专利摘要:
The present invention relates to non-stick coating primer compositions based on polyimide resin and / or polyamide-imide resin. The present invention also relates to methods for preparing such compositions. Finally, the present invention relates to non-stick coatings incorporating such compositions and a method of manufacturing articles comprising such release coatings.
公开号:FR3037965A1
申请号:FR1555826
申请日:2015-06-24
公开日:2016-12-30
发明作者:Barbara Gantillon
申请人:SEB SA;
IPC主号:
专利说明:

[0001] FIELD OF THE INVENTION The present invention relates generally to polyimide resin and / or polyamide-imide non-stick coating primer compositions. The present invention also relates to methods for preparing such compositions. Finally, the present invention relates to non-stick coatings incorporating such compositions and to a method of making articles comprising such release coatings. Non-stick coatings based on fluorocarbon resin, especially polytetrafluoroethylene (PTFE), are widely used in the field of culinary articles. They are made from at least one primer layer containing a fluorocarbon resin and a tackifying resin. This primer layer is then coated with one or more fluorocarbon resin-based layers, especially PTFE, in which the amount of fluorocarbon resin is gradually increased. The adhesion resins, allowing the adhesion of this primer layer and the other fluorinated layers on the support, are generally of the polyamide-imide (PAI), polyimide (PI), poly (phenylene sulphide) (PPS) type, Polyethersulfone (PES), and polyetheretherketone (PEEK). In the particular case where light-colored primer layers are desired, the PES, PPS or PEEK resins are preferred. However, the use of these resins is not easy because they are poorly soluble other than in polar aprotic solvents, which are for the most part subject to labeling as a harmful or even toxic product in the regulations. REACH. These resins are in practice used in powder form. However, obtaining small particle size powders is difficult and expensive, making it difficult to grind these polymers to an average size of less than 10 microns. It follows that the distribution of these resins in the primer layer is not homogeneous and leads to large easy deliveries to loss of adhesion to use. from this point of view, the adhesion resins which are in solution or in powder dilutable in water are more to be used. However, they incorporate amounts of solvent.
[0002] When they are delivered as a dilutable powder in water, the solvent stress is certainly overcome, but these adhesion resins also show a thermal stability which is considered insufficient even if it does not affect most properties of the resulting coating. Indeed, during the sintering step of the fluorocarbon resin, in particular PTFE, (made at more than 370 ° C. and preferably at 415 ° C.), a small fraction of the adhesion resin, in particular PAI resin. , decomposes. In addition, the use of a labile amine for the implementation in the aqueous phase of the tackifying resin, in particular PAI resin, leads to generating a proportion of volatile organic compounds which is not negligible and which induces unacceptable yellowing of the resulting coating. On the other hand, the preparation of silica grafted with polyamic acids is known (Peng Liu, Iranian Polymer Journal 14, (11) 2005, 968-972). These grafted silicas have improved temperature stability; however, on the one hand, the starting compound is an already existing silica, and, on the other hand, all the modifications are carried out in a solvent medium and their use is suggested in solvent media. Patent documents EP0386379 and FR2625450 both describe, in a similar manner, mixtures of PAI resin and an aminosilane. In the described procedure, the aminosilane is mixed with the PAI resin precursor already in aqueous solution, that is to say that it already incorporates an amine for salification and, in view of the choice of PAI resin described in the examples, a solvent, this solvent being necessary for carrying out the mixture in liquid form. These patent documents are not exempt from the presence of a volatile amine capable of generating yellowing or the presence of potentially toxic polar aprotic solvent. Finally, and in a quite conventional manner, the formulation of the primer compositions in practice requires the introduction of colloidal silica to reinforce the obtained primer film. The amounts used are from 10 to 20% by weight (based on dry film). The addition of smaller amounts does not provide sufficient reinforcement and it is difficult in practice to introduce higher quantities. But even at these levels, the silica particles are aggregated with each other, which results in nanoporosities which are harmful to the impermeability of the film and which lead to the appearance of the film in the primary film. corrosion points in prohibitive quantity. To overcome these disadvantages and to obtain non-stick coatings with enhanced thermal stability and strength while maintaining good resilience, corrosion resistance, and greatly diminished staining or yellowing, the Applicant has developed polyimide resin and / or polyamide-imide resin release liner primer compositions obtained by reacting the polyimide resin and / or the polyamide-imide resin with a coupling agent and an alkoxysilane and / or a metal alkoxylate the coupling agent for coupling between the PI resin and / or PAI and the alkoxysilane and / or the metal alkoxylate. Such a reaction leads to the crosslinking of the assembly by a sol-gel type reaction and an organic-inorganic hybrid structure is obtained with the in-situ formation of a network of 5 nanometric sized silica domains perfectly dispersed in the PI resin matrix and / or PAI. The materials with an organic-inorganic hybrid structure thus obtained are nanocomposites which aim to be a synergistic combination between: an organic phase: the PAI and / or PI adhesion resin plays the role of an organic polymer matrix. It provides flexibility through its amide functions and high thermostability through its imide cycles to the resulting coating. On the other hand, the ductility of such a polymer matrix facilitates its implementation, especially in the case where the carrier (such as a disk) must then be stamped; and an inorganic phase: an interpenetrated silica filler within the polymer matrix to enhance the mechanical (hardness, stiffness), thermal and anticorrosive performance of the resulting coating. This charge is incorporated by in-situ generation by sol-gel of a network of inorganic nanometric domains (called "nanoformed") from an inorganic precursor of metal oxide type. The present invention therefore consists in associating a PAI and / or PI bonding resin (organic phase) with a neoformed inorganic phase via a coupling agent linked to the organic and inorganic phases by covalent bonds. Such coupling agents have a function capable of opening and binding to the imide cycles of the PAI and / or PI resin and functions capable of generating the silica under the chosen operating conditions. Hybrid polyamide-imide resin / silica materials are known to those skilled in the art.
[0003] Thus, patent document KR20090111951 discloses a method of manufacturing a polyamideimide / silica hybrid resin material for coating electric wires. In the process described, colloidal silica is added to an organic silane to form a colloidal silica sol based on silica silane (i.e., colloidal silica with organic groups on its surface). . Then, an organic solvent is added to the colloidal silica sol, which is incorporated in polyamide-imide resin to make a hybrid of silica and polyamide-imide resin. Finally, an aminosilane is added to the hybrid soil solution and the mixture is stirred. The method of KR20090111951 teaches a method for grafting existing silica via a coupling agent onto the PAI resin. But, it is not a sol-gel process with in-situ generation of silica, making it possible to obtain nanometric silica domains very well dispersed in the polymer matrix. Furthermore, the document US2005 / 0245715 describes a process for producing a composite film of polymer resin and silica from carboxysilanes and a polymer resin, which uses an amine coupling agent or with an epoxy group on halogenated base. However, the polymer resin used in the process of this document is a polyamide-amic acid (PAA), which is a precursor of the PAI resin, and not directly a PAI resin itself.
[0004] The composite films of this document are mainly used in the field of electronic and microelectronic devices and photoelectric elements. The subject of the present invention is therefore a non-stick coating primer composition which overcomes the above-mentioned problems. This is in particular a non-stick coating primer composition comprising: - a polyimide resin and / or a polyamide-imide resin, - an alkoxysilane and / or a metal alkoxylate, - a coupling agent capable of coupling the polyimide resin and / or the polyamide-imide resin and the alkoxysilane and / or the metal alkoxylate, and - a polar aprotic solvent. By coupling agent capable of coupling the polyimide resin 10 and / or the polyamide-imide resin and the alkoxysilane and / or the metal alkoxylate, is meant, within the meaning of the present invention, a compound having, on the one hand, one or more functional groups which can bind to the PI and / or PAI resin, in particular to the imide rings of the PI and / or PAI resin, and, on the other hand, one or more functional groups that are capable of reacting with the alkoxysilane and / or the metal alkoxylate to form in-situ silica. Preferably, the primer composition according to the invention comprises a polyamide-imide resin.
[0005] Advantageously, the polyimide resin and / or the polyamide-imide resin may be present in the primer composition according to the invention in a proportion of 20 to 70% by weight, and preferably 20 to 60% by weight, by weight. relative to the total weight of said primer composition.
[0006] Advantageously, the alkoxysilane of the primer composition according to the invention may be chosen from methyltrimethoxysilane (MTMS), tetramethoxysilane (TMOS), tetraethoxysilane (TEOS), tetrapropoxysilane, methyltriethoxysilane (MYES) and dimethyldimethoxysilane. phenyltriethoxysilane, and mixtures thereof. As an alkoxysilane, tetraethoxysilane (TEOS) is preferably used in the primer composition according to the invention.
[0007] Advantageously, the metal alkoxylate of the primer composition according to the invention may be chosen from aluminates and titanates. Advantageously, the alkoxysilane and / or the metal alkoxylate of the primer composition according to the invention may be hydrolysed in an acid medium or in a basic medium. Preferably, the alkoxysilane and / or the metal alkoxylate is hydrolysed in a basic medium. In acidic medium, the hydrolysis reaction is rapid in front of the condensation reaction causing gelation of the mixture; on the contrary, in basic medium, the condensation reaction is faster than the hydrolysis to obtain colloidal solutions. Advantageously, the primer composition according to the invention may further comprise an alcohol. As alcohols that may be used in the primer composition according to the invention, mention may especially be made of terpineol, propan-2-ol, methanol, 2- (2-butoxyethoxy) ethanol, isopropanol, and glycols ( such as butylglycol, ethylene glycol-butyl ether (or EGBE), terpineol, texanol (chemical name: 2,2,4-trimethylpentane-1,3-diol monoisobutyrate), diethylene glycol monomethyl ether, methoxypropanol and mixtures thereof.
[0008] Advantageously, the total relative content by dry weight of the coupling agent with respect to the polyimide resin and / or the polyamide-imide resin may be between 2 and 20% in the primer composition according to the invention. As coupling agents that may be used in the primer composition according to the invention, there may be mentioned silazanes (and preferably hexamethyldisilazane), silane derivatives, and mixtures thereof. As silane derivatives which may be used in the primer composition according to the present invention, there may be mentioned in particular aminosilanes, such as 3-aminomethyltrimethoxysilane (APrTMOS or APTMOS), 3-aminopropyltriethoxysilane (APTES or APrTEOS), 3 aminopropyltri (methoxyethoxyethoxy) silane, 4-aminobutyltriethoxysilane, 3-aminophenyltrimethoxysilane (APTMOS), m-aminophenyltrimethoxysilane, p-aminophenyltrimethoxysilane, 3-aminophenyltriethoxysilane (APTEOS), 11-aminoundecyltriethoxysilane, aminopropyl- silanetriol, bis (methyldiethoxysilylpropylamine), bis (triethoxysilylpropyl) amine, bis (trimethoxysilylpropyl) amine, bis ((3-trimethoxysilyl) propyl) ethylenediamine, and mixtures thereof. Preferably, the coupling agent of the primer composition according to the invention is 3-aminopropyltriethoxysilane (APTES).
[0009] As silane derivatives which can be used in the primer composition according to the invention, epoxysilanes (preferably yglycidyloxypropyltrimethoxysilane (GPTMS)), γ-glycidopropyltriethoxysilane, γ-glycidoxypropyltrimethoxysilane (GTMOS), γ-glycidoxypropyltriethoxysilane (GTEOS), vinyltriethoxysilane, methacryloxyethyltriethoxysilane, methacryloxypropyltrimethoxysilane, methyltriethoxysilane, dimethyldiethoxysilane, silane isocyanates of the formula OCN-R1-Si (R2) 3 in which R1 is an alkene group. C1-C6 (such as methylene, ethylene, propylene, butylene, pentylidene and hexamethylene) or a C1-C6 arylene group (such as phenylene or naphthylene) and R2 is the same as R1 or is different from R1 and is then an alkoxy group C1-C6, and mixtures thereof.
[0010] Couples which may be used in the context of the present invention may also be amino acids, such as a tyrosine of the formula ## STR1 ## or a glycine, of the formula ## STR2 ## Advantageously, the solvent aprotic polar is present in the primer composition according to the invention in a proportion of 1 to 70% by weight relative to the total weight of the primer composition. Advantageously, the polar aprotic solvent may comprise at least one of N-formylmorpholine (NFM), N-ethylmorpholine, dimethylsulfoxide (DMSO), N-acetylmorpholine (NAM), N-ethylpyrrolidone ( NEP), N-butylpyrrolidone (NBP), N-methylpyrrolidone (NMP), 1,3-dioxolane, 2,5,7,10-tetraoxaundecane, N-methylpyrrolidine ketone, N, N- dimethylformylamide, N, N15 dimethylacetamide. Advantageously, the primer composition according to the invention may be free of thermostable binder, and in particular fluorocarbon resin. Advantageously, the primer composition according to the invention may further comprise at least one filler or at least one pigment. The present invention also relates to a non-stick coating hybrid primer composition comprising a polyimide resin and / or polyamide-imide resin matrix, in which silica domains having a size of less than 200 nm are dispersed in an aprotic solvent. polar, the size of the silica domains being measured either wet by laser particle size in the hybrid primer composition according to the invention, or by transmission electron microscopy (TEM analysis) analysis on the film of cooked primer obtained at from the hybrid primer composition according to the invention. The polyimide resin and / or polyamide-5 imide resin matrix in which the silica domains are dispersed may advantageously be in colloidal dispersion in the polar aprotic solvent. Advantageously, the silica domains in the hybrid primer composition according to the invention may have a size of less than 100 nm, and preferably of between 10 and 50 nm. Advantageously, the relative dry weight content of the silica domains with respect to the polyimide resin matrix and / or polyamide-imide resin may be between 10 and 25%, and preferably between 10 and 20%, in the hybrid primer composition according to the invention. Advantageously, the polar aprotic solvent may be present in the hybrid primer composition according to the invention in a proportion of 1 to 70% by weight relative to the total weight of the hybrid primer composition. Advantageously, the polar aprotic solvent may comprise at least one of N-formylmorpholine (NFM), N-ethylmorpholine, dimethylsulfoxide (DMSO), N-acetylmorpholine (NAM) and N-ethylpyrrolidone (CIP). ), N-butylpyrrolidone (NBP) and N-methylpyrrolidone (NMP), 1,3-dioxolane, 2,5,7,10-tetraoxaundecane, N-methylpyrrolidine ketone, N, N-dimethylformylamide, N, N-dimethylacetamide. Advantageously, the hybrid primer composition according to the invention may be free of thermostable binder, and especially fluorocarbon resin. Advantageously, the hybrid primer composition according to the invention may further comprise at least one filler or at least one pigment.
[0011] In the context of the present invention, it will be preferable to use, as filler in the primer composition according to the invention or in the hybrid primer composition according to the invention, silica nanoparticles, alumina, Talc, kaolin, barite, wollastonite, silicon carbide and mixtures thereof. In the context of the present invention, it will be preferable to use, as pigment in the primer composition according to the invention or in the hybrid primer composition 10 according to the invention, cobalt aluminate (CoA1204), titanate of chromium, antimony, iron oxides, nickel titanate, carbon black, silico-aluminates, titanium dioxide, inorganic pigments with crystalline spinel structure based on different metal oxides, 15 mica flakes coated with iron oxide or titanium oxide, iron oxide-coated aluminum flakes, perylene red, thermochromic semiconductor pigments (for example, semiconducting metal oxides such as Fe203, Bi203, or BiVO4 ...) and mixtures thereof.
[0012] The present invention also relates to a non-stick coating comprising at least one layer of non-stick coating primer composition according to the invention or at least one layer of non-stick coating hybrid primer composition according to the invention.
[0013] The layer or layers of primer composition according to the invention or hybrid primer composition according to the invention are typically applied directly to a support, in particular on the support of a culinary article, the support being or not previously subjected to a surface treatment. On this or these primary layers, is usually applied a first topcoat, itself preferably covered with at least a second topcoat.
[0014] The at least one finishing layer comprises at least one thermostable binder compatible with the at least one layer of primer composition or hybrid primer composition. As thermostable binder used in the finishing layer or layers according to the invention, there may be mentioned enamels, fluorocarbon resins (alone or in admixture), inorganic polymers or organic-inorganic hybrids synthesized by sol-gel method. . The present invention further relates to a process for preparing a non-stick coating primer composition according to the invention or a non-stick coating hybrid primer composition according to the invention, the process comprising the following steps: introducing the coupling agent into a solution comprising the polyimide resin and / or the polyamide-imide resin and the polar aprotic solvent; and b) adding in alkaline medium the alkoxysilane and / or metal alkoxylate, and water to the mixture of step a).
[0015] If it is a question of the preparation of a non-stick coating hybrid primer composition according to the invention, the subject of the present invention is also a process comprising the following steps: a) the introduction of the coupling agent in a solution comprising the polyimide resin and / or the polyamide-imide resin and the polar aprotic solvent; and b) adding the prehydrolysed alkoxysilane and / or metal alkoxylate to the mixture of step a). In this particular case, this process according to the invention may advantageously also comprise a step c) of hydrolyzing the alkoxysilane and / or the metal alkoxylate to obtain the alkoxysilane and / or the metal alkoxylate hydrolysed, step c) of hydrolysis being carried out before step b) and comprising: - hydrolysis in alkaline medium of the alkoxysilane and / or metal alkoxylate in a mixture of water and water. alcohol, or - the basic hydrolysis of the alkoxysilane and / or the metal alkoxylate in a mixture of water and polar aprotic solvent. The PI and / or PAI resin, the coupling agent, the polar aprotic solvent, the alkoxysilane and the metal alkoxylate are as defined previously.
[0016] Whether for the preparation of a non-stick coating primer composition according to the invention or that of a non-stick coating hybrid primer composition according to the invention, the processes according to the invention may advantageously also comprise a step d) adding fillers and / or pigments to the mixture resulting from step b). The fillers and / or pigments are as defined above. Likewise, whether for the preparation of a non-stick coating primer composition according to the invention or that of a non-stick coating hybrid primer composition according to the invention, the processes according to the invention may advantageously comprise in addition to a step e) of dissolving the polyimide resin and / or the polyamide-imide resin in the polar aprotic solvent, this step e) being carried out before step a). The present invention further relates to a method of manufacturing an article comprising a non-stick coating according to the invention, the method comprising the following steps: A) providing a support having two opposite faces; B) applying to at least one of the faces of said support 14 - at least one layer of the nonstick coating primer composition according to the invention, or - at least one layer of the hybrid primer composition of nonstick coating according to the invention, or - at least one layer of non-stick coating primer composition or of non-stick coating hybrid primer obtained according to the processes according to the invention for preparing a nonstick coating primer composition or a hybrid primer composition of non-stick coating; C) cooking the assembly at a temperature between 390 ° C and 430 ° C.
[0017] Advantageously, the method of manufacturing an article according to the invention may further comprise a step B ') of application to the layer obtained in step B), before the cooking of step C), at least one non-stick coating topcoat. Advantageously, the application step B ') can be carried out on the layer obtained in the wet step B). When the layer obtained in step B) is dried before step B '), it can then become hydrophobic and prevent the adhesion of the subsequently deposited topcoat.
[0018] The nonstick coating topcoat is as defined above. Finally, the present invention also relates to an article that can be obtained according to the method of manufacturing an article according to the invention.
[0019] Various types of articles according to the invention, of different shapes and made of different materials, can be envisaged.
[0020] Thus, it may be an article comprising a support made of a material chosen from metals, glass, ceramics and plastics. As metallic supports that can be used in the context of the present invention, mention may advantageously be made of aluminum or anodized or non-anodized aluminum alloys, or of polished, brushed or microblasted aluminum, sandblasted, chemically treated or stainless steel polished, brushed or micro-blasted, or cast iron or aluminum, titanium or hammered or polished copper. The article according to the invention may in particular be a culinary article, and in particular a culinary article one of whose faces constitutes an internal face intended to be in contact with foods placed inside said article 15 and the other face is a convex outer face intended to be in contact with a heat source. By way of non-limiting examples of cooking utensils in accordance with the present invention, mention may in particular be made of culinary articles such as pots and pans, woks and sautees, casseroles and pots, pressure cookers, crepe makers, grills, baking molds and plates, raclette cups, barbecue plates and grills, baking bowls, deep fryers and rice cookers.
[0021] Other types of supports that are not limited to the culinary field alone can also be envisaged. Thus, it is also possible to envisage, as articles in accordance with the invention, household electrical appliances such as irons, curling irons, hair straighteners, etc., isothermal pots (for coffee makers for example) or mixing bowls. The invention is illustrated in more detail in the following examples. In these examples, unless otherwise indicated, all percentages and parts are expressed as percentages by weight. EXAMPLES Tests Determination of the Dry Extract of a Composition PRINCIPLE The solids content of a composition is the residual solid part remaining after evaporation of the volatile matter it contains. The temperature and drying time are important because high boiling solvents, monomer fractions, reactive diluents and reaction by-products (depending on their degree of retention) leave the film very slowly. training. It is therefore very important to conventionally define standard drying conditions as close as possible to the practice. PROCEDURE To measure this dry extract, the procedure is as follows: an aluminum cup is weighed: mo = mass of the cup; there is between 0.5 g and 3 g of composition to be studied in this cup; the filled cup is weighed: ml mass of the filled cup; the filled cup is placed in an oven at 210 ° C. for two hours; After baking and after cooling, the cup is weighed: m2 = mass of the cup filled after steaming and cooling; the dry extract is given by the formula below: Dry extract = 100 * [(m2-mo) (m-mo) Measurement of the size and size distribution of the particles by diffraction of light The particle size of the colloidal solution obtained by hydrolyzing the TEOS (see Example 1 below) is characterized using a laser diffraction granulometer sold under the trade name Nanosizer from the company Malvern which measures the Brownian motion of the particles. in suspension and connects it to the size of the colloids (a small particle moves faster than a larger particle) via diffraction of light. Evaluation of the adhesion of a coating to a smooth aluminum support A grid test is carried out according to the NF T 30-038 standard (Standard NF EN ISO 2409), followed by immersion of the coated support for 18 hours ( consisting of alternating 3 cycles of 3 hours in boiling water and 3 cycles of 3 hours in oil at 200 ° C). Then, it is observed whether or not the non-stick coating has a detachment. The quotation is carried out as explained in the table below.
[0022] 3037965 18 Dimension Description 0 The edges of the incisions are perfectly smooth: none of the grid squares have come off.
[0023] 1 Detachment of small scales of the lining at the intersections of the incisions, which affects about 5% of the grid portion.
[0024] 2 The liner has become detached along the edges or at the intersections of the incisions, and the detached surface represents significantly more than 5% up to about 15% of the grid portion.
[0025] 3 The lining was detached along the edges of the incisions partly or wholly in wide strips or was partly or completely detached in various places from the grids. The detached area is significantly more than 15% to about 35% of the grid portion.
[0026] 4 The lining has become detached along the edges of the incisions in wide strips or some squares have become detached in part or in whole. The detached area is significantly more than% up to about 65% of the grid portion.
[0027] 5 All grades of flaking that can not be scored according to rating 4. Evaluation of yellowing 5 The yellowing after curing of the coated supports is visually evaluated by inter-carrier comparison.
[0028] Morphological analysis The morphological analysis of the silica fillers in a polymer resin matrix is carried out by TEM analysis.
[0029] TEM is an efficient method for visualizing the morphology of silica fillers in a polymer matrix, such as a PAI resin, whether these fillers are preformed (colloidal type Ludox) or obtained in situ by a sol method. -gel.
[0030] EXAMPLE 1 In a first step, a basic solution of hydrolysed TEOS is prepared by mixing with magnetic stirring at room temperature the following compounds: - pure TEOS: 262.28 g NEP: 142.43 g a mixture of water and a base: o water: 52.21 g 20 o ammonia 10.25% by weight in water: 42.85 g TOTAL: 499.77 g This solution is kept under slow stirring for 2 hours at room temperature. An opalescent solution, stable for several months, is obtained which has the following characteristics. Characteristics: - pH: 9.6 30 - viscosity: 280 mPa.s - TEOS level: 52.5% / mass of total wet solution - aspect: translucent, iridescent color 3037965 20 - particle size controlled by laser granulometry : 20 to 40 nm - pot-life: more than several months In a second step, a PAI resin in solvent form is introduced at 29% by weight in CIP, in a reactor. After dilution of the PAI resin in NEP, APTES is added. The neutralization reaction of the terminal acid groups with aminosilane leads to the chemical grafting of the silane. The reaction is carried out at room temperature with gentle stirring for 2 hours. The hydrolyzed TEOS solution as described in the 1st step is then added and the mixture is allowed to stir slowly at room temperature for 20 to 24 hours. The proportions of the mixture are shown below - 29 wt% PAI resin in CIP 218.35 g - CIP 98.31 g - APTES 5.40 g - basic solution of hydrolysed TEOS 177.94 g TOTAL 500, The mass ratio (expressed in dry / dry) of PAI / SiO 2 resin is 77/23.
[0031] The colloidal solution of PAI / silica hybrid material in the CIP thus obtained has a solids content of 16.5%, a pH of 10.2 and a measured viscosity in section 4 (according to DIN EN ISO 2433 / ASTM D5125). ) 80 seconds. This solution is stable up to 3 weeks of storage at room temperature. According to a first embodiment (application on a preformed support), this colloidal solution of hybrid material 3037965 is used as such and coated by thin-layer spraying on an aluminum support in the form of a cap (support preformed) previously subjected to a surface treatment.
[0032] The performances obtained are as follows: The thin layer produced above, analyzed by TEM, shows that an organic / inorganic hybrid material with non-agglomerated nanometric domains of silica has been obtained (co-continuous silica networks). and 10 PAI resin). TEM analysis shows individual silica particles with a diameter of less than 100 nm, without agglomerates or aggregates. The silica fillers are present throughout the thickness of the film, as illustrated in FIG. 1, which is a TEM image of a section of the formed coating showing a homogeneous distribution of the nanoscale silica particles in the PAI resin matrix. and their dimensions: the average diameter of the silica particles is of the order of 37 ± 4 nm. The presence of a co-continuous silica network is evidenced by calcination. A film is obtained whose chemical analysis by infrared spectrometry reveals two silica characteristic bands at a = 1075 cm -1 and a = 804 cm -1 (condensation of Si-O-Si siloxane bridges). The use of this hybrid primer layer in a three-layer coating system (organic / inorganic hybrid primer layer + first PAI-resin-free topcoat and PTFE-based wet-on-wet + second layer PTFE finish) and sintered under standard conditions (11 minutes at 430 ° C) gives ratings of 0 to the three cycles of the adhesion test. The hybrid coating thus obtained is non-yellowing (-35% yellowing relative to a standard primary system with PTFE as described in Comparative Example 1). A corrosion test of the hybrid coating, made by 24 hours of contact with salt water at 10% and boiling, results in the absence of corrosion points.
[0033] Furthermore, according to a second embodiment (application on a support with post-forming of the support), the hybrid primer composition obtained in step 2 is applied to an aluminum disk that has been etched beforehand by etching, dried and then steamed. A first PAI-free PTFE-based topcoat is then applied to this primer layer in wet-on-wet, and then a second PTFE-based top coat is applied to the first topcoat. The whole is sintered under standard conditions (11 minutes at 430 ° C.). The thus coated support is stamped to give a coated cap on its inner face. This postformed coated cap exhibits similar performance to the preformed coated cap previously described, illustrating the drawability of this hybrid coating. EXAMPLE 2 A PAI resin in solvent form, 29% by weight in CIP, is introduced into a reactor. It is diluted with NEP, then we just add APTES. The neutralization reaction of the terminal acid groups by the aminosilane leads to the chemical grafting of the silane. The reaction is carried out at room temperature with gentle stirring for 2 hours. TEOS is then added with demineralised water and base, and the mixture is allowed to stir slowly at room temperature for 20 to 24 hours. The proportions of the various constituents are as follows: PAI resin at 29% by weight in the NEP 218.35 g - CIP 149.20 g 10 - APTES 5.40 g - pure TEOS 93.38 g - demineralised water 18.41 10.25% by weight of ammonia in water 15.26 g TOTAL 500 g The mass ratio (expressed in dry / dry) of PAI / SiO 2 resin is 77/23. The colloidal solution of PAI / silica hybrid material in the CIP thus obtained has a solids content of 16.5%, a pH of 10.2 and a viscosity measured in section 4 (according to DIN EN ISO 2433 / ASTM D5125). ) of 65 seconds. This solution is stable up to 3 weeks of storage at room temperature. This solution is used as it is and coated by thin-film spraying on an aluminum support in the form of a cap (preformed support) previously subjected to a surface treatment. The performances obtained are as follows: The implementation of this hybrid primer layer in a three-layer coating system (organic / inorganic hybrid primer layer + first PAI-resin-free topcoat and applied PTFE-based in wet-on-wet + second PTFE-based topcoat) and sintered under standard conditions (11 minutes at 430 ° C) gives ratings of 0 to the three cycles of the adhesion test. The hybrid coating thus obtained is non-yellowing (-30% yellowing relative to a standard primary system with PTFE as described in Comparative Example 1). A corrosion test of the hybrid coating, carried out by 24 hours of contact with 10% salt water and boiling, results in the absence of corrosion points. COMPARATIVE EXAMPLE 1 An aqueous semi-finished mixture is prepared comprising the following compounds, the respective amounts of which are given in g below: PAI resin at 29% by weight in the NEP: 220.0 g-CIP: 79 22.0 g - demineralized water: 350.0 g - colloidal silica: 63.5 g TOTAL: 734.5 g The colloidal silica used is unmodified on the surface, has a surface area of 220 g. m2 / g approximately, and is in the form of an aqueous dispersion of nanoparticles with a solids content of 30% by weight in water.
[0034] To carry out this aqueous semi-finished mixture, the following procedure is carried out: the PAI resin is introduced into a Discontimill reactor with the solvent and triethylamine; The mixture thus obtained is then milled in the discontimill reactor at ambient temperature; then water is added very gradually to effect the passage into the aqueous phase and to obtain a dispersed polyamide-amic acid; the grinding reaction is maintained for 2 hours to obtain an intermediate mixture. The properties of the intermediate mixture thus obtained are as follows: theoretical solids content: 9.5% measured solids content: 9.0% This is a honey-colored translucent product, viscous viscosity (in cross-section) 4 according to DIN EN ISO 2433 / ASTM D5125): 140 sec. The colloidal silica dispersion with a size of about 40 to 200 nm is introduced into the intermediate mixture at room temperature in order to obtain the aqueous mixture. semi-finished.
[0035] The properties of the aqueous semi-finished mixture thus obtained are as follows: theoretical solids content: 11.3%, dry extract measured in the solution: 11.0%, this is a translucent product of honey color, viscous, 25% viscosity (in section 4 according to DIN EN ISO 2433 / ASTM D5125): 150 sec, the silica content is 23% by mass relative to the polyamide-amic acid.
[0036] Subsequently, from the aqueous semi-finished mixture, an aqueous tackifier composition comprising the following compounds is produced: - 60% by weight PTFE dispersion in water: 30.5 g 5 - dispersion of carbon black at 25% by weight in water 3.5 g - aqueous semi-finished mixture above 50.0 g - nonionic surfactant system at 12.5% solids content. 5.1 g. 1.4 g - - demineralised water -. 9.5 g Total: 100.0 g This aqueous tackifier composition has the following characteristics. the content of fluororesin in the dry primer composition is of the order of 71.9% by weight relative to the total dry weight of the composition, the level of polyamide-amic acid in the dry primary composition is of the order of 17.1% by weight relative to the total dry weight of the composition, the content of silica in the composition is 23/77 by weight relative to the dry weight of polyamide-amic acid, The theoretical solids content is 25.5%. The viscosity (in section 2.5 according to DIN EN ISO 2433 / ASTM D5125) is 65 sec. This aqueous primer composition is spray-coated in a thin layer on an aluminum support in the form of a cap (preformed support) previously subjected to a surface treatment. The performances obtained are as follows: The implementation of the thin layer of primer in a three-layer coating system (primer layer as described above + first layer of finish without PAI resin and PTFE-based dry applied on dry + PTFE-based topcoat) and sintered under standard conditions (11 minutes at 430 ° C) gives ratings of 3 or 4 to the three cycles of the test. adhesion. A corrosion test of the coating obtained, made by 24 hours of contact with salt water at 10% and boiling, results in 5 points of corrosion. This result is non-compliant. The primer primer layer comprising a colloidal silica dispersion is analyzed by TEM. FIG. 2, which is a TEM image of a section of the primer layer thus formed, shows agglomerates of fillers over the entire thickness of the film, of circular or oval shape, and of equivalent dimensions over the entire thickness of the film (agglomerates length between about 0.5 μm and about 3 μm).
权利要求:
Claims (16)
[0001]
REVENDICATIONS1. A non-stick coating primer composition comprising: - a polyimide resin and / or a polyamide-imide resin, - a metal or silicon alkoxylate - a coupling agent capable of coupling the polyimide resin and / or the polyamide-imide resin and the alkoxysilane and / or the metal alkoxylate, and - a polar aprotic solvent.
[0002]
2. Composition according to claim 1, in which the alkoxysilane is chosen from methyltrimethoxysilane (MTMS), tetramethoxysilane (TMOS), tetraethoxysilane (TEOS), tetrapropoxysilane, methyltriethoxysilane (MTES), dimethyldimethoxysilane, phenyltriethoxysilane and their derivatives. mixtures.
[0003]
3. Composition according to any one of the preceding claims, in which the total relative content by dry weight of the coupling agent relative to the polyimide resin and / or the polyamide-imide resin is between 2 and 20% in said primary composition.
[0004]
4. Composition according to any one of the preceding claims, wherein the coupling agent is selected from silazanes, silane derivatives and mixtures thereof.
[0005]
5. Composition according to any one of the preceding claims, wherein the polar aprotic solvent is present in a proportion of 1 to 70% by weight relative to the total weight of the composition. 3037965 29
[0006]
6. Composition according to any one of the preceding claims, characterized in that it is free of fluorocarbon resin. 5
[0007]
7. A non-stick coating hybrid primer composition obtained from the primer composition as defined in any one of claims 1 to 6, comprising a polyimide resin matrix and / or polyamide-imide resin in which are dispersed silica domains having a size of less than 200 nm, in a polar aprotic solvent.
[0008]
The hybrid primer composition according to claim 7, wherein the relative dry weight content of the silica domains with respect to the polyimide resin matrix and / or polyamide-imide resin is between 10 and 25% in said composition. of hybrid primary. 20
[0009]
9. Hybrid primer composition according to any one of claims 7 to 8, wherein the polar aprotic solvent is present in a proportion of 1 to 70% by weight relative to the total weight of the composition. 25
[0010]
10. Hybrid primer composition according to any one of claims 7 to 9, characterized in that it is free of fluorocarbon resin.
[0011]
11. A non-stick coating comprising at least one layer of the non-stick coating hybrid primer composition of any one of claims 7 to 10.
[0012]
A process for preparing a release coating primer composition according to any one of claims 1 to 6 or a non-stick coating primer composition according to any one of claims 7 to 10, the process comprising the steps of: a) introducing the coupling agent into a solution comprising the polyimide resin and / or the polyamide-imide resin and the polar aprotic solvent; and b) adding in alkaline medium the metal alkoxylate or silicon, and water to the mixture of step a). 10
[0013]
A process for preparing a non-stick coating hybrid primer composition according to any one of claims 7 to 10, the process comprising the following steps: a) introducing the coupling agent into a solution comprising the resin polyimide and / or the polyamide-imide resin and the polar aprotic solvent; and b) adding the metal alkoxylate or prehydrolysed silicon to the mixture of step a). 20
[0014]
The process according to claim 13 for preparing a non-stick coating hybrid primer composition, further comprising a step c) of hydrolyzing the alkoxylate to obtain the pre-hydrolyzed alkoxylate, step c) hydrolysis being carried out before step b) and comprising: - hydrolysis in basic medium of the alkoxylate in a mixture of water and alcohol, or - hydrolysis in basic medium of the alkoxylate in a mixture of water and aprotic polar solvent.
[0015]
A method of manufacturing an article comprising a release liner according to claim 11, the method comprising the following steps: A) providing a backing having two opposing faces; B) applying to at least one side of said support - at least one layer of the non-stick coating hybrid primer composition according to any one of claims 7 to 10, or - at least one layer of a non-stick coating hybrid primer composition obtained according to any one of claims 13 to 14; C) firing the assembly at a temperature between 390 ° C and 430 ° C.
[0016]
16. Article obtainable by the process as defined in claim 15.
类似技术:
公开号 | 公开日 | 专利标题
EP3313797B1|2019-03-20|Non-stick coating primer compositions and processes for the preparation thereof
JP5931902B2|2016-06-08|Metal oxide nanofillers, their synthesis, and their use in fluororesin non-stick coatings
EP2334445B1|2015-11-11|Cooking item comprising a non-stick coating with improved properties of adhesion to the substrate
EP2728040B1|2019-11-27|Ceramic coating with improved scratch resistance and heat conduction properties
EP3158018B1|2020-11-18|Aqueous semi-finished and primary non-stick coating compositions comprising heterocyclic polymers
EP2139964A2|2010-01-06|Nonstick coating with improved hydrophobic properties
WO2006000685A1|2006-01-05|Non-stick coating with improved resistance to scratching and culinary item provided with said coating
EP3082527B1|2020-11-04|Aqueous compositions for primary anti-adhesive coating and preparation method thereof
FR2989379A1|2013-10-18|PRIMARY COMPOSITIONS OF ANTI-ADHESIVE COATINGS AND PROCESS FOR THEIR PREPARATION
FR3022835A1|2016-01-01|CULINARY ARTICLE WITH ANTI-ADHESIVE COATING COMPRISING A HOT-MOBILE SURFACE
EP3324798B1|2020-02-05|Cooking vessel with a layer comprising fluorocarbon resin and rare earth oxide and method of making
WO2013030503A2|2013-03-07|Utensil comprising a non-stick coating having improved properties of adhesion to the support
US10100199B2|2018-10-16|Methylsilyl derivatised silica particles, colloids, methods for manufacture and kits comprising the same
EP3914652A1|2021-12-01|Induction-compatible sol-gel coating
同族专利:
公开号 | 公开日
BR112017026571A2|2018-08-14|
US10752783B2|2020-08-25|
WO2016207563A1|2016-12-29|
FR3037965B1|2017-07-14|
CN107810245B|2020-10-20|
EP3313797A1|2018-05-02|
EP3313797B1|2019-03-20|
JP6758331B2|2020-09-23|
KR20180022819A|2018-03-06|
TR201905384T4|2019-05-21|
ES2720061T3|2019-07-17|
US20180086919A1|2018-03-29|
CN107810245A|2018-03-16|
JP2018524445A|2018-08-30|
引用文献:
公开号 | 申请日 | 公开日 | 申请人 | 专利标题
FR2625450A1|1988-01-05|1989-07-07|Corning Glass Works|ARTICLE HAVING AN ANTI-ADHERENT COATING HAVING IMPROVED SUBSTRATE ADHESION AND DURABILITY, ITS MANUFACTURE AND COMPOSITION IMPLEMENTED|
EP0386379A1|1989-03-08|1990-09-12|Corning Incorporated|Article provided with a non-stick coating, with improved adhesion to the substrate and durability, its manufacturing process and composition used|
US20050245715A1|2004-04-30|2005-11-03|Eternal Chemical Co., Ltd.|Precursor solution for polyimide/silica composite material, its manufacture method, and polymide/silica composite material having low volume shrinkage|
FR2915205A1|2007-04-18|2008-10-24|Seb Sa|ANTI-ADHESIVE COATING WITH IMPROVED HYDROPHOBIC PROPERTIES|
WO2005073282A1|2004-01-30|2005-08-11|Mitsui Chemicals, Inc.|Novel polymers and uses thereof|
KR100977411B1|2008-04-23|2010-08-24|한국전기연구원|Manufacturing Method of Polyamideimide/silica hybrid material for coating electrical wire and the material, electrical wire|
KR101543478B1|2010-12-31|2015-08-10|코오롱인더스트리 주식회사|Transparent Polyimide film and Method for Preparing the Same|
CN102220085B|2011-05-09|2013-04-17|东华大学|Polyimide coating with high-temperature resistance and preparation method thereof|JP6883429B2|2014-05-20|2021-06-09|ピーピージー・インダストリーズ・オハイオ・インコーポレイテッドPPG Industries Ohio,Inc.|Sol-gel compositions with improved hardness and impact resistance, methods of forming coatings and coated articles|
US10508175B2|2015-03-27|2019-12-17|Samsung Electronics Co., Ltd.|Composition and polyamideimide composite and polyamideimide film and electronic device|
US10633556B2|2017-12-28|2020-04-28|Flora Coatings Llc|Method of producing ambient curing sprayable transparent smart quasi-ceramic coating|
WO2020001399A1|2018-06-24|2020-01-02|Nano And Advanced Materials Institute Limited|Multi-layered, food-safe and non-stick coating|
CN112724825A|2020-12-24|2021-04-30|湖北金天叶科技有限公司|Food-grade non-stick coating for tobacco machinery and preparation method thereof|
法律状态:
2016-07-08| PLFP| Fee payment|Year of fee payment: 2 |
2016-12-30| PLSC| Search report ready|Effective date: 20161230 |
2017-06-30| PLFP| Fee payment|Year of fee payment: 3 |
2018-06-27| PLFP| Fee payment|Year of fee payment: 4 |
2019-07-01| PLFP| Fee payment|Year of fee payment: 5 |
2020-04-24| CA| Change of address|Effective date: 20200316 |
2021-03-12| ST| Notification of lapse|Effective date: 20210205 |
优先权:
申请号 | 申请日 | 专利标题
FR1555826A|FR3037965B1|2015-06-24|2015-06-24|ANTI-ADHESIVE COATING PRIMARY COMPOSITIONS AND METHODS OF PREPARING THE SAME|FR1555826A| FR3037965B1|2015-06-24|2015-06-24|ANTI-ADHESIVE COATING PRIMARY COMPOSITIONS AND METHODS OF PREPARING THE SAME|
JP2017567193A| JP6758331B2|2015-06-24|2016-06-23|Anti-adhesion coating primer compositions and methods for their preparation|
KR1020187001778A| KR20180022819A|2015-06-24|2016-06-23|Non-stick coating primer composition and method of making same|
PCT/FR2016/051552| WO2016207563A1|2015-06-24|2016-06-23|Non-stick coating primer compositions and processes for the preparation thereof|
EP16741099.2A| EP3313797B1|2015-06-24|2016-06-23|Non-stick coating primer compositions and processes for the preparation thereof|
ES16741099T| ES2720061T3|2015-06-24|2016-06-23|Primer compositions for non-stick coating and their preparation procedures|
TR2019/05384T| TR201905384T4|2015-06-24|2016-06-23|Anti-stick coating primer compositions and methods for their preparation.|
CN201680036694.1A| CN107810245B|2015-06-24|2016-06-23|Non-stick coating primer composition and preparation method thereof|
BR112017026571A| BR112017026571A2|2015-06-24|2016-06-23|Nonstick Coating Primer Compositions and Method for Their Preparation|
US15/567,417| US10752783B2|2015-06-24|2016-06-23|Non-stick coating primer compositions and processes for the preparation thereof|
[返回顶部]