专利摘要:
Hydrocarbon polymer comprising two dithiocyclocarbonate end groups of formula (1) below, process for the preparation and use: in which F1 is: and F2 is:
公开号:FR3036399A1
申请号:FR1554501
申请日:2015-05-20
公开日:2016-11-25
发明作者:Stephane Fouquay;Guillaume Michaud;Frederic Simon;Jean-Francois Carpentier;Sophie Guillaume;Elise Vanbiervliet
申请人:Centre National de la Recherche Scientifique CNRS;Universite de Rennes 1;Bostik SA;
IPC主号:
专利说明:

[0001] The present invention relates to hydrocarbon polymers comprising two terminal groups (2-thione-1,3-oxathiolan-4-yl). ) alkyloxycarbonyl (also referred to herein as "dithiocyclocarbonate" terminated hydrocarbon polymers), process for their preparation and their use in the manufacture of coating compositions, putties or adhesives.
[0002] It is known to use polyurethanes to make various coating compositions, mastics or adhesives. These compositions may be in the form of one-component or two-component compositions. In the latter case, the reagents necessary for the synthesis of the polyurethane are stored separately, optionally in the presence of other ingredients (additives), and are intended to be mixed before use of the composition, to synthesize the polyurethane at the last moment. . The synthesis of polyurethanes is traditionally done by reaction of a diisocyanate with a diol.
[0003] Now diisocyanates are toxic compounds as such, and are generally obtained from phosgene, itself very toxic by inhalation or by contact. The manufacturing process used in the industry generally involves the reaction of an amine with an excess of phosgene to form an isocyanate.
[0004] In addition, polyisocyanates are very sensitive compounds in the presence of atmospheric moisture and require taking appropriate measures to prevent their premature crosslinking, and therefore their loss of reactivity, during handling and storage (anhydrous conditions).
[0005] The search for alternatives to the synthesis of polyurethanes, without using isocyanate (or NIPU for "non-Isocyanate PolyUrethane" in English, ie "polyurethane without isocyanate"), therefore represents a major challenge.
[0006] 3036399 2 This research has been studied extensively. The most studied approaches concern the use of polymers capable of reacting with amines or oligomers of amines to form polyurethanes or derivatives structurally close to polyurethanes, such as poly (thio) urethanes, which will be generically designated in the present application by "polyurethane polymers". The patent application WO 2014/091173 in the name of Bostik and the CNRS describes hydrocarbon polymers comprising two terminal (2-oxo-1,3-dioxolan-4-yl) terminated groups which can be obtained by polymerization by means of ring opening by metathesis from at least one cyclic cycloolefin, at least one noncyclic unsaturated chain transfer agent comprising a terminal group (2-oxo-1,3-dioxolan-4-yl), and at least one metathesis catalyst. These polymers can then react with a (poly) amine to form hydroxyl-functional polyurethanes without isocyanates that can be used to formulate coating, putty or adhesive compositions. However, this reaction is relatively long and remains to be improved. Example 4 of patent application WO 2014/091173 discloses, in particular, the reaction of an unsaturated polyolefin comprising two (2-oxo-1,3-dioxolan-4-yl) methyloxycarbonyl end groups with a primary diamine of the following type: polyether diamine, used in stoichiometric proportions, to form a polyurethane that can be formulated as a two-component adhesive composition. The duration of this reaction is 12 hours at 80 ° C. The patent application WO 2005/016908 of HENKEL describes the synthesis of hydroxyl dithiocyclocarbonate (DTC-OH) 5-membered: OH (DTC-OH) 3036399 3 and its various uses to form inter alia, synthons (thio) urethanes possessing thiols and hydroxyl groups, intended for the manufacture of adhesives, surface coating or mastics: These synthons are obtained without the use of isocyanate, by reaction of (DTC-OH) with a diamine. They can then be crosslinked on themselves in the presence of oxygen and a crosslinking catalyst to reach molar masses greater than 500 g / mol. The poly (thio) urethanes obtained are different from those of the present invention.
[0007] The patent application WO 2005/016908 also discloses the use of (DTC-OH) to prepare conventional polyurethanes having two terminal (2-thione-1,3-oxathiolan-4-yl) methyloxycarbonyl groups (DTC-OH). -Polyurethane) and low molar masses (less than 2700 g / mol), but their manufacture uses isocyanates. It is an object of the present invention to provide novel polyurethane polymer synthesis intermediates for use in the manufacture of coating, putty or adhesive compositions, and to overcome in whole or in part the disadvantages of the prior art. In particular, the present invention aims to provide novel intermediates whose synthesis does not use isocyanates and are capable of reacting more quickly with a (poly) amine, compared to hydrocarbon polymers with terminations (2-oxo -1,3-dioxolan-4-yl) of the application WO 2014/091173.
[0008] Thus, the present invention relates to a hydrocarbon polymer comprising two dithiocyclocarbonate end groups, said hydrocarbon polymer having the following formula (I): R 1 R 5 R 6 R 3 R 4 R 7 R 8 R 13 aF 2 R 3 R 4 R 7 8 R 1 R 5 R 9 R 9 R 12 In which: each carbon-carbon bond of the noted chain is a double bond or a single bond, in accordance with the valence rules of organic chemistry; the groups R1, R2, R3, R4, R5, R6, R7 and R8, which are identical or different, are chosen from a hydrogen atom, a halogen atom, an alkyl group, a heteroalkyl group, an alkoxycarbonyl group or a heteroalkoxycarbonyl group, at least one, and preferably one, of the groups R1 to R8 being part of the same hydrocarbon or heterocycle ring, saturated or unsaturated, with at least one other, and preferably with another, groups R1 to R8, according to the valence rules of organic chemistry; at least one of the pairs (R1, R2), (R3, R4), (R5, R6) and (R7, R8) may be an oxo group; x and y, which are identical or different, are integers in a range from 0 to 5, preferably from 0 to 2, even more preferably x is equal to 1 and y is equal to 1, the sum x + y being preferably in a range from 0 to 4 and even more preferably from 0 to 2; the groups R 9, R 10, R 11 and R 12, which may be identical or different, are chosen from a hydrogen atom, a halogen atom, a hydrogen atom and a hydrogen atom; alkyl group, a heteroalkyl group, an alkoxycarbonyl group or a heteroalkoxycarbonyl group, at least one of the groups R9 to R12 being part of the same hydrocarbon or heterocycle ring, saturated or unsaturated, with at least one of the groups R9 to R12, according to the valence rules of organic chemistry; the group R13 is CH2, O, S, C (= O) or NR0, Ro being an alkyl group, preferably linear, comprising from 1 to 22, preferably from 1 to 14, carbon atoms; and n is an integer greater than or equal to 2 and m is an integer greater than or equal to 0, the molar ratio m / n ranging from 0/100 to 90/10, and preferably ranging from 25/100 to 75 / 25; n and m being further such that the number-average molar mass Mn of the hydrocarbon polymer of formula (1) ranges from 500 to 50,000 g / mol, preferably from 600 to 45,000 g / mol, more preferably from 700 to 40 000 g / mol, in particular from 4000 to 30000 g / mol, and more preferably from 8000 to 20 000 g / mol, and the polymolecularity (PDI) of the hydrocarbon polymer of formula (1) ranging from 1.0 to 3.0 preferably from 1.0 to 2.0; F1 is represented by the following formula: and F2 is represented by the following formula: wherein: A is C1-C9 alkylene and preferably methylene, Z is such that the divalent group -AZ-sus- described is the group -AC (= O) O- or -A-OC (= 0) - and preferably -AC (= O) 0-; 3036399 6 p1 and p2, which are identical or different, each represent an integer equal to at 0, 1, 2 or 3 and preferably pl = p2 = 0. Of course, all formulas are given here in accordance with the valence rules of organic chemistry.
[0009] The main chain of the polymer of formula (1) thus comprises one or two types of repeating units, a first type of repetition unit repeated n times and a second type of repetition unit, optional, repeated m times. As it appears above, the terminal groups F1 and F2 are generally symmetrical with respect to the main chain, that is to say that they correspond substantially, with the exception of the indices p1 and p2. According to a first embodiment in which F1 and F2 are identical or different: Z is such that F1 and F2 are: ## STR2 ## and p2 are integers ranging from 0 to 3, preferably p1 or p2 = 0, and more preferably p = p2 = 0, - A is a C1 to C9 alkylene group, preferably a methylene group According to a second embodiment where Fl and F2 are the same or different: - Z is such that F 1 and F 2 are integers ranging from 1 to 3, preferably p 1 or p 2 = 1, and more preferably p 1 = p 2 = 1, 25 - A is an alkylene group C1 to C9, preferably a methylene group, According to another preferred embodiment of the invention, x is 1 and y is 1.
[0010] In the present application, in the absence of any indication to the contrary: - "Terminal group" means a group located at the end of the chain (or end of the main chain) of a substantially linear polymer. The linear polymer according to the invention comprises a main chain, both ends of which are the terminal groups of the polymer according to the invention. "Dithiocyclocarbonate group" means a group F1 or F2 as described above. "Alkyl group" means a linear or branched hydrocarbon compound, cyclic (including polycyclic) or acyclic, and comprising, unless otherwise indicated generally from 1 to 22 carbon atoms. Such an alkyl group most often comprises from 1 to 14, preferably from 1 to 8, carbon atoms. "Heteroalkyl" means according to the invention an alkyl group in which at least one of the carbon atoms is substituted by a heteroatom selected from the group formed by O and S. - "Alkoxycarbonyl group" means a linear or branched, saturated or partially unsaturated (monovalent) alkyl group comprising from 1 to 22, preferably from 1 to 14, carbon atoms, as well as a divalent 20 C00- group. "Heteroalkoxycarbonyl" means, according to the invention, an alkoxycarbonyl group in which at least one of the carbon atoms is substituted by a heteroatom chosen from the group formed by O and S. - By "halogen atom", iodo, chloro, bromo or fluoro, preferably chloro. "Hydrocarbon ring" means a cyclic (including polycyclic) hydrocarbon compound, saturated or unsaturated, which may contain from 3 to 22 carbon atoms and optionally at least one C = O group. "Heterocycle" means a hydrocarbon ring which may comprise an atom other than carbon in the ring chain, such as, for example, oxygen, sulfur or the NRO group as defined above, namely an alkyl group. , preferably linear, comprising from 1 to 22, preferably from 1 to 14, carbon atoms. By "at least one of the groups R 1 to R 8 that may form part of the same hydrocarbon or heterocycle ring, saturated or unsaturated, with at least one other of the groups R 1 to R 8, according to the valence rules of organic chemistry" according to the invention is meant that these groups, whether or not they are borne by the same carbon, are bonded together by a hydrocarbon chain (which may include the carbon atoms of the main chain of the polymer of formula (1)) optionally comprising at least one group, a C = O group and / or at least one heteroatom such as S or O, so as to form a hydrocarbon ring or a heterocycle, as defined above.
[0011] In some cases, these groups may designate chemical bonds. For example, when one of the groups R 3 or R 4 with one of the groups R 5 or R 6 together with the carbon atoms of the main chain of the polymer of formula (1) supporting them, an epoxide ring, these designate a bond connecting the carbon atom supporting them to the oxygen atom of the epoxy group. These definitions are also applicable to groups R13 to R16. - By "pair (R1, R2) may be an oxo group" means according to R1. According to the invention, the pair (R 1, R 2) is such that it is , where C is the carbon atom that supports the two groups forming the pair (R 1, R 2).
[0012] This is also applicable to the pairs (R3, R4), (R5, R6) and (R7, R8). The polymolecularity PDI (or DM dispersity) is defined as the Mw / Mn ratio, that is to say the ratio of the weight average molecular weight of the polymer to the number average molar mass of said polymer. The two average molar masses Mn and Mw are measured according to the invention by Size Exclusion Chromatography (SEC), usually with PEG (PolyEthyleneGlycol) or PS (PolyStyrene) calibration, PS preference. The measurements are generally made in a solvent for solubilizing the sample to be analyzed. The various polymers of the invention can be solubilized for example in dichloromethane (DCM) or tetrahydrofuran (THF).
[0013] Preferably, the groups R5 to R8 are each a hydrogen atom. More preferably, the groups R 1 to R 8 are hydrogen atoms. If pl = 0 or p2 = 0, then there is no divalent group (CH2) 0 or 5 (CH2) p2 in the formula Fl or F2 and - (CH2) 0- becomes a single bond "-" or - (CH2) p2- becomes a single bond "-". When the index m, n or n-1, x or y, which applies to a set of two square brackets equals zero, this means that there is no group between the 0s means "brackets to which this index applies. Thus, 10 (single bond), and ° signifies "" (double bond). Each of the double bonds of the polymer of formula (1) is oriented geometrically cis or trans, and is preferably of cis orientation. The geometric isomers of the polymer of formula (1) are generally present in variable proportions, with most often a majority of cis (Z) and preferably all the double bonds are oriented cis (Z). It is also possible according to the invention to obtain only one of the geometric isomers, according to the reaction conditions and in particular according to the nature of the catalyst used. The polymers of formula (1) according to the invention may be solid polymers or liquid (very fluid) polymers at ambient temperature (approximately 23 ° C.). Preferably, they are liquid polymers at 23 ° C, that is to say having a viscosity ranging from 1 to 500,000 mPa.s at 23 ° C. In general, the viscosity can be measured in a manner well known to those skilled in the art. In particular, the viscosity can be measured with a Brookfield viscometer, by selecting the needle and the speed of the module appropriately according to the viscosity range to be measured. According to a variant of the invention, when m is equal to 0, the polymer of formula (1) can be represented by the following formula (2): ## STR2 ## in which: x, y, n, F1, F2 , R1 to R8 are as described in any one of the preceding paragraphs.
[0014] Formula (2) illustrates the case where the main chain of the polymer of formula (1) has only one type of repeating unit, repeated n times. When according to a preferred variant of this variant, m is equal to 0 and R1 to R8 denote hydrogen atoms, with at least one of the pairs (R1, R2), (R3, R4), (R5, R6) and / or (R7, R8) may be an oxo group, the polymer of formula (2) is solid at room temperature. According to another variant of the invention, preferably: - m is different from zero and / or - at least one of the groups R1 to R8 and / or R9 to R12 comprises an alkyl group (and therefore denotes a different group of a hydrogen atom and a halogen atom) or - at least one of the groups R1 to R8 is part of the same hydrocarbon or heterocycle ring, saturated or unsaturated, with at least one other group R1 at R8, according to the valence rules of organic chemistry, with - at least one of the pairs (R1, R2), (R3, R4), (R5, R6) and / or (R7, R8) possibly denoting an oxo group .
[0015] In this case, the polymer of formula (1) is liquid at room temperature. The invention also relates to dithiocyclocarbonate-terminated hydrocarbon polymers of formula (1H) and (2H) wherein the main chains of the polymers of formulas (1) and (2) are saturated, i.e. have only saturated bonds: F1 R2 R5 R6 R3 R4 R7 R8 R13 F2 R3 R4 R7 n- R9 R12 R10 R1 (1H) R1 R2 R5 RF R4 R7 lR8 F2 (2H) in which: x, y, n, m, F1, F2, R1 to R13 are as described in any one of the preceding paragraphs. The polymers of formula (1H) and (2H) can be prepared by hydrogenation of the unsaturated diepoxidized polymers of formulas (1E) and (2E) defined below, and then reaction of the polymers thus hydrogenated with carbon disulphide (CS2): F2e (1E) F F 15 (2E) in which: R 1 to R 8, x, y, n of formulas (1E) and (2E) have the same meanings as given previously, - Fl e is represented by the formula following: (CH 2 5 - F 2e is represented by the following formula: (C H 9) - A, Z, p 1 and p 2 of the formulas F 1 and F 2 e have the same meanings as given previously.
[0016] The invention also relates to a process for preparing at least one hydrocarbon polymer comprising two dithiocyclocarbonate end groups according to the invention, said process comprising at least: I) a metathesis ring opening polymerization step (or Opening Metathesis Polymerization "in the presence of: at least one metathesis catalyst, preferably a catalyst comprising ruthenium, even more preferably a" Grubbs "type catalyst, at least one agent Mono or di-epoxidized chain transfer agent (CTA) in the form of the following formula (C1) or (C2), respectively: Fie F2e (C1) - e (C2) in which: - Fl e is represented by the following formula: - and F2e is represented by the following formula: - A, Z, p1 and p2 of formulas F1 and F2e are as defined in any one of the preceding paragraphs, 5 - the bond - r- is a li a carbon-carbon single bond oriented geometrically on one side or the other with respect to the double bond (cis or trans) in formula (C2); - at least one compound of formula (A) below: (A) 10 in which: the groups R1, R2, R3, R4, R5, R6, R7 and R8, which are identical or different, are chosen from an atom of hydrogen, a halogen atom, an alkyl group, a heteroalkyl group, an alkoxycarbonyl group or a heteroalkoxycarbonyl group, at least one of the groups R1 to R8 being part of the same hydrocarbon or heterocycle ring, saturated or unsaturated with at least one other of the groups R1 to R8, according to the valence rules of the organic chemistry, and - at least one of the pairs (R1, R2), (R3, R4), (R5, R6) and (R7, R8) may be an oxo group; x and y are integers independently ranging from 0 to 5, preferably ranging from 0 to 2, even more preferably x is equal to 1 and y is equal to 1, the sum x + y preferably ranging from 0 at 4 and even more preferably from 0 to 2; And optionally at least one compound of formula (B): R 13 R 9 (B) in which: the groups R 9, R 10, R 11 and R 12, which are identical or different, are chosen from a hydrogen atom, a halogen atom, a heteroalkyl group, an alkoxycarbonyl group and a heteroalkoxycarbonyl group; at least one, and preferably one, of the groups R9 to R12 which may be part of the same ring or heterocycle which is saturated or unsaturated with at least one another, and preferably with another, R9 to R12 groups, according to the valence rules of organic chemistry; and - the group R13 is CH2, O, S, C (= O) or NR0, Ro being an alkyl group, preferably linear, having from 1 to 22, preferably from 1 to 14, carbon atoms; during a reaction time ranging from 2 to 24 hours and at a temperature ranging from 20 to 60 ° C; then II) a dithiocarbonation step of the polymer obtained in the preceding step by reaction with carbon disulphide (CS2) in the presence of a lithium halogen compound, such as lithium bromide, at a temperature ranging from 20 to 45 ° C until the hydrocarbon polymer comprising two dithiocyclocarbonate end groups according to the invention. When the hydrocarbon polymer comprising two dithiocyclocarbonate end groups according to the invention has a saturated main chain, as envisaged by formulas (1H) and (2H) defined above, the above preparation process comprises between steps I) and II), a step of selectively hydrogenating the double bonds of the polymer derived from step I) having two epoxy end groups and corresponding to the unsaturated diepoxidized polymer of formula (1E) or (2E). The selective hydrogenation of the polymer of formula (1E) or (2E) resulting from stage I) having two terminal epoxy groups, leading to the corresponding hydrogenated polymer of formula (1H) or (2H) respectively, can be carried out according to the process described in WO 9,535,290 of EASTMAN CHEMICAL. Metathesis ring opening polymerization (or "Ring-Opening Metathesis Polymerization") is a reaction well known to those skilled in the art.
[0017] The time and temperature for the polymerization reaction described in step I) generally depend on the reaction conditions and in particular the catalytic loading rate. The skilled person is able to adapt them depending on the circumstances. In the present application, the metathesis ring opening polymerization reaction is carried out in the presence of a mono-functional CTA of formula (C1) or of a difunctional CTA of formula (C2). The CTA of formula (C1) is said to be monofunctional when it comprises an epoxide group. The CTA of formula (C2) is said to be difunctional when it comprises two epoxide groups, which may be identical or different. According to a first embodiment of the preparation process according to the invention (called "monofunctional CTA route"), the CTA used is of formula (C1).
[0018] According to a first variant of the preparation process according to the invention according to the "monofunctional CTA route", the CTA of formula (C1) corresponds to the following formula (C1 a): c (C1 a) in which: an integer ranging from 0 to 3, and preferably equal to 0, 3036399 16 - A is a C1 to C9 alkylene group, preferably a methylene group. The compound of formula (C1 a) can be obtained according to scheme (1) below, in which p1 and A retain the meanings given above, and following the procedure described in patent application CN 102,757,409, : () (C1 a) Scheme (1) According to a second variant of the preparation process according to the invention according to the "monofunctional CTA route", the CTA of formula (C1) corresponds to the following formula (C1b): CH 2) P, o (C1 b) in which: - p1 is an integer from 1 to 3, and preferably equal to 1, 15 - A is a C1 to C9 alkylene group, preferably a methylene group. The compound of formula (C1b) can be obtained by transesterification according to scheme (2) below, in which p1 and A retain the same meanings as given above, and Me denotes the methyl group, and following one of the procedures described in the publication entitled "Kinetics of Epoxidation of Alkyl Esters of Undecylenic Acid: 3036399 17 Comparison of Traditional Routes Vs. Ishii-Venturello Chemistry "by GD Yadav and DV Satoskar (JAOCS, Vol.74, no.4 (1997), pages 397-407), especially those described in Tables 9 and 10: OH rie (C1b) 5 Scheme (2) The epoxy alkanoates used in this reaction can be synthesized following the procedures described in US Pat. Nos. 3,448,125 to Rohm & Haas and 0,208,272 to Montedison.
[0019] According to a second embodiment of the preparation method according to the invention (called "difunctional CTA route"), the CTA used is of formula (C2). According to a first variant of the preparation process according to the invention according to the "CTA difunctional route", the CTA of formula (C2) corresponds to the following formula (C2a): (CH 0 (C2a) in which: "has the same meaning as given above; 3036399 18 - pl and p2 are integers ranging from 0 to 3, preferably p1 or p2 = 0, and more preferably pl = p2 = 0, - A is a C1-alkylene group; at C9, preferably a methylene group.
[0020] The compound of formula (C2a) can be obtained according to scheme (3) below, corresponding to an original variant of scheme (1) in which p1, p2, A and retain the same meanings as previously given. Na0 (CH) p (CH2) p, ONa Cl0 (C2a) Scheme (3) According to a second variant of the preparation process according to the invention according to the "CTA difunctional route", the CTA of formula (C2) corresponds to the following formula (C2b): o; CH (C2b) in which: - - r 'r has the same meaning as previously given; p1 and p2 are integers ranging from 1 to 3, preferably p1 or p2 = 1, and more preferably p1 = p2 = 1, A is a C1 to C9 alkylene group, preferably a methylene group. The compound of formula (C2b) can be obtained according to scheme (4) below, corresponding to an original variant of scheme (2) in which p1, p2, A, etc, retain the same meanings as previously given, and Me designates the methyl group: (CH 2; I p rie HO 0 (C2b) Scheme (4) The molar ratio of CTA of formula (C1) to the compound of formula (A), or the sum of compounds of formulas (A) and (B) if the compound of formula (B) is present, is from 1.10-3 to 1.0 and preferably from 1.10-2 to 0.250 The molar ratio of CTA of formula (C2) to the compound of formula (A), or on the sum of the compounds of formulas (A) and (B) if the compound of formula (B) is present, ranges from 0.5 × 10 -3 to 0.5 and preferably from 0.5 × 10 -3 to The compounds of formula (A) generally comprise from 6 to 30, preferably from 6 to 22, carbon atoms Preferably, the compounds of formula (A) are such that x = y = 1.
[0021] More preferably, the cyclic compounds of formula (A) according to the invention are chosen from the group formed by cycloheptene, cyclooctene, cyclononene, cyclodecene, cycloundecene, cyclododecene and 1,5-cyclooctadiene. cyclononadiene, 1,5,9-cyclodecatriene, 5-alkyl-cyclooctenes including C1-C22 alkyl and preferably C1-C14 alkyl, and mixtures thereof.
[0022] Cyclooctene (COE), and 5-alkyl-cyclooctene R where R is an alkyl group comprising from 1 to 22, preferably 1 to 14, carbon atoms, are preferred according to the invention; cyclooctene being very particularly preferred. For example, R is n-hexyl. The compounds of formula (B) generally comprise from 6 to 30, preferably from 6 to 22, carbon atoms. More preferably, the cyclic compounds of formula (B) are chosen from the group formed by norbornene (NBN), dicyclopentadiene and 7-oxanorbornene which are respectively of the following formulas: The cyclic compounds of formula (B) may also be chosen from the group formed by the compounds of the following formulas: embedded image in which: R is an alkyl group comprising from 1 to 22, preferably 1 to 14, carbon atoms. For example, R is n-hexyl. Cyclic compounds of formula (B) may also be selected from the group consisting of adducts (or adducts in English) from the Diels-Alder reaction using cyclopentadiene or furan as starting material, as well as compounds derived from norbornene as described in WO 2001/04173 (such as: isobornyl norbornene carboxylate, phenyl norbornene carboxylate, norbornene ethylhexyl carboxylate, phenoxyethyl norbornene carboxylate and alkyl norbornene dicarboxymide, the alkyl comprising the most often from 3 to 8 carbon atoms) and those described in WO 2011/038057 (norbornene dicarboxylic anhydrides and optionally 7-oxanorbornene dicarboxylic anhydrides). The metathesis-ring-opening polymerization stage I) is most often carried out in the presence of at least one solvent, generally chosen from the group formed by the aqueous or organic solvents typically used in the polymerization reactions and which are inert under the conditions of the above-described polymerization. The dithiocarbonation step II) and / or the optional hydrogenation step may be carried out in the same solvent as step I). In particular, when the same solvent is used, the dithiocyclocarbonate-terminated hydrocarbon polymer according to the invention can be generated by successively carrying out step I) and step II), without having to isolate the epoxy-terminated polymer. of formula (1E) or (2E) from step I) between the two steps.
[0023] Examples of solvents that can be used include aromatic hydrocarbons, chlorinated hydrocarbons, ethers, aliphatic hydrocarbons, alcohols, water or mixtures thereof. Preferably, the solvent is selected from the group consisting of benzene, toluene, para-xylene, methylene chloride, dichloroethane, dichlorobenzene, chlorobenzene, tetrahydrofuran, diethyl ether, pentane, and the like. hexane, heptane, methanol, ethanol, water or mixtures thereof. More preferably, the solvent is selected from the group consisting of benzene, toluene, para-xylene, methylene chloride, dichloroethane, dichlorobenzene, chlorobenzene, tetrahydrofuran, diethyl ether, pentane, and the like. hexane, heptane, methanol, ethanol, and mixtures thereof. More preferably, the solvent is toluene, heptane, or a mixture of toluene and methylene chloride. The solubility of the polymer formed during the polymerization reaction depends generally and mainly on the choice of solvent and the molar mass of the polymer obtained. It is also possible that the reaction is carried out without solvent. The metathesis catalyst, such as for example a "Grubbs" type catalyst, is generally a commercial product. The metathesis catalyst is most often a catalyst comprising at least one transition metal, such as ruthenium, most often in the form of complex. Preferably, the metathesis catalyst is selected from ruthenium complexes such as a ruthenium-carbene complex. More preferably, the metathesis catalyst is selected from the "Grubbs" type catalysts. The term "Grubbs type catalyst" is generally understood to mean, according to the invention, a Grubbs 1st or 2nd catalyst, but also any other type of Grubbs (ruthenium-carbene type) catalyst accessible to the person skilled in the art, such as by for example the substituted Grubbs catalysts described in US Pat. No. 5,849,851.
[0024] A 1st generation Grubbs catalyst is generally of formula (G1): P (Cy) 3 (G1), wherein: - Ph is phenyl - Cy is cyclohexyl, and - P (Cy) 3 is a tricyclohexylphosphine group. The IUPAC name of the catalyst (G1) is: benzylidenebis (tricyclohexylphosphine) dichlororuthenium (CAS number 172222-30-9).
[0025] A 2nd generation Grubbs catalyst is generally of formula (G2): wherein: Ph is phenyl, Cy is cyclohexyl, and P (Cy) 3 is tricyclohexylphosphine. The IUPAC name of the catalyst (G2) is: benzylidene [1,3-bis (2,4,6-trimethylphenyl) -2-imidazolidinylidene] dichloro (tricyclohexylphosphine) ruthenium (CAS number 246047-72-3).
[0026] Preferably, the catalyst is a 2nd generation Grubbs catalyst, as defined for example by the formula (G2). Generally, the carbon disulfide (C52) and the epoxy-terminated polymer from the previous step are used in a stoichiometric proportion, i.e. two moles of carbon disulfide are reacted with one mole of carbon. epoxy terminated polymer from step HC HC3 (G2), 3036399 24 above, so that all the epoxy functions of said is reacted with carbon disulfide. A slight variation with respect to the stoichiometries given above, in particular a slight defect of CS2, can be envisaged without any inconvenience. In the latter case, it can be envisaged to work, for example, with a molar ratio of the amount of CS 2 to the amount of epoxy-terminated polymer from the previous step ranging from 0.96 to 1. The invention also relates to a process for the preparation of poly (thio) urethane comprising the reaction of at least one dithiocyclocarbonate-terminated hydrocarbon polymer according to the invention, capable in particular of being obtained by the preparation method according to the invention, with at least one compound comprising at least one, preferably at least two, amine groups, for example chosen from monoamines, diamines, triamines and other polyamines; and the poly (thio) urethanes obtainable by this preparation process. By "poly (thio) urethane" is meant in the present application a polymer comprising at least two groups (thio) urethane, the definition is given below. By "(thio) urethane group" is meant herein an S-thiocarbamate group, especially having the formula -O (C = S) -NH-. The amine compounds that can be used according to the invention are preferably such that at least one amine group, preferably all the amine groups, are primary amine groups. These amino compounds can be oligomers. These oligomers generally have a number average molar mass of less than 2000 g / mol. The synthesis reaction of the poly (thio) urethane according to the invention can take place at a temperature below 100 ° C., or even at ambient temperature (that is to say about 23 ° C.) when the hydrocarbon polymer with dithiocyclocarbonate terminations used is liquid at 23 ° C.
[0027] It has been observed that under identical temperature conditions, and in the presence of the same amine compound, this synthesis reaction according to the invention was faster than that employing a hydrocarbon terminated polymer (2-oxo-1). , 3-dioxolan-4-yl) according to the application WO 2014/091173. The process of preparation described above can therefore advantageously be implemented in the form of a two-component composition.
[0028] Thus, the invention also relates to a two-component composition comprising: in a first compartment, at least one hydrocarbon polymer comprising two dithiocyclocarbonate end groups according to the invention, and in a second compartment, at least one amine compound as described previously. Preferably, the dithiocyclocarbonate-terminated hydrocarbon polymer (s) and amino compound (s) are used in amounts such that each of the dithiocyclocarbonate groups of the polymer (s) reacted with an amine group of a compound amine to form a (thio) urethane group. More preferably, the dithiocyclocarbonate-terminated hydrocarbon polymer (s) are reacted with one or more primary (poly) amine (s) in stoichiometric amounts, i.e. the molar ratio of The number of dithiocyclocarbonates groups on the number of primary amine groups is approximately equal to 1. The poly (thio) urethanes thus obtained, which are new, have been advantageously prepared without isocyanate. The poly (thio) urethane according to the invention also has SH pendant groups in the main chain of the polymer, unlike the polyurethanes of the prior art. As such, the poly (thio) urethane according to the invention may be more specifically designated by the term polymercapto (thio) urethane. Thanks to its SH functions, the polymer according to the invention can crosslink on itself, once in contact with air, which is particularly suitable for use thereof in the form of a two-component composition. Indeed, the SH groups are capable of reacting spontaneously with each other, in the presence of oxygen (even in the form of traces), to form SS disulfide bridges between the polymeric chains of poly (thio) urethane and thus to create a three-dimensional polymeric network. A representation of such a polymer network is given by way of example in FIG. 1 of the present application. The poly (thio) urethanes according to the invention thus have the advantage of being able to be formulated (that is to say with the possible addition of additives) in the form of particularly reactive two-component compositions, and to possess once crosslinked, particularly interesting mechanical properties, especially for the field of adhesives, sealants and surface coating.
[0029] The crosslinked poly (thio) urethanes according to the invention exhibit, in particular, cohesion values greater than 1.5 MPa (megapascal). Such cohesive values allow use as an adhesive, for example in the field of construction, transport or industry in general.
[0030] The mechanical properties, and in particular the cohesion values, of the crosslinked poly (thio) urethanes according to the invention can be measured in accordance with the standard ISO 527-1 or ASTM D 638-03, and in particular according to the protocol described hereinafter. after. The principle of measuring the tensile strength and tensile elongation of the tensile test-tested compositions is to stretch in a tensile machine, the moving jaw of which travels at a constant speed of 100 mm / min. a standard test specimen made of the crosslinked adhesive composition and to record, at the moment when the test piece breaks, the tensile stress applied (in MPa) and the elongation of the specimen (in%). The standard test piece is dumbbell-shaped, as shown in International Standard ISO 37. The narrow part of the dumbbell used has a length of 20 mm, a width of 4 mm and a thickness of 300 μm. To prepare the dumbbell, the adhesive composition was heated to 100 ° C and then extruded onto an A4 sheet of silicone paper in an amount sufficient to form a film having a thickness of 300 μm thereto. The film is left for 7 days at 23 ° C. and 50% relative humidity for crosslinking, then the dumbbell is obtained by simple cutting in the crosslinked film.
[0031] The invention will be better understood from the following examples. EXAMPLES The following examples illustrate the invention without limiting its scope. I - Examples 1 to 5: Synthesis of a Dithiocyclocarbonate Terminated Polymer According to the Invention The dithiocyclocarbonate-terminated hydrocarbon polymers of Examples 1 to 3 were obtained using the following steps: a synthesis step of s) cycloolefin (s) of formulas (A) and / or (B), 2- a step of synthesis of the transfer agent (CTA) of formula (C1) or (C2), 3-a polymerization step by ring opening by metathesis of cycloolefin of formula (A) and optionally of compound of formula (B) in the presence of a Grubbs catalyst and the transfer agent, step 1 being preferably optional when the cycloolefin ( s) formulas (A) and (B) are commercially available.
[0032] The metathesis ring opening polymerization reactions carried out in Examples 1 to 5 are represented by general schemes (5) and (6), respectively using a monofunctional CTA (C1) and a difunctional CTA (C2), and will be explained case by case in the examples. 3036399 (A) R5 28 (C1) (B) R13 R12 R11 Ff R1O F e R13 F1e R9 R12 R1O R11 CS2 F1 R1: 3 F1 R9 R12 R10 R11 Diagram (5) 3036399 29 (A) (B) (FIG. C2) R8 q Life laughs R1 k Diagram (6) In these diagrams (5) and (6): 5 - 1 equiv. means an equivalent and corresponds to the amount of metathesis catalyst used; DCM stands for dichloromethane; (A) and (B) are the cycloolefins corresponding to the formulas (A) and (B) respectively defined above; (C1) and (C2) are the transfer agents respectively corresponding to formulas (C1) and (C2) defined above; the bond is a single carbon-carbon bond oriented geometrically on one side or the other with respect to the double bond (cis or trans) for (C2); - G2 is the metathesis catalyst of formula (G2) as defined above; - F1 and F2 are identical and both correspond to the dithiocyclocarbonate-ester type group below: ## STR1 ## where: ## STR1 ## where: p = p1 or p2 and A are as defined above; 10 - Fl e and F2e are identical and correspond to Fl and F2, respectively, that is, that they both correspond to either the epoxy-ester type group below: o H2) p or to the type group epoxy ester below: ## STR3 ## in which: p = p1 or p2 and A are as previously defined; n is the number of moles of cycloolefin (s) of formula (A); m is the number; mole of cycloolefin (s) of formula (B), q is the number of moles of CTA of formula (C1), or (C2) The number of monomeric units in the polymer obtained at the end of the Polymerization reaction is equal to n + m.
[0033] In each of Examples 1 to 9 described below, the ROMP reaction lasts 24 hours at a temperature of 40 ° C. All polymerizations were performed in a similar manner. The only differences are in the nature and initial concentration of the chain transfer agent (s) (CTA) of type (C1) or (C2) used. The CTAs used in Examples 1 to 9 are the following: glycidyl acrylate (denoted CTA1) (CTA1) (which corresponds to a CTA of formula (C1) in which: p1 = 0, A is a methylene group; CH2-); diglycidyl fumarate (denoted CTA2) o (CTA2) (which corresponds to a CTA of formula (C2) in which: p1 = p2 = 0, A is a methylene -CH2- group); and two reaction possibilities (i and ii) exist, depending on whether the cycloolefin of formula (A) alone (Examples 1 to 3) is used, or whether the cycloolefins of formulas (A) and (B) are used. ) as a mixture (Examples 4 and 5). i) - Examples 1 to 3: Polymerization of the cycloolefins of formula (A) The cycloolefins of formula (A) used in Examples 1 to 5 are the following: 0 (COE) and c6H13 (5-hexyl-COE).
[0034] Cyclooctene (COE) is a commercial product of Sigma Aldrich. 5-n-hexyl-cyclooctene (5-hexyl-COE) can be synthesized from 5,6-epoxycyclooctene (5-Epoxy-COE) according to the route shown in reaction scheme (7) below, with the following yields indicated in parentheses: 12 h concentrated HCl O'C at 23 ° C.
[0035] (7) 5-Oxocyclooctene (5-O = COE, referenced 2 in scheme (5) above) was synthesized according to the procedure given in the publication of A. Diallo et al., Polymer Chemistry, Flight. 5, Issue 7, April 7, 2014, pages 25832591 (which referred to Hillmyer et al, Macromolecules, 1995, 28, pp. 63116316). The 5-hexyl-cyclooctene (5-hexyl-COE referenced in Scheme 15 (5) above) was synthesized according to the procedure given in the publication of A. Diallo et al., Polymer Chemistry, supra referred to Kobayashi et al., J. Am Chem Soc 2011, 133, pp. 5794-5797). The raw materials, reagents and solvents used for the synthesis of these cycloolefins of formula (A) are commercially available from Sigma Aldrich. In the following examples: The NMR spectra were recorded under AM-500 Bruker and AM-400 Brüker spectrometers at 25 ° C. in CDCl3. Chemical shifts were referenced to tetramethylsilane (TMS) using resonance (1H) or (13C) deuterated solvents. The number and weight average molecular weights (Mn and Mw) and the PDI polydispersity (Mw / Mn) of the polymers were determined by steric exclusion chromatography (SEC) in THF, with PS calibration using a Polymer instrument. Laboratories PL-GPC 50. The reactions were carried out, as a precaution, under anhydrous conditions (inert gas, dry solvent).
[0036] Example 1 Synthesis of a polymer comprising two [2-thione-1,3-oxathiolan-4-yl] methyl ester end groups from cyclooctene (COE) and glycidyl acrylate (CTA1) The reaction was implemented according to the following scheme (8), in a molar ratio m / n equal to 0/100 and according to the procedure described below: 1CTA Grubbs 2 "gener 40" C 15 Schéma (8) 3036399 34 Mode Procedure: The cycloolefin of formula (A) (108.00 mmol), hydroquinone (0.54 mmol) and dry CH 2 Cl 2 (50 ml) were mixed in a 1000 ml flask. The flask and its contents were then put under argon. CTA (10.80 mmol) of type (C1) was introduced into the flask by syringe. The flask was then immersed in an oil bath at 40 ° C. and then G2 catalyst (54.00 μmol) dissolved in CH 2 Cl 2 (20 ml) was immediately added via a cannula. 24 hours after the addition of the catalyst, the solution is concentrated by partially evaporating the CH 2 Cl 2 (up to the solubility limit of the polymer). The product is recovered after precipitation in methanol (15 mL), filtration and drying at 20 ° C under vacuum. The above isolated product (0.05 mmol), lithium bromide (0.05 mmol) and dry THF (10 mL) were placed in a 50 mL flask in which was also placed a magnetic stirring bar coated with Teflon °. The flask and its contents were then put under argon. The carbon disulphide (0.10 mmol) was then introduced into the flask drop by syringe. The flask was then immersed in an oil bath at 40 ° C for 17 h. A product was recovered after precipitation in methanol (20 mL), filtration and drying at 23 ° C under vacuum.
[0037] Results: The polymer obtained is solid at room temperature. The conversion ratio of the cycloolefin of formula (A) determined by NMR (expressed in%), the number-average molar mass of the polymer obtained (expressed in grams per mole) and the polymolecularity (PDI) of said polymer, determined by SEC, gave the following results: Table 1: I..ssai ei I f. mo I.eiioL. The 1 H NMR (CDCl 3, 500 MHz, 25 ° C.) and 13 C (CDCl 3, 125 MHz, 25 ° C.) analyzes of the polymer obtained for this test confirmed the structure of the expected polymer as shown in Scheme (8).
[0038] EXAMPLE 2 Synthesis of the Polymer of Example 1 from Cyclooctene (COE) and Diglycidyl Fumarate (CTA2) The reaction was carried out according to the following scheme (9), in a mole ratio m / n equal at 0/100 and according to the procedure described below: q (CTA2) Grubbs gener. (9) Procedure: The cycloolefin of formula (A) (108.00 mmol) and dry CH 2 Cl 2 (50 ml) are mixed in a 1000 ml flask. The flask and its contents were then put under argon. CTA (5.40 mmol) of type (C2) was introduced into the flask by syringe. The flask was then immersed in an oil bath at 40 ° C., then G2 catalyst (54.00 μmol) dissolved in CH 2 Cl 2 (20 ml) was immediately added by means of a cannula. ). 24 hours after the addition of the catalyst, the solution is concentrated by partially evaporating the CH 2 Cl 2 (up to the solubility limit of the polymer). The product is recovered after precipitation in methanol (15 mL), filtration and drying at 20 ° C under vacuum. The above isolated product (0.05 mmol), lithium bromide (0.05 mmol) and dry THF (10 mL) were placed in a 50 mL flask in which was also placed a coated stirring bar. Teflon °. The flask and its contents were then put under argon. The carbon disulphide (0.10 mmol) was then introduced into the flask drop by syringe. The flask was then immersed in an oil bath at 40 ° C for 17 h. A product was recovered after precipitation in methanol (20 mL), filtration and drying at 23 ° C under vacuum. Results: The polymer obtained is solid at room temperature. The conversion ratio of the cycloolefin of formula (A) determined by NMR (expressed in%), the number-average molecular weight of the polymer obtained (expressed in grams per mole) and the polymolecularity (PDI) of said polymer, determined by SEC, gave the following results: Table 2: 1 H NMR (CDCl 3, 500 MHz, 25 ° C) and 13 C (CDCl 3, 125 MHz, 25 ° C) analyzes of the polymer obtained for this test confirmed the polymer structure expected as shown in the diagram (9). Example 3 Synthesis of a Polymer Comprising Two [2-thione-1,3-oxathiolan-4-yl] methyl ester Terminal Groups from 5-hexylcyclooctene (5-hexyl-COE) and diglycidyl fumarate (CTA2 The reaction was carried out according to the following scheme (10), in a molar ratio m / n equal to 0/100 and according to the same procedure as example 2: [C 1: 0 P-; 1. ## STR1 ## in which (CTA2) 0CM Grubbs, ener, 24 h.sup.-40, GC S2 (H., F117.i Scheme (10) Results: The polymer obtained is liquid at room temperature.
[0039] The conversion ratio of the cycloolefin of formula (A) determined by NMR (expressed in%), the number-average molecular weight of the polymer obtained (expressed in grams per mol) and the polymolecularity (PDI) of said polymer, determined by SEC, gave the following results: Table 3: 5.a () t. ' RU] Mol! Tif) LI C. MI CUSi011. The 1 H NMR (CDCl 3, 500 MHz, 25 ° C.) and 13 C (CDCl 3, 125 MHz, 25 ° C.) analyzes of the polymer obtained for this test confirmed the structure of the expected polymer as shown in the diagram. (10). 3036399 38 ii) - Example 4 to 5: Polymerization of a mixture of cycloolefins of formulas (A) and (B): The cycloolefins of formula (A) and (B) used in Examples 4 and 5 are respectively the following: (COE) CH 2 (NBN-ester) Cyclooctene (COE) with purity greater than 95%, norbornene (NBN) and methyl 5-norbornene-2-carboxylate (NBN-ester) greater than 99% purity are commercially available from Sigma Aldrich. These products were previously distilled on CaH2, before being used in Examples 4 and 5. Example 4 Synthesis of a polymer comprising two terminal groups [2-thione-1,3-oxathiolan-4-yl] methyl ester from cyclooctene (COE), norbornene (NBN) and diglycidyl fumarate (CTA2) The reaction was carried out according to the following scheme (11), in a molar ratio m / n equal to 50/50. and according to the procedure described hereinafter: ## STR2 ## Scheme (11) Procedure: In a 1000 mL flask, the cycloolefins of Formulas (A) and (B), corresponding to COE (54.00 mmol) and NBN (54.00 mmol) respectively, and dry CH2Cl2 (50 mL). The flask and its contents were then put under argon. CTA (5.40 mmol) of type (C2) was then introduced into the flask by syringe. The flask was then immersed in an oil bath at 40 ° C. and immediately followed by cannulation of catalyst G2 (54 μmol) dissolved in CH2Cl2 (20 mL). 24 hours after the addition of the catalyst, the solution is concentrated by partially evaporating the CH 2 Cl 2 (up to the solubility limit of the polymer). The product is recovered after precipitation in methanol (15 mL), filtration and drying at 20 ° C under vacuum. The above isolated product (0.05 mmol), lithium bromide (0.05 mmol) and dry THF (10 mL) were placed in a 50 mL flask in which was also placed a magnetic stirring bar coated Teflon °. The flask and its contents were then put under argon. Sulphide 3036399 carbon (0.10 mmol) was then introduced into the flask drop by syringe. The flask was then immersed in an oil bath at 40 ° C for 17 h. A product was recovered after precipitation in methanol (20 mL), filtration and drying at 23 ° C under vacuum.
[0040] Results: The polymer obtained is liquid at room temperature. The conversion rates of the cycloolefins of formula (A) and (B) determined by NMR (expressed in%), the number-average molecular weight of the polymer obtained (expressed in grams per mol) and the polymolecularity (PDI) of the polymer. determined by SEC. The results were recorded in the following Table 4: Table 4: Test n: [A] .. [BHCIAIL [Ru] iinohnorj Mn conversion, Ec PDI no4 8 1 1 -2, 1 uuu The 1H NMR analyzes (CDCl3, 500 MHz, 25 ° C) and 13C (CDCl3, 125 MHz, 25 ° C) of the polymer obtained confirmed the structure of the expected polymer as shown in scheme (11). EXAMPLE 5 Synthesis of a Polymer Comprising Two [2-thione-1,3-oxathiolan-4-yl] methyl ester End-groups from Cyclooctene (COE) and Methyl 5-norbornene-2-carboxylate (NBN) -ester and diglycidyl fumarate (CTA2) The reaction was carried out according to the following scheme (12), in a molar ratio m / n equal to 50/50 and according to the same procedure as Example 4: 3036399 ## STR2 ## Scheme (12) Results: The polymer obtained is liquid at room temperature.
[0041] The conversion rates of the cycloolefins of formula (A) and (B) determined by NMR (expressed in%), the number-average molecular weight of the polymer obtained (expressed in grams per mol) and the polymolecularity (PDI) of the polymer. determined by SEC. The results are shown in the following Table 5: Table 5: Assay n: [AFFBi'ITCT13] [Ru nol] NinErc PDI conversion fg me 5 1 1 1 1 H NMR (CDCl 3, 500 MHz, 25 ° C. and 13C (CDCl3, 125 MHz, 25 ° C) of the obtained polymer confirmed the structure of the expected polymer as shown in Scheme (12).
[0042] Comparative Example 6 Synthesis of a polymer comprising two end groups methylene cyclocarbonate from cyclooctene (COE) and bis [(2-oxo-1,3-dioxolan-4-yl) methyl fumarate] (CTA5) The reaction was carried out according to the following scheme (13), in a molar ratio m / n equal to 0/100 and according to the same metathesis ring opening polymerization procedure as Example 2 (CL (CTA5) DCM Grubbs 24 Ho 'C Scheme (13) Results: The polymer obtained is solid at room temperature The results of the conversion rate of the cycloolefin of formula (A) determined by NMR (expressed in%) the number average molecular weight of the polymer obtained (expressed in grams per mol) and the polymolecularity (PDI) of said polymer, determined by SEC, are given in Table 6 below: Table 6: Test II: Al: Pl: ICI- [Ru] Emulsion 11131:, .. Conversion 141n, Ec PLIT Luno!) 8 1 1 1 3036399 4 The 1 H NMR (CDCl 3, 500 MHz, 25 ° C.) and 13 C (CDCl 3, 125 MHz, 25 ° C.) analyzes of the polymer obtained for this test confirmed the structure of the expected polymer as shown in scheme (13).
[0043] III - Example 7 to 9: Syntheses of poly (thio) urethanes from the unsaturated polyolefins of Examples 2, 5 and 6: Comparative Example 7: Synthesis of a polyurethane from the solid unsaturated polyolefin of Comparative Example 6 The polyolefin of Comparative Example 6 was reacted at 80 ° C., separately and in a stoichiometric ratio, with a primary diamine of the polyether diamine type (JEFFAMINE EDR 148, Huntsman) until complete disappearance. the infrared band characteristic of the 1,3-dioxolan-2-one groups (at 1800 cm-1) and appearance of the characteristic bands of the carbamate bond (band at 1700 cm-1).
[0044] The reaction time at the complete disappearance of the infrared band characteristic of the 1,3-dioxolan-2-one groups was about 12 hours at 80 ° C. EXAMPLE 8 Synthesis of a Poly (thio) urethane from the Solid Unsaturated Polyolefin of Example 2 According to the Invention Example 7 was reproduced by replacing the polyolefin of Example 6 with the solid polyolefin of Example 2 until complete disappearance of the infrared band characteristic of 2-thione-1,3-oxathiolan-4-yl groups (C = S band at 1200 cm -1 Infra-Red), appearance of characteristic bands of the thiocarbamate linkage (C = S band at 1530 cm -1 Infra-Red) and the appearance of the characteristic bands of the thiol and disulfide functions (HS band at 2500 cm -1 and SS band at 510 cm -1 in Raman). The duration of the reaction noted during the complete disappearance of the infrared band characteristic of the 1,3-dioxolan-2-one groups was less than 3 hours at 80 ° C.
[0045] EXAMPLE 9 Synthesis of a Polyurethane from the Liquid Unsaturated Polyolefin of Example 5 According to the Invention Example 7 was reproduced by replacing the polyolefin of Example 2 with the polyolefin of Example 5 and carrying out the reaction at room temperature (23 ° C.) until complete disappearance of the infrared band characteristic of the 2-thione-1,3-oxathiolan-4-yl groups (C = S band at 1200 cm -1). -1 Infra-Red), appearance of bands characteristic of the thiocarbamate bond (C = S band at 1530 cm-1 in Infra-Red) and the appearance of the characteristic bands of the thiol and disulfide functions (HS band at 2500 cm -1 and SS band at 510 cm -1 in Raman). The duration of the reaction noted during the complete disappearance of the infrared band characteristic of the 1,3-dioxolan-2-one groups was less than 3 h at 23 ° C. In each case, the products of Examples 8 and 9 could be formulated as a two-component mixture having satisfactory adhesive properties.
权利要求:
Claims (8)
[0001]
REVENDICATIONS1. A hydrocarbon polymer comprising two dithiocyclocarbonate end groups, said hydrocarbon polymer having the following formula (1): ## STR1 ## wherein each carbon-carbon bond of the chain noted is a double bond or a single bond; the groups R1, R2, R3, R4, R5, R6, R7 and R8, which are identical or different, are chosen from a hydrogen atom, a halogen atom, an alkyl group, a heteroalkyl group, an alkoxycarbonyl group or a heteroalkoxycarbonyl group; at least one of the groups R1 to R8 being part of the same hydrocarbon or heterocycle ring, saturated or unsaturated, with at least one of the groups R1 to R8; at least one of the pairs (R1, R2), (R3, R4), (R5, R6) and (R7, R8) may be an oxo group; x and y, which are identical or different, are integers ranging from 0 to 5; the groups R 9, R 10, R 11 and R 12 which are identical or different, are chosen from a hydrogen atom, a halogen atom, an alkyl group, a heteroalkyl group, an alkoxycarbonyl group or a heteroalkoxycarbonyl group; at least one of the groups; groups R9 to R12 which may form part of the same saturated or unsaturated hydrocarbon or heterocycle ring, with at least one of the groups R9 to R12; The group R13 is CH2, O, S, C (= O) or NR0, Ro being an alkyl group having from 1 to 22 carbon atoms; and n is an integer greater than or equal to 2 and m is an integer greater than or equal to 0, the molar ratio m / n ranging from 0/100 to 90/10; n and m being such that the number-average molar mass Mn of the hydrocarbon polymer of formula (1) ranges from 500 to 50,000 g / mol, and the polymolecularity (PDI) of the hydrocarbon polymer of formula (1) ranges from 1.0 at 3.0; F1 is represented by the following formula: and F2 is represented by the following formula:
[0002]
2); 32 wherein: A is a C1 to C9 alkylene group; Z is such that the divalent group -A-Z- is the group -A-C (= O) O- or -A- OC (= O) - and preferably -A-OC (= O) -; p1 and p2, which are identical or different, each represent an integer equal to 0, 1, 2 or
[0003]
3. A hydrocarbon polymer comprising two dithiocyclocarbonate end groups according to claim 1, characterized in that it has a number-average molar mass Mn ranging from 600 to 45000 g / mol. 3. A hydrocarbon polymer comprising two dithiocyclocarbonate end groups according to claim 1 or 2, characterized in that Z is such that the divalent group -AZ- is the group -A-OC (= O) -, and / or pl = p2 = 0, 25 and / or A is the methylene group, and / or the groups R1 to R8 are each a hydrogen atom. 5 10 3036399 47
[0004]
4. A hydrocarbon polymer comprising two dithiocyclocarbonate end groups according to any one of claims 1 to 3, characterized in that x = y = 1.
[0005]
5. Hydrocarbon polymer comprising two dithiocyclocarbonate end groups according to any one of claims 1 to 4, characterized in that its main chain is saturated.
[0006]
6. Process for the preparation of at least one hydrocarbon polymer comprising two terminal dithiocyclocarbonate groups, characterized in that it comprises: I) a step of polymerization by ring opening by metathesis, in the presence of: at least one catalyst metathesis, - of at least one mono or di-epoxidized chain transfer agent of formula (C1) or (C2) below: ## STR1 ## in which: F1 e is represented by following formula: (C - and F2e is represented by the following formula: feH2). A, Z, p1 and p2 of formulas F1 and F2e are as defined in any one of the preceding claims, the bond is a carbon-to-carbon single bond geometrically oriented on one side or the other by relative to double bond (cis or trans) in formula (C2); at least one compound of the following formula (A): ## STR3 ## in which: the groups R 1, R 2, R 3, R 4, R 5, R 6, R 7 and R 8, which are identical or different, are chosen from hydrogen atom, a halogen atom, an alkyl group, a heteroalkyl group, an alkoxycarbonyl group or a heteroalkoxycarbonyl group, at least one of the groups R1 to R8 being part of the same hydrocarbon or heterocycle ring, saturated or unsaturated with at least one of R1 to R8 and at least one of (R1, R2), (R3, R4), (R5, R6) and (R7, R8) being an oxo group; x and y are as defined in any one of the preceding claims; and optionally at least one compound of formula (B): R 13 (B) in which: the groups R 9, R 10, R 11 and R 12, which are identical or different, are chosen from a hydrogen atom, an atom of halogen, a heteroalkyl group, an alkoxycarbonyl group and a heteroalkoxycarbonyl group, at least one of R9 to R12 groups being part of the same ring or saturated or unsaturated heterocycle with at least one other groups R9 to R12; and - the group R13 is CH2, O, S, C (= O) or NR0, Ro being an alkyl group having from 1 to 22 carbon atoms; during a reaction time ranging from 2 to 24 hours and at a temperature ranging from 20 to 60 ° C; then optionally a step of selective hydrogenation of the double bonds of the polymer resulting from stage I) having two terminal epoxy groups; then II) a dithiocarbonation step of the product obtained in the preceding step by reaction with carbon disulfide (CS2) in the presence of a halogenated lithium compound, at a temperature ranging from 20 to 60 ° C.
[0007]
7. Preparation process according to claim 6, said process being such that: the molar ratio of the CTA of formula (Cl) on the compound of formula (A), or on the sum of the compounds of formulas (A) and ( B) if the compound of formula (B) is present, ranges from 1.10-3 to 1.0 or the molar ratio of CTA of formula (C2) to the compound of formula (A), or the sum of the compounds of formulas (A) and (B) if the compound of formula (B) is present, is from 0.5 × 10 -3 to 0.5.
[0008]
8. A two-component composition comprising: in a first compartment, at least one hydrocarbon polymer comprising two dithiocyclocarbonate end groups according to any one of claims 1 to 5 or as obtained by the process of preparation of claim 6, and in a second compartment, at least one compound comprising at least one amine group.
类似技术:
公开号 | 公开日 | 专利标题
EP3298062B1|2019-05-22|Hydrocarbon polymers comprising two |alkyloxycarbonyl end groups
EP2931760B1|2016-09-28|Hydrocarbon-based polymers comprising two end groups with 2-oxo-1,3-dioxolan-4-yl endings, preparation thereof and use thereof
EP3280706B1|2019-05-22|Hydrocarbon polymers comprising twoexo-vinylene cyclic carbonate terminal groups
EP3247733A1|2017-11-29|Hydrocarbonated polymers with two alcoxysilane end groups
EP3404047B1|2020-12-02|Hydrocarbon polymers with two alkoxysilane end groups
EP3242902A1|2017-11-15|Hydrocarbon polymers with two alcoxysilane end groups
EP3284766A1|2018-02-21|Novel hydrocarbon polymers with dithiocyclocarbonate end groups
WO2018002473A1|2018-01-04|New hydrocarbon polymers comprising two alkoxysilane end groups, and methods for preparing same
EP3523286B1|2021-02-24|Novel hydrocarbon polymers having exo-vinylene cyclic carbonate terminal groups
FR3051471A1|2017-11-24|HYDROCARBON POLYMERS WITH TWO ALCOXYSILANE TERMINAL GROUPS
FR3053341A1|2018-01-05|NOVEL HYDROCARBON POLYMERS WITH TWO ALCOXYSILANE TERMINAL GROUPS
EP3688039A1|2020-08-05|Liquid hydrocarbon copolymers having two cyclocarbonate ether end groups
WO2014091174A2|2014-06-19|Hydrocarbon polymers comprising a 2-oxo-1,3-dioxolan-4-yl end group, preparation and use thereof
WO2019063945A1|2019-04-04|Liquid hydrocarbon copolymers having two cyclocarbonate ester end groups
WO2018050993A1|2018-03-22|Hydrocarbon polymers with two 2-oxo-1,3-dioxolan-4-carboxylate end groups
WO2020079370A1|2020-04-23|Hydrocarbon copolymers with alternating blocks and alkoxysilane end groups
WO2018215451A1|2018-11-29|Liquid hydrocarbon copolymers comprising two alkoxysilane end groups, and production method thereof
EP3272783A1|2018-01-24|Hydrocarbon polymers with two azlactone end groups
同族专利:
公开号 | 公开日
WO2016185106A1|2016-11-24|
ES2739173T3|2020-01-29|
EP3298062A1|2018-03-28|
FR3036399B1|2017-06-16|
EP3298062B1|2019-05-22|
引用文献:
公开号 | 申请日 | 公开日 | 申请人 | 专利标题
WO1995035290A1|1994-06-17|1995-12-28|Eastman Chemical Company|Process for the selective hydrogenation of epoxyalkenes to epoxyalkanes|
EP1233030A1|1999-09-30|2002-08-21|Kyowa Yuka Co., Ltd.|Method of diminishing odor emission|
WO2005016908A1|2003-08-15|2005-02-24|Henkel Kommanditgesellschaft Auf Aktien|Cyclic dithiocarbonates, their preparation and application|
WO2013137175A1|2012-03-15|2013-09-19|日本ゼオン株式会社|Polymerizable composition, resin molded article, and resin composite molded article|
WO2014091173A1|2012-12-14|2014-06-19|Bostik Sa|Hydrocarbon-based polymers comprising two end groups with 2-oxo-1,3-dioxolan-4-yl endings, preparation thereof and use thereof|
GB791285A|1954-02-09|1958-02-26|Rohm & Haas|Epoxidation of unsaturated fatty acid esters|
IT1187681B|1985-07-05|1987-12-23|Montedison Spa|METHOD FOR THE PREPARATION OF 3,4-ALCHYL EPOXYBUTIRRATES|
EP0773948A4|1992-04-03|1998-09-02|California Inst Of Techn|High activity ruthenium or osmium metal carbene complexes for olefin metathesis reactions and synthesis thereof|
GB9916235D0|1999-07-09|1999-09-15|Univ Durham|Process for polymerisation of olefins and novel polymerisable olefins|
US8283410B2|2009-03-30|2012-10-09|Isp Investments Inc.|Ring-opening metathesis polymerization of norbornene and oxanorbornene moieties and uses thereof|
CN102757409B|2012-07-19|2014-07-16|湖南罗比特化学材料有限公司|Preparation method of glycidyl acrylate|FR3071501A1|2017-09-28|2019-03-29|Bostik Sa|LIQUID HYDROCARBON COPOLYMERS WITH TWO TERMINAL GROUPS ETHER CYCLOCARBONATE|
FR3071502B1|2017-09-28|2020-06-19|Bostik Sa|LIQUID HYDROCARBON COPOLYMERS WITH TWO ESTER CYCLOCARBONATE TERMINAL GROUPS|
CN112352008A|2018-07-04|2021-02-09|巴斯夫欧洲公司|Bonding method using two-component adhesive based on compound with cyclic thiocarbonate unit|
CN113372555A|2021-06-25|2021-09-10|浙江大学|Composite material with low dielectric constant and low dielectric loss as well as preparation method and application thereof|
法律状态:
2016-04-12| PLFP| Fee payment|Year of fee payment: 2 |
2016-11-25| PLSC| Search report ready|Effective date: 20161125 |
2017-04-13| PLFP| Fee payment|Year of fee payment: 3 |
2018-04-11| PLFP| Fee payment|Year of fee payment: 4 |
2019-04-10| PLFP| Fee payment|Year of fee payment: 5 |
2021-02-12| ST| Notification of lapse|Effective date: 20210105 |
优先权:
申请号 | 申请日 | 专利标题
FR1554501A|FR3036399B1|2015-05-20|2015-05-20|HYDROCARBON POLYMERS COMPRISING TWO TERMINAL GROUPSALKYLOXYCARBONYL|FR1554501A| FR3036399B1|2015-05-20|2015-05-20|HYDROCARBON POLYMERS COMPRISING TWO TERMINAL GROUPSALKYLOXYCARBONYL|
PCT/FR2016/050914| WO2016185106A1|2015-05-20|2016-04-20|Hydrocarbon polymers comprising two alkyloxycarbonyl end groups|
ES16723423T| ES2739173T3|2015-05-20|2016-04-20|Hydrocarbon polymers comprising two terminal groupsalkyloxycarbonyl|
EP16723423.6A| EP3298062B1|2015-05-20|2016-04-20|Hydrocarbon polymers comprising two alkyloxycarbonyl end groups|