专利摘要:
Ceramic core used for the manufacture of a turbomachine hollow turbine blade according to the lost-wax foundry technique, the blade comprising calibrated dust-removal holes formed in an apex of at least one cavity and opening into a bathtub of this blade, the core comprising, on a core portion (22A) intended to form a calibrated dust removal hole of a determined height sufficient to guarantee the holding of the core portion, a through hole (31) of longitudinal axis defining on the core part and in a direction perpendicular to this longitudinal axis on the one hand a core cylinder (30) of a determined diameter corresponding to the dedusting hole to be formed and on the other hand a core volume remaining (33 ) to be closed after casting, so that the calibrated dust removal hole is obtained without drilling and without the use of connecting rods.
公开号:FR3047767A1
申请号:FR1651134
申请日:2016-02-12
公开日:2017-08-18
发明作者:Adrien Bernard Vincent Rollinger;Mirna Bechelany
申请人:Safran SA;
IPC主号:
专利说明:

Field of the invention
The present invention relates to the general field of turbomachine turbine blades, and more particularly to turbine blades provided with integrated cooling circuits produced by the lost-wax casting technique.
Prior art
In a manner known per se, a turbomachine comprises a combustion chamber in which air and fuel are mixed before being burned. The gases from this combustion flow downstream of the combustion chamber and then feed a high pressure turbine and a low pressure turbine. Each turbine has one or more rows of stationary blades (called distributors) alternating with one or more rows of moving blades (called moving wheels), circumferentially spaced around the rotor of the turbine. These turbine blades are subjected to very high temperatures of the combustion gases, which reach values much higher than those which can bear without damage these blades which are in direct contact with these gases, which necessarily implies to ensure their cooling continuously by an integrated cooling circuit which, when it wishes to ensure efficient and precise cooling without significantly increasing the air flow and without penalizing the engine performance, has multiple cavities. The hollow vanes thus formed are manufactured by the so-called "lost wax" foundry process which requires the use of a model piece or core whose outer surface corresponds to the internal surface of the finished blade, as described in patent application FR2961552. filed in the name of the plaintiff. The air required for the operation of the engine generally contains various dusts (in particular fine sand) which can accumulate in the cooling circuits of the turbine blades causing the closing of the outflow orifices at the outlet of the cavities and thus threatening the integrity of the dawn. To overcome this problem, the turbine blades are equipped at the top of the cavity calibrated dust holes, obtained by high precision machining or from connecting rods of alumina or quartz inserted in the ceramic core, and whose role is to generate these holes and to ensure the evacuation of these particles after their stall (that is to say their dissolution). The use of these connecting rods, however, poses certain problems. Firstly, the alumina rods are very difficult to remove by the basic solutions (or in the standard unsteady conditions of the ceramic cores) and require a high residence time, a very high concentration of sodium hydroxide or potassium hydroxide and temperatures and pressures. very high likely to be aggressive vis-à-vis the alloy (stress corrosion). Similarly, the quartz rods have a low mechanical strength thus penalizing their use in a lost wax casting process or the core which has a different coefficient of thermal expansion (CTE) and is also often of different composition, undergoes several mechanical stresses . Next, the use of rods is not applicable in all core manufacturing processes. In the case, for example, of cores produced by additive manufacturing or cores obtained by machining in a ceramic block, the rods can not be embedded in the core during manufacture (in contrast to the injection molding process). Finally, the use of rods is not applicable to all core geometries including those using thin plates whose rods must then marry the shape.
In addition, the assembly of several ceramic cores is generally done by the foot and the head of the cores (non-functional parts of the core), the excess material resulting from the casting (consequence of the assembly of the cores) must be eliminated during the machining of the bathtub which requires the use of various techniques of reloading (refilling) or brazing plates. However, these brazed plates are not robust (these can be detached and it may be necessary to thicken them locally) and the reloading is often not accurate (depth relumped uncertain). Therefore, the calibrated drilling dusting holes proves particularly difficult because this drilling takes place at the previously restamped place, with a smaller diameter while respecting the minimum dimensioned to remove debris.
Object and summary of the invention
The present invention therefore aims to overcome the aforementioned drawbacks by proposing a geometric layout of the core to simply obtain dust collection holes more reliably than currently and in particular without harming the strength of this core. Another purpose is to eliminate the final drilling operation of the bath of the prior art to obtain these holes. For this purpose, there is provided a ceramic core used for the manufacture of a turbomachine hollow turbine blade according to the lost wax foundry technique, said blade having calibrated dusting holes formed in a vertex of at least a cavity and opening into a bath of said blade, characterized in that it comprises, on a core portion intended to form a calibrated dust removal hole of a determined height sufficient to guarantee the mechanical strength of said core portion, a longitudinally extending through orifice defining on said core portion and in a direction perpendicular to said longitudinal axis on the one hand a core cylinder of a determined diameter corresponding to said dusting hole to be formed and on the other hand a core volume remaining intended to be closed after casting, so that said calibrated hole dust removal is obtained without drilling and without using rods of lia ison.
Thus, the dedusting holes can be obtained directly from the foundry by injection, additive manufacturing or machining ceramic cores without drilling or use of connecting rods. Any possible source of differential thermal expansion is suppressed, the mechanical strength of the core is improved and correlatively the mechanical properties of the blade are thus maintained. With this core, the machining operation of the prior art to take into account constraining uncertainties and can adversely affect the geometry of the plates of a multi-cavity circuit is also removed.
According to the envisaged embodiment, said core portion may form a portion of a side column for creating a lateral cavity of said blade or an inter-cavity connection zone between said at least one cavity and said tub.
Preferably, on a core portion corresponding to said bath to be created, there is provided a recessed area to allow a centering of said through hole in said connecting zone, so as to ensure a better holding of said core portion during the casting.
Advantageously, when the dimensioning of the blade imposes it, said remaining core volume comprises at least one lateral stiffener (two stiffeners giving it a quadrilobed shape) dimensioned so as to guarantee better holding of said core portion during casting. The invention also relates to the method of forming calibrated dust removal holes in a turbomachine hollow turbine blade produced by the lost-wax casting technique by means of a ceramic core as explained above and any turbomachine turbine equipped with a plurality of cooled vanes made from such a method.
BRIEF DESCRIPTION OF THE DRAWINGS Other characteristics and advantages of the present invention will emerge from the description given below, with reference to the appended drawings which illustrate an embodiment of this embodiment devoid of any limiting character and in which: FIG. partial view of a turbine blade core according to the invention, - Figure 2 is a view of a portion of the core of Figure 1 at a side plate, - Figures 2A and 2B are views respectively. after casting and after machining once the core portion of FIG. 2 is removed; FIG. 3 is a view of a portion of the core of FIG. 1 at a connection with the bath, and FIGS. 3B are respectively views after casting and after machining once the core portion of Figure 3 removed.
Detailed description of an embodiment
FIG. 1 represents, at the level of its head assembly, a ceramic core intended for the production of a turbomachine hollow turbine blade. The ceramic core 10, in the example illustrated, comprises seven parts or columns. The first column 12, which is intended to end up on the side of the arrival of the combustion gases, corresponds to a leading edge cavity which will be created after foundry, while the second column 14 corresponds to a central cavity which it is adjacent. The latter receives a flow of cooling air through a pipe resulting after foundry, the presence of a first column foot of the core. Three other columns 16, 18, 20 correspond to adjacent cavities which receive a second flow of cooling air supplied by another pipe resulting from the presence of a second column foot of the core. Finally, the core further comprises sixth and seventh lateral columns 22, 24 corresponding to lateral cavities created after casting and separated one and the other of the second and third columns 14, 16 by a determined spacing necessary for the creation of a solid inter-cavity wall during casting of the molten metal.
The first and second columns 12 and 14 are connected to each other by a series of bridges 26, to which will correspond, after casting, air supply ports for cooling the leading edge cavity. Regarding the fourth column 18, other bridges 28 vertically inclined forming core thinned regions can create stiffened blade regions. The size of the various bridges is determined to prevent them from breaking when handling the core 10, which would render it unusable. The bridges are, in the example considered, distributed spaced substantially regularly over the height of the core, particularly at the first column of the core.
According to the invention, the dedusting holes of the turbine blades necessary for the evacuation of dust (in particular fine sand) which can accumulate in the cooling circuits, are obtained by a geometric arrangement of a part of core, directly raw foundry, without drilling and without the use of connecting rods that they are holes in the side cavities of the core than those ensuring the connection with the bathtub. If the nucleus thus formed stands out from the existing cores, the lost wax manufacturing process of the blade once this nucleus is made is first and foremost consists in forming an injection mold in which the core is placed before injection wax. The wax model thus created is then dipped in slips consisting of ceramic suspension to make a casting mold (also called shell mold). Finally, the wax is removed and the shell mold is baked into which the molten metal can then be cast. Final machining (however simplified compared with those of the prior art) described above will then allow to get the finished dawn.
According to the invention and as illustrated in Figure 2, it is provided to locally develop, at the core portion 22A, the geometry of the side columns 22, 24 (portions of the ceramic core generating the lateral cavities) of so as to form on the one hand a core cylinder 30 of a determined diameter (calibrated on the order of 0.5mm to 0.8mm) corresponding to the dedusting hole to be made, and in addition of the smallest possible height to guaranteeing the mechanical strength of the plate and secondly a core volume 33 corresponding to the remaining space of the core and intended to be plugged after casting. This geometry can be obtained conventionally by integrating a stirrup-type disturbance into the mold of the plate (at a through-orifice of longitudinal axis delimiting in a direction perpendicular to this axis the cylinder 30 and the remaining volume 33) for the case of ceramic injection or without additional stress for the case of additive manufacturing or machining of cores.
When the dimensioning of the turbine blade imposes it and taking into account the fragile appearance of the ceramic, it is necessary to guarantee the mechanical strength of the core being careful not to mechanically weaken the plates obtained after casting, for example by stiffening by adding one or more stiffeners thus preventing the plates from breaking at these locations. It should be noted that such lateral stiffeners (illustrated by the reference 39 in FIG. 2B) have a very small impact on the injection (the overall section does not vary too much, the part lost with the drilling being compensated with the addition of the stiffener).
Similarly, the ceramic cores made by injection to be demolded, it must of course be ensured that these cores have sufficient remains relative to a technical release axis. Indeed, if this demolding axis is not well oriented, the plate can be greatly weakened. FIG. 2A illustrates the upper part of the dawn (bath) obtained at the end of the casting (foundry blank) with the two cavities 32, 34 corresponding to the two lateral columns and the excess material which surrounds them due to the assembly of these columns. In Figure 2B, there is the same bath after machining this excess material and it is found that with the invention, two holes 36A, 38A; 36B, 38B are formed at each cavity (instead of only one in the prior art). One of them 36A, 36B having the dimension of the core cylinder 30 will provide the dust removal function, the other hole 38A, 38B which has no particular function and the size of the remaining core volume 33, is intended to be plugged. Thus, with the invention, the operation of filling and drilling, the most delicate and with the least robustness in the embodiment of the prior art, is removed. The problem existing in the prior art of the uncertain depth of filling no longer impedes the good realization of the bath because it no longer has to be pierced.
The connection with the tub is illustrated in FIG. 3. As for the side plates, to obtain a dusting hole, a local geometrical arrangement of the connection is provided, forming on either side of the through-hole 41 on the one hand a core cylinder 40 of a determined diameter corresponding to the diameter of the dedusting hole to be made and, on the other hand, the remaining core volume 43 intended to be closed after casting. The core cylinder also has a smallest possible height to ensure the good behavior of the core and prevent the formation of cracks. As before, the through orifice may be formed by the use of a bridge-type interferer integrated in the foundry mold. However, the space available between the cavities and the bath being very small and intercavities link being thin (so with a small section), it is also planned to develop on a portion of the core at the level of the bathtub to create a recessed area to allow to obtain a space d more important. In addition, the through hole 41 for receiving the disruptor being found thereby centered on the inter-cavity connection, it also provides better strength during casting.
FIG. 3A illustrates the upper part of the dawn (bath) obtained at the end of the casting (foundry blank) with the extension 42 resulting from the removal of the core from the space d. In Figure 3B, there is the same bathtub after machining of this riser and it is found that with the invention, two holes 44, 46 are formed at the bath. Note the presence of two lateral stiffeners 48A, 48B, giving a quadrilobed shape to the second hole (corresponding to a section of the volume 43) and dimensioned to ensure the strength of the core. In the case of a ceramic injection, this also makes it possible to increase the section and to guarantee a better filling and in the cases of an additive manufacturing and a machining of cores, the stiffeners stiffen the connection and prevent the deformation of the elements. nuclei.
Of course, as stated above, in the case of ceramic injection, it is necessary that the core remains demoldable and thus the added bond must be also, and the hole in it.
With the invention, it is thus proposed a way to combine the functions of maintaining the core and development of dedusting holes (function usually provided by rods) suitable for any type of core manufacturing process and any type of geometry of this nucleus.
权利要求:
Claims (10)
[1" id="c-fr-0001]
Ceramic core used for the manufacture of a turbomachine hollow turbine blade according to the lost-wax foundry technique, said blade having calibrated dusting holes formed in an apex of at least one cavity and opening into a cavity. tub of said blade, characterized in that it comprises a through hole (41) of longitudinal axis defining, in a direction perpendicular to said longitudinal axis and on a core portion (22A) for forming a calibrated hole dust removal of a determined height sufficient to guarantee the mechanical strength of said core portion, on the one hand a core cylinder (30, 40) of a determined diameter corresponding to said dedusting hole to be formed and secondly a core volume remaining (33, 43) to be closed after casting, so that said calibrated hole dust removal is obtained without drilling and without the use of connecting rods.
[2" id="c-fr-0002]
2. Ceramic core according to claim 1, characterized in that said core portion forms a portion (22A) of a side column (22, 24) for creating a lateral cavity of said blade.
[3" id="c-fr-0003]
Ceramic core according to claim 1, characterized in that said core portion forms an inter-cavity connection zone between said at least one cavity and said bath.
[4" id="c-fr-0004]
4. Ceramic core according to claim 3, characterized in that it comprises, on a core portion corresponding to said bath to be created, a recessed area to allow a centering of said through hole in said connecting zone, so as to guarantee better holding of said core portion during casting.
[5" id="c-fr-0005]
Ceramic core according to claim 2 or claim 3, characterized in that said remaining core volume comprises at least one lateral stiffener (39; 48A, 48B) dimensioned so as to guarantee a better holding of said core portion during the casting.
[6" id="c-fr-0006]
6. Ceramic core according to claim 5, characterized in that said remaining core volume comprises two lateral stiffeners (48A, 48B) facing each other giving it a quadrilobed shape.
[7" id="c-fr-0007]
7. Use of a ceramic core according to any one of claims 1 to 6 for the manufacture of a turbomachine hollow turbine blade according to the lost-wax casting technique.
[8" id="c-fr-0008]
8. A turbomachine comprising a hollow turbine blade manufactured according to the technique of lost wax casting from a ceramic core according to any one of claims 1 to 6.
[9" id="c-fr-0009]
9. A method of forming calibrated dust removal holes in a turbomachine hollow turbine blade produced by the lost-wax casting technique by means of a ceramic core whose outer surface is intended to form the internal surface of the finished blade, characterized in that it comprises a step of forming a through hole (41) of longitudinal axis delimiting, in a direction perpendicular to said longitudinal axis and on a core portion (22A) intended to form a calibrated hole for dedusting a sufficiently determined height to guarantee the mechanical strength of said core portion, firstly a core cylinder (30, 40) of a determined diameter corresponding to said dusting hole to be formed and secondly a remaining core volume (33, 43) to be closed after casting, so that said calibrated dust removal hole is obtained without drilling and without the use of connecting rods.
[10" id="c-fr-0010]
10. The method of claim 9, characterized in that said through orifice is formed by the use of a stirrup-type disturbance.
类似技术:
公开号 | 公开日 | 专利标题
CA2576709C|2014-01-14|Manufacturing process for a turbine engine part that includes cooling air exhaust orifices
EP3414031A1|2018-12-19|Method for forming dust-removal holes for a turbine blade and associated ceramic core
FR2900850A1|2007-11-16|PROCESS FOR MANUFACTURING CERAMIC FOUNDRY CORES FOR TURBOMACHINE BLADES
JP6355839B2|2018-07-11|Die casting system with ceramic mold for forming components usable in gas turbine engines
EP3274559A1|2018-01-31|Ceramic core for a multi-cavity turbine blade
EP3164237B1|2019-10-02|Method for manufacturing a two-component blade for a gas turbine engine and blade obtained by such a method
EP0663249B1|1999-03-10|Method for the production of ceramic shell moulds for casting with a lost mould
CA2887335C|2020-08-18|Method for manufacturing at least one metal turbine engine part
FR3022811A1|2016-01-01|METHOD FOR MANUFACTURING CORE ASSEMBLY FOR MANUFACTURING A DAWN
EP2895285B1|2019-08-14|Foundry model
FR2997442A1|2014-05-02|Blade, useful in turboshaft engine, comprises blade body, blade head, pressure and suction side walls, where pressure side wall has concave curvature at head and suction side wall is straight at the hollow portion
WO2019202281A1|2019-10-24|Method for producing a metal bladed element for a turbomachine of an aircraft
FR2977510B1|2019-08-16|FOUNDRY CORE, METHOD FOR MANUFACTURING TURBINE BLADE UTILIZING SUCH CORE.
FR3023196A1|2016-01-08|IMPROVED MOLDING PROCESS FOR TURBOMACHINE HOLLOW DUST
EP3544754A1|2019-10-02|Cluster model and shell for obtaining an accessory for the independent handling of formed parts, and associated method
EP3402621B1|2020-12-16|Refractory core comprising a main body and a shell
EP3395469B1|2019-11-13|Assembly for manufacturing a turbine engine blade
CA2960059A1|2016-03-10|Method for producing a ceramic core
FR3076752A1|2019-07-19|METHOD FOR MAKING A MULTI-PALE MODEL, TOOLING AND ASSEMBLY OF A MULTI-PALE MODEL AND A HOLDING ELEMENT
FR3023197A1|2016-01-08|METHOD FOR MOLDING A CERAMIC BATH TANK
FR3080051A1|2019-10-18|CORE FOR FOUNDRY OF AERONAUTICAL PIECE
FR3085288A1|2020-03-06|METHOD FOR MANUFACTURING A METAL ASSEMBLY FOR A TURBOMACHINE BY LOST WAX FOUNDRY
WO2021001633A1|2021-01-07|Method for manufacturing a metal part
WO2021186124A1|2021-09-23|Method for chemical pickling of a cast metal part with porous ceramic core|
FR3094032A1|2020-09-25|AIRCRAFT TURBOMACHINE BLADE AND ITS MANUFACTURING PROCESS BY LOST WAX MOLDING
同族专利:
公开号 | 公开日
RU2745073C2|2021-03-18|
BR112018016416A2|2018-12-26|
US20190022743A1|2019-01-24|
CA3014022A1|2017-08-17|
US10537935B2|2020-01-21|
RU2018132349A|2020-03-12|
CN108698117A|2018-10-23|
CN108698117B|2020-08-21|
RU2018132349A3|2020-04-17|
EP3414031A1|2018-12-19|
FR3047767B1|2019-05-31|
WO2017137709A1|2017-08-17|
引用文献:
公开号 | 申请日 | 公开日 | 申请人 | 专利标题
US20100303625A1|2009-05-27|2010-12-02|Craig Miller Kuhne|Recovery tip turbine blade|
FR2961552A1|2010-06-21|2011-12-23|Snecma|IMPACT COOLED CAVITY TURBINE TURBINE BLADE|
FR2986982A1|2012-02-22|2013-08-23|Snecma|FOUNDRY CORE ASSEMBLY FOR MANUFACTURING A TURBOMACHINE BLADE, METHOD FOR MANUFACTURING A BLADE AND AUBE ASSOCIATED|
WO2015195110A1|2014-06-18|2015-12-23|Siemens Energy, Inc.|Turbine blade investment casting using film hole protrusions for integral wall thickness control|
RU2093304C1|1995-12-28|1997-10-20|Всероссийский научно-исследовательский институт авиационных материалов|Cooled turbine blade and method for its manufacture|
US6637500B2|2001-10-24|2003-10-28|United Technologies Corporation|Cores for use in precision investment casting|
FR2889088B1|2005-07-29|2008-08-22|Snecma|CORE FOR BLADE OF TURBOMACHINE|
FR2900850B1|2006-05-10|2009-02-06|Snecma Sa|PROCESS FOR MANUFACTURING CERAMIC FOUNDRY CORES FOR TURBOMACHINE BLADES|
FR2943092B1|2009-03-13|2011-04-15|Snecma|TURBINE DAWN WITH DUST-BASED CLEANING HOLE|
FR2990367B1|2012-05-11|2014-05-16|Snecma|TOOLING FOR MANUFACTURING A FOUNDRY CORE FOR A TURBOMACHINE BLADE|
FR3021697B1|2014-05-28|2021-09-17|Snecma|OPTIMIZED COOLING TURBINE BLADE|FR3079551B1|2018-03-29|2020-04-24|Safran Helicopter Engines|TURBINE DISTRIBUTOR BLADE HAVING AN INTERNAL COOLING WALL ARISING FROM ADDITIVE MANUFACTURING|
US11041395B2|2019-06-26|2021-06-22|Raytheon Technologies Corporation|Airfoils and core assemblies for gas turbine engines and methods of manufacture|
US11053803B2|2019-06-26|2021-07-06|Raytheon Technologies Corporation|Airfoils and core assemblies for gas turbine engines and methods of manufacture|
法律状态:
2017-01-09| PLFP| Fee payment|Year of fee payment: 2 |
2017-08-18| PLSC| Publication of the preliminary search report|Effective date: 20170818 |
2018-01-23| PLFP| Fee payment|Year of fee payment: 3 |
2020-01-22| PLFP| Fee payment|Year of fee payment: 5 |
2021-01-20| PLFP| Fee payment|Year of fee payment: 6 |
2022-01-19| PLFP| Fee payment|Year of fee payment: 7 |
优先权:
申请号 | 申请日 | 专利标题
FR1651134A|FR3047767B1|2016-02-12|2016-02-12|METHOD FOR FORMING DEDUSTING HOLES FOR TURBINE BLADE AND CERAMIC CORE THEREFOR|
FR1651134|2016-02-12|FR1651134A| FR3047767B1|2016-02-12|2016-02-12|METHOD FOR FORMING DEDUSTING HOLES FOR TURBINE BLADE AND CERAMIC CORE THEREFOR|
BR112018016416-0A| BR112018016416A2|2016-02-12|2017-02-10|ceramic core, use of a ceramic core, turbine motor, and method for forming calibrated dust removal holes.|
US16/077,171| US10537935B2|2016-02-12|2017-02-10|Method of forming dust-removal holes for a turbine blade, and an associated ceramic core|
PCT/FR2017/050310| WO2017137709A1|2016-02-12|2017-02-10|Method for forming dust-removal holes for a turbine blade and associated ceramic core|
CN201780011177.3A| CN108698117B|2016-02-12|2017-02-10|Method for forming dust removal holes of turbine blades and related ceramic core|
CA3014022A| CA3014022A1|2016-02-12|2017-02-10|Method for forming dust-removal holes for a turbine blade and associated ceramic core|
RU2018132349A| RU2745073C2|2016-02-12|2017-02-10|Method for the formation of dust removing holes for the turbine blade and the coupled ceramic core|
EP17709141.0A| EP3414031A1|2016-02-12|2017-02-10|Method for forming dust-removal holes for a turbine blade and associated ceramic core|
[返回顶部]