![]() PROCESS FOR THE METATHESIS OF OLEFINS USING A CATALYST CONTAINING SILICON AND MOLYBDENE
专利摘要:
The invention relates to a method for metathesis of olefins implemented with a catalyst comprising a mesoporous matrix and at least the molybdenum and silicon elements, said elements being incorporated in said matrix by means of at least one precursor comprising molybdenum and silicon and having at least one sequence of Si-O-Mo bonds. 公开号:FR3039546A1 申请号:FR1557370 申请日:2015-07-31 公开日:2017-02-03 发明作者:Audrey Bonduelle;Alexandra Chaumonnot;Damien Delcroix;Christophe Vallee;Souad Rafik-Clement;Severine Forget 申请人:IFP Energies Nouvelles IFPEN; IPC主号:
专利说明:
The present invention relates to a process for metathesis of olefins using a catalyst prepared from a precursor comprising molybdenum and silicon and having at least one sequence of Si-O-Mo bonds. Prior art The metathesis of olefins is an important reaction in various fields of chemistry. In organic synthesis, this reaction, catalyzed by organometallic complexes, is used to obtain various molecules with high added value. In petrochemicals, the metathesis of olefins is of great practical interest, particularly for the rebalancing of light olefins from steam cracking, such as ethylene, propylene and butenes. In particular, the cross metathesis of ethylene with butene-2 to give propylene is a reaction of interest given the increasing demand for propylene on the market. Different types of catalysts are likely to be used in the metathesis reaction. It is possible to use homogeneous catalysts, the constituent elements of which are all soluble in the reaction medium, or else heterogeneous catalysts insoluble in the reaction medium. The metathesis of light olefins uses heterogeneous catalysts. A known solution is the technology described in US Pat. No. 8,586,813, 2013, which uses a catalyst based on tungsten oxide deposited on a silicic support W03 / SiO2. However, heterogeneous tungsten catalysts operate at a relatively high temperature, generally at a temperature above 300 ° C and are only moderately active It is moreover known that rhenium oxide-based metathesis catalysts Re207 such as those described in the publication by Chauvin et al. Journal of Molecular Catalysis 1991, 65, 39 show good activity at temperatures near ambient temperature. Other catalysts based on molybdenum oxide such as those described in DP Debecker et al., J. Catal., 2011, 277, 2, 154 and GB 1,164,687 and GB 1,117,968 by Shell company were also developed. The Shell process uses, for example, catalysts based on molybdenum oxides and cobalt deposited on an aluminomeric support C0M0O4 / Al2O3 and doped with phosphorus, as described in US Pat. No. 4,754,099. An interest of molybdenum (Mo) is that it is cheaper than Rhenium (Re). In addition, its stability and activity are intermediate between those of Rhenium (Re) and tungsten (W). In particular, molybdenum can be active from room temperature. The preparation of catalysts based on molybdenum oxides (M0O3) is conventionally carried out by impregnation with an aqueous solution of a molybdenum salt or a heteropolyanion containing molybdenum such as, for example, isopolyanion ammonium heptamolybdate on a support such as silica, alumina or a porous aluminosilicate. Catalysts prepared from ammonium heptamolybdate precursors, however, lack activity and stability. Catalysts based on other heteropolyanions, such as H3PM012O40, have been prepared and can significantly increase the activity, but still need to be improved. There is therefore still a need to develop new catalysts with improved performances in terms of activity and selectivity for the metathesis reaction of olefins and more particularly for the metathesis between ethylene and butene-2 for the production of propylene . The applicant, in his research to improve the performance of heterogeneous olefin metathesis catalysts, has developed novel catalysts for the metathesis reaction of olefins. These catalysts are prepared from a mesoporous matrix and at least one precursor comprising molybdenum and silicon and having at least one sequence of Si-O-Mo bonds. It has been unexpectedly found that the use of this type of precursors for the preparation of the catalyst according to the invention improves the activity and the stability of the heterogeneous catalyst obtained for the metathesis reaction of olefins, compared to catalysts prepared by means of other precursors of the prior art which do not have a sequence of Si-O-Mo bonds. The conversion of olefins is improved. The stability of the catalyst is also improved. An object of the present invention is to provide a process for metathesis of olefins using a catalyst having improved performance in terms of activity and selectivity with respect to the use of heterogeneous catalysts of the prior art. The catalysts according to the invention have the advantage of being able to operate on longer cycle times before regeneration, which has a strong economic impact on the operating costs of the process according to the invention. Object of the invention The present invention relates to an olefin metathesis process carried out by bringing olefins into contact with a catalyst comprising a mesoporous matrix and at least the molybdenum and silicon elements, said elements being incorporated into said matrix by means of at least one precursor comprising molybdenum and silicon and having at least one sequence of Si-O-Mo bonds. Advantageously, the precursor according to the present invention is a molybdenum coordination complex containing a siloxy ligand and comprising at least one sequence of Si-O-Mo bonds and / or a molybdenum-based heteropolyanion precursor comprising at least one sequence of Si-O-Mo bonds. When the precursor according to the present invention is a molybdenum coordination complex containing a siloxy ligand, it advantageously corresponds to formula (I) Mom (= Y) n (EN) n (X) z (= CR2) r (OSiR3) p (I) in which - the groups Y, which are identical to or different from one another, can be chosen from O, S and NR ' the X groups, which are identical to or different from one another, may be chosen from halides, such as F, Cl, Br, I, substituted or unsubstituted alkyl, cycloalkyl or aryl groups, substituted or unsubstituted cyclopentadienyls, and alkoxy groups, aryloxy, amide, hydrido, carboxylate, acetylacetonate, sulfonate, β-diketiminate, iminopyrrolide, amidinate, thiocyanate or NR2-CS2 ', the groups R, which are identical to or different from one another, may be chosen from alkyl, cycloalkyl and aryl groups, substituted or unsubstituted, preferably comprising between 1 and 10 carbon atoms, or from substituted and unsubstituted alkoxy and aryloxy groups, the groups R ', which are identical to or different from one another, may be chosen from alkyl, cycloalkyl and aryl groups; , substituted or not, - m is gal to 1 or 2, - n is 0 to 4, - n 'is 0 to 2, - z is 0 to 9, - r is 0 to 2, - p is 1 to 10. Advantageously, when the precursor according to the invention is a molybdenum coordination complex precursor containing a siloxy ligand, it corresponds to formula (la): Mom (EN) n '(OSiR 3) P (la) in which - the groups R, which are identical to or different from one another, may be chosen from alkyl groups, cycloalkyls and aryls, which may or may not be substituted, preferably comprising from 1 to 10 atoms of carbons, or from substituted and unsubstituted alkoxy and aryloxy groups, m is 1 or 2, n is between 0 and 2, p is from 1 to 10. Advantageously, when the precursor according to the invention is a molybdenum coordination complex precursor containing a siloxy ligand, it corresponds to the formula (Ib) in which the groups R, which are identical to or different from one another, may be chosen from substituted or unsubstituted alkyl, cycloalkyl and aryl groups, preferably comprising between 1 and 10 carbon atoms, or from substituted and unsubstituted alkoxy and aryloxy groups, m is 1 or 2, n is 0 to 4, p is 1 to 10. According to the invention, the molybdenum coordination complex precursor containing a siloxy ligand may also contain in its coordination sphere one or more L-type ligands, optionally polydentate. The ligand of type L can be chosen from phosphorus compounds such as phosphines, phosphinites, phosphonites, phosphites, oxygenated compounds such as ethers, nitrogen compounds such as amines, aromatic nitrogen compounds such as pyridine and / or phenanthroline, and / or sulfur compounds such as thioethers. The molybdenum coordination complex precursor containing a siloxy ligand may, for example, be chosen from the following compounds: MoO (OSiMe3) CN (CS2-NEt2) 2, Mo (= N- (2,6-di- / PrC6H3) ) (/ Bu) (= CH / Bu) (OSi (0 / Bu) 3), Mo (= S) (= N / Pr) (OSitBu3) 2, Mo (= 0) (OSitBu3) 4, Mo ^ N ) (OSiPh3) 3 (C6H5N) or Mo ^ OSiMe ^ g. When the precursor according to the present invention is a molybdenum-based heteropolyanion precursor, it advantageously corresponds to formula (II) in which: • x is at least 1, • m is greater than or equal to 1, • b is greater than or equal to 0, • m + b is greater than or equal to 5, • y is greater than or equal to 20, • h is 0 to 12, q is 1 to 20, n is 0 to 200, x, m, b, y, h, n and q are integers, M being a metallic element. other than silicon and molybdenum. Advantageously, when the precursor according to the invention is a heteropolyanion precursor, it corresponds to formula (II): in which, • x is 1 or 2, • m is greater than or equal to 1, • b is greater than or equal to 0, • m + b is greater than or equal to 5, • y is between 20 and 50, • h is between 0 and 12, • q is between 3 and 12, • n is 0 to 200; X, m, b, y, h, n and q being integers, M being a metal element selected from aluminum, zinc, nickel, cobalt, tungsten, vanadium, niobium, tantalum , iron and copper, preferably M is a metal element selected from aluminum, cobalt and tungsten, more preferred among aluminum and cobalt and even more preferably, the metal element M is cobalt. The molybdenum-based heteropolyanion precursor of formula (II) can be incorporated into the mesoporous matrix in the form of salts or in the form of acid. In the case where the heteropolyanion precursor is incorporated in acid form, the charge q 'is compensated by H + protons. When the heteropolyanion is introduced in salt form, the counterions of the heteropolyanion salt are chosen from all the cations known to those skilled in the art. Examples that may be mentioned include proton, ammoniums, phosphoniums, alkalis, alkaline earths, transition elements, and the like. The salt may comprise a mixture of the same cation or different cations. The molybdenum coordination complex precursor containing a siloxy ligand of formula (I), (la), or (Ib), is incorporated by its chemical nature in neutral form. One or more molybdenum heteropolyanion precursors of the formula (II) can be used. One or more molybdenum coordination complex precursors containing a siloxy ligand of formula (I), (Ia), or (Ib) may be used. The molybdenum-based heteropolyanion precursor may contain one or more metal elements M chosen from aluminum, zinc, nickel, cobalt, tungsten, vanadium, niobium, tantalum, iron and copper, in substitution for one or more molybdenum atoms contained in said heteropolyanion precursor of formulas described above. Preferably, the metal element M is chosen from aluminum, cobalt and tungsten, more preferably from aluminum and cobalt and even more preferably, the metal element M is cobalt. When the molybdenum-based heteropolyanion precursor used in the preparation of the catalyst used in the metathesis process according to the invention does not contain a metal element M, it is advantageously chosen from the group formed by a Strandberg heteropolyanion of Si2Mo5C formula> 238 nH20, an Anderson heteropolyanion of formula SiMo60248 ', nH20, a Keggin heteropolyanion of formula S1M012O404-, nH20, a lacunar Keggin heteropolyanion of formula SiMon0398 nH20, a lacunar Keggin heteropolyanion of formula SiMogO ^ 10 ', nH20, a Dawson heteropolyanion of the formula Si2Moi80628', nH20, a Preysler heteropolyanion of the formula Si5Mo3oOno20 nH20. When the molybdenum-based heteropolyanion precursor used in the preparation of the catalyst used in the metathesis process according to the invention contains a metal element M other than molybdenum and silicon, preferably M being cobalt, it is advantageously selected from the group consisting of a Strandberg heteropolyanion of formula Si2Mo4CoO2312 ', nH20, an Anderson heteropolyanion of formula SiMosCoCW2', nH20, a Keggin heteropolyanion of formula SiMonCoO4O8-, nH20, a lacunar Keggin heteropolyanion of formula SiMo-ioCoO3g12 n, H 2 O, a lacunated Keggin heteropolyanion of the formula SiMo 8 CoO 3 O 4, nH 2 O, a Dawson heteropolyanion of the formula Si 2 Mo-17CoO 2 O 12 H 2 O, a Preysler heteropolyanion of the formula SisMo 2 CoO 2 O 4, nH 2 O (the preparation of which is specifically described in application FR 2.764.211). The mesoporous matrix according to the invention is advantageously an oxide-based matrix of at least one element X chosen from silicon, aluminum, titanium, zirconium, magnesium, lanthanum, cerium and their mixtures. Preferably, the element X is aluminum or a mixture of aluminum and silicon. Even more preferably, the element X is aluminum. Said so-called mesoporous oxide-based matrix is understood according to the present invention as a matrix comprising pores ranging in size from 2 to 50 nm according to the IUPAC classification (KSW Sing, DH Everett, WRA Haul, L. Moscow, J. Pierotti, J. Rouquerol, T. Siemieniewska, Pure Appl Chem 1985, 57, 603), and / or a mesoporous mesostructured matrix, that is to say having mesopores of uniform size and distributed over periodically in said matrix and / or a matrix with hierarchical porosity, that is to say comprising micropores and / or macropores additional to the mesopores. Preferably, a mesoporous matrix based on aluminum oxide having a specific surface area of 10 to 500 m 2 / g, and preferably of at least 50 m 2 / g, and a pore volume of at least 0, are used. 1 ml / g, and preferably a pore volume of between 0.3 and 1.2 ml / g according to the BET method. The catalyst used according to the invention comprises a mass content of molybdenum element provided by the precursor of formula (I), (Ia), or (Ib) and / or of formula (II) according to the invention of between 1 and 40% preferably between 2 and 30%, preferably between 2 and 20%, expressed as a percentage by weight of molybdenum with respect to the mass of the mesoporous matrix. The catalyst used according to the invention comprises a mass content of silicon element provided by the precursor of formula (I), (Ia), or (Ib), and / or of formula (II) according to the invention between 0.01 and 50%, preferably between 0.02 and 35%, preferably between 0.02 and 25% expressed as a percentage by weight of silicon element relative to the mass of the mesoporous matrix. Preferably, when the precursor is a molybdenum coordination complex containing a siloxy ligand according to the invention, the mass content of silicon element provided by the precursor according to the invention is between 1 and 25% expressed as a percentage by weight of silicon element with respect to the mass of the mesoporous matrix. Preferably, when the precursor is a heteropolyanion based on molybdenum according to the invention, the mass content of silicon element provided by the precursor according to the invention is between 0.02 and 10% expressed as a percentage by weight of silicon element relative to the mass of the mesoporous matrix. Preferably, when the precursor is a mixture of precursors, the mass content of silicon element provided by the precursor according to the invention corresponds to the sum of the silicon element mass contents provided by each of the precursors. The catalyst according to the invention can be prepared according to methods known to those skilled in the art. In a variant of the process for preparing the catalyst used according to the invention, the precursor comprising molybdenum and silicon is deposited and exhibiting at least one sequence of Si-O-Mo bonds on the surface of a mesoporous matrix based on preformed oxide. The preformed mesoporous matrix may be commercial or well synthesized according to the methods known to those skilled in the art, in particular by using the "traditional" inorganic synthesis methods: precipitation / gelling from salts under mild conditions of temperature and humidity. pressure; or "modern" metallo-organic: precipitation / gelling from alkoxides under mild conditions of temperature and pressure. In the rest of the text and for the sake of simplification, these methods are simply called "sol-gel". The preformed mesoporous matrix may be in powder form or shaped, for example in the form of pelletized, crushed, sieved powder, granules, tablets, balls, wheels, spheres or extrusions (hollow cylinders or no, multilobed cylinders with 2, 3, 4 or 5 lobes for example, twisted cylinders), or rings, etc. The deposition or incorporation of the precursor comprising molybdenum and silicon and having at least one sequence of Si-O-Mo bonds on the mesoporous matrix can be done before, during or after forming the mesoporous matrix. The deposition or the incorporation of the precursor according to the invention on the mesoporous matrix can be done by the so-called methods of dry impregnation, excess impregnation, CVD (Chemical vapor deposition according to the English terminology), CLD ( Chemical liquid deposition according to the English terminology), etc. described for example in "Catalysis by transition metal sulphides, from molecular theory to industrial application, Ed Herve Toulhouat and Pascal Raybaud, p137" can be used. The catalyst may be prepared by dry impregnation according to the process comprising the following steps: a) solubilization of the precursor comprising molybdenum and silicon and having at least one sequence of Si-O-Mo bonds of formula (I), ), or (Ib), and / or of formula (II) in a volume of solution corresponding to the pore volume of a mesoporous matrix based on preformed oxide, b) impregnation of the preformed oxide-based mesoporous matrix with the solution obtained in step a), optional maturation of the solid thus obtained, c) optional step of drying, calcination and / or steam treatment of the solid obtained at the end of step b), at a pressure greater than or equal to 0.1 MPa or less than or equal to 0.1 MPa, in a temperature range from 50 ° C. to 1000 ° C., d) step of thermal activation of the solid obtained at the end of the step c) at a pressure greater than or equal to 0.1 MPa or less less than or equal to 0.1 MPa, in a temperature range of 100 ° C to 1000 ° C. The maturation optionally used in step b) is carried out in a controlled atmosphere and temperature so as to promote the dispersion of said precursor over the entire surface of the preformed oxide-based mesoporous matrix. Advantageously, the maturation is carried out at a temperature between 20 and 120 ° C and a pressure between 0P1 and 1 MPa. Steps c) and / or d) can be carried out under an oxidizing, reducing or neutral atmosphere. Preferably, the optional c) drying step is carried out in a temperature range of from 20 ° C to 200 ° C, preferably from 50 ° C to 150 ° C and preferably from 100 ° C to 130 ° C. during a period of less than 72 hours and preferably less than 24 hours. Preferably, the thermal activation step d) is carried out under a neutral atmosphere at atmospheric pressure in a temperature range from 200 ° C. to 800 ° C., preferably from 350 ° C. to 650 ° C. Preferably, the neutral atmosphere is nitrogen in a flow rate range from 0.01 to 20 Nl / h per gram of solid obtained after step c), preferably from 0.1 to 10 Nl / h per gram of solid obtained at the end of step (c). The catalyst may be prepared by excess impregnation, according to the process comprising the following steps: a ') solubilizing the precursor comprising molybdenum and silicon and having at least one Si-O-Mo linkage of formula (I), (la), or (Ib), and / or of formula (II) in a volume of solution corresponding to between 1.5 and 20 times the pore volume of the preformed oxide-based mesoporous matrix, b ') impregnation of the mesoporous matrix based on preformed oxide, with the solution obtained in step a '), filtration and recovery of the solid, optional maturation of the solid thus obtained, c') optional step of drying, calcination and / or treatment at the vapor of the solid obtained after step b ') at a pressure greater than or equal to 0.1 MPa or less than or equal to 0.1 MPa, in a temperature range from 50 ° C to 1000 ° C, d) thermal activation step of the solid obtained at after step c ') at a pressure greater or equal to 0.1 MPa or less than or equal to 0.1 MPa, in a temperature range from 100 ° C to 1000 ° C. The maturation optionally used in step b ') is carried out in a controlled atmosphere and temperature so as to promote the dispersion of said precursor over the entire surface of the preformed oxide-based mesoporous matrix. Advantageously, the maturation is carried out at a temperature between 20 and 120 ° C and a pressure between 0P1 and 1 MPa. Preferably, the solubilization of the precursor comprising molybdenum and silicon and having at least one sequence of Si-O-Mo bonds, of formula (I), (Ia), or (Ib), and / or of formula (II) in step a) is carried out in a volume of solution corresponding to between 2 and 10 times the pore volume of the preformed oxide-based mesoporous matrix. The steps c ') and / or d') can be carried out under an oxidizing, reducing or neutral atmosphere. Preferably, the optional drying step c ') is carried out in a temperature range from 20 ° C to 200 ° C, preferably from 50 ° C to 150 ° C and preferably from 100 ° C to 130 ° C during a period of less than 72 hours and preferably less than 24 hours. Preferably, the thermal activation step is carried out under a neutral atmosphere at atmospheric pressure in a temperature range of from 200 ° C to 800 ° C, preferably from 350 ° C to 650 ° C. Preferably, the neutral atmosphere is nitrogen in a flow rate range from 0.01 to 10 Nl / h per gram of solid obtained after step c '), preferably from 0.1 to 5 Nl / h per gram of solid obtained at the end of step c '). Organic compounds, called organic additives, can also be used in the preparation of the catalyst. At least one organic additive may be introduced by impregnation onto the mesoporous matrix before the step of impregnating the precursor (step b or b '), by co-impregnation with the precursor or by post-impregnation impregnation of the precursor. The organic compounds or additives used are chosen from chelating agents, non-chelating agents, reducing agents and additives known to those skilled in the art. Said organic compounds or additives are advantageously chosen from optionally etherified mono-, di- or polyalcohols, carboxylic acids (citric acid, acetic acid, etc.), sugars, non-cyclic mono, di or polysaccharides, such as glucose, fructose, maltose, lactose or sucrose, cyclic or non-cyclic esters, cyclic or non-cyclic ethers, ketones, compounds combining several of these functions (ketones, carboxylic acids, ethers, esters, alcohols, amines, etc.). ), crown ethers, cyclodextrins and compounds containing at least sulfur, or phosphorus or nitrogen such as nitriloacetic acid, ethylenediaminetetraacetic acid, or diethylenetriamine, amino acids and zwitterionic compounds, taken alone or in mixture. The impregnating and / or solubilizing solvent may be chosen from any solvent known to those skilled in the art such as water, organic solvents, ionic liquids, etc. A solvent mixture may also be used. When the precursor is a molybdenum-based heteropolyanion according to the invention, use is preferably made of water or a protic polar solvent such as alcohols: ethanol, methanol, etc. When the precursor is a molybdenum coordination complex containing a siloxy ligand, an aprotic organic solvent is preferably used, such as hydrocarbons: pentane, heptane, cyclohexane, aromatics: toluene, xylene, etc. ethers: diethyl ether, tetrahydrofuran (THF) ... When a molybdenum-based heteropolyanion precursor and a siloxy ligand-containing molybdenum coordination complex are used together, a polar aprotic organic solvent, such as dimethylsulfoxide (DMSO), dimethylformamide (DMF) or acetonitrile. One or more other metallic elements can also be used in the composition of the catalyst used in the process according to the invention. This metal element may be selected from zinc, nickel, cobalt, tungsten, vanadium, niobium, tantalum, iron and copper. This metal element is introduced at a content of between 0.01 and 10%, and preferably between 0.02 and 5% expressed in% by weight of metal relative to the mass of the mesoporous matrix based on oxide. This metal element may be provided by a compound chosen from salts and / or oxides of zinc, nickel, cobalt, tungsten, vanadium, niobium, tantalum, iron and copper, preferably salts and / or oxides of zinc, nickel, cobalt, tungsten. Preferably, the compound is a salt, a carboxylate, an alkoxide or a cobalt oxide. Preferably, the compound is Co (NO 3) 2 or CoO. Very preferably, the compound is Co (N03) 2 · This compound can be introduced by impregnation onto the mesoporous matrix before impregnation of the precursor (s) according to the invention comprising molybdenum and silicon and having at least one Si-O-Mo linkage of formula ( I), (la), or (Ib), and / or of formula (II) in co-impregnation with (said) precursor (s) according to the invention or in post-impregnation after impregnation (of) of said precursor ( s) according to the invention. Depositing or incorporating the precursor (s) comprising molybdenum and silicon and having at least one sequence of Si-O-Mo bonds of formula (I), (Ia), or (Ib), and or of formula (II) on the mesoporous matrix can also be done directly during the synthesis of the mesoporous matrix based on oxide. The synthetic methods used may be hydrolytic or non-hydrolytic "sol-gel" methods by precipitation or evaporation. Evaporative methods may require the use of specific synthetic processes such as atomization (also called spray-drying according to the English terminology), the deposition of thin films, etc. In the particular case of a spray-dried hydrolytic sol-gel synthesis leading to the production of a catalyst having a mesostructured oxide-based matrix, the catalyst used in the process according to the invention can be prepared according to the process comprising the following steps: a1) solubilizing the precursor comprising molybdenum and silicon and having at least one sequence of Si-O-Mo bonds of formula (I), (la), or (Ib), and / or of formula ( II) and precursors of the mesoporous matrix based on the oxide of at least one element X in an aqueous or hydro-organic solution in the presence of a pore-forming agent so as to form a colloidal solution, b1) atomizing said solution colloidal composition so as to obtain spherical solid elementary particles incorporating the oxide-based mesostructured matrix and the precursor comprising molybdenum and silicon and having at least one sequence of Si-O-Mo bonds, of formula (I), (la), or (Ib), and / or of formula (II), c1) optional step of drying, calcining and / or steam treatment of solid particles obtained at the end of step b1) at a pressure greater than or equal to 0.1 MPa or less than or equal to 0.1 MPa, d1) step of thermal activation of the solid particles dried at the end of step c1), at a pressure greater than or equal to 1 bar or less than or equal to 0.1 MPa, in a temperature range of 100 to 1000 ° C. Preferably, the optional drying step c1) is carried out in a temperature range from 20 to 200 ° C, preferably from 50 ° C to 150 ° C and preferably from 100 ° C to 130 ° C for a shorter period. at 72 hours and preferably less than 24 hours. Step c1) may be carried out under an oxidizing, reducing or neutral atmosphere. The thermal activation step d1) can be carried out under an oxidizing, reducing or neutral atmosphere. Preferably, the thermal activation step d1) is carried out under a neutral atmosphere at atmospheric pressure in a temperature range from 200 to 800 ° and preferably from 350 to 650 ° C. Preferably, the neutral atmosphere is nitrogen in a flow rate range of 0.01 to 10 Nl / h per gram of solid obtained at the end of step c1), preferably from 0.1 to 5 Nl / h per gram of solid obtained at the end of step c1). By hydro-organic solution is meant a solution of mixing between water and an organic solvent. Preferably the hydro-organic solution is a hydro-ethanolic solution. The blowing agent used in step a1) is, for example, an ionic or nonionic surfactant compound or a mixture of both. The precursor (s) of the mesoporous matrix are the precursors of the oxide matrix of at least one element X selected from silicon, aluminum, titanium, zirconium and mixtures thereof. This precursor (s) may be any compound comprising the element X and capable of releasing this element in solution in reactive form. Thus, the precursor (s) of at least said element X of the matrix is (are) advantageously an inorganic salt of said element X of formula XZn, (n = 3 or 4), Z being a halogen, the group NO 3 or perchlorate, preferably Z is chlorine. The precursor (s) of at least one of said X element (s) may also be a precursor (s) alkoxide (s) of formula X (OR) n where R = ethyl, isopropyl, n-butyl, s-butyl, t-butyl, etc. or a chelated precursor such as X (C5H802) n, with n = 3 or 4. The precursor (s) of at least one of said X element (s) considered may still be an oxide (s) (s) or a hydroxide (s) of said element X. In the preferred case where X is aluminum or a mixture of aluminum and silicon, the silicic and / or aluminic precursors are precursors of inorganic oxides well known to those skilled in the art. The silicic precursor is obtained from any source of silica and advantageously a sodium silicate precursor of formula Na 2 SiO 3, a chlorinated precursor of formula SiCl 4, an alkoxide precursor of formula Si (OR) 4 where R = H methyl, ethyl, or a chloroalkoxide precursor of formula Si (OR) 4-aCla wherein R = H, methyl, ethyl, a being between 0 and 4. The silicic precursor may also advantageously be an alkoxide precursor of formula Si ( OR) 4-aR'a wherein R = H, methyl, ethyl and R 'is an alkyl chain or a functionalized alkyl chain, for example by a thiol, amino, β-diketone or sulfonic acid group, a being between 0 and 4. A preferred silicic precursor is tetraethylorthosilicate (TEOS). The aluminum precursor is advantageously an inorganic aluminum salt of formula AIZ3, Z being a halogen or the NO 3 group. Preferably, Z is chlorine. The aluminum precursor may also be an inorganic aluminum salt of formula AI 2 Z '3, Z' being the sulfate group SO 4. The aluminum precursor may also be an alkoxide precursor of formula AI (OR ") 3 or R" = ethyl, isopropyl, n-butyl, s-butyl or t-butyl or a chelated precursor such as aluminum acetylacetonate (Al (CH702 ) 3). The aluminum precursor may also be an aluminum oxide or hydroxide, for example AlOONa. In the case where the catalyst used in the process according to the invention is obtained in powder form at the end of the various preparation processes described above, the latter can be shaped according to the methods well known to humans. of career. Thus, it may be in the form of pelletized, crushed, sieved powder, granules, tablets, balls, wheels, spheres or extrudates (hollow or non-hollow cylinders, multilobed cylinders with 2, 3, 4 or 5 lobes for example, twisted rolls), or rings, etc. Preferably, said catalyst is in the form of extrudates. During said shaping operation, the catalyst used in the process according to the invention may optionally be mixed with at least one porous oxide material having the role of binder so as to generate the physical properties of the catalyst which are suitable for the process according to the invention. invention (mechanical strength, attrition resistance, etc.). Said porous oxide material is preferably a porous oxide material chosen from the group formed by alumina, silica, silica-alumina, magnesia, clays, titanium oxide, zirconium oxide, lanthanum, cerium oxide, aluminum phosphates and a mixture of at least two of the oxides mentioned above. Said porous oxide material may also be chosen from mixtures of alumina-boron oxide, alumina-titanium oxide, alumina-zirconia and titanium-zirconia oxide. Aluminates, for example aluminates of magnesium, calcium, barium, manganese, iron, cobalt, nickel, copper and zinc, as well as mixed aluminates, for example those containing at least two of the metals mentioned above, are advantageously used as porous oxide material. It is also possible to use titanates, for example titanates of zinc, nickel or cobalt. It is also advantageous to use mixtures of alumina and silica and mixtures of alumina with other compounds such as group VIB elements, phosphorus, fluorine or boron. It is still possible to use simple, synthetic or natural clays of 2: 1 dioctahedral phyllosilicate or 3: 1 trioctahedral phyllosilicate such as kaolinite, antigorite, chrysotile, montmorillonite, beidellite, vermiculite, talc. , hectorite, saponite, laponite. These clays can be optionally delaminated. It is also advantageous to use mixtures of alumina and clay and mixtures of silica-alumina and clay. The various mixtures using at least two of the compounds mentioned above are also suitable for acting as binder. Optionally, at least one organic adjuvant is also mixed during said shaping step. The presence of said organic adjuvant facilitates extrusion shaping. Said organic adjuvant may advantageously be chosen from polyvinylpyrrolidones, cellulosic polymers and their derivatives, preferably chosen from cellulose ethers such as, for example, Methocel, marketed by Dow Chemical, polyvinyl alcohols, polyethylene glycols, polyacrylamides. polysaccharides, natural polymers and their derivatives, such as, for example, alginates, polyesters, aromatic polyamides and polyamides, polyethers, poly (aryl ethers), polyurethanes, polysulfones such as polyether sulfonates, heterocyclic polymers, preferably chosen from polyimides, polyether imides, polyesters imides, polyamide imides, and polybenzimidazole. The proportion of said organic adjuvant is advantageously between 0 and 20% by weight, preferably between 0 and 10% by weight and preferably between 0 and 7% by weight, relative to the total mass of the mesoporous shaped matrix. . Metathesis reaction The olefin metathesis process carried out by contacting the olefins with the catalyst defined above is advantageously carried out at a temperature of between 0 and 500 ° C., preferably between 0 and 400 ° C., more preferably between At 20 and 350 ° C and more preferably at 30 to 350 ° C. The metathesis reaction of the olefins can be carried out in the gas phase or in the liquid phase. The reaction may be carried out batchwise, in a stirred reactor, or continuously, passing the olefinic reactant (s) through a fixed bed, moving bed, or fluidized bed of the catalyst. The pressure at which the process according to the invention is carried out is not critical. However, for liquid phase operation, it is advantageous to maintain a pressure at least equal to the vapor pressure of the reaction mixture at the reaction temperature. The reaction is preferably carried out in the absence of solvents. However, the reaction can be carried out in the presence of a solvent such as a hydrocarbon, or a halogenated, aliphatic, cyclanic or aromatic hydrocarbon. The olefins capable of reacting in metathesis in the process according to the invention may be linear olefins corresponding to the general formula R 1 R 2 C = CR 3 R 4, where R 1, R 2, R 3 and R 4, which are identical or different, are hydrogen or a hydrocarbyl radical of 1 to 20 carbon atoms, or olefins of cyclic structure, the ring having from 3 to 20 carbon atoms. It is possible either to react an olefin on itself or to react several olefins together in a mixture. The process according to the invention is in particular the cross-metathesis reaction of ethylene with butene-2 to give propylene, or the reverse conversion reaction of propylene to a mixture of ethylene and butene-2. Other olefins capable of reacting in metathesis are the linear or cyclic monoolefins or polyolefins carrying functional groups such as, for example, halogens or ester groups. The process can also carry out, in co-metathesis, a mixture of the preceding olefins. In the case of the propylene production by metathesis between ethylene and butene-2, butene-2 may preferably come from a dimerization reaction of ethylene in the presence of a homogeneous or heterogeneous catalyst known to the art. 'Man of the trade. For example, butene-2 can come from a dimerization of ethylene in the presence of a nickel complex of the NiCl 2 (PBu 3) 2 type producing a mixture of butene-1 and butene-2 by homogeneous catalysis. For example, butene-2 can come from a dimerization of ethylene in the presence of a nickel-based heterogeneous catalyst of N1SO4 / Al2O3 type producing a mixture of butene-1 and butene-2 by heterogeneous catalysis. In the case of propylene production by metathesis between ethylene and a mixture of butene-2 and butene-1, an isomerization catalyst of butene-1 to butene-2 is preferably used to maximize the yield of propylene . For example, an MgO or K20 type oxide catalyst can be used to isomerize butene-1 to butene-2. Ethylene can advantageously be obtained by dehydration of ethanol biosourced by any dehydration method known to those skilled in the art to allow the production of biobased propylene. EXAMPLES In the examples, the coordination complex precursor containing a siloxy ligand, tris (triphenylsilyloxy) molybdenum nitride stabilized with pyridine Mo (N) (OSiPh3) 3 (Pyridine) and heteropolyanionic precursors phosphomolybdic acid ΡΜθι2Ο403 ' .3Η + and silicomolybdic acid SiMoi204o4'.4H + are commercial. The cobaltosilicomolybdic acid heteropolyanion precursor SiCoMonO4o4'.4H + is synthesized according to a method described in the patent application FR 2.764.211. Example 1A (not in accordance with the invention): preparation of 6.7% Mo / Al 2 O 3 by dry impregnation of a solution of PMoi 2 O 4n 3 · 3H + .30H 2 O 1.5 g of PMoi 2 O 3 · 3 · 3H + · 30H 2 O are dissolved at 60 ° C. in 7.3 ml of distilled water. At complete dissolution, an alumina (Sbet = 198 m2 / g, Vp = 0.47 ml / g) is impregnated with this solution. The solid obtained is matured for 24 hours at 25 ° C. under air. The resulting solid is dried in an oven at 120 ° C. for 24 hours and then activated under nitrogen at 550 ° C. for 2 hours. Example 1B (in accordance with the invention): preparation of 6.7% Mo / Al 2 O 3 by dry impregnation of a solution of SiMo 3 O 4 · 4.4H + .28H 2 O 1.4 g of SiMol 2 O 4 · 4 · 4H + .28H 2 O are dissolved at 60 ° C. in 7, 3 ml distilled water. At complete dissolution, an alumina (Sbet = 198 m2 / g, Vp = 0.47 ml / g) is impregnated with this solution. The solid obtained is matured for 24 hours at 25 ° C. under air. The resulting solid is dried in an oven at 120 ° C. for 24 hours and then activated under nitrogen at 550 ° C. for 2 hours. Example 1C (in accordance with the invention): preparation of 6.1% Mo + 0.3% Co / Al 2 O 3 by dry impregnation of a solution of SiCoM0: n04n4 ~ .4H + .28HpO 1.4 g of SiCoMon04o4'.4H + .28H20 are dissolved at 60 ° C in 7.3 ml of distilled water. An alumina (Sbet = 198 m2 / g, Vp = 0.47 ml / g) is impregnated with this solution. The solid obtained is matured for 24 hours at 25 ° C. under reflux. The resulting solid is oven-dried at 120 ° C for 24 h and then activated under azide at 550 ° C for 2 h. Example 1D (in accordance with the invention): preparation of 6.7% Mo + 0.9% Co / AbO3 by dry impregnation of a solution of SiMoipQ4n4'.4H + .28H2O and CofNOg) 1, 4 g of SiMo 2 O 4 O 4 · 4H + .28H 2 O and 0.69 g of Co (NC 3) 2.6H 2 O are dissolved at 60 ° C. in 7.3 ml of distilled water. An alumina (Sbet = 198 m2 / g, Vp = 0.47 ml / g) is impregnated with this solution. The solid obtained is matured for 24 hours at 25 ° C. under air. The resulting solid is oven-dried at 120 ° C for 24 h and then activated under nitrogen at 550 ° C for 2 h. Example 1E (according to the invention): preparation of 6.7% Mo / AbOg by dry impregnation of a solution of Mo 2 NHOSiPhsMPvridine II, 6 g of Mo (N) (OSiPh 3) 3 (Pyridine) are dissolved at 60 ° C in 7.3 ml of well-water. An alumina (Sbet = 198 m2 / g, Vp = 0.47 ml / g) is impregnated with this solution. The solid obtained is matured for 24 h at 25 ° C. under rr. The resulting solid is oven-dried at 120 ° C for 24 h and then activated under azide at 550 ° C for 2 h. Example 1F (in Accordance with the Invention): Preparation of 6.7% Mo / AbOg by Dry Impregnation of a Solution of SiMoi ™ 04n4'.4H + .28H O and MofENUOSiPhgWPvridine) 0.7 g of SiMoi204o4.4H + 2.8 H 2 O and 5.8 g of Mo (EN) (OSiPh 3) 3 (Pyridine) are dissolved at 60 ° C. in 7.3 ml of distilled water. An alumina (Sbet = 198 m2 / g, Vp = 0.47 ml / g) is impregnated with this solution. The solid obtained is matured for 24 hours at 25 ° C. under air. The resulting solid is oven-dried at 120 ° C for 24 h and then activated under nitrogen at 550 ° C for 2 h. Example 2: Metathesis of propylene to ethylene and butene-2 2 g of catalyst prepared in Examples 1A to 1F are mixed at a height of 50% by weight with silicon carbide (SiC) in a double-jacketed fixed bed reactor. The coolant of the jacket is heated to 70 ° C. Pure propylene is fed by a Gilson pump to the reactor and the pressure is set at 4.5 MPa. The productivity of the catalysts expressed in millimoles of propylene consumed per gram of catalyst per hour is quantified as a function of the time noted t (in hours noted h) in FIG. 1. The activity of all the catalysts 1B to 1F conforming to the invention prepared by impregnation of molybdenum precursors having Si-O-Mo bonds is greater than the activity of catalyst 1A not according to the invention and prepared by impregnation of a precursor based on molybdenum having no bonds Si-O-Mo: The stability of the catalysts 1B to 1F according to the invention is better than the stability of the catalyst 1A not in accordance with the invention.
权利要求:
Claims (17) [1" id="c-fr-0001] A process for metathesis of olefins carried out by placing the olefins in contact with a catalyst comprising a mesoporous matrix and at least the molybdenum and silicon elements, said elements being incorporated in said matrix by means of at least one precursor comprising molybdenum and silicon and having at least one sequence of Si-O-Mo bonds. [2" id="c-fr-0002] The method of claim 1 wherein the precursor is a molybdenum coordination complex containing a siloxy ligand and comprising at least one Si-O-Mo linkage and / or a molybdenum-based heteropolyanion precursor containing at least one a sequence of Si-O-Mo bonds. [3" id="c-fr-0003] 3. Process according to claim 1 or 2 wherein when the precursor is a molybdenum coordination complex containing a siloxy ligand, it corresponds to the formula (I) in which the Y groups, which are identical to or different from each other, are chosen from O, S and NR '; the X groups, which are identical to or different from one another, are chosen from halides, such as F, Cl, Br, I, the groups; substituted or unsubstituted alkyls, cycloalkyls or aryls, substituted or unsubstituted cyclopentadienyls, alkoxy, aryloxy, amide, hydrido, carboxylate, acetylacetonate, sulfonate, β-diketiminate, iminopyrrolidide, amidinate, thiocyanate or NR2-CS2 'groupings, , which are identical to or different from one another, are chosen from substituted or unsubstituted alkyl, cycloalkyl and aryl groups, preferably comprising from 1 to 10 carbon atoms, or from substituted and unsubstituted alkoxy and aryloxy groups, R 'groups , identical to or different from each other, are chosen from alkyl, cycloalkyl and aryl groups, substituted or unsubstituted, m is 1 or 2, n is 0 to 4, n is 0 to 2, z is 0 to 9 and r is 0 to 2; between 1 and 10. [4" id="c-fr-0004] 4. Process according to claim 2 or 3, in which when the precursor is a molybdenum coordination complex precursor containing a siloxy ligand, it corresponds to the formula (la): in which the groups R, which are identical to or different from one another, may be chosen from substituted or unsubstituted alkyl, cycloalkyl and aryl groups, preferably comprising between 1 and 10 carbon atoms, or from substituted and unsubstituted alkoxy and aryloxy groups, m is equal to 1 or 2, n is between 0 and 2, p is between 1 and 10. [5" id="c-fr-0005] The process according to claim 2 or 3 wherein when the precursor is a molybdenum coordination complex precursor containing a siloxy ligand, it has the formula (Ib) in which - the groups R, which are identical to or different from one another, may be chosen from substituted or unsubstituted alkyl, cycloalkyl and aryl groups, preferably comprising from 1 to 10 carbon atoms, or from substituted and unsubstituted alkoxy and aryloxy groups; no, - m is 1 or 2, n is between 0 and 4, p is between 1 and 10. [6" id="c-fr-0006] 6. Method according to one of the preceding claims wherein the molybdenum coordination complex containing a siloxy ligand contains in its coordination sphere one or more L-type ligands, optionally polydentate selected from phosphorus compounds, oxygenates, compounds nitrogenous aromatic compounds and / or sulfur compounds such as thioethers. [7" id="c-fr-0007] 7. Method according to one of the preceding claims wherein the molybdenum coordination complex precursor containing a siloxy ligand is selected from the following compounds: MoO (OSiMe3) CN (CS2-NEt2) 2, Mo (= N- ( 2,6-di- / PrC6H3)) (/ Bu) (= CHfiu) (OSi (Ofiu) 3), Mo (= S) (= N / Pr) (OSitBu3) 2, Mo (= 0) (OSitBu3) 4, Mo (sN) (OSiPh3) 3 (C6H5N) or Mo2 (OSiMe3) 6. [8" id="c-fr-0008] 8. Process according to claim 1 or 2, in which, when the precursor according to the invention is a heteropolyanion precursor, it corresponds to formula (II): • x is equal to 1 or 2, • m is greater than or equal to 1, • b is greater than or equal to 0, • m + b is greater than or equal to 5, • y is between 20 and 50, • h is between 0 and 12, q is 3 to 12, n is 0 to 200; X, m, b, y, h, n and q being integers, M being a metal element selected from aluminum, zinc, nickel, cobalt, tungsten, vanadium, niobium, tantalum , iron and copper. [9" id="c-fr-0009] The process according to claim 8 wherein the molybdenum heteropolyanion precursor is selected from the group consisting of a Strandberg heteropolyanion of the formula S12M05O238 ', nH20, an Anderson heteropolyanion of the formula SiMo60248 nH20, a heteropolyanion of Keggin of formula S1M012O404-, nH20, a lacunar Keggin heteropolyanion of formula SiMon0398 ', nH20, a lacunar Keggin heteropolyanion of formula SiMogC ^ 10 ", nH20, a Dawson heteropolyanion of formula Si2Moi80628', nH20, a Preysler heteropolyanion of SisMosoO-20 formula, nH20. [10" id="c-fr-0010] The process according to claim 8 wherein the molybdenum-based heteropolyanion precursor is selected from the group consisting of a Strandberg heteropolyanion of the formula Si2Mo4CoC> 2312 nH20, an Anderson heteropolyanion of the formula SiMo5CoO2412 nH20, a heteropolyanion Keggin of formula SiMonCoO4O8 nH20, a lacunar Keggin heteropolyanion of formula SiMoOcoC> 3912 nH20, a lacunar Keggin heteropolyanion of formula SiMo8CoO3414 nH20, a Dawson heteropolyanion of formula Si2Mol7Co06212 ", nH20, a Preysler heteropolyanion of formula Si5Mo29CoOno24 nH20. [11" id="c-fr-0011] 11. Method according to one of the preceding claims wherein the mesoporous matrix is an oxide-based matrix of at least one element X selected from silicon, aluminum, titanium, zirconium, magnesium, lanthanum. , cerium and their mixtures. [12" id="c-fr-0012] 12. Method according to one of the preceding claims wherein the catalyst is prepared by dry impregnation according to the process comprising the following steps: a) solubilization of the precursor comprising molybdenum and silicon and having at least one sequence of Si-O bonds; -Mo, in a volume of solution corresponding to the pore volume of a mesoporous matrix based on preformed oxide, b) impregnation of the preformed oxide-based mesoporous matrix with the solution obtained in step a), possible maturation of the solid thus obtained, c) optional step of drying, calcining and / or steam treatment of the solid obtained at the end of step b), at a pressure greater than or equal to 0.1 MPa or less, or equal to 0.1 MPa, in a temperature range from 50 ° C. to 1000 ° C., d) step of thermal activation of the solid obtained at the end of step c), at a pressure greater than or equal to 0.1 MPa or less than or equal to 0.1 MPa, in a temperature range of 100 ° C to 1000 ° C. [13" id="c-fr-0013] 13. Method according to one of claims 1 to 11 wherein the catalyst is prepared by excess impregnation according to the process comprising the following steps: a ') solubilization of the precursor comprising molybdenum and silicon and having at least one sequence of bonds Si-O-Mo, of formula (I), (la), or (Ib), and / or of formula (II) in a volume of solution corresponding to between 1.5 and 20 times the pore volume of the mesoporous matrix based on preformed oxide, b ') impregnation of the preformed oxide-based mesoporous matrix with the solution obtained in step a'), filtration and recovery of the solid, optional maturation of the solid thus obtained, c ') optional step of drying, calcining and / or steam treatment of the solid obtained at the end of step b ') at a pressure greater than or equal to 0.1 MPa or less than or equal to 0.1 MPa, in a temperature range of from 50 ° C to 1000 ° C, a step of thermal activation of the solid obtained at the end of step c ') at a pressure greater than or equal to 0.1 MPa or less than or equal to 0.1 MPa, in a temperature range of 100 ° C at 1000 ° C. [14" id="c-fr-0014] 14. Method according to one of claims 1 to 11 wherein the catalyst is prepared according to the process comprising the following steps: a1) solubilization of the precursor comprising molybdenum and silicon and having at least one sequence of Si-O-Mo bonds and precursors of the mesoporous matrix based on the oxide of at least one element X in an aqueous or hydro-organic solution in the presence of a pore-forming agent so as to form a colloidal solution, b1) atomizing said colloidal solution in order to obtain spherical solid elementary particles incorporating the oxide-based mesostructured matrix and the precursor comprising molybdenum and silicon and having at least one Si-O-Mo linkage of formula (I), (la) , or (Ib), and / or of formula (II), c1) optional step of drying, calcining and / or steam treatment of the solid particles obtained at the end of step b1 ) at a pressure greater than or equal to 0.1 MPa or less than or equal to 0.1 MPa, d1) a step of thermal activation of the solid particles dried at the end of step c1), at a pressure greater than or equal to at 1 bar or less than or equal to 0.1 MPa, in a temperature range of 100 to 1000 ° C. [15" id="c-fr-0015] 15. Method according to one of the preceding claims wherein the metathesis reaction is carried out at a temperature between 0 and 500 ° C. [16" id="c-fr-0016] 16. Process according to one of the preceding claims, in which the olefins are linear olefins corresponding to the general formula R1R2C = CR3R4, where R1, R2, R3 and R4, which are identical or different, are hydrogen or a hydrocarbyl radical of 1 to 20 carbon atoms, or olefins of cyclic structure, the ring having from 3 to 20 carbon atoms. [17" id="c-fr-0017] 17. Method according to one of claims 15 or 16 wherein the metathesis reaction is the cross metathesis reaction of ethylene with butene-2, or the reverse reaction of conversion of propylene to a mixture of ethylene and butene-2.
类似技术:
公开号 | 公开日 | 专利标题 WO2017021235A1|2017-02-09|Olefin metathesis method using a catalyst containing silicon and molybdenum WO2017021232A1|2017-02-09|Olefin metathesis method using a catalyst containing aluminium and molybdenum incorporated by means of at least two precursors FR3038851B1|2019-11-08|CATALYST BASED ON TANTALUM BASED ON SILICA FOR THE TRANSFORMATION OF ETHANOL TO BUTADIENE TW200927284A|2009-07-01|Hydrogenation catalyst and process for preparing alcohols by hydrogenation of carbonyl compounds FR2977890A1|2013-01-18|PROCESS FOR THE METATHESIS OF OLEFINS USING A CATALYST BASED ON A SPHERICAL MATERIAL COMPRISING OXIDATED METAL PARTICLES PIEGEED IN A MESOSTRUCTURED MATRIX WO2010113993A1|2010-10-07|Process for producing olefin FR3038849B1|2019-11-29|MESOPOROUS MIXED OXIDE CATALYST COMPRISING SILICON FR3054455A1|2018-02-02|HETEROGENEOUS CATALYSTS CONTAINING NICKEL AND SILICON AND THEIR USE FR2951164A1|2011-04-15|METHOD OF OLIGOMERIZING AN OLEFIN HYDROCARBON LOAD USING A CATALYST BASED ON A MACROPOROUS SILICA ALUMINA WO2017021234A1|2017-02-09|Olefin metathesis method using a catalyst containing aluminium and molybdenum FR3039544A1|2017-02-03|PROCESS FOR THE METATHESIS OF OLEFINS USING A CATALYST CONTAINING SILICON AND MOLYBDENUM INCORPORATED BY MEANS OF AT LEAST TWO PRECURSORS FR3084361A1|2020-01-31|PROCESS FOR THE METATHESIS OF OLEFINS USING A CATALYST CONTAINING SILICON, MOLYBDENE AND SULFUR FR3054545A1|2018-02-02|NOVEL OLIGOMERIZATION PROCESS FOR OLEFINS FR3084363A1|2020-01-31|PROCESS FOR THE METATHESIS OF OLEFINS USING A CATALYST CONTAINING SILICON, MOLYBDENE AND AN ALKALINE ELEMENT FR3084362A1|2020-01-31|PROCESS FOR THE METATHESIS OF OLEFINS USING A CATALYST CONTAINING SILICON, MOLYBDENE AND AN ALKALINE ELEMENT FR3103192A1|2021-05-21|OLEFINS METATHESIS PROCESS USING A HIGH ALKALINE CATALYST CONTAINING SILICON, MOLYBDENE JP5720256B2|2015-05-20|Amide group reduction catalyst and process for producing aminomethyl compound using the catalyst KR101410369B1|2014-06-20|Silico-metal-phosphate catalyst and preparing method of 1,3-butadiene and methylethylketone using the same FR3038852B1|2019-11-29|STABILIZED PRODUCTION OF 1,3-BUTADIENE IN THE PRESENCE OF A TANTALIUM OXIDE DOPED BY AN ALDOLIZING ELEMENT KR20120077926A|2012-07-10|Alumina catalyst with dispersed chrome oxide, method of preparing the same and method of preparing propylene by using the same FR3087357A1|2020-04-24|NOVEL OLEFIN OLIGOMERIZATION PROCESS USING CATALYSTS BASED ON A SPHERICAL MATERIAL COMPRISING METALLIC PARTICLES OF NICKEL OXIDE TRAPS IN A MESOSTRUCTURED MATRIX KR100974542B1|2010-08-11|Fischer-Tropsch synthesis method using iron-based catalyst and supercritical fluids of C5-C7 normal paraffin
同族专利:
公开号 | 公开日 KR20180033508A|2018-04-03| CN108137439A|2018-06-08| RU2018107136A3|2019-11-29| WO2017021235A1|2017-02-09| SA518390840B1|2021-09-21| US20190009260A1|2019-01-10| TW201716360A|2017-05-16| FR3039546B1|2017-08-11| CN108137439B|2021-07-20| US10737254B2|2020-08-11| RU2018107136A|2019-08-28|
引用文献:
公开号 | 申请日 | 公开日 | 申请人 | 专利标题 US2547380A|1945-10-01|1951-04-03|Union Oil Co|Catalyst for hydrocarbon conversion| WO1997047385A1|1996-06-13|1997-12-18|Elf Antar France|Method for preparing hydro-treating catalysts| FR2764211A1|1997-06-09|1998-12-11|Elf Antar France|PROCESS FOR PREPARING HYDROTREATMENT CATALYSTS| FR2826880A1|2001-07-04|2003-01-10|Inst Francais Du Petrole|Improved catalyst composition for the metathesis of olefins comprises a compound of rhenium, molybdenum or tungsten with addition of silicon|WO2020020730A1|2018-07-25|2020-01-30|IFP Energies Nouvelles|Method for olefin metathesis using a catalyst containing silicon, molybdenum and an alkaline element| FR3084362A1|2018-07-25|2020-01-31|IFP Energies Nouvelles|PROCESS FOR THE METATHESIS OF OLEFINS USING A CATALYST CONTAINING SILICON, MOLYBDENE AND AN ALKALINE ELEMENT| FR3084361A1|2018-07-25|2020-01-31|IFP Energies Nouvelles|PROCESS FOR THE METATHESIS OF OLEFINS USING A CATALYST CONTAINING SILICON, MOLYBDENE AND SULFUR| FR3103192A1|2019-11-15|2021-05-21|IFP Energies Nouvelles|OLEFINS METATHESIS PROCESS USING A HIGH ALKALINE CATALYST CONTAINING SILICON, MOLYBDENE|JP5437628B2|2005-06-06|2014-03-12|ダウグローバルテクノロジーズエルエルシー|Metathesis process for preparing olefins with α, ω-functional groups| DE102007039526A1|2007-08-21|2009-02-26|Lanxess Deutschland Gmbh|Catalyst systems and their use for metathesis reactions| CN101230076A|2007-09-30|2008-07-30|赢创德固赛有限责任公司|Ruthenium homonuclear bimetal and heteronuclear bimetal alkylidene complex containing N-heterocyclic carbenes| US8362311B2|2009-09-30|2013-01-29|Massachusetts Institute Of Technology|Highly Z-selective olefins metathesis| FR2977890B1|2011-07-15|2013-07-19|IFP Energies Nouvelles|PROCESS FOR THE METATHESIS OF OLEFINS USING A CATALYST BASED ON A SPHERICAL MATERIAL COMPRISING OXIDATED METAL PARTICLES PIEGEED IN A MESOSTRUCTURED MATRIX|
法律状态:
2016-07-19| PLFP| Fee payment|Year of fee payment: 2 | 2017-02-03| PLSC| Publication of the preliminary search report|Effective date: 20170203 | 2017-07-31| PLFP| Fee payment|Year of fee payment: 3 | 2018-07-25| PLFP| Fee payment|Year of fee payment: 4 | 2019-07-25| PLFP| Fee payment|Year of fee payment: 5 | 2020-07-28| PLFP| Fee payment|Year of fee payment: 6 | 2021-07-26| PLFP| Fee payment|Year of fee payment: 7 |
优先权:
[返回顶部]
申请号 | 申请日 | 专利标题 FR1557370A|FR3039546B1|2015-07-31|2015-07-31|PROCESS FOR THE METATHESIS OF OLEFINS USING A CATALYST CONTAINING SILICON AND MOLYBDENE|FR1557370A| FR3039546B1|2015-07-31|2015-07-31|PROCESS FOR THE METATHESIS OF OLEFINS USING A CATALYST CONTAINING SILICON AND MOLYBDENE| CN201680044734.7A| CN108137439B|2015-07-31|2016-07-26|Olefin metathesis process using silicon and molybdenum containing catalysts| PCT/EP2016/067832| WO2017021235A1|2015-07-31|2016-07-26|Olefin metathesis method using a catalyst containing silicon and molybdenum| US15/749,297| US10737254B2|2015-07-31|2016-07-26|Olefin metathesis method using a catalyst containing silicon and molybdenum| RU2018107136A| RU2018107136A3|2015-07-31|2016-07-26| KR1020187002982A| KR20180033508A|2015-07-31|2016-07-26|Olefin metathesis method using a catalyst containing silicon and molybdenum| TW105124191A| TW201716360A|2015-07-31|2016-07-29|Process for the metathesis of olefins using a catalyst containing silicon and molybdenum| SA518390840A| SA518390840B1|2015-07-31|2018-01-30|Olefin Metathesis Method using A Catalyst Containing Silicon and Molybdenum| 相关专利
Sulfonates, polymers, resist compositions and patterning process
Washing machine
Washing machine
Device for fixture finishing and tension adjusting of membrane
Structure for Equipping Band in a Plane Cathode Ray Tube
Process for preparation of 7 alpha-carboxyl 9, 11-epoxy steroids and intermediates useful therein an
国家/地区
|