A method of enriching an electrode of an electrochemical device with an ionic species, said method comprising the steps of: - providing a substrate (1) provided with at least one stack comprising: - immersing in an electrolytic solution (5 ): - apply, using a current or voltage generator, a current or voltage between the first current collector (2) and the counter-electrode (6), so as to migrate the ionic species from the counter-electrode (6) to the first electrode (3) and to enrich the first electrode (3) in the ionic species.
公开号:FR3029016A1
申请号:FR1461380
申请日:2014-11-24
公开日:2016-05-27
发明作者:Steve Martin;Helene Porthault;Sylvain Poulet
申请人:Commissariat a lEnergie Atomique CEA;Commissariat a lEnergie Atomique et aux Energies Alternatives CEA;
IPC主号:
专利说明:

[0001] Process for enriching an electrode of an electrochemical device in ionic species
[0002] TECHNICAL FIELD OF THE INVENTION The invention relates to a process for enriching an electrode of an electrochemical device in ionic species and also relates to an electrode thus obtained. STATE OF THE ART Microbatteries "all solid" are batteries of which all the components (current collectors, positive electrode and negative electrode, electrolyte) are in the form of a stack of thin layers. The active stack has a thickness of the order of 10 to 15pm. Conventionally, these microbatteries are produced by depositing successively on a substrate 1 at least (FIG. 1): a cathodic current collector 2a and a cathodic current collector 2b; a positive electrode or cathode 3, the positive electrode being deposited on the cathode current collector 2b, a solid electrolyte 4, the solid electrolyte 4 completely covering the cathode 3, but not completely the cathode collector 2a, a negative electrode or anode 10, the negative electrode being in contact with the anode collector 2b.
[0003] The thin layers are generally produced by vacuum deposition techniques such as physical vapor deposition (PVD for "Physical Vapor 3029016 2 Deposition") or chemical vapor deposition (CVD for "Chemical Vapor Deposition") or by thermal evaporation according to the nature of the materials that constitute them.
[0004] The operating principle of these microbatteries is based on the insertion and de-insertion of alkali metal ions or protons into the positive electrode. Currently, most of the microbatteries use ionic ions, lithium ions, from one of the materials forming the electrodes.
[0005] Generally, the lithium ions come either from a lithium metal electrode (in the case of "lithium-metal" microbatteries) or from an electrode formed of a lithiated insertion material such as, for example, a mixed oxide. cobalt / lithium, nickel / lithium or manganese / lithium (in the case of "lithium-ion" microbatteries).
[0006] Since the melting point of lithium is 181 ° C., the lithium metal electrodes can not be used in microbatteries at elevated temperatures.
[0007] Mixed oxide type lithic insertion materials, for their part, require thermal annealing at a temperature of at least 600 ° C., to promote crystallization and improve the reversibility of the cycling of lithium ions in the material. However, such annealing is incompatible with certain technologies such as the so-called "Above-IC" technology, which aims to place the microbatteries in the upper part of the integrated circuits, which do not support such temperatures. In order to overcome these disadvantages, document FR 2 873 854 proposes to manufacture an electrode made of lithiated material, the use of which does not require annealing at temperatures exceeding 300 ° C.
[0008] Non-lithiated electrode material, for example TiS2, is subjected to an in situ lithiation step. For this, one or more layers of non-lithiated material 3029016 3 are associated with one or more layers of lithium. Since lithium tends to diffuse into the non-lithiated electrode material, electrodes made of lithiated material are obtained. However, to obtain a homogeneous composition, it is necessary to promote the diffusion of lithium by thermal annealing in an inert atmosphere at temperatures of the order of 100 ° C. to 300 ° C. and / or to multiply the number of layers of material. /lithium. In addition, since metallic lithium is highly reactive with respect to the environment, the electrode must be encapsulated in a material that is suitable for protecting it from the surrounding environment, especially moisture. The last layer should be a layer of non-lithiated material to prevent lithium from reacting with the external environment. EP 2 320 502 proposes to perform the lithiation of the non-lithiated electrode material by short-circuiting the electrodes of the battery. To carry out the lithiation, the following layers are deposited on a substrate: a first electrode (cathode) made of titanium oxysulphide TiOS; a solid electrolyte made of LIPON; a second electrode (anode) made of germanium or silicon.
[0009] The two electrodes thus formed are short-circuited. Lithium is then deposited on the anode. The anode material then becomes conductive under the influence of lithium and the battery starts to operate in short circuit. The lithium present in the anode, diffuses through the electrolyte, to the cathode where it fits into the cathode material. Short circuit 25 is maintained until complete evaporation of lithium. The lithium ions are predominantly arranged in the cathode layer. However, short-circuiting of the battery can cause rapid and uncontrollable diffusion of lithium ions, which is likely to cause localized overlithiation phenomena and / or degradation of the electrode / electrolyte interfaces.
[0010] SUMMARY OF THE INVENTION The object of the invention is to overcome the drawbacks of the prior art and, in particular, to propose a method of enriching an electrode of an electrochemical device, which is simple and easy to implement. implement, and to obtain homogeneous electrodes and good quality. This object is achieved by a method of enriching an electrode of an electrochemical device with an ionic species, said method comprising the steps of: providing a substrate provided with at least one stack comprising: a first collector a first electrode covering at least a portion of the first collector, the first electrode being in electrical contact with the first current collector, a protective layer completely covering the first electrode and at least a portion of the first collector; at least a portion of the first current collector, the protective layer being electrically insulating and ionically conductive, - immerse in an electrolytic solution: o the substrate provided with the stack, o a counter-electrode, based on a conductive material Comprising said ionic species, - applying, by means of a current or voltage generator, a current or a voltage electrical connection between the first current collector and the counter-electrode, so as to migrate the ionic species from the counter-electrode to the first electrode and enrich the first electrode ionic species.
[0011] This object is also achieved by an enriched electrode obtainable by the method and also by a microbattery, a battery or an electrochromic system comprising such an electrode.
[0012] Other advantages and features will become more clearly apparent from the following description of particular embodiments of the invention given by way of non-limiting example and shown in the accompanying drawings, in which: FIG. 1 schematically represents, in section, an electrochemical device according to the prior art; FIG. 2 schematically represents, in section, a step of the process of enriching an electrode of an electrochemical device; According to the invention, FIGS. 3 to 7 show, schematically, a top view of an electrochemical device at different stages of the production process according to the invention; FIG. 8 is a diagrammatic representation of FIG. section, an electrochemical device containing an electrode enriched according to the method of the invention, - Figure 9 represents cycling curves for different current of a microbattery obtained according to the method of the invention. DESCRIPTION OF A PREFERRED EMBODIMENT OF THE INVENTION The method for enriching an ionic species electrode can be used for different types of electrochemical device.
[0013] Preferentially, it is used to enrich an electrode of a battery, a microbattery or an electrochromic system. As shown in FIG. 2, the substrate 1 used for the enrichment process 5 is provided with at least one stack comprising: a first current collector 2 covering at least a portion of the substrate 1, a first electrode 3 covering at least a part of the first collector 2, the first electrode 3 being in electrical contact with the first current collector 2, said electrode 3 being intended to be enriched in an ionic species, o a protective layer 4 completely covering the first electrode and at least a portion of the first current collector 2, the protective layer 4 being electrically insulating and ionically conductive. The substrate 1 provided with the stack is immersed in an electrolytic solution 5. Preferably, the part of the first current collector 2 not covered by the protective layer 4 is kept out of the electrolytic solution 5, ie only the part of the current collector 2 covered by the protective layer 4 is immersed in the solution 5. This makes it possible to prevent the deposit of the alkaline ionic species on the first current collector 2. Preferably, the substrate 1 is an electrically insulating substrate for Avoid depositing the alkaline species on the substrate. By electrically insulating means that it is electrically insulating material or that it is electrically conductive material and covered with an electrically insulating layer. A counter-electrode 6, based on electrically conductive material and comprising said ionic species, is immersed in the electrolytic solution 5.
[0014] Counter electrode 6 is configured to be the source of the ionic species. The ionic species is, according to one embodiment, an alkaline ionic species: the counter electrode 6 is based on an alkali metal. Preferably, the counter electrode 6 is lithium, sodium or potassium. The ionic species that will be inserted into the first electrode 3 corresponds, respectively, to lithium ions, sodium ions or potassium ions. In another embodiment, the ionic species is a non-alkaline ionic species. The counter-electrode 6 is in this case, for example, copper.
[0015] A current or voltage is applied between the first current collector 2 and the counterelectrode 6, so as to migrate the alkaline ionic species from the counterelectrode 6 to the first electrode 3 and to enrich the first electrode 3 in alkaline ionic species.
[0016] The ionic species diffuses through the ionically conductive protective layer 4. The current or the electrical voltage is applied by means of a current generator 7 or voltage.
[0017] The passage of each electron, supplied by the generator 7, corresponds to the insertion of an ion into the first electrode 3. This method makes it possible to control the kinetics of insertion of the ionic species, and the quantity of species ionic electrode inserted into the electrode material, selecting the current or voltage applied and the duration of the electrochemical treatment. The current densities are less than 100 mA / cm 2. Advantageously, they are less than 1 mA / cm 2. The applied voltage will be selected by those skilled in the art depending on the electrode material. Advantageously, it will be less than 5V.
[0018] The duration of the enrichment step is advantageously less than 1 hour. It depends on the current and the thickness of the electrode. The enrichment is homogeneous over the entire electrode material and the surface condition is not deteriorated.
[0019] In the case of lithium ion enrichment, i.e. in the case of lithiation, localized over-lithiation phenomena are avoided. The electrode obtained is homogeneous and has good electrochemical performance. The Applicant has found, against all odds, that the method of lithiation of an electrode material by an electrochemical route in solution is particularly suitable for devices in thin layers (microbatteries and electrochromic systems). Indeed, this kind of solution process is normally not recommended for these devices since the direct immersion of the devices in a liquid solution will result in an absorption of the electrolyte solution in the pores. electrode material. Therefore, at the end of the lithiation process, the electrode will be irremediably soiled with residues of the electrolyte solution, which will make the subsequent steps of making the microbattery impossible and / or reduce the performance of the electrochemical device. Moreover, in the case of the applicant's method, the enrichment step is carried out through the protective layer, which makes it possible to avoid the absorption of molecules on the electrode material.
[0020] Preferably, the first electrode 3 is of non-lithiated material. The non-lithiated material is preferably chosen from vanadium oxide (V x O y), tungsten oxide (WO x) or molybdenum oxide (MoOx). The non-lithiated material may still be a titanium oxysulfide (TiOxSy).
[0021] Even more preferably, the first electrode 3 is made of TiOS, silicon, germanium, graphite, indium, tin or V205.
[0022] Preferably, the protective layer 4 corresponds, advantageously, to the solid electrolyte layer of the microbattery, or of the electrochromic system.
[0023] There is no need to remove the protective layer after enrichment of the first electrode 3. The second electrode 10 may be deposited directly on the protective layer 4. The solid electrolyte may be boron oxynitride and Lithium (LiBON), Lithium Silicon Phosphate (LiSiPON), etc. Preferably, the solid electrolyte is phosphonium oxynitride and lithium (LiPON) called "lipon". LIPON is a good ionic conductor. The solid electrolyte may also be Li2S-P2S5. It is commonly accepted by those skilled in the art that the state of the interfaces between the electrodes and the electrolyte is a major factor controlling the performance of the battery. The electrochemical lithiation step through the solid electrolyte layer is, a priori, not recommended. However, against all odds, the Applicant has found that the electrochemical enrichment process does not degrade, or little, the surface of the solid electrolyte in contact with the bath. The preservation of the surface state of the solid electrolyte is also attributed to the limitation of the natural oxidation of this surface by the contribution of the ions at the origin of the enrichment process in ionic species.
[0024] Preferably, the electrolyte solution comprises at least one carbonated solvent and at least one salt of the ionic species. By carbonate is meant a compound comprising a group comprising a carbon atom bonded to three oxygen atoms (CO32-).
[0025] Propylene carbonate (PC), dimethyl carbonate (DMC), ethylene carbonate (EC) and diethylene carbonate (DEC) are, for example, carbonated solvents. These solvents have given good results. A solvent or a mixture of several carbonated solvents may be used to form the electrolytic solution. In the case of lithiation, the salt of the ionic species is, for example, a lithium salt of LiPF6 type. This type of ionic salt makes it possible to ensure good ionic conductivity of the Li + ions between the first electrode 3 and the counterelectrode 6 made of lithium.
[0026] As shown in FIG. 3, according to a preferred embodiment, an electrically conductive track 8 is deposited on the substrate 1. The track 8 is electrically connected to the first current collector 2. The track 8 is advantageously formed before the deposition of the first electrode 3 and / or before the deposition of the first current collector. The electrically conductive track 8 is, preferably, copper or titanium. Copper is advantageously a good electrical conductor and has low development costs. In general, the track 8 is made from an electrically conductive material that can not be ally with the ionic species to be transferred. Preferably, a second current collector 9 is also deposited on the substrate 1. The second current collector 9 is electrically dissociated from the first current collector 2.
[0027] Conventionally, the current collectors 2, 9 are formed by metal layers, for example platinum, chromium, gold, titanium, etc. The protective layer 4 is deposited so as to encapsulate the first electrode 3.
[0028] In a preferred embodiment, the protective layer 4 is deposited on the substrate, so as to completely cover both the first electrode 3, the first current collector 2 and the second current collector 9. In this configuration , the current generator 7 or voltage 5 is connected to the electrically conductive track 8 and against the electrode 6, so as to allow the lithiation of the first electrode 3. According to a preferred embodiment, and as shown in FIG. 4, a part of the electrically conductive track 8 is covered by the protective layer 4. The current generator 7 or voltage is advantageously connected to the electrically conductive track 8 not covered by the protective layer 4 In such a configuration, the immersion step is facilitated since only the portion of the electrically conductive track 8 that is not covered te by the protective layer should not be immersed. There is no risk of immersing the first current collector 2 because it is protected by the protective layer 4.
[0029] According to an alternative embodiment, as the first 2 and second 9 current collectors are electrically dissociated, the second current collector 9 may not be covered by the protective layer 4. The second collector 9 will not participate in the process enrichment because it will be electrically dissociated from the generator 7 voltage or current.
[0030] After the enrichment of the first electrode 3 in alkaline ionic species, and before the deposition of the second electrode 10, the protective layer 4 is etched, so as to release at least a part of the first current collector 2 (FIG. ).
[0031] 3029016 12 By release is meant that it is made accessible by removing the protective layer 4. It can be subsequently connected to another element or be covered by another element. Advantageously, the second current collector 9 is also released.
[0032] The first 9 and second 10 current collectors are, for example, based on platinum, chromium, gold, titanium, molybdenum, nickel, or even copper. A second electrode 10 is deposited on the protective layer 4 (FIG. 6). The second electrode 10 is electrically connected to the second current collector 9. The second electrode 10 is not present in the stack during the enrichment of the first electrode 3.
[0033] A wide range of material can be used to make the second electrode. The second electrode 10 is, for example, silicon, germanium, graphite, indium or tin.
[0034] According to a preferred embodiment, the substrate 1 comprises several stacks so as to simultaneously form a plurality of first enriched electrodes. The electrodes are advantageously connected to the same current or voltage generator during the enrichment process.
[0035] As shown in FIGS. 3 to 7, in the case of a substrate 1 provided with several stacks, a single protective layer 4 is advantageously used to cover all the stacks. The enrichment of each electrode is achieved through this single protective layer 4.
[0036] Alternatively, each stack could be covered with a clean protective layer.
[0037] 3029016 13 After the deposition of a second electrode 10 on each of the stacks, the substrate 1 is advantageously etched or cut, so as to separate the different stacks from each other (Figure 7). The cutting can be performed by any suitable technique. Preferably, the substrate 1 is cut with a laser. Preferably, the substrate 1 is made of glass or silicon. This substrate can be of any homogeneous or heterogeneous type. In the case of a substrate of electrically conductive material, the substrate 1 is electrically isolated from the electrolytic bath.
[0038] Figure 8 shows a microbattery obtained by the method. The battery is shown diagrammatically, in section, with respect to the axis AA 'of FIG. 7. In the embodiments described above, the second current collector 9 is deposited, prior to the deposition of the second electrode 10. According to FIG. an alternative embodiment, the second current collector 9 is deposited after the deposition of the second electrode 10, so as to cover the second electrode 10.
[0039] The process will now be described by means of the following example given by way of illustration and not limitation. In the example, the electrodes of four microbatteries were enriched simultaneously.
[0040] The stack is made on a borosilicate type glass substrate with a thickness of 100 μm. Anodic and cathodic titanium current collectors of 250 nm thickness are formed on a physical vapor deposition substrate (PVD).
[0041] A copper conductive track of a thickness of 200 nm is then deposited by PVD on this substrate. The conductive track is in contact with each cathode collector of each stack to be formed. A positive electrode or TiOS cathode with a thickness of 1.2 μm is deposited by PVD on each cathode collector. The solid electrolyte, LiPON 2 pm thick, is deposited by PVD so as to cover all the surfaces of the positive electrode layers and cathodic collectors. Only a portion of the copper track is not covered by this layer of solid electrolyte. The substrate provided with the different stacks is immersed in an electrolytic bath. A counter-electrode of metallic lithium is also immersed in the electrolytic bath. This electrode corresponds to the anode of the enrichment device. The electrolytic solution may, for example, be composed of carbonates type solvents EC, PC, DMC, DEC, etc. and a lithium salt of LPF6 type, which ensures good ionic conductivity of Li + ions between the cathode and the lithium metal anode. An electrical generator, current or voltage, is connected firstly to the portion of the copper track not covered by the solid electrolyte and secondly to a lithium metal counter electrode.
[0042] A current density of 50pA / cm 2 is applied for a period of 1 hour. The glass substrate, provided with the stack, is removed from the electrolytic bath. The assembly is rinsed to remove electrolyte solution residues.
[0043] The LiPON electrolyte layer is then etched to release contact of the cathode and anode collectors. A 65nm thick silicon negative electrode layer is deposited over the solid electrolyte and is in contact with the anode collector. Finally, the glass substrate is laser cut to separate each of the microbatteries.
[0044] The performance of the obtained microbatteries was tested. Figure 9 shows the evolution of the potential at the terminals of the battery according to the state of charge (the capacity) of this battery. The charge-discharge curves show the perfect functionality of the device 15 for different test current values (10pA - curve A, 20pA - curve B, and 40pA - curve C). The enrichment method allows a very precise control of the lithiation rate of an electrode of a thin film electrochemical device.
[0045] The amount of lithium inserted is controlled by the current (or voltage) applied during the production process. The electrodes enriched by the process have a homogeneous lithiation.
[0046] Electrochemical devices, including such an enriched electrode, as for example a battery, a microbattery or an electrochromic system have good electrochemical performance. The electrode enriched in alkaline ionic species can be, more particularly, used for the production of lithium batteries in thin layers and, in particular, for the production of microbatteries, intended to enter the manufacture of smart cards, intelligent labels, real-time clock supply (RTC), implanted medical systems ("pacemaker" or hearing implants, for example). These electrodes can still be used for producing microsystems of the physical, chemical or biological sensor type, for producing actuators, or microfluidic devices. Electrochromic cells or thin layer supercapacitors are still fields of application for such electrodes.
权利要求:
Claims (17)
[0001]
REVENDICATIONS1. A method of enriching an electrode of an electrochemical device with an ionic species, said method comprising the steps of: - providing a substrate (1) provided with at least one stack comprising: o a first current collector (2 ) covering at least a portion of the substrate (1), o a first electrode (3) covering at least a portion of the first collector (2), the first electrode (3) being in electrical contact with the first current collector (2) a protective layer (4) completely covering the first electrode (3) and at least a part of the first current collector (2), the protective layer (4) being electrically insulating and ionically conductive, - plunging into a solution electrolytic device (5): o the substrate (1) provided with the stack, o a counter-electrode (6), based on a conducting material comprising the said ionic species, - applying, using a generator of current or voltage, a current or an electrical voltage between the first current collector (2) and the counterelectrode (6), so as to migrate the ionic species from the counter-electrode (6) to the first electrode (3) and to enrich the first electrode (3) in the ionic species.
[0002]
2. Method according to claim 1, characterized in that an electrically conductive track (8) is deposited on the substrate, said track (8) being electrically connected to the first current collector (3), in that the protective layer (4) completely covers the first current collector (3), and in that the current or voltage generator (7) is connected to the electrically conductive track (8) and the counter-electrode (6). 3029016 18
[0003]
3. Method according to claim 2, characterized in that a portion of the electrically conductive track (8) is covered by the protective layer (4) and in that the generator (7) current or voltage is connected to the electrically conductive track (8) not covered by the protective layer (4).
[0004]
4. Method according to one of claims 2 and 3, characterized in that the track (8) electrically conductive is copper or titanium. 10
[0005]
5. Method according to any one of claims 1 to 4, characterized in that a second electrode (10) is deposited on the protective layer (4) after enrichment of the first electrode (3) ionic species. 15
[0006]
6. Method according to claim 5, characterized in that the second electrode (10) is silicon, germanium, graphite, indium or tin.
[0007]
7. Method according to one of claims 5 and 6, characterized in that the protective layer (4) is etched, before the deposition of the second electrode (10), so as to release at least a portion of the first collector current (2).
[0008]
8. Process according to any one of claims 1 to 7, characterized in that the ionic species is an alkaline ionic species, such as lithium, sodium or potassium, or a non-alkaline ionic species, such as copper.
[0009]
9. Method according to any one of claims 1 to 8, characterized in that the protective layer (4) is LIPON or Li2S-P2S5. 3029016 19
[0010]
10. Method according to any one of claims 1 to 9, characterized in that the first electrode (3) is TiOS, silicon, germanium, graphite, indium, tin or V205. 5
[0011]
11. Method according to any one of claims 1 to 10, characterized in that the electrolyte solution (5) comprises at least one carbonated solvent and at least one salt of the ionic species.
[0012]
12. Method according to any one of claims 1 to 11, characterized in that the substrate (1) is made of glass or silicon.
[0013]
13. Method according to any one of claims 1 to 12, characterized in that the substrate (1) comprises several stacks so as to simultaneously form a plurality of first enriched electrodes. 15
[0014]
14. The method of claim 13, characterized in that said first electrodes are connected to the same generator of current or voltage during the enrichment process. 20
[0015]
15. An enriched electrode obtainable by the method according to any one of claims 1 to 14.
[0016]
Battery or microbattery comprising an enriched electrode according to claim 15.
[0017]
Electrochromic system comprising an enriched electrode according to claim 15.
类似技术:
公开号 | 公开日 | 专利标题
EP3024066B1|2017-11-22|Method of enrichment with ionic species of an electrode of a microbattery
EP0568524B1|1995-03-08|Composite element comprising a titanium chalcogen or oxychalcogen layer, suitable in particular for use as a positive electrode in a thin-layer fuel cell
EP1771899B1|2008-02-27|Method of producing a lithium-bearing electrode
FR2860925A1|2005-04-15|Microbattery includes a first electrode and electrolyte comprising a material with a tetrahedral structure with a central atom of phosphorus, boron, silicon, sulfur, molybdenum, vanadium or germanium
EP2409352B1|2014-11-05|Lithium microbattery and method for the production thereof
CH646817A5|1984-12-14|SOLID BATTERY.
EP2071657B1|2010-05-12|Encapsulated lithium electrochemical device
EP0201422B1|1990-03-14|Integrable solid cell and process for its manufacture
EP3012886A1|2016-04-27|Electrochemical device, such as a microbattery or an electrochromic system, and method for manufacturing same
WO2013076260A1|2013-05-30|Method for the production of an all-solid battery
FR2947386A1|2010-12-31|NON-BALANCED LITHIUM-ION MICROBATTERIUM, PROCESS FOR PRODUCING LITHIUM MICROBATTERIUM, AND LITHIUM MICROBATTERIUM
FR2952477A1|2011-05-13|METHOD FOR FORMING THIN-FILM LITHIUM-ION BATTERY
EP3108524B1|2019-12-18|Positive electrode for lithium-sulphur electrochemical accumulator having a specific structure
FR2550015A1|1985-02-01|Thin-layer electrochemical generator comprising an electrodeposited positive electrode
EP3071959B1|2020-09-09|Electrochemical system comprising a comparison electrode and corresponding manufacture method
FR2986867A1|2013-08-16|Reference potential electrode for lithium ion battery, has protective layer for protecting electrochemical reference metal layer, where metal layer is placed between electric conducting element and protective layer
FR3002482A1|2014-08-29|METHOD FOR PRODUCING 3D STRUCTURED THIN LAYERS
FR3077681A1|2019-08-09|THIN FILM BATTERY
EP2893584B1|2017-09-27|Method for producing a lithium-based electrolyte for a solid microbattery
FR3095721A1|2020-11-06|Storage device and manufacturing process
FR3054727A1|2018-02-02|ELECTROCHEMICAL DEVICE, SUCH AS A MICROBATTERY OR ELECTROCHROME DEVICE, AND METHOD FOR PRODUCING THE SAME
FR3056339A1|2018-03-23|METHOD FOR PRODUCING AN ELECTROCHEMICAL DEVICE
FR3089692A1|2020-06-12|Stacking of electrodes, galvanic cell and production method
CH712500B1|2021-03-15|Rechargeable lithium-ion battery electrochemical cell and its manufacturing process.
WO2018091808A1|2018-05-24|Lithium microbattery and production method
同族专利:
公开号 | 公开日
FR3029016B1|2016-12-09|
US20160149203A1|2016-05-26|
EP3024066A1|2016-05-25|
US9876219B2|2018-01-23|
EP3024066B1|2017-11-22|
引用文献:
公开号 | 申请日 | 公开日 | 申请人 | 专利标题
JPS62226563A|1986-03-27|1987-10-05|Fuji Elelctrochem Co Ltd|Nonaqueous electrolyte secondary battery|
US5558953A|1993-10-21|1996-09-24|Matsushita Electric Industrial Co., Ltd.|Electrocrystallized lithuim metal, method for producing the same, and lithium secondary battery|
WO1999043034A1|1998-02-18|1999-08-26|Polyplus Battery Company, Inc.|Plating metal negative electrodes under protective coatings|
WO2014017968A1|2012-07-26|2014-01-30|Lifesize Ab|Sustainable current collectors for lithium batteries|
FR2873854A1|2004-07-30|2006-02-03|Commissariat Energie Atomique|PROCESS FOR PRODUCING A LITHIUM ELECTRODE, LITHIUM ELECTRODE THAT CAN BE OBTAINED BY THIS METHOD AND USES THEREOF|
FR2938977B1|2008-11-21|2011-04-01|Commissariat Energie Atomique|MICROBATTERY ON MONOLITHIC ENCAPSULATION SUBSTRATE|
FR2943181B1|2009-03-16|2011-05-13|Commissariat Energie Atomique|LITHIUM MICROBATTERIUM AND METHOD FOR MANUFACTURING THE SAME|
KR101146616B1|2009-06-30|2012-05-14|지에스나노텍 주식회사|Thin film battery and method of connecting electrode terminal of thin film battery|
US20110045351A1|2009-08-23|2011-02-24|Ramot At Tel-Aviv University Ltd.|High-Power Nanoscale Cathodes for Thin-Film Microbatteries|
FR2952477B1|2009-11-06|2011-12-09|St Microelectronics Tours Sas|METHOD FOR FORMING THIN-FILM LITHIUM-ION BATTERY|
FR2982083B1|2011-11-02|2014-06-27|Fabien Gaben|METHOD FOR PRODUCING SOLID ELECTROLYTE THIN FILMS FOR LITHIUM ION BATTERIES|CN105906051B|2016-06-06|2019-01-18|山东大学|A kind of electrochemistry microorganism autotrophic denitrification sewage water treatment method and system|
US10749199B2|2017-11-29|2020-08-18|International Business Machines Corporation|Li1+xAlxTi2-x3 solid-state thin film electrolyte for 3D microbattery and method of fabrication|
US20220035215A1|2018-09-17|2022-02-03|The Regents Of The University Of Calfornia|High-efficiency electrodeposition for coating electrochromic films|
CN111799445B|2020-08-24|2022-03-04|中南大学|Lithium metal anode and preparation and application thereof|
法律状态:
2015-11-30| PLFP| Fee payment|Year of fee payment: 2 |
2016-05-27| PLSC| Search report ready|Effective date: 20160527 |
2016-11-30| PLFP| Fee payment|Year of fee payment: 3 |
2017-11-30| PLFP| Fee payment|Year of fee payment: 4 |
优先权:
申请号 | 申请日 | 专利标题
FR1461380A|FR3029016B1|2014-11-24|2014-11-24|METHOD FOR ENRICHING AN ELECTRODE OF AN ELECTROCHEMICAL DEVICE IN ION SPECIES|FR1461380A| FR3029016B1|2014-11-24|2014-11-24|METHOD FOR ENRICHING AN ELECTRODE OF AN ELECTROCHEMICAL DEVICE IN ION SPECIES|
US14/951,061| US9876219B2|2014-11-24|2015-11-24|Method for performing enrichment of an electrode of an electrochemical device with ionic species|
EP15196056.4A| EP3024066B1|2014-11-24|2015-11-24|Method of enrichment with ionic species of an electrode of a microbattery|
[返回顶部]