程玻璃有限公司|Pattern coating glass and preparation method thereof| CN104411103B|2014-05-31|2017-05-10|福州大学|Manufacturing method of graphical thick film silver paste conducting layer|KR102138005B1|2018-10-26|2020-07-28|계명대학교 산학협력단|Thin film pattern formation method using 3D printing and Manufacturing method of bio-diagnosis apparatus by the same| WO2020099729A1|2018-11-14|2020-05-22|Saint-Gobain Glass France|Method for the selective etching of a layer or a stack of layers on a glass substrate| CN114174237A|2019-06-28|2022-03-11|维特罗平板玻璃有限责任公司|Substrate with burnable coating mask|
法律状态:
2017-02-21| PLFP| Fee payment|Year of fee payment: 2 | 2017-09-01| PLSC| Publication of the preliminary search report|Effective date: 20170901 | 2018-02-21| PLFP| Fee payment|Year of fee payment: 3 | 2020-02-28| PLFP| Fee payment|Year of fee payment: 5 | 2021-02-26| PLFP| Fee payment|Year of fee payment: 6 |
优先权:
[返回顶部]
申请号 | 申请日 | 专利标题 FR1651629|2016-02-26| FR1651629A|FR3048244B1|2016-02-26|2016-02-26|METHOD FOR SELECTIVELY ENGRAVING LAYER OR LAYER STACK ON GLASS SUBSTRATE|FR1651629A| FR3048244B1|2016-02-26|2016-02-26|METHOD FOR SELECTIVELY ENGRAVING LAYER OR LAYER STACK ON GLASS SUBSTRATE| MX2018010130A| MX2018010130A|2016-02-26|2017-02-23|Method for the selective etching of a layer or a stack of layers on a glass substrate.| EP17710352.0A| EP3419944A1|2016-02-26|2017-02-23|Method for the selective etching of a layer or a stack of layers on a glass substrate| KR1020187024207A| KR20180115702A|2016-02-26|2017-02-23|Method for selectively patterning a layer or stack of layers on a glazing substrate| CN201780013221.4A| CN108698921A|2016-02-26|2017-02-23|The method for being etched selectively to layer or layer heap stack on the glass substrate| PCT/FR2017/050405| WO2017144823A1|2016-02-26|2017-02-23|Method for the selective etching of a layer or a stack of layers on a glass substrate| 相关专利
Sulfonates, polymers, resist compositions and patterning process
Washing machine
Washing machine
Device for fixture finishing and tension adjusting of membrane
Structure for Equipping Band in a Plane Cathode Ray Tube
Process for preparation of 7 alpha-carboxyl 9, 11-epoxy steroids and intermediates useful therein an