专利摘要:
The present invention relates to a fabric softening composition comprising a cationic fabric softening agent and a thickening polyurethane resulting from the condensation of: a) at least one compound of formula (I): wherein: R is a carbon chain, saturated or unsaturated, linear or branched, having 17 to 24 carbon atoms, [(EO) m - (OP) n - (OB) p] represents an alkoxylated chain consisting of alkoxylated units, divided into blocks, alternating or statistical, selected from the ethoxylated units EO, the propoxylated units OP and the butoxylated units OB, m, n and p represent, independently of each other, 0 or an integer varying between 1 and 30, the sum of m, n and p being between 20 and 30, b) at least one polyol, for example at least one poly (alkylene glycol) and c) at least one polyisocyanate.
公开号:FR3023846A1
申请号:FR1456934
申请日:2014-07-18
公开日:2016-01-22
发明作者:Yves Kensicher;Yves Matter;Jean-Marc Suau
申请人:Coatex SAS;
IPC主号:
专利说明:

[0001] The present invention relates to the technical field of fabric softening compositions. Such fabric softening compositions are, for example, intended to be used in the rinse cycle of a washing or laundering process. In general, the softening compositions comprise a softening agent dispersed in an aqueous solution. The use of cationic softening agents is described in particular in documents US 2013/0065813, US 2008/0051309, US 2004/0087470 and US 6,020,304. These same documents also describe the use of thickeners, whose object is to facilitate the dosage during use and to satisfy consumers who generally consider that the effectiveness of the compositions is related to their viscosity.
[0002] Different classes of thickeners can be used to increase the viscosities of fabric softening compositions containing a softening cationic agent. It is possible, for example, to use thickeners of natural origin (for example, gelatins, starches, carrageenans), natural thickeners based on cellulose, also known as cellulose ethers, of the HEC type or of the HMHEC type ( Hydrophobically Modified HEC), acrylic thickeners or thickeners bearing urethane linkages. For example, documents US 2009/0124533 and US 6,020,304 describe the use of thickeners resulting from the condensation of a polyalkylene glycol with an isocyanate compound having a hydrophobic chain end. More specifically, the document US 2009/0124533 describes the use of a thickener which is the product of the addition of an isocyanate compound with a polyalkylene glycol and which has at the end of the chain a C14-C20 alkyl radical, saturated and not ethoxylated. US 6,020,304 describes the use of a thickener having urethane linkages with chain ends C8-C24, linear or branched, alkyl or alkenyl, non-ethoxylated.
[0003] In the context of the present invention, the thickening polyurethanes or HEURs result from the condensation between 3 constituents, namely: a poly (alkylene glycol) type compound, a polyisocyanate and a reagent which confers associativity of the alkyl, aryl or aryalkyl consisting of a hydrophobic end group.
[0004] US 2009/02911876 discloses an aqueous laundry treatment composition comprising a cationic softening agent and a viscosity modifier which is a linear water-soluble polymer. A polymer described as particularly preferred in this document is a polyurethane having at the end of a chain a structure consisting of 0 to 30 ethoxylated units and 11 to 25 carbon atoms. As demonstrated in the experimental part of the present patent application, the inventors have realized that within this broad definition, certain polyurethanes were more particularly effective for thickening fabric softening compositions.
[0005] An object of the present invention is a fabric softening composition, comprising a cationic fabric softening agent and a HEUR type thickener, allowing better thickening than the thickeners described in the prior art.
[0006] Another object of the present invention is the use of a special thickening polyurethane for thickening a softening composition containing a cationic fabric softening agent. DEFINITIONS In the description of the present invention, the term "HEUR" is an acronym for "Hydrophobically modified Ethoxylated URethane". In the description of the present invention, unless otherwise indicated, the percentages expressed represent percentages by weight and are expressed relative to the total weight of the reference element. For example, when it is stated that a polymer comprises 10% of a monomer or a reagent, it is understood that the polymer comprises 10% by weight of this monomer or reagent relative to the total weight of this monomer or reagent. polymer. In the description of the present invention, the term "at least one" refers to one or more compounds (for example: one or more compounds of formula (I), one or more polyols, one or more polyisocyanates), such as mixture of 2 to 5 compounds. By "alkyl" is meant a linear or branched C, H 2 '1 group, where x ranges from 1 to 30, preferably from 10 to 30, or even from 12 to 28.
[0007] By "alkenyl" is meant a linear or branched CyH2y-i group, where y ranges from 1 to 30, preferably from 10 to 30, or even from 12 to 28. DETAILED DESCRIPTION OF THE INVENTION The polyurethanes of the present invention are thickeners particularly suitable for fabric softening compositions. An object of the present invention relates to a thickener belonging to the category of HEUR (Hydrophobically modified Ethoxylated URethane). It is a polymer, associative and nonionic, thickener for fabric softening compositions. The thickening polyurethanes or HEURs of the present invention result from the reaction between a poly (alkylene glycol) type compound, a polyisocyanate and a reagent which confers associativity and which consists of a hydrophobic end group. In the context of the present invention, the terms "reaction", "condensation" and "polycondensation" are used in an equivalent manner.
[0008] More specifically, in the context of the present invention, the polyurethane thickener for fabric softening compositions results from the polymerization of: a) at least one compound of formula (I): R - [(OE) ', - ( OP) '- (0B) p I - OH (I) in which: R is a linear or branched, saturated or unsaturated carbon chain having from 17 to 24 carbon atoms, [(OE)', - (OP)) '- (0B) p [represents an alkoxylated chain consisting of alternately or randomly divided alkoxylated units selected from ethoxylated units EO, propoxylated units OP and butoxylated units OB, m, n and p represent, independently each other, 0 or an integer ranging between 1 and 30, the sum of m, n and p being between 20 and 30, b) of at least one polyol, for example at least one poly (alkylene glycol) and c) at least one polyisocyanate. It is understood that these three components a), b) and c) are indispensable in the constitution of the polyurethanes according to the invention. Those skilled in the art may optionally add other constituents. These polyurethanes are particularly suitable for thickening formulations for softening tissues, which furthermore comprises a cationic fabric softening agent. In a detailed manner, the polyurethane according to the present invention comprises as constituent a) at least one compound of formula (I). The compounds of formula (I) consist of a hydrophobic part, which is a saturated or unsaturated carbon chain, linear or branched, having from 17 to 24 carbon atoms. They also consist of a hydrophilic part, which is a polyalkoxylated chain having between 20 and 30 alkoxylated units. The polyurethane according to the present invention may comprise several compounds of formula (I) different.
[0009] The inventors have indeed realized that, compared to the teaching of the document US 2009/02911876 which describes the use of a polyurethane having end of chain a structure consisting of 0 to 30 ethoxylated units and of 11 to 25 carbon atoms in a field of application identical to that of the present invention, it was possible within this broad definition to select certain polyurethanes more particularly effective for thickening fabric softening compositions. This selection lies, first of all, in the choice of a narrower length of hydrophobic chain, namely 17 to 24 carbon atoms. It also resides in the choice of a polyalkoxylated chain length consisting of at least 20 alkoxylated units and at most 30 alkoxylated units. According to one embodiment, said thickening polyurethane results from the condensation of at least one compound of formula (I) in which R is a carbon chain having at least one linear or branched unsaturation having from 17 to 24 carbon atoms. According to another embodiment, said thickening polyurethane results from the condensation of at least one compound of formula (I) in which R is a carbon chain, saturated or unsaturated, linear or branched, having from 18 to 23 carbon atoms, for example from 19 to 22 carbon atoms. In this embodiment, R is a carbon chain, saturated or unsaturated, linear or branched, having 18, 19, 20, 21, 22 or 23 carbon atoms.
[0010] According to this embodiment, R is, preferably, a carbon chain having an odd number of carbon atoms. According to another embodiment, said thickening polyurethane results from the condensation of at least one compound of formula (I) in which R is a linear carbon chain having one or more unsaturations, having from 17 to 24 carbon atoms. According to one embodiment, said thickening polyurethane results from the condensation of at least one compound of formula (I) in which R is a linear or branched saturated carbon chain having from 17 to 24 carbon atoms. All these embodiments can, moreover, be combined with each other. The compounds of formula (I) also comprise a polyalkoxylated chain consisting of at least 20 alkoxylated units. In addition, the compounds of formula (I) contain a polyalkoxylated chain consisting of at most 30 alkoxylated units. According to one embodiment of the present invention, in formula (I) below: R - [(OE) ', - (OP)' - (OB) p I - OH (I) - m represents an integer varying between 1 and 30 (different from 0) and - n and p represent, independently of one another, 0 or an integer varying between 1 and 29, the sum of m, n and p being between 20 and 30, for example being equal to 20, 25 or 30. According to another embodiment of the present invention, in formula (I) above: - m and n represent an integer ranging between 1 and 30 (different from 0) and - p is equal to 0, the sum of m, n and p being between 20 and 30, for example being equal to 20, 25 or 30.
[0011] According to another embodiment, in formula (I) above: n and p are 0 and m represents an integer ranging between 20 and 30, for example between 21 and 29, or, for example equal to 25.
[0012] According to this embodiment, said alkoxylated chain of the compound of formula (I) consists exclusively of EO ethoxylated units. According to another embodiment of the present invention, said thickening polyurethane results from the condensation of at least one compound of formula (I) in which n and p are zero and m represents an integer ranging between 20 and 30. Another embodiment of the present invention, said thickening polyurethane results from the condensation of at least one compound of formula (I) wherein n and p are zero and m represents an integer ranging between 25 and 30.
[0013] Furthermore, the polyurethane comprises as component b) at least one polyol which may be a poly (alkylene glycol). By "poly (alkylene glycol)" is meant a polymer of an alkylene glycol derived from an olefinic oxide. The poly (alkylene glycol) chains of component b) according to the present invention contain a proportion of ethyleneoxy groups, a proportion of propyleneoxy groups and / or a proportion of butyleneoxy groups. The poly (alkylene glycol) chains according to the present invention may for example comprise a major proportion of ethyleneoxy groups in combination with a secondary proportion of propyleneoxy groups. Specific examples of alkylene glycol polymers include: polyalkylene glycols having an average molecular weight of 1,000, 4,000, 6,000 and 10,000 g / mol; polyethylene polypropylenes glycols having a percentage of ethylene oxide of between 20 and 80% by weight and a percentage of propylene oxide of between 20 and 80% by weight.
[0014] According to one aspect of the present invention, the polyurethanes result from the condensation in particular of a poly (alkylene glycol) which comprises more than 80% by weight of ethylene oxide. According to one aspect of the present invention, the polyurethanes result from the condensation in particular of a poly (alkylene glycol) which is poly (ethylene glycol). It may be, for example, a poly (ethylene glycol) whose molecular mass varies between 2,000 g / mol and 20,000 g / mol, for example between 8,000 g / mol and 15,000 g / mol ( terminals included). By way of example, mention may be made of poly (ethylene glycol) (or PEG) with a molecular mass ranging between 10,000 g / mol and 12,000 g / mol (inclusive) or that with a molecular weight ranging between 5,000 and 7,000. 000 g / mol (inclusive). By way of example, mention may also be made of poly (ethylene glycol) (or PEG) having more than 180 units of EO, for example 181 or more, or that having less than 180 EO units, for example 179 or less. The polyurethane according to the present invention may comprise several different polyalkylene glycols. In addition, the polyurethane comprises as component c) at least one polyisocyanate. By "polyisocyanate" is meant a compound which comprises at least 2 isocyanate functional groups -N = C = O. According to one aspect of the present invention, the polyurethanes result from the condensation, in particular of a polyisocyanate which is chosen from the group consisting of toluene diisocyanate, toluene diisocyanate dimers, toluene diisocyanate trimers and 1,4-butane diisocyanate. , 1,6-hexane diisocyanate, isophorone diisocyanate (IPDI), 1,3-cyclohexane diisocyanate, 1,4-cyclohexane diisocyanate, 4,4'-diisocyanatodicyclohexylmethane, 1-methyl-2,4- diisocyanatocyclohexane, diphenyl methylene diisocyanate (MDI), for example 2,2'-MDI, 2,4'-MDI, 4,4'-MDI or their mixtures, dibenzyl diisocyanate, a mixture of 1-methyl-2, 4-diisocyanatocyclohexane and 1-methyl-2,6-diisocyanatocyclohexane, hexamethylene diisocyanate biuret, hexamethylene diisocyanate biuret dimers, hexamethylene diisocyanate biuret trimers, 2,2,4-trimethylhexamethylene diisocyanate and a mixture of at least two of these compounds.
[0015] In another aspect of the present invention, the polyurethanes result from the condensation of at least one polyisocyanate which is isophorone diisocyanate (IPDI). According to another aspect of the present invention, the polyurethanes result from the condensation of at least one polyisocyanate selected from the group mentioned above with the exception of isophorone diisocyanate (IPDI). According to one embodiment of the present invention, it is excluded that the polyurethane thickener for fabric softening compositions results from the condensation of: a) an alcohol-type compound, as described above, b) of poly (ethylene glycol) having 180 EO units and c) isophorone diisocyanate. According to one aspect of the invention, said thickening polyurethane results from the condensation of: a) 1% to 29% by weight of at least one compound of formula (I), b) 70% to 98% by weight of at least one poly (alkylene glycol) and c) 1% to 29% by weight of at least one polyisocyanate, the sum of these mass percentages being equal to 100%.
[0016] According to another aspect of the invention, said thickening polyurethane results from the condensation of: a) 3% to 10% by weight of at least one compound of formula (I), b) 80% to 94% by weight of at least one poly (alkylene glycol) and c) 3% to 10% by weight of at least one polyisocyanate, the sum of these mass percentages being equal to 100%. The manufacture of polyurethanes, which belong to the family of thickeners of the HEUR type, is known to those skilled in the art, which may refer to the teaching of the documents cited above in the technological background of the present invention.
[0017] An object of the present invention also relates to a process for preparing a polyurethane as described above, said process consisting of a condensation of its various constituents.
[0018] Formulation of the HEUR thickener The polyurethane according to the invention, which results from the reaction of the at least 3 constituents mentioned above, may be in different forms (solid or liquid). The powder form may be preferred by the formulator for incorporation into a given formulation or because of certain constraints (equipment available, volumes to be prepared). Nevertheless, it may be preferable to use a polyurethane in liquid form, in particular for better dispersibility when added to aqueous systems and a shorter dissolution time. Most commercial associative thickeners are now sold in liquid form.
[0019] Thus the polyurethane according to the invention can also be formulated or co-formulated with other constituents or components, this independently of the final composition for softening the tissues. In particular, the polyurethane according to the invention can be formulated in water.
[0020] According to one embodiment, said aqueous formulation according to the invention consists of: 1) 1% to 50% by weight of at least one polyurethane according to the invention, as described above and 2) 50% to 99% in weight of water, the sum of these mass percentages being equal to 100%.
[0021] According to another embodiment, said aqueous formulation according to the invention consists of: 1) 2% to 25% by weight of at least one polyurethane according to the invention, as described above and 2) 75% to 98% % by weight of water, the sum of these mass percentages being equal to 100%. The polyurethane according to the invention may be co-formulated in water, in the presence of at least one surfactant. This surfactant makes it possible to formulate the thickener in the form of a less viscous liquid aqueous solution which can thus more easily be used by the formulator. Thus, according to one embodiment of the present invention, said aqueous formulation comprises a polyurethane, as described above, as well as water and a surfactant. By "surfactant" or "surfactant" is meant a molecule or a polymer consisting of at least one hydrophilic part and at least one hydrophobic part. The surfactant used in the context of the present invention may be of a different nature, for example it may be anionic or nonionic. This surfactant may be selected from ionic surfactant classes (in this case preferably anionic), and / or nonionic and / or mixed (comprising in the same molecule a nonionic and anionic structure). The preferred surfactant is composed of at least one surfactant selected from the class of nonionic surfactant, optionally in the presence of an anionic surfactant. Among the suitable anionic surfactants, mention may be made of sodium, lithium, potassium, ammonium or magnesium salts derived from alkyl ether sulphates with C6 to C12 alkyl, in a linear, iso, oxo, geminate, cyclic or aromatic configuration, or C12 alkyl sulfates, alkyl phosphate esters or dialkyl sulfosuccinates.
[0022] The anionic surfactants are preferably used with at least one nonionic surfactant. Examples of mixed surfactants include alkoxylated alkyl phenol sulfonates. The nonionic surfactants can be used alone or in combination with an anionic surfactant. As preferred examples of suitable nonionic surfactants, mention may be made of: ethoxylated C4-C18 alcohols (2 to 15 OE), ethoxylated C4-C18 Guerbet alcohols (2 to 40%), C10-C18 mono-branched alcohols ethoxylated (2-40E), C18 sorbitol esters, ethoxylated sorbitol esters (2-20EE units), ethoxylated C4-C18 acids (less than 15E), ethoxylated castor oil (30E), at 40 ° C.), ethoxylated hydrogenated castor oil (7 to 60 ° C.), esters such as, for example, glycerol palmitate, glycerol stearate, ethylene glycol stearate, diethylene glycol stearate, sodium stearate. propylene glycol, polyethylene glycol stearate 200 and ethoxylated C18 esters (2 to 15 OE). The hydrophobic chains may correspond to linear, iso, oxo, cyclic or aromatic structures.
[0023] According to one embodiment, the polyurethane of the present invention is formulated in the presence of at least one nonionic surfactant, optionally combined with at least one anionic surfactant, with a total content by weight ranging from 5 to 30% by weight, by example of 8 to 20% by weight or 10 to 17% by weight. In this case, the weight ratio between the two surfactants may, for example, vary between 25/75 and 75/25. According to one embodiment of the present invention, the polyurethane of the present invention is formulated in the presence of more than two surfactants, for example three or four.
[0024] According to one embodiment, said aqueous formulation according to the invention consists of: 1) 2% to 50% by weight of at least one polyurethane according to the invention, as described above, preferably 5% to 30% by weight, 2) 5% to 40% by weight of at least one surfactant, preferably 8% to 30% by weight and 3) 10% to 93% by weight of water, preferably 40% to 85% by weight, the sum of these mass percentages being equal to 100%. The polyurethane according to the invention may be formulated in a solvent miscible with water. The main reason for adding an organic co-solvent is to lower the viscosity of this polyurethane in water, to facilitate handling. The polyurethane is, for example, formulated with one or more polar solvents belonging in particular to the group consisting of water, methanol, ethanol, propanol, isopropanol, butanols, acetone, tetrahydrofuran or their mixtures .
[0025] A particular example of a water-miscible organic solvent is diethylene glycol monobutyl ether (also known as Butyl Carbitol ™) or ethylene or propylene glycol. The viscosity of the polyurethane as it is before incorporation into a fabric softening composition is preferably less than 10,000 mPa.s at 25 ° C and 100 rpm, so that it is easier to pour from the storage container and more rapidly incorporated into the composition to be thickened at room temperature. The water-miscible solvent chosen for such commercial compositions has, to date, exclusively been an organic solvent.
[0026] According to one aspect of the invention, the HEUR thickener formulation further comprises at least one additive selected from the group consisting of a biocide, a pH regulator, an antifoam agent, an encapsulant and mixtures thereof. "Biocide" means a chemical substance intended to destroy, repel or render harmless harmful organisms, to prevent their action or to combat them in any other way, by chemical or biological action. By "pH regulating agent" is meant an agent capable of significantly varying the pH of the formulation. The pH regulating agent can increase the pH, which is the case with bases, such as NaOH. Alternatively, the pH regulating agent can reduce the pH, which is the case of acids. By way of examples, one or more neutralization agents are used having a monovalent neutralizing function and / or a divalent or polyvalent neutralizing function, such as, for example: for the monovalent function, those chosen from the group consisting of alkaline cations, in particular sodium, potassium, lithium, ammonium or aliphatic and / or cyclic primary, secondary or tertiary amines such as, for example, stearylamine, ethanolamines (mono-, di-, triethanolamine). ), mono and diethylamine, cyclohexylamine, methylcyclohexylamine - for the divalent / polyvalent function, those selected from the group consisting of divalent alkaline earth cations, in particular magnesium, calcium, zinc, as well as trivalent cations, especially aluminum, or certain higher valence cations. By "antifoaming agent" is meant a substance or formulation intended to destroy air bubbles in a homogeneous or heterogeneous liquid medium (or on its surface) or to prevent their formation.
[0027] By "encapsulating agent" is meant an agent creating a hydrophobic environment, for example a solvation cage. In particular, cyclodextrin is mentioned as encapsulant. According to one embodiment, said aqueous formulation according to the invention consists of: 1) 2% to 50% by weight of at least one polyurethane according to the invention, as described above, preferably 5% to 30% by weight, 2) 5% to 40% by weight of at least one surfactant, preferably 8% to 30% by weight, 3) 10% to 93% by weight of water, preferably 40% to 85% by weight and 4) 0 to 5% by weight of at least one other additive selected from the group consisting of a biocide, a pH regulator, an anti-foaming agent, an encapsulant and mixtures thereof, preferably 0.5 at 4% by weight, the sum of these mass percentages being equal to 100%.
[0028] The present invention also relates to a fabric softening composition comprising a thickening polyurethane according to the invention, as described above, as well as a cationic fabric softening agent.
[0029] The cationic conferring softening agent is dispersed within the aqueous composition. Such fabric softening compositions are, for example, intended to be used in the rinse cycle of a washing or laundering process.
[0030] The use of thickener within the softening composition according to the invention facilitates the dosage during use. In addition, consumers generally consider that the effectiveness of the compositions is related to their viscosity. Thus, it is commercially interesting that the softening composition according to the invention comprises a thickener.
[0031] According to one embodiment of the present invention, the viscosity of said fabric softening composition, measured with a Brookfield type RVT viscometer, after 24 hours of storage in the unstirred bottle, at a temperature of 25 ° C at the speed of rotation speed of 20 rpm, is greater than 300 mPa.s, for example greater than 400 or 500 mPa.s.
[0032] The present invention also relates to fabric softening compositions which disperse readily in water at the time of use, particularly in washing machines equipped with automatic dispensing mechanisms.
[0033] According to one embodiment of the present invention, the fabric softening compositions have a thickening / viscosity stable over time, for a period of at least 7 days, preferably for a period of at least 14 days . By "stable" is meant that the viscosity as measured with a Brookfield type RVT viscometer, after 7 days of storage, preferably after 14 days of storage, in the unstirred bottle, at a temperature of 25 ° C. 20 rpm, is at least equal to 50% of the viscosity measured according to the same protocol after 24 hours of storage in the unstirred bottle, at a temperature of 25 ° C.
[0034] Thus, according to this embodiment, the fabric softening composition comprising: - a cationic fabric softening agent and - a thickening polyurethane resulting from the condensation of: a) at least one compound of formula (I) : R - [(0E) ', - (OP)' - (OB) p [- OH (I) wherein: R is a linear or branched, saturated or unsaturated, carbon chain having from 17 to 24 atoms of carbon, [(0E) ', - (0P)' - (0B) p [represents an alkoxylated chain consisting of alkoxylated units, divided into blocks, alternating or random, chosen from the ethoxylated units OE, the propoxylated units OP and the butoxylated units OB, 20 m, n and p represent, independently of each other, 0 or an integer varying between 1 and 30, the sum of m, n and p being between 20 and 30, b) from at least one polyol, for example at least one poly (alkylene glycol) and at least one polyisocyanate, and having a rheological profile such that: its pi viscosity, as measured with a Brookfield type RVT viscometer, after 24 hours of storage, in the unstirred flask, at a temperature of 25 ° C at a speed of rotation of 20 rpm, is greater than 300 mPa.s, for example greater than 400 mPa.s or 500 mPa.s and its viscosity p.2, as measured with a Brookfield type RVT viscometer, after 7 days of storage, for example after 14 days. storage days in the unstirred flask at a temperature of 25 ° C at a rotation speed of 20 rpm is greater than 50% of the pI value, for example greater than 60 or 70% of the pi value
[0035] The cationic fabric softening agent is chosen so as to bring softness and swelling to the tissues treated during rinsing, after leaching. It is also likely to provide antistatic properties. Without being bound by the following theory concerning the mechanism of action of the cationic fabric softening agents, it is probable that the fixation, via the cationic unit, of fatty chains on the surface of the fibers lubricates them and allows them to to move relative to each other, thus reducing the impression of stiffness associated with an untreated linen. According to the present invention, the cationic fabric softening agent can in particular be a compound comprising an N + cationic nitrogen atom, at least one fatty chain, for example a carbon chain of 4 to 36 atoms, and at least one functional group. ester. The fatty chain may include atoms other than carbon atoms. For example, it may comprise Si silica atoms. The N + cationic nitrogen atom may be linked to the fatty chains via the ester functions, for example by means of: - chains - (CH2) '- O - C (= 0) -, in which n varies between 0 and 5 and / or - chains = C (- O - C (= O) - (CH2) '- CH3) 2 in which n varies between 4 and 36 atoms of carbon. It may, for example, be an "esterquat" type compound (EQ). Various types of quaternary ammonium compounds containing an ester can be used in the context of the present invention, including quaternary ammonium triester (TEQ) compounds and quaternary ammonium diester (DEQ) compounds. These compounds may also comprise a mixture of mono- (I), di- (II) and tri- (III) ester components.
[0036] According to one embodiment of the present invention, said cationic fabric softening agent is a quaternary triester ammonium compound (TEQ) and / or a quaternary ammonium ester compound (DEQ). Esterquat-type compounds are commercially available. They are sometimes called, in an equivalent manner, cationic surfactants. The compounds of esterquat type according to the invention may, for example, consist of two or three ester radicals substituted with alkyl or alkenyl groups, according to the definition given above.
[0037] The cationic fabric softening agent is, for example, chosen, without limitation, from the list of products below: Methyl bis [ethyl (tallowate)] -2-hydroxyethyl ammonium methyl sulfate (RewoquatTMWE 18, RewoquatTMWE 15, RewoquatTMWE 38, Evonik company), origin: animal tallow, Di-Palm carboxyethyl hydroxyethyl methyl ammonium methosulphate (RewoquatTM WE HV, Evonik company), origin: palm oil, N, N'-di (alkylcarboxyethyl) N-hydroxyethyl-N-methylammonium methyl sulfate (RewoquatTM WE 45, Evonik company), - unsaturated fatty acids C10-20 and C16-18, mono-, di- and tri-esters (HisofterTM HK 9061, HisofterTM MEQ 710, HisofterTM NEQ 70 , Ohsung Chem), - StepantexTM DC 90 commercial product (Stepan company), origin: rapeseed oil, - unsaturated C16-18 and C18 fatty acids (StepantexTM GA 90, Stepantex PA 88E, StepantexTM SP 90, Stepan company) origin: partially hydrogenated palm oil, - commercial product S tepantexTmVA or StepantexTM VL 90A (Stepan company), origin: partially hydrogenated tallow, - Methyl bis [ethyl (tallowate)] -2-hydroxyethyl ammonium methyl sulphate, (StepantexTMVK90, StepantexTMVT 90, Stepan company), origin: partially hydrogenated tallow, - C16-18 and C18 unsaturated fatty acids (StepantexTM VL 85G, StepantexTM VL 88E, Stepan company), origin: partially hydrogenated tallow, StepantexTM VR 90 commercial product (Stepan company), origin: tallow, Di (Tallowamidoethyl) hydroxyethylmethylammonium methylsulfate ( IncrosoftTM T90, Croda Company), origin: tallow, - Di (oleyl-carboxyethyl), or Hydroxyethyl Methyl Ammonium Methylsulfate, (IncrosoftTM TSO 90, Croda company), - C16-C18 dialkyl chloride, ammonium dimethyl ester chloride quaternary (ArmosoftTM DEQ, Akzo company), origin: tallow, - N, N-di (canola-oyloxyethyl) -N, N-dimethylammonium chloride (Adogen TM CDMC, Degussa company), origin: Canola oil, - Tallowo Ylethyl Hydroxyethyl Hydroxyethylmonium Methosulfate and Ditallowoylethyl Hydroxyethylmonium Methosulfate (BritesoftTM EQ 90, Chemelco Company), - commercial product Tetranyl LI / 90STM or Tetranyl AT1 (Kao company), origin: animal tallow, - hydroxyethylmonium methosulfate (TetranylTmC0 40 and Tetranyl AO-1, Kao ), - commercial product Tetranyl L6 / 90TM (Kao company), origin: palm oil, - Hydroxyethyl Methyl Ammonium Methylsulfate (ElotantTM EQ 200E, ElotantTM EQ 100, LG Household), - commercial product ElotantTM EQ 400 or ElotantTM EQ 500 ( LG Household) and - commercial product ArquatTM 2HT-75 (Akzo company). According to one aspect of the invention, the aqueous composition further comprises at least one additive selected from the group consisting of a fragrance, a biocide, a pH regulator, an antifoam agent, a coloring agent, an agent antistatic agent, an opacifying agent, a bleaching agent (for example a peracid), an enzymatic agent and an optical brightener. The aqueous composition according to the present invention may comprise a mixture of two or more of these additives.
[0038] According to one aspect of the present invention, the aqueous composition comprises from 0.02% to 5% by weight of active material of said polyurethane. According to another aspect of the present invention, the aqueous composition comprises from 0.05% to 2% by weight of active material of said polyurethane. By "weight of active ingredient" is meant the dry weight of polyurethane according to the invention, independently of the other ingredients of the composition. According to one aspect of the present invention, the aqueous composition comprises from 1% to 30% by weight of cationic fabric softening agent, preferably from 2% to 12% by weight or from 2.5 to 10% by weight. dry.
[0039] Process for the Preparation of the Softening Composition The softening composition is prepared according to the standard methods known to those skilled in the art. The cationic fabric softening agent is generally in a solid form at room temperature, so it is necessary to melt it before incorporating it into an aqueous composition. Thus, this agent is heated to a temperature at least greater than its melting temperature.
[0040] According to one embodiment, the cationic fabric softening agent is heated at a temperature of between 45 ° C. and 70 ° C., for example between 50 ° C. and 65 ° C., before being incorporated into the remainder of the formulation. . According to one embodiment of the method for preparing the softening composition, the cationic agent for softening the tissues in liquid form, in the molten state, is incorporated in a volume of water, for example demineralised, preheated to a minimum. temperature at least higher than the melting temperature of the cationic fabric softening agent. Thus, according to this embodiment of the process for preparing the softening composition, said volume of water, for example demineralised, is heated to a temperature greater than 45 ° C., for example greater than 50 ° C., for example to 70 ± 2 ° C. The incorporation of the cationic agent in liquid form, in the molten state, into the said volume of water is preferably stirred. After incorporation of the fabric softening agent into the determined amount of water, the solution is allowed to cool to a temperature below the melting temperature of the cationic fabric softening agent. According to one embodiment, the solution is allowed to cool to a temperature below 40 ° C, for example below 35 ° C, for example a temperature of 30 ± 2 ° C. Then, if necessary, the additive (s) selected from the group consisting of a fragrance, a biocide, a pH regulator, an antifoaming agent, a coloring agent, an antistatic agent, an opacifier, bleaching (eg a peracid), an enzymatic agent and an optical brightener. Finally, the polyurethane thickener according to the present invention is added as described above. The addition of the polyurethane can be done with stirring or using any means allowing homogeneous incorporation of said polyurethane in the formulation. Use According to one aspect of the present invention, said thickening polyurethane resulting from the condensation of: a) at least one compound of formula (I): R - [(OE) ', - (OP)' - (0B) p I OH (I) in which: R is a linear or branched, saturated or unsaturated, carbon chain having from 17 to 24 carbon atoms, [(OE) ', - (OP)' - (0B) p] represents a alkoxylated chain consisting of alkoxylated units, divided into blocks, alternating or random, chosen from the ethoxylated units OE, the propoxylated units OP and the butoxylated units OB, m, n and p represent, independently of each other, 0 or a number an integer varying between 1 and 30, the sum of m, n and p being between 20 and 30, b) at least one polyol, for example at least one poly (alkylene glycol) and c) at least a polyisocyanate is used to thicken a softening composition containing a cationic fabric softening agent. Said polyurethane may in particular be used to thicken a fabric softening composition at a viscosity p1, as measured with a Brookfield type RVT viscometer, after 24 hours of storage, in the unstirred bottle, at a temperature of 25.degree. the speed of rotation of 20 rpm, greater than 300 mPa.s, for example greater than 400 mPa.s or 500 mPa.s. Said polyurethane may in particular be used to thicken a fabric softening composition to: - a viscosity! II, as mentioned above and - a viscosity p.2, as measured with a Brookfield viscometer type RVT, after 7 days storage, for example after 14 days of storage, in the unstirred bottle, at a temperature of 25 ° C at the speed of rotation of 20 rpm, greater than 50% of the value of p1, for example greater than 60 or at 70% of the pi value
[0041] The examples which follow make it possible to better understand the present invention without limiting its scope.
[0042] EXAMPLES The Brookfield viscosity of fabric softening compositions was measured using a Brookfield type RVT viscometer after 24 hours of storage in the unstirred vial at a temperature of 25 ° C at 20 ° C. revolutions per minute (example 1) or 10 revolutions per minute (example 2) with the appropriate mobile. Playback is performed after 1 minute of rotation. A Brookfield viscosity measurement of -B1 (20 (mPa · $) is obtained, Brookfield viscosities are also measured at T = 7 and at T = 14 J.
[0043] Example 1 This example illustrates the use of thickening polyurethanes according to the invention in a fabric softening composition comprising a cationic esterquat agent. All raw materials are commercially available. Process for the Preparation of the Fabric Softening Composition 55.6 g of StepquartxTM VT90 (90%) esterquat cationic agent from Stepan are melted at 60 ° C.
[0044] 944.4 g of demineralized water are heated to 70 ° C. The water is stirred and the cationic agent is poured into the hot water. The mixture is allowed to cool to 30 ° C with continuous stirring. 5 g of perfume are added, in this case lavandin essential oil (Lavendula burnatii) and 0.7 g of violet dye with a 1% solids content (INCI name: violet pigment 23).
[0045] 1005.5 g of softening base are obtained in which the thickener to be tested is added. More specifically, polyurethanes according to the invention (tests 1-4 and 1-5) are used, using a compound of formula (I). In parallel, this example also illustrates polyurethanes outside the invention (tests 1-1, 1-2, 1-3 and 1-6).
[0046] Test 1-1 (outside the invention) Said polyurethane results from the condensation of, expressed in% by weight relative to the total weight of the polyurethane: - 20.1% by weight of an alcohol of formula: 2-hexyl-2-decanyl - (0E) 25 - OH (16 carbon atoms, branched chain), - 74.9% by weight of PEG 10,000 and - 5.0% by weight of isophorone diisocyanate (IPDI). Test 1-2 (outside the invention) Said polyurethane results from the condensation of, expressed in% by weight relative to the total weight of the polyurethane: - 26.1% by weight of an alcohol of formula: R - [(0E) ' In which: - m = 36, n = 0 and p = 0 and - R is a C20: 0 chain, branched to 20 carbon atoms, - - (OP) '- (0B) p [- OH (I) 69.3% by weight of PEG 10,000 and - 4.6% by weight of isophorone diisocyanate (IPDI). Test 1-3 (outside the invention) Said polyurethane results from the condensation of, expressed in% by weight relative to the total weight of the polyurethane: - 4.4% by weight of an alcohol of formula: R - [(0E) ' In which: - m = 0, n = 0 and p = 0 and - R is a C12: 0 chain, linear to 12 carbon atoms, -, - (OP) '- (0B) p [- OH (I) 90.4% by weight of PEG 10,000 and - 5.2% by weight of isophorone diisocyanate (IPDI).
[0047] Test 1-4 (according to the invention) Said polyurethane results from the polymerization of, expressed in% by weight relative to the total weight of the polyurethane: - 17.6% by weight of a compound of formula (I): R - [(0E) ', - (OP)' - (0B) p I - OH (I) in which: -m = 20, n = Oetp = O and - R is a C18: 1 chain, linear to 18 carbon atoms with unsaturation, - 76.6% by weight of PEG 10,000 and - 5.8% by weight of isophorone diisocyanate (IPDI).
[0048] Test 1-5 (according to the invention) Said polyurethane results from the polymerization of, expressed in% by weight relative to the total weight of the polyurethane: - 21% by weight of a compound of formula (I): R - [( Wherein: - m = 25, n = 0 and p = 0 and - R is a C22: 0 chain, linear at 22 atoms carbon, 73.5% by weight of PEG 10,000 and 5.5% by weight of isophorone diisocyanate (IPDI). Test 1-6 (outside the invention) The exemplified polyurethane results from the condensation of two different alcohols of formula (I). More specifically, said polyurethane results from the condensation of, expressed in% by weight relative to the total weight of the polyurethane: - 8.9% by weight of a compound of formula (I): R - [(0E) ', - (OP) '- (0B) p I - OH (I) in which: - m = 23, n = 0 and p = 0 and - R is a C12: 0 chain, linear to 12 carbon atoms, - 11, 6% by weight of a compound of formula (I) ': R - [(OE)', - (OP) '- (0B) p I - OH (I)' in which: - m = 25, n = 0 and p = 0 and - R is a C32: 0 chain, branched to 32 carbon atoms, - 73.9% by weight of PEG 10,000 and - 5.6% by weight of isophorone diisocyanate (IPDI).
[0049] Polyurethanes are formulated in water in the presence of a surfactant which is Mergital® D8. PU / surfactant / water ratios are 17.5 / 9.5 / 73. Then they are added to the fabric softening composition in mass ratios shown in Table 1 below.
[0050] All the results were summarized in Table 1. For each of the tests, the viscosities -B1 (20 were determined, according to the methods described above at T = 24 h, at T = 7 d and at T = 14 d at room temperature.
[0051] Test 1-1 1-2 1-3 1-4 1-5 1-6 HInv HInv HInv INV INV HInv Mass of softening composition (g): 100 100 100 100 100 100 Mass of thickener pU to be tested (g): 0.307 0.308 0.307 0.301 0.310 0.308! -Isk20 at T, 24h (mPa · $) -, u / 125 245 170 465 665 205! -1131 (20 at T = 7 d (mPa · $) - p 2 70 135 105 305 520 190, u2 /, u / (%) at T = 7j 56 55 62 65 6 78 92 7! -1131 (20 at T = 14 d (mPa. $) - p2 60 115 235 360 μ2 / μ1 (%) at Table 1 HInv: Excluding Invention INV: Invention There is a significantly improved thickening in the formulations using a polyurethane thickener according to tests 1-4 and 1-5 (according to the invention), compared to those of tests 1-1 to 1-3 and 1-6 (outside the invention) Furthermore, the thickening polyurethanes according to the invention allow a stable thickening at 7 days and at 14 days: the ratio 11.2 /! Ji (%) is greater than 50% for all tests carried out with a thickening polyurethane corresponding to x criteria of the present invention, which is not the case for the thickeners outside invention. EXAMPLE 2 This example illustrates the use of a thickening polyurethane according to the invention in a fabric softening composition, comprising a cationic agent of quat type. All raw materials are commercially available. Process for preparing the fabric softening composition 50 g of ArquatTm 2HT-75 (75%) cationic agent from Akzo were melted at 60 ° C. 950 g of demineralized water are heated to 70 ° C. The water is stirred and the cationic agent is poured into the hot water. The mixture is allowed to cool to 30 ° C with continuous stirring. 1000 g of softening composition is obtained in which the thickener to be tested is added.
[0052] Test 2-1 (according to the invention) Said polyurethane results from the polymerization of, expressed in% by weight relative to the total weight of the polyurethane: - 21% by weight of a compound of formula (I): R - [( Wherein: - m = 25, n = 0 and p = 0 and - R is a C22: 0 chain, linear at 22 atoms carbon, 73.5% by weight of PEG 10,000 and 5.5% by weight of isophorone diisocyanate (IPDI). Polyurethane is formulated in water in the presence of a surfactant which is Mergital® D8. PU / surfactant / water ratios are 17.5 / 9.5 / 73.
[0053] Then, it is added to the fabric softening composition in mass ratios shown in Table 2 below. All results are summarized in Table 2.
[0054] The p.Bkio viscosities were determined according to the method described above at T = 0, before addition of the polyurethane, at T = 24 h and at T = 7 days, at room temperature. Test 2-1 Invention Mass of softening composition (g): 100 1-1131 (10 before addition pU (mPa.s) 1510 Mass of thickener pU to be tested (g): 0.299! -1131 (10 to T = 24 h (mPa. $) - Pi 3 220 1.113k10 at T = 7 d (mPa. $) - P2 3020 μ2 / μl (%) at T = 7 d 93.8 Table 2
权利要求:
Claims (10)
[0001]
REVENDICATIONS1. A fabric softening composition comprising: - a cationic fabric softening agent and - a polyurethane thickener resulting from the polymerization of: a) at least one compound of formula (I): R - [(OE) ', - (OP) '- (0B) p I - OH (I) in which: R is a linear or branched, saturated or unsaturated carbon chain having from 17 to 24 carbon atoms, [(OE)', - ( OP) '- (0B) p [represents an alkoxylated chain consisting of alkoxylated units, divided into blocks, alternating or random, chosen from ethoxylated units EO, propoxylated units OP and butoxylated units OB, m, n and p represent , independently of each other, 0 or an integer ranging between 1 and 30, the sum of m, n and p being between 20 and 30, b) of at least one polyol, for example at least one poly (alkylene glycol) and c) at least one polyisocyanate.
[0002]
2. Composition according to claim 1, wherein said polyurethane thickener results from the polymerization of at least one compound of formula (I) in which R is a carbon chain having at least one unsaturation, linear or branched, having from 17 to 24. carbon atoms.
[0003]
3. Composition according to any one of the preceding claims, according to which said thickening polyurethane results from the condensation of at least one compound of formula (I) in which n and p are zero and m represents an integer ranging between 20 and 30. .
[0004]
4. Composition according to any one of the preceding claims, wherein said thickening polyurethane results from the condensation of at least one compound of formula (I) in which n and p are zero and m represents an integer ranging between 25 and 30.
[0005]
5. Composition according to any one of the preceding claims, according to which said thickening polyurethane results from the condensation of: a) from 1% to 29% by weight of at least one compound of formula (I), b) by 70% 98% by weight of at least one poly (alkylene glycol) and c) from 1% to 29% by weight of at least one polyisocyanate, the sum of these mass percentages being equal to 100%. 10
[0006]
6. Composition according to claim 5, wherein said thickening polyurethane results from the condensation of: a) from 3% to 10% by weight of at least one compound of formula (I), b) from 80% to 94% by weight; weight of at least one poly (alkylene glycol) and c) from 3% to 10% by weight of at least one polyisocyanate, the sum of these mass percentages being equal to 100%.
[0007]
A composition according to any one of the preceding claims, wherein said cationic fabric softening agent is a quaternary triester ammonium compound (TEQ) and / or a quaternary ammonium ester compound (DEQ).
[0008]
8. Composition according to any one of the preceding claims, having a viscosity greater than 300 mPa.s, as measured with a Brookfield type RVT viscometer, after 24 hours of storage in the unstirred flask, at a temperature of 25 ° C. at the speed of rotation of 20 rpm.
[0009]
A composition according to any one of the preceding claims having a rheological profile such as: - its pI viscosity, as measured with a Brookfield type RVT viscometer, after 24 hours of storage, in the unstirred vial, at a temperature from 25 ° C to 20 rpm is greater than 300 mPa.s and its p.2 viscosity, as measured with a Brookfield type RVT viscometer, after 7 days of storage, e.g. The storage days in the unstirred flask at a temperature of 25 ° C at a rotation speed of 20 rpm is greater than 50% of the value of 1.-11.
[0010]
10. Use of a thickening polyurethane resulting from the condensation of: a) at least one compound of formula (I): R - [(OE) ', - (OP)' - (OB) p I - OH (I) in which: R is a linear or branched, saturated or unsaturated, carbon chain having from 17 to 24 carbon atoms, [(OE) ', - (OP)' - (0B) p [represents an alkoxylated chain consisting of alternately or randomly divided alkoxylated units selected from the ethoxylated units OE, the propoxylated units OP and the butoxylated units OB, m, n and p represent, independently of one another, 0 or an integer varying between 1 and 30, the sum of m, n and p being between 20 and 30, b) of at least one polyol, for example of at least one poly (alkylene glycol) and c) of at least one polyisocyanate, for thickening a softening composition containing a cationic fabric softening agent.
类似技术:
公开号 | 公开日 | 专利标题
EP3169764A1|2017-05-24|Fabric softening composition comprising a heur thickener
EP2134826B1|2015-11-04|Anti-grey detergent
WO2007134977A1|2007-11-29|Encapsulated bleaching agent particles
WO2007087953A1|2007-08-09|Washing or cleaning composition comprising dye transfer inhibitor
WO2019102115A1|2019-05-31|Self-invertible inverse latex comprising alkyl polyglycosides as an inverting agent and use thereof as a thickening agent for a detergent or cleaning formulation for industrial or domestic use
WO2006077049A2|2006-07-27|Antiadhesive polymer for prevention of adhesion of microorganisms to textiles and for prevention of laundry odours
WO2007107191A1|2007-09-27|Multiphase laundry detergent, dishwasher detergent or cleaning composition with vertical phase boundaries
WO2016009149A1|2016-01-21|Fabric softening composition comprising a heur thickener
EP3177661A1|2017-06-14|Thickening agent for aqueous systems, formulations containing same and use thereof
WO2016020622A1|2016-02-11|Use in detergent compositions of polymers obtained by low-concentration, inverse emulsion polymerization with a low content of neutralized monomers
WO2009019136A1|2009-02-12|Color-safe detergent or cleaning agent having optical brightener
KR20180064519A|2018-06-14|Liquid detergent formulations or cleaning formulations containing N, N'-diarylam- i-cysteine derivatives
WO2009106378A1|2009-09-03|Low-concentration liquid detergents or cleaners containing perfume
EP1198551B1|2005-06-29|Bleaching compositions
JP5779498B2|2015-09-16|Liquid softener composition
EP3611246B1|2021-03-10|Fabric treatment compositions comprising benefit agent capsules
WO2008012141A2|2008-01-31|Detergent having improved dispersing power
EP1375633B1|2006-09-27|Detergent compositions comprising polymers
EP3041920B1|2018-10-10|Detergent composition with improved performance
EP2929003A1|2015-10-14|Removal of greasy stains
DE102013216776A1|2015-02-26|Detergents and cleaning agents with improved performance
DE102007023872A1|2008-11-27|Detergent, useful to improve the graying-inhibiting action during washing of textile products, comprises anti-grey polycarbonate, polyurethane and polyurea-polyorganosiloxane compound and a surfactant
DE102007016382A1|2008-10-09|Detergent, preferably aqueous liquid detergent useful in the washing of textile products, comprises surfactant and ingredients of washing- and cleaning- agent comprising |-dioxolan-2-one compound or |-diazepan-2-one compound
DE102017223455A1|2019-06-27|Liquid washing or cleaning agent containing a glucosamine derivative
EP3218464A1|2017-09-20|Detergents and cleaning agents having improved performance
同族专利:
公开号 | 公开日
FR3023846B1|2017-12-22|
US20170198238A1|2017-07-13|
EP3169764A1|2017-05-24|
MX2016017050A|2017-05-12|
WO2016009150A1|2016-01-21|
CN106459845A|2017-02-22|
CA2951115A1|2016-01-21|
引用文献:
公开号 | 申请日 | 公开日 | 申请人 | 专利标题
US6001797A|1998-07-20|1999-12-14|Colgate-Palmolive Co.|Liquid fabric softening compositions containing a fatty alcohol ethoxylate diurethane polymer as a thickener|
US20090291876A1|2005-06-14|2009-11-26|Paul William Blanco|Fabric Softening Composition|
US4155892A|1975-10-03|1979-05-22|Rohm And Haas Company|Polyurethane thickeners for aqueous compositions|
JPS5277292A|1975-12-22|1977-06-29|Toray Industries|Production of fiber structure|
JPS5634752A|1979-08-29|1981-04-07|Tokai Seiyu Kogyo Kk|Production of fiber-finishing agent|
JP2625374B2|1993-12-16|1997-07-02|グンゼ株式会社|Durable soft finish|
FR2732031B1|1995-03-23|1997-04-30|Coatex Sa|USE OF AMPHOTERIC AGENTS AS MODIFIERS OF LAMELLAR PHASES OF LIQUID OR PASTY DETERGENT OR COSMETIC COMPOSITIONS|
US6020304A|1996-04-01|2000-02-01|The Procter & Gamble Company|Fabric softener compositions|
US6440431B1|1998-12-17|2002-08-27|Shiseido Co., Ltd.|Cosmetic composition|
US6924261B2|2002-11-01|2005-08-02|Colgate-Palmolive Co.|Aqueous composition comprising oligomeric esterquats|
US7432325B2|2004-11-15|2008-10-07|Rohm And Haas Company|Nonionic associative thickener containing condensation polymer backbone|
US7754671B2|2004-12-27|2010-07-13|The Dial Corporation|Liquid laundry detergent containing an ethoxylated anionic/nonionic surfactant mixture and fabric conditioner|
US7776108B2|2005-06-07|2010-08-17|S.C. Johnson & Son, Inc.|Composition for application to a surface|
EP1849855A1|2006-04-27|2007-10-31|Degussa GmbH|thixotropic softening compositions|
DE102006027490A1|2006-06-14|2007-12-20|Borchers Gmbh|Water-soluble or -dispersible polyurethane for use as a thickener for aqueous paint or adhesives, obtained by reacting polyether-polyol with di-isocyanate and an unsaturated mono-alcohol or mono-alcohol alkoxylate|
US8828098B2|2006-12-18|2014-09-09|3M Innovative Properties Company|Extenders for fluorochemical treatment of fibrous substrates|
US7741401B2|2007-03-21|2010-06-22|Rohm And Haas Company|Thickener blend composition and method for thickening aqueous systems|
FR2945964B1|2009-05-28|2012-02-17|Coatex Sas|USE OF A ACRYLIC COMBED POLYMER CONTAINING A ACRYLIC ESTER AS A DISPERSING AGENT AND ANTI-DEMOUSSANT IN AQUEOUS SUSPENSION OF CALCIUM SULPHATE HEMIHYDRATE|
FR2948374B1|2009-07-23|2012-06-08|Cray Valley Sa|AQUEOUS SELF-RELEASING POLYMER DISPERSION BASED ON HARD-CORE STRUCTURED POLYMER PARTICLES AND SOFT BARK AND COATING OR TREATING COMPOSITIONS|
US20120082629A1|2010-09-01|2012-04-05|Basf Se|Associative Thickeners For Aqueous Preparations|
CA2848579A1|2011-09-13|2013-03-21|The Procter & Gamble Company|Fluid fabric enhancer compositions|
FR3000086B1|2012-12-20|2014-12-26|Coatex Sas|AGENT FOR OBTAINING A STABLE AQUEOUS COMPOSITION COMPRISING SUSPENDED PARTICLES|
FR3000085B1|2012-12-20|2016-06-10|Coatex Sas|POLYMERIC AGENT FOR OBTAINING A STABLE AQUEOUS COMPOSITION COMPRISING SUSPENDED PARTICLES|
FR3023845B1|2014-07-18|2018-01-05|Coatex Sas|FABRIC SOFTENING COMPOSITION COMPRISING A HEAVY THICKENING.|FR3023845B1|2014-07-18|2018-01-05|Coatex Sas|FABRIC SOFTENING COMPOSITION COMPRISING A HEAVY THICKENING.|
FR3075206B1|2017-12-19|2020-07-24|Coatex Sas|THICKENING AGENT AND SOFTENING COMPOSITION|
EP3956104A1|2019-04-16|2022-02-23|3M Innovative Properties Company|Abrasive article and method of making the same|
WO2021161129A1|2020-02-10|2021-08-19|3M Innovative Properties Company|Coated abrasive article and method of making the same|
WO2022023879A1|2020-07-28|2022-02-03|3M Innovative Properties Company|Coated abrasive article and method of making the same|
法律状态:
2015-06-29| PLFP| Fee payment|Year of fee payment: 2 |
2016-01-22| PLSC| Publication of the preliminary search report|Effective date: 20160122 |
2016-06-13| PLFP| Fee payment|Year of fee payment: 3 |
2017-06-13| PLFP| Fee payment|Year of fee payment: 4 |
2018-06-12| PLFP| Fee payment|Year of fee payment: 5 |
2019-06-19| PLFP| Fee payment|Year of fee payment: 6 |
2021-04-09| ST| Notification of lapse|Effective date: 20210305 |
优先权:
申请号 | 申请日 | 专利标题
FR1456934A|FR3023846B1|2014-07-18|2014-07-18|FABRIC SOFTENING COMPOSITION COMPRISING A HEAVY THICKENING.|FR1456934A| FR3023846B1|2014-07-18|2014-07-18|FABRIC SOFTENING COMPOSITION COMPRISING A HEAVY THICKENING.|
MX2016017050A| MX2016017050A|2014-07-18|2015-07-16|Fabric softening composition comprising a heur thickener.|
CN201580031070.6A| CN106459845A|2014-07-18|2015-07-16|Fabric softening composition comprising a HEUR thickener|
EP15756197.8A| EP3169764A1|2014-07-18|2015-07-16|Fabric softening composition comprising a heur thickener|
US15/315,259| US20170198238A1|2014-07-18|2015-07-16|Fabric-softening composition comprising an heur thickener|
PCT/FR2015/051946| WO2016009150A1|2014-07-18|2015-07-16|Fabric softening composition comprising a heur thickener|
CA2951115A| CA2951115A1|2014-07-18|2015-07-16|Fabric softening composition comprising a heur thickener|
[返回顶部]