专利摘要:
A new alumina gel having a high dispersibility index, and in particular a dispersibility index greater than 70%, a crystallite size of between 1 and 35 nm, and a sulfur content of between 0.001% and 2% by weight and a sodium content of between 0.001% and 2% by weight, the weight percentages being expressed relative to the total mass of alumina gel. The present invention also relates to the process for preparing said gel comprising at least one step of precipitating at least one aluminum salt, at least one step of heating the suspension obtained and a final heat treatment step to form the gel of alumina.
公开号:FR3022235A1
申请号:FR1455421
申请日:2014-06-13
公开日:2015-12-18
发明作者:Malika Boualleg;Celine Bouvry;Patrick Euzen
申请人:IFP Energies Nouvelles IFPEN;
IPC主号:
专利说明:

[0001] TECHNICAL FIELD The present invention relates to the preparation of alumina gels. In particular, the present invention relates to a novel alumina gel having high dispersibility as well as to its precipitation preparation process. PRIOR ART Several operating protocols known in the prior art lead to dispersible alumina gels. Several patents describe in particular a preparation process called "sol-gel". U.S. Patent No. 4,676,928 discloses a method for producing a water-dispersible alumina comprising a step of forming an aqueous dispersion of alumina, a step of adding an acid to produce an acidic dispersion having a pH between 5 and 9, a maturation step at an elevated temperature above 70 ° C for a time sufficient to transform the alumina colloidal gel, then a drying step of said colloidal gel obtained. No. 5,178,849 also describes a process for producing an alpha alumina comprising a step of dispersing an aluminum hydrate having a dispersibility of less than 70%, a step of acidifying the dispersion obtained at a lower pH. at 3.5 to at least partially dissolve the aluminum hydrate, a hydrothermal treatment step of the acid dispersion obtained at a temperature between 150 and 200 ° C, a pressure of between 20 atm for a period of time between 0 , 15 and 4 hours to obtain a colloidal boehmite having a dispersibility greater than 90%.
[0002] The alumina gel preparation by precipitation is also well known in the prior art. In particular, US Pat. No. 7,790,652 describes the preparation by precipitation of an alumina support having a very specific porous distribution, which can be used as a catalyst support in a process for hydroconversion of heavy hydrocarbon feeds. The alumina support is prepared according to a method comprising a first step of forming an alumina dispersion by mixing, in a controlled manner, a first aqueous alkaline solution and a first aqueous acid solution, at least one of said 2 Acidic and basic solutions, or both comprising an aluminum compound. The acidic and basic solutions are mixed in such proportions that the pH of the resulting dispersion is between 8 and 11. The acidic and basic solutions are also mixed in amounts to obtain a dispersion containing the desired amount of alumina in particular, the first step makes it possible to obtain 25 to 35% by weight of alumina with respect to the total amount of alumina formed at the end of the two precipitation stages. The first stage operates at a temperature of between 20 and 40 ° C. When the desired amount of alumina is formed, the temperature of the slurry is raised to a temperature between 45 and 70 ° C, and then the heated slurry is then subjected to a second precipitation step by contacting said slurry with a second alkaline aqueous solution and a second acidic aqueous solution, at least one or both of the two solutions comprising an aluminum compound. Similarly, the pH is adjusted between 8 and 10.5 by the proportions of the acid and basic solutions added and the remaining quantity of alumina to be formed in the second stage is provided by the amounts of the second acid and basic solutions added. The second step operates at a temperature of between 20 and 40 ° C. The alumina gel thus formed comprises at least 95% of boehmite. The dispersibility of the alumina gel thus obtained is not mentioned. The alumina gel is then filtered, washed and optionally dried according to the methods known to those skilled in the art, without prior curing step, to produce an alumina powder which is then shaped according to the known methods of the invention. skilled in the art, then calcined to produce the final alumina support. The first precipitation step of the preparation method of US Pat. No. 7,790,652 is limited to a low alumina production of between 25 and 35% by weight, since higher alumina production at the end of the first stage does not allow optimal filtration of the gel obtained. Moreover, the increase in the production of alumina in the first step of US Pat. No. 7,790,652 would not allow the shaping of the gel thus obtained. The present invention proposes to overcome the disadvantages of the preparation process according to US Pat. No. 7,790,652. The Applicant has thus discovered a novel process for the preparation by precipitation of an alumina gel that can make it possible to obtain said alumina gel. at the end of a single precipitation step, operating at low temperature, the second precipitation step 3022235 being optional. In particular, the new process for preparing the alumina gel according to the invention makes it possible to obtain at least 40% by weight of alumina in equivalent Al 2 O 3 with respect to the total amount of alumina formed at the end of said process of preparation of the gel, from the first precipitation step, the amount of alumina formed at the end of the first precipitation step can even reach 100%, a second precipitation step not being necessary in this case. Moreover, the new preparation process according to the invention is characterized by the presence of a final heat treatment step and in particular a final ripening step making it possible to obtain an alumina gel having improved filterability, allowing a better productivity of the process according to the invention as well as an extrapolation of the process at the industrial level easier. Said process according to the invention also makes it possible to obtain an alumina gel having a better dispersibility index with respect to the alumina gels of the prior art, thus facilitating its shaping according to the known techniques of the skilled person.
[0003] An object of the present invention is therefore to provide an alumina gel having a high dispersibility index, and in particular a dispersibility index greater than 70%, and up to 100%. Another object of the present invention is to provide a new process for the preparation of said alumina gel by precipitation, in an aqueous reaction medium, of at least one basic precursor and at least one acidic precursor, at least one basic or acidic precursors or both comprising aluminum, in relative proportions and in very specific amounts defining the operating conditions of said step and making it possible to obtain an alumina gel having a high dispersibility index, and in particular a dispersibility index greater than 70%, preferably between 70 and 100%, preferably between 80 and 100%, very preferably between 85 and 100% and even more preferably between 90 and 100%. and 100%. SUMMARY AND OBJECT OF THE INVENTION The present invention relates to an alumina gel having a high dispersibility index, and in particular a dispersibility index greater than 70%, a crystallite size of from 1 to 35 nm, and that a sulfur content of between 0.001% and 2% by weight and a sodium content of between 0.001% and 2% by weight, the weight percentages being expressed relative to the total mass of alumina gel.
[0004] An advantage of the invention is to provide a new alumina gel having a very high dispersibility compared to the alumina gels of the prior art. An alumina gel characterized by a high dispersibility index will be more easily formed in accordance with all the shaping techniques known to those skilled in the art, such as, for example, by extrusion kneading, by granulation or by the the oil drop, a gel with a low dispersibility index. The subject of the present invention is also a process for the preparation of said alumina gel, said process comprising at least the following stages: a) at least one step of precipitation of alumina, in an aqueous reaction medium, of at least one precursor basic material selected from sodium aluminate, potassium aluminate, ammonia, sodium hydroxide and potassium hydroxide and at least one acidic precursor selected from aluminum sulfate, sodium chloride, aluminum, aluminum nitrate, sulfuric acid, hydrochloric acid, and nitric acid, wherein at least one of the basic or acidic precursors comprises aluminum, the relative flow of the acid precursors and basic is chosen so as to obtain a pH of the reaction medium of between 8.5 and 10.5 and the flow rate of the aluminum-containing acidic and basic precursor (s) is adjusted so as to obtain a progress rate of the first step 20 between 40 and 1 00%, the advancement rate being defined as the proportion of alumina formed in Al 2 O 3 equivalent during said first precipitation step relative to the total amount of alumina formed at the end of the precipitation step or steps, said step a) operating at a temperature between 10 and 50 ° C, and for a time between 2 minutes and 30 minutes, b) a heat treatment step of the suspension obtained at the end of step a) at a temperature between 50 and 200 ° C for a duration of between 30 minutes and 5 hours, c) a filtration step of the suspension obtained at the end of the heat treatment step b), followed by at least a washing step of the gel obtained.
[0005] An advantage of the invention is to provide a new process for the preparation by precipitation of an alumina gel making it possible to obtain at least 40% by weight of alumina in Al.sub.2 O.sub.3 equivalent relative to the total amount of alumina. formed at the end of the precipitation step or steps, the first precipitation step, the amount of alumina formed at the end of the first precipitation step can even reach 100%, a second precipitation step n not being necessary in this case. Furthermore, the process according to the invention characterized by the combination of this alumina precipitation step allowing the production of a high quantity of alumina and a final heat treatment stage of the suspension obtained, allows the obtaining an alumina gel having improved filterability, thereby promoting the productivity of the process according to the invention as well as an extrapolation of the process at the industrial level. Another advantage of the invention is to provide a novel process for the preparation of an alumina gel by precipitation which may comprise a single precipitation step, which is inexpensive compared with the conventional alumina preparation methods of the prior art. such as, for example, sol-gel preparation methods. Another advantage of the invention is to provide a novel method of preparing by precipitation of an alumina gel having a high dispersibility index with respect to the prior art gels. DESCRIPTION OF THE INVENTION The present invention relates to an alumina gel having a dispersibility index greater than 70%, a crystallite size of from 1 to 35 nm, and a sulfur content measured by the X-ray fluorescence method. between 0.001% and 2% by weight and a sodium content, measured by ICP or inductively coupled plasma spectrometry of between 0.001% and 2% by weight, the weight percentages being expressed relative to the total mass of gel alumina.
[0006] Throughout the rest of the text, the dispersibility index is defined as the weight percentage of peptised alumina gel which can be dispersed by centrifugation in a 3600 G polypropylene tube for 10 minutes. Dispersibility is measured by dispersing 10% boehmite or alumina gel in a water slurry also containing 10% nitric acid based on the boehmite mass. Then, the suspension is centrifuged at 3600G rpm for 10 min. The sediments collected are dried at 100 ° C. overnight and then weighed. The dispersibility index, denoted ID, is obtained by the following calculation: ID (° / 0) = 100% - mass of dried sediments (%).
[0007] Preferably, the alumina gel according to the invention has a dispersibility index of between 70 and 100%, preferably between 80 and 100%, very preferably between 85 and 100% and even more preferably between 90 and 100%.
[0008] Preferably, the alumina gel according to the invention has a crystallite size of between 2 and 35 nm. In particular, the alumina gel or boehmite in powder form according to the invention is composed of crystallites whose size, obtained by the Scherrer formula in X-ray diffraction according to the crystallographic directions (020) and (120) is respectively between 2 and 20 nm and between 2 and 35 nm. Preferably, the alumina gel according to the invention has a crystallite size in the crystallographic direction (020) of between 2 and 15 nm and a crystallite size in the crystallographic direction (120) of between 2 and 35 nm. X-ray diffraction on alumina or boehmite gels was performed using the conventional powder method using a diffractometer. Scherrer's formula is a formula used in X-ray diffraction on polycrystalline powders or samples which connects the half-height width of the diffraction peaks to the size of the crystallites. It is described in detail in the reference: Appl. Cryst. (1978). 11, 102-113 Scherrer after sixty years: A survey and some new results in the determination of crystallite size, J. I. Langford and A. J. C. Wilson.
[0009] According to the invention, the alumina gel prepared according to the invention has a content of impurities and in particular of sulfur, measured by the X-ray fluorescence method, of between 0.001% and 2% by weight and a sodium content. measured by ICP or Inductively Coupled Plasma Spectrometry between 0.001 and 2% by weight, the weight percentages being expressed relative to the total mass of alumina gel.
[0010] Preferably, the alumina gel prepared according to the invention comprises a sulfur content of between 0.001% (3/0 and 1% by weight, preferably between 0.001% and 0.40% by weight, very preferably between 0.003% and 0.001% by weight). 0.33 (3/0 weight, and more preferably between 0.005 and 0.25 weight%.
[0011] Preferably, the alumina gel prepared according to the invention comprises a sodium content of between 0.001% (3/0 and 1% by weight, preferably between 0.001 and 0.15% by weight). preferred between 0.0015 and 0.10% by weight, and even more preferably between 0.002 and 0.040% by weight.
[0012] The present invention also relates to a process for the preparation of said alumina gel. According to the invention, said preparation process comprises at least a first step a) of precipitation of alumina, in an aqueous reaction medium, of at least one basic precursor chosen from sodium aluminate and potassium aluminate. , ammonia, sodium hydroxide and potassium hydroxide and at least one acidic precursor selected from aluminum sulphate, aluminum chloride, aluminum nitrate, sulfuric acid, hydrochloric acid, and nitric acid, wherein at least one of the basic or acidic precursors comprises aluminum, the relative flow rate of the acidic and basic precursors is chosen so as to obtain a pH of the reaction medium comprised between 8.5 and 10.5 and the flow rate of the aluminum-containing acidic and basic precursor (s) is adjusted so as to obtain a forwarding rate of the first step of between 40 and 100%, the rate of progress being defined as the proportion of alumina f ormée in equivalent A1203 during said step a) of precipitation with respect to the total amount of alumina formed at the end of the precipitation step (s) and more generally at the end of the preparation process according to the invention, said step a) operating at a temperature between 10 and 50 ° C, and for a duration ccmprise between 2 minutes and 30 minutes.
[0013] In general, the "rate of progress" of the nth precipitation stage is understood to mean the percentage of alumina formed in Al 2 O 3 equivalent in the said nth stage, relative to the total amount of alumina formed at the same time. resulting from all the precipitation steps and more generally after the steps of preparation of the alumina gel.
[0014] In the case where the progress rate of said precipitation step a) is 100%, said precipitation step a) generally makes it possible to obtain an alumina suspension having an Al 2 O 3 concentration of between 20 and 100. g / 1, preferably between 20 and 80 g / l, more preferably between 20 and 50 g / l.
[0015] Step a) Precipitation The mixture in the aqueous reaction medium of at least one basic precursor and at least one acidic precursor requires either that at least the basic precursor or the acidic precursor comprises aluminum, or that the two basic and acidic precursors include aluminum. Basic precursors comprising aluminum are sodium aluminate and potassium aluminate. The preferred basic precursor is sodium aluminate. Acidic precursors comprising aluminum are aluminum sulphate, aluminum chloride and aluminum nitrate. The preferred acidic precursor is aluminum sulphate.
[0016] Preferably, the basic precursor (s) and acid (s) are added in said first precipitation step a) in aqueous solutions. Preferably, the aqueous reaction medium is water. Preferably, said step a) operates with stirring.
[0017] Preferably, said step a) is carried out in the absence of organic additive. The acidic and basic precursors, whether they contain aluminum or not, are mixed, preferably in solution, in the aqueous reaction medium, in such proportions that the pH of the resulting suspension is between 8.5 and 10. 5.
[0018] According to the invention, it is the relative flow rate of the acidic and basic precursors that they contain aluminum or not, which is chosen so as to obtain a pH of the reaction medium of between 8.5 and 10.5. . In the preferred case where the basic and acidic precursors are respectively sodium aluminate and aluminum sulphate, the mass ratio of said basic precursor to said acidic precursor is advantageously between 1.6 and 2.05. For the other basic and acidic precursors, whether they contain aluminum or not, the base / acid mass ratios are established by a curve of neutralization of the base by the acid. Such a curve is easily obtained by those skilled in the art. Preferably, said precipitation step a) is carried out at a pH of between 8.5 and 10 and very preferably between 8.7 and 9.9. The acidic and basic precursors are also mixed in amounts to obtain a suspension containing the desired amount of alumina, depending on the final concentration of alumina to be achieved. In particular, said step a) makes it possible to obtain 40 to 100% by weight of alumina in Al 2 O 3 equivalent relative to the total amount of alumina formed at the end of the precipitation stage or steps. According to the invention, it is the flow rate of the acidic and basic precursor (s) containing aluminum which is adjusted so as to obtain a forwarding rate of the first stage of between 40 and 100%.
[0019] Preferably, the rate of progress of said precipitation step a) is between 40 and 99%, preferably between 45 and 90% and preferably between 50 and 85%. the progress obtained at the end of the precipitation step a) is less than 100%, a second precipitation step is necessary so as to increase the amount of alumina formed. In this case, the advancement rate being defined as being the proportion of alumina formed in A1203 equivalent during said step a) of precipitation with respect to the total amount of alumina formed at the end of the two precipitation steps of process of preparation according to the invention. Thus, depending on the concentration of alumina targeted at the end of the precipitation step (s), preferably between 20 and 100 g / l, the quantities of aluminum to be provided by the acid and / or basic precursors are calculated and the flow rate of the precursors is adjusted according to the concentration of said added aluminum precursors, the amount of water added to the reaction medium and the rate of progress required for the precipitation step (s).
[0020] The flow rate of the aluminum-containing acidic and / or basic precursor (s) depends on the size of the reactor used and thus on the amount of water added to the reaction medium.
[0021] Preferably, said precipitation step a) is carried out at a temperature between 10 and 45 ° C, preferably between 15 and 45 ° C, more preferably between 20 and 45 ° C and most preferably between 20 and 45 ° C. and 40 ° C. It is important that said precipitation step a) operates at a low temperature. In the case where said preparation process according to the invention comprises two precipitation stages, the precipitation step a) is advantageously carried out at a temperature below the temperature of the second precipitation stage. Preferably, said precipitation step a) is carried out for a period of between 5 and 20 minutes, and preferably of 5 to 15 minutes.
[0022] Step b) heat treatment In accordance with the invention, said preparation method comprises a step b) of heat treatment of the suspension obtained at the end of the precipitation step a), said heat treatment stage operating at a temperature between 60 and 200 ° C for a period of between 30 minutes and 5 hours, to obtain the alumina gel. Preferably, said heat treatment step b) is a ripening step. Preferably, said heat treatment step b) operates at a temperature between 65 and 150 ° C, preferably between 65 and 130 ° C, preferably between 70 and 110 ° C, very preferably between 70 and 95 ° C. ° C. Preferably, said heat treatment step b) is carried out for a duration of between 40 minutes and 5 hours, preferably between 40 minutes and 3 hours, and preferably between 45 minutes and 2 hours.
[0023] Optional second precipitation step According to a preferred embodiment, in the case where the advancement rate obtained at the end of the precipitation step a) is less than 100%, said preparation method preferably comprises a second precipitation step a ') after the first precipitation step. Said second precipitation step makes it possible to increase the proportion of alumina produced.
[0024] Said second precipitation step a ') is advantageously carried out between said first precipitation step a) and the heat treatment step b). In the case where a second precipitation step is carried out, a step of heating the suspension obtained at the end of step a) of precipitation is advantageously carried out between the two precipitation steps a) and '). Preferably, said step of heating the suspension obtained at the end of step a), carried out between said step a) and the second precipitation step a ') operates at a temperature of between 20 and 90 ° C. preferably between 30 and 80 ° C, preferably between 30 and 70 ° C and very preferably between 40 and 65 ° C. Preferably, said heating step is carried out for a period of between 7 and 45 minutes and preferably between 7 and 35 minutes.
[0025] Said heating step is advantageously carried out according to all the heating methods known to those skilled in the art. According to said preferred embodiment, said method of preparation comprises a second step of precipitation of the suspension obtained at the end of the heating step, said second stage operating by adding to said suspension at least one basic precursor selected among sodium aluminate, potassium aluminate, ammonia, sodium hydroxide and potassium hydroxide and at least one acidic precursor selected from aluminum sulphate, aluminum chloride, aluminum nitrate, sulfuric acid, hydrochloric acid, and nitric acid, wherein at least one of the basic or acidic precursors comprises aluminum, the relative flow rate of the acidic and basic precursors is chosen so as to obtain a pH of the reaction medium of between 8.5 and 10.5 and the flow rate of the acidic and basic precursor (s) containing aluminum is adjusted so as to obtain an advancement rate of the second stage inclusive entry e 0 and 60%, the advancement rate being defined as the proportion of alumina formed in equivalent A1203 during said second precipitation step relative to the total amount of alumina formed at the end of the two stages of precipitation and preferably at the end of step a ') of the process according to the invention, said step operating at a temperature between 40 and 90 ° C, and for a period of between 2 minutes and 50 minutes.
[0026] As in the first precipitation step a), the addition to the heated suspension of at least one basic precursor and at least one acid precursor requires either at least the basic precursor or the acidic precursor. comprises aluminum, that the two basic precursors and acid include aluminum.
[0027] Basic precursors comprising aluminum are sodium aluminate and potassium aluminate. The preferred basic precursor is sodium aluminate. Acidic precursors comprising aluminum are aluminum sulphate, aluminum chloride and aluminum nitrate. The preferred acidic precursor is aluminum sulphate. Preferably, said second precipitation step operates with stirring.
[0028] Preferably, said second step is carried out in the absence of organic additive. The acidic and basic precursors, whether they contain aluminum or not, are mixed, preferably in solution, in the aqueous reaction medium, in such proportions that the pH of the resulting suspension is between 8.5 and 10. 5.
[0029] As in step a) of precipitation, it is the relative flow rate of the acidic and basic precursors that they contain aluminum or not, which is chosen so as to obtain a pH of the reaction medium comprised between 8.5 and 10.5. In the preferred case where the basic and acidic precursors are respectively sodium aluminate and aluminum sulphate, the mass ratio of said basic precursor to said acidic precursor is advantageously between 1.6 and 2.05. For the other basic and acidic precursors, whether they contain aluminum or not, the base / acid mass ratio is established by a curve of neutralization of the base by the acid. Such a curve is easily obtained by those skilled in the art.
[0030] Preferably, said second precipitation step is carried out at a pH of between 8.5 and 10 and preferably between 8.7 and 9.9. The acidic and basic precursors are also mixed in amounts to provide a suspension containing the desired amount of alumina, depending on the final alumina concentration to be achieved. In particular, said second precipitation step makes it possible to obtain from 0 to 60% by weight of alumina in Al 2 O 3 equivalent relative to the total amount of alumina formed at the end of the two precipitation stages and preferably at the end of from step a '). As in step a) of precipitation, it is the flow rate of the acidic and basic precursor (s) containing aluminum which is adjusted so as to obtain a progress rate of the second stage between 0 and 60%, the percentage of progress being defined as the proportion of alumina formed during said second precipitation step relative to the total amount of alumina formed at the end of the two precipitation steps of the process according to the invention and preferably at the end of step a ').
[0031] Preferably, the rate of advancement of said second precipitation step a) is from 1 to 60, preferably from 10 to 55 (3/0 and preferably from 15 to 55%. concentration of alumina referred to after the precipitation step (s), preferably between 20 and 100 g / l, the amounts of aluminum to be provided by the acid precursors and / or basic are calculated and the flow rate of precursors is set according to the concentration of said added aluminum precursors, the amount of water added to the reaction medium and the rate of progress required for each of the precipitation steps.
[0032] As in step a) of precipitation, the flow rate of the acid-containing precursor (s) and / or base (s) containing aluminum depending on the size of the reactor used and thus the quantity of water added to the reaction medium. .
[0033] By way of example, if one works in a 3 1 reactor and is aimed at alumina suspension with a final concentration of Al 2 O 3 of 50 g / l, the target rate of advancement is 50%. equivalent A1203 for the first precipitation stage. Thus, 50% of the total alumina must be provided during step a) of precipitation. The alumina precursors are sodium aluminate at a concentration of 155 g / l in Al 2 O 3 and aluminum sulphate at a concentration of 102 g / l in Al 2 O 3. The precipitation pH of the first stage is set at 9 And the second to 9. The amount of water added to the reactor is 622 ml. For the first step a) of precipitation operating at 30 ° C. and for 8 minutes, the flow rate of aluminum sulphate should be 10.5 ml / min and the flow rate of sodium aluminate is 13.2 15 ml / min. The mass ratio of sodium aluminate to aluminum sulfate is therefore 1.91. For the second precipitation stage, operating at 70 ° C., for 30 minutes, the aluminum sulfate flow rate should be 2.9 ml / min and the sodium aluminate flow rate is 3.5 ml / min. The mass ratio of sodium aluminate to aluminum sulfate is therefore 1.84.
[0034] Preferably, the second precipitation step is carried out at a temperature between 40 and 80 ° C, preferably between 45 and 70 ° C and very preferably between 50 and 70 ° C. Preferably, the second precipitation step is carried out for a period of between 5 and 45 minutes, and preferably of 7 to 40 minutes.
[0035] The second precipitation step generally makes it possible to obtain a suspension of alumina having an Al 2 O 3 concentration of between 20 and 100 g / l, preferably between 20 and 80 g / l, preferably between 20 and 50 g. / I.
[0036] In the case where said second precipitation step is carried out, said preparation process also advantageously comprises a second step of heating the suspension obtained at the end of said second precipitation step to a temperature of between 50 and 95 ° C. C and preferably between 60 and 90 ° C.
[0037] Preferably, said second heating step is carried out for a period of between 7 and 45 minutes. Said second heating step is advantageously carried out according to all the heating methods known to those skilled in the art.
[0038] Said second heating step makes it possible to increase the temperature of the reaction medium before subjecting the suspension obtained in step b) of heat treatment. Filtration step c) According to the invention, the process for preparing the alumina gel according to the invention also comprises a step c) of filtering the suspension obtained at the end of the heat treatment step b) followed by at least one washing step of the gel obtained. Said filtration step is advantageously carried out according to the methods known to those skilled in the art. The filterability of the suspension obtained at the end of step a) of precipitation or of both precipitation stages is improved by the presence of said final heat treatment step b) of the suspension obtained, said heat treatment stage favoring the productivity of the process according to the invention, as well as an extrapolation of the process at the industrial level. Said filtration step is advantageously followed by at least one washing step with water and preferably from one to three washing steps, with a quantity of water equal to the amount of filtered precipitate. The preparation process according to the present invention comprising at least one alumina precipitation step making it possible to obtain at least 40% by weight of alumina with respect to the total amount of alumina formed in A1203 equivalent at the end of the process. of the process, and at least one final heat treatment stage of the suspension obtained thus makes it possible to obtain the alumina gel according to the invention having a dispersibility index greater than 70% and a crystallite size of between 2 and 35 nm .
[0039] The present invention also relates to the alumina gel obtainable by the preparation process according to the invention. The invention is illustrated by the following examples, which in no way present a limiting character.
[0040] Examples: Example 1: (Comparative) A commercial powder of a Pural SB3 alumina gel is prepared in a sol-gel route by hydrolysis-polycondensation of an aluminum alkoxide.
[0041] The characteristics of Pural SB3 boehmite gel are summarized in Table 1. Table 1: Characteristics of Pural SB3. Commercial alumina gel Dispersibility index 98 Size (020) (nm) 3.1 Size (120) (nm) 4.7 Sodium Na (ppm) <limit of detection Sulfur S (ppm) <limit of detection sulfur is measured by the X-ray fluorescence method, and the sodium content is measured by ICP or inductively coupled plasma spectrometry are below the detection limit of these measurement methods. Example 2 (Comparative): The synthesis of an alumina gel is carried out according to a preparation method not in accordance with the invention in that the precipitation step is carried out at high temperature, that is to say at a temperature of 60 ° C. The agitation is 350 rpm throughout the synthesis. The synthesis is carried out in a reactor of 5 1 in 2 stages, a precipitation stage and a stage of ripening of the suspension obtained. The final target alumina concentration is 50 g / I.
[0042] A step of precipitating Al2 (504) aluminum sulphate and NaA100 sodium aluminate is carried out at 60 ° C and pH = 10.2 during a 20 minute cure. The concentrations of the aluminum precursors used are as follows: Al 2 (504) = 102 g / l in Al 2 O 3 and Naa 100 to 155 g / l in Al 2 O 3 A solution of aluminum sulphate Al 2 (504) is added continuously for 30 minutes. 25.9 ml / min at a rate of sodium aluminate NaA100 in a basis / acid mass ratio = 2.0 so as to adjust the pH to a value of 10.2. All precursors are contacted at a temperature of 60 ° C. A suspension containing a precipitate of alumina is obtained. Since the final concentration of alumina is 50 g / l, the flow rate of aluminum sulphate precursors Al 2 (504) and sodium aluminum aluminate NaA 100 introduced in the first precipitation step are 25 respectively. 9 ml / min and 34.1 ml / min. These flow rates of acidic and basic precursors containing aluminum make it possible to obtain at the end of the first precipitation step a degree of advance of 100%.
[0043] The resulting suspension is then subjected to a temperature rise of 60 to 90 ° C. The suspension then undergoes a ripening step in which it is maintained at 90 ° C for 60 minutes.
[0044] The suspension obtained is then filtered by displacement of water on a sintered Buchner type tool and the resulting alumina gel is washed 3 times with 3.5L of distilled water at 70 ° C. The filtration and washing time is 3h. The characteristics of the alumina gel thus obtained are summarized in Table 2.
[0045] TABLE 2 Characteristics of the alumina gel obtained according to Example 2. Example 3 Dispersibility index Ta (10% (° / 0)) 0 Size (020) (nm) 2.9 Size (120) (nm) 3.4 Sodium Na (° / 0) 0.0068 Sulfur S (° / 0) 0.042 Filtering time 3 h Example 2 not in accordance with the invention demonstrates the importance of operating during the precipitation step at low temperature and in particular during the first precipitation step. Thus, a precipitation step carried out at a temperature of 70 ° C., outside the ranges claimed, does not make it possible to obtain a dispersible gel. In contrast, the 10% dispersion of alumina gel thus obtained in a water suspension also containing 10% nitric acid relative to the alumina gel mass, followed by centrifugation of the suspension at 3600G for 10 minutes. min leads to 100% sediment.
[0046] EXAMPLE 3 (COMPARATIVE) The synthesis of an alumina gel is carried out according to a non-conforming preparation process in that the process for preparing the gel according to Example 3 does not include a heat treatment step and in that the first precipitation step a) does not produce an amount of alumina greater than 40%, based on the total amount of alumina formed at the end of the second precipitation step. Example 3 is carried out according to the preparation method described in US Pat. No. 7,790,562. The synthesis is carried out in a reactor of 7 liters and a final suspension of 5 liters in two precipitation stages. The amount of water added to the reactor is 3868 ml.
[0047] The final target alumina concentration is 30 g / l. A first step of co-precipitation of aluminum sulphate Al2 (504) and of sodium aluminate NaA100 is carried out at 30 ° C. and pH = 9.3 for a period of 8 minutes. The concentrations of the aluminum precursors used are as follows: Al 2 (504) = 102 g / l in Al 2 O 3 and Naa 100 to 155 g / l in Al 2 O 3. The agitation is 350 rpm throughout the synthesis. A solution of aluminum sulphate Al2 (504) is added continuously for 8 minutes at a flow rate of 19.6 ml / min to a solution of sodium aluminate NaA100 in a weight ratio base / acid = 1.80 to adjust the pH to a value of 9.3. The temperature of the reaction medium is maintained at 30 ° C. A suspension containing a precipitate of alumina is obtained. The final concentration of alumina targeted being 30 g / l, the flow rate of aluminum sulphate precursors Al 2 (504) and aluminum aluminate NaA 100 containing aluminum introduced in the first precipitation step are respectively 19.6 ml / min. and 23.3 ml / min. These flow rates of acid and basic precursors containing aluminum make it possible to obtain at the end of the first precipitation step a degree of progress of 30%. The suspension obtained is then subjected to a temperature rise of 30 to 57 ° C.
[0048] A second step of co-precipitation of the suspension obtained is then carried out by adding aluminum sulphate Al 2 (504) at a concentration of 102 g / l of Al 2 O 3 and of sodium aluminate NaAl 3 at a concentration of 155 g / l. L in A1203. A solution of aluminum sulphate Al2 (504) is therefore added continuously to the heated suspension obtained at the end of the first precipitation step for 30 minutes at a flow rate of 12.8 ml / min at a solution of sodium aluminate NaA100 in a weight ratio base / acid = 1.68 so as to adjust the pH to a value of 8.7. The temperature of the reaction medium in the second step is maintained at 57 ° C. A suspension containing a precipitate of alumina is obtained.
[0049] The final concentration of alumina targeted being 30 g / l, the flow rate of the aluminum sulphate precursors Al 2 (SO 4) and aluminum aluminate NaA 100 containing aluminum introduced in the second precipitation stage are respectively 12.8 ml. / min and 14.1 ml / min. These flow rates of acidic and basic precursors containing aluminum make it possible to obtain at the end of the second precipitation stage a 70% degree of advance. The suspension thus obtained does not undergo a ripening step. The suspension obtained is then filtered by displacement of water on a sintered Buchner type tool and the resulting alumina gel is washed 3 times with 5 l of distilled water at 70 ° C. Filtration and washing time is 4 hours. The characteristics of the alumina gel thus obtained are summarized in Table 3.
[0050] TABLE 3 Characteristics of the alumina gel obtained according to Example 3. Example 3 Dispersibility index Ta = 10 ° / 0 (° / 0) 60 Size (020) (nm) 2.9 Size (120) (nm) 4.1 Sodium Na (ppm) 0.011 S sulfur (ppm) 0.057 Filtration time 4 h Example 4 (according to the invention): The synthesis of an alumina gel is carried out according to a preparation method according to the invention. invention in a reactor of 71 and a final suspension of 51 in 3 steps, two precipitation steps followed by a ripening step. The final alumina concentration is 45g / I. The amount of water added to the reactor is 3267 ml. The agitation is 350 rpm throughout the synthesis.
[0051] A first step of co-precipitation in water, aluminum sulphate Al2 (504) and sodium aluminate NaA100 is carried out at 30 ° C and pH = 9.5 for a period of 8 minutes. The concentrations of aluminum precursors used are as follows: Al 2 (504) = 102 g / l in Al 2 O 3 and Naa 100 to 155 g / l in Al 2 O 3. A solution of aluminum sulphate Al 2 (SO 4) is added continuously for 8 hours. minutes at a rate of 69.6 ml / min to a solution of sodium aluminate NaA100 at a flow rate of 84.5 ml / min in a mass ratio acid / acid = 1.84 so as to adjust the pH to a value 9.5. The temperature of the reaction medium is maintained at 30 ° C.
[0052] A suspension containing a precipitate of alumina is obtained. The final concentration of alumina targeted being 45 g / l, the flow rate of aluminum sulphate precursors Al 2 (SO 4) and aluminum aluminate Na 3 100 containing aluminum introduced in the first precipitation stage are respectively 69.6 ml / min. and 84.5 ml / min. These flow rates of aluminum-containing acidic and basic precursors make it possible to obtain at the end of the first precipitation stage an advancement rate of 72%. The resulting suspension is then subjected to a temperature rise of 30 to 68 ° C. A second step of co-precipitation of the suspension obtained is then carried out by adding aluminum sulphate Al 2 (SO 4) at a concentration of 102 g / l of Al 2 O 3 and of sodium aluminate NaA 100 at a concentration of 155 g / l in A1203. A solution of aluminum sulphate Al2 (SO4) is therefore added continuously to the heated suspension obtained at the end of the first precipitation step for 30 minutes at a flow rate of 7.2 ml / min to an aluminate solution. of sodium NaA100 in a base / acid mass ratio = 1.86 so as to adjust the pH to a value of 9. The temperature of the reaction medium in the second step is maintained at 68 ° C. A suspension containing a precipitate of alumina is obtained. As the final concentration of alumina is 45 g / l, the flow rate of aluminum sulphate precursors Al 2 (SO 4) and aluminum aluminate Na 3 100 containing aluminum introduced into the second precipitation stage are respectively 7.2 ml / min and 8.8 ml / min. These flow rates of acid and basic precursors containing aluminum make it possible to obtain at the end of the second precipitation stage a progress rate of 28%.
[0053] The resulting suspension is then subjected to a temperature rise of 68 to 90 ° C. The slurry then undergoes a heat treatment step in which it is held at 90 ° C for 60 minutes.
[0054] The suspension obtained is then filtered by displacement of water on a sintered Buchner type tool and the resulting alumina gel is washed 3 times with distilled water. The filtration and washing time is 3h. The characteristics of the alumina gel thus obtained are summarized in Table 4.
[0055] Table 4: characteristics of the alumina gel obtained according to Example 4. Example 3: Dispersibility index Ta = 10`) 0 (`) / 0) 100 Size (020) (nm) 2.8 Size (120) (nm) 3.5 Sodium Na (°) / 0) 0.074 S sulfur (°) / 0) 0.0364 Filtration time 3 h A gel having a dispersibility index of 100% is thus obtained. Moreover, the gel 10 obtained by the process according to the invention characterized by the presence of a final heat treatment step makes it possible to obtain an alumina gel having good filterability, that is to say a time filtration system compatible with an extrapolation at the industrial level of the process, thus allowing a better productivity of said process. It is also noted that the alumina gel obtained according to the preparation method according to the invention is easily shaped. The preparation process according to the invention making it possible to obtain a 100% dispersible gel is also less expensive than the conventional alumina preparation processes of the prior art, such as for example the sol-gel type preparation processes. Example 5 (Comparative): Example 5 not according to the invention is carried out in the same manner and under the same operating conditions as Example 3 except that The suspension obtained at the end of the second precipitation stage does not undergo a ripening stage. The suspension obtained at the end of the second precipitation step is filtered by displacement of water on a sintered Buchner type tool and the resulting alumina gel is washed 3 times with 3.5 l of distilled water.
[0056] The filtration and washing time is 24 hours.
[0057] The characteristics of the alumina gel thus obtained are summarized in Table 5. Table 5: Characteristics of the alumina gel obtained according to Example 5. Example 5 Dispersibility index Ta = 10`) 0 (`) / 0) 100 Size (020) (nm) 2.8 Size (120) (nm) 3.5 Sodium Na (`) / 0) 0.442 Sulfur S (`) / 0) 0.0284 Filtration time 24h 5 22
权利要求:
Claims (13)
[0001]
1. Alumina gel having a dispersibility index greater than 70%, a crystallite size of between 1 and 35 nm and a sulfur content of between 0.001% and 2% by weight and a sodium content of between 0.001% and 2% by weight, the weight percentages being expressed relative to the total mass of alumina gel.
[0002]
2. Alumina gel according to claim 1 having a dispersibility index between 80 and 100%. 10
[0003]
3. Process for the preparation of the alumina gel according to one of claims 1 or 2, said process comprising at least the following steps: a) at least a first step of precipitation of alumina, in an aqueous reaction medium, from at least one basic precursor selected from sodium aluminate, potassium aluminate, ammonia, sodium hydroxide and potassium hydroxide and at least one acidic precursor selected from aluminum sulphate, aluminum chloride, aluminum nitrate, sulfuric acid, hydrochloric acid, and nitric acid, wherein at least one of the basic or acidic precursors comprises aluminum, the relative acidic and basic precursors are chosen so as to obtain a pH of the reaction medium of between 8.5 and 10.5 and the flow rate of the acidic and basic precursor (s) containing aluminum is adjusted so as to obtain a advancement of said first step between 40 and 100 %, the advancement rate being defined as the proportion of alumina formed in Al 2 O 3 equivalent during said first precipitation step relative to the total amount of alumina formed at the end of the precipitation step or steps, said first precipitation step operating at a temperature between 10 and 50 ° C, and for a period of between 2 minutes and 30 minutes, b) a heat treatment step of the suspension obtained at the end of step a) at a temperature between 50 and 200 ° C for a period of between 30 minutes and 5 hours, 0) a filtration step of the suspension obtained at the end of the heat treatment step b), followed by at least one washing step of the gel obtained.
[0004]
4. Preparation process according to claim 3 wherein the basic precursor is sodium aluminate. 35
[0005]
5. Preparation process according to one of claims 3 or 4 wherein the acidic precursor is aluminum sulfate. 23 3022235
[0006]
6. Preparation process according to one of claims 4 and 5 wherein the mass ratio of said basic precursor on said acid precursor is between 1.6 and 2.05.
[0007]
7. Preparation process according to one of claims 3 to 6 wherein the rate of progress of said precipitation step a) is between 45 and 90%.
[0008]
8, preparation process according to one of claims 3 to 7 wherein said step a) of precipitation is carried out at a temperature between 20 and 45 ° C.
[0009]
9. Preparation process according to one of claims 3 to 8 wherein, in the case where the advancement rate obtained at the end of the first step a) of precipitation is less than 100%, said method of preparation comprises a second precipitation step a ') after the first precipitation step.
[0010]
10. Preparation process according to claim 9 wherein a step of heating the suspension obtained at the end of step a) of precipitation is carried out between the two precipitation steps a) and a '), said step heating operating at a temperature between 20 and 90 ° C and for a period of between 7 and 45 minutes.
[0011]
11. A method of preparation according to one of claims 9 or 10 wherein said second precipitation step a ') of the suspension obtained at the end of the heating step, operates by adding in said suspension of at least one basic precursor selected from sodium aluminate, potassium aluminate, ammonia, sodium hydroxide and potassium hydroxide and at least one acidic precursor selected from aluminum sulfate, sodium chloride, aluminum, aluminum nitrate, sulfuric acid, hydrochloric acid, and nitric acid, wherein at least one of the basic or acidic precursors comprises aluminum, the relative flow rate of the acid precursors and basic is chosen so as to obtain a pH of the reaction medium of between 8.5 and 10.5 and the flow rate of the acidic and basic precursor (s) containing aluminum is adjusted so as to obtain a progress rate of the second step between 0 and 60%, said advance rate cement of the second stage being defined as being the proportion of alumina formed in equivalent A1203 during said second precipitation step a ') with respect to the total amount of alumina formed at the end of step a'), said second step a ') operating at a temperature between 40 and 90 ° C, and for a time between 2 minutes and 50 minutes, 24 3022235
[0012]
12. Preparation process according to claim 11 wherein the mass ratio of said basic precursor on said acid precursor is between 1.6 and 2.05, the basic precursors and acid being respectively sodium aluminate and aluminum sulphate . 5
[0013]
13. Preparation process according to one of claims 11 or 12 wherein the second precipitation step a ') is carried out at a temperature between 45 and 70 ° C.
类似技术:
公开号 | 公开日 | 专利标题
EP3154908B1|2020-01-08|Method for preparing gel with high dispersibility
EP3154677B1|2019-02-06|Amorphous mesoporous alumina with high connectivity and production method thereof
EP0153227B1|1988-10-12|Cerium dioxide with morphological characteristics, and process for its preparation
JP2005255450A|2005-09-22|Zirconium oxide crystal particle and method for producing the same
FR2684662A1|1993-06-11|COMPOSITION BASED ON CERIC OXIDE, PREPARATION AND USE
EP1098848B1|2003-10-15|Novel dispersible aluminium hydrate, method for preparing same and use for preparing catalysts
EP3154907B1|2019-04-03|Amorphous mesoporous alumina with optimised pore distribution and method for preparing same
EP3408226B1|2021-03-17|Method for producing an alumina gel having a high dispersibility and a specific crystallite size
EP3233735B1|2020-06-10|Method for the preparation of alumina beads formed by dewatering a highly dispersible gel
FR3067022A1|2018-12-07|PROCESS FOR THE PREPARATION OF A MESOPOROUS ALUMINA FROM A PREPARED DISPERSIBLE GEL WITHOUT PUSHED DRYING
WO2018077764A1|2018-05-03|Method for preparing a composite porous material
FR3037054A1|2016-12-09|PROCESS FOR THE PREPARATION OF A BOEHMITE HAVING PARTICULATE CRYSTALLITES
WO2019011569A1|2019-01-17|Method for hydrogenating aromatics using a catalyst obtained by impregnation comprising a specific support
JP6014830B2|2016-10-26|Method for producing Nb-W oxide catalyst, Nb-W oxide catalyst
JP2021151942A|2021-09-30|Porous silica alumina particles and method for producing the same
FR3112540A1|2022-01-21|Process for the preparation of a high dispersibility alumina gel
Yarovaya et al.2011|Synthesis of copper | oxide hydrosols
同族专利:
公开号 | 公开日
FR3022235B1|2021-05-07|
RU2017100950A3|2019-02-28|
EP3154908A1|2017-04-19|
US20180334391A1|2018-11-22|
US10858262B2|2020-12-08|
RU2694751C2|2019-07-16|
JP6789360B2|2020-11-25|
JP2017521343A|2017-08-03|
WO2015189203A1|2015-12-17|
CN106687412A|2017-05-17|
DK3154908T3|2020-04-20|
CN106687412B|2018-03-13|
EP3154908B1|2020-01-08|
US20170121181A1|2017-05-04|
RU2017100950A|2018-07-13|
BR112016028715A2|2017-08-22|
JP2020073429A|2020-05-14|
引用文献:
公开号 | 申请日 | 公开日 | 申请人 | 专利标题
GB2123804A|1982-06-23|1984-02-08|Grace W R & Co|Dispersible alpha-aluminate monohydrate|
EP0147167A2|1983-12-22|1985-07-03|Aluminum Company Of America|Continuous process for neutralization of aluminate solution to form gels and appartatus therefor|
US6713428B1|1998-07-06|2004-03-30|Instuit Francais Du Petrole|Dispersible aluminium hydrate, method for preparing same and use for preparing catalysts|
US7790652B2|2003-09-17|2010-09-07|Shell Oil Company|Process and catalyst for the hydroconversion of a heavy hydrocarbon feedstock|
GB1603464A|1977-03-25|1981-11-25|Grace W R & Co|Alumina compositions|
SU1787941A1|1991-03-07|1993-01-15|Inst Chimii Tech Redkik|Method of aluminium hydroxide production|
EP0885844B1|1996-03-05|2003-06-04|Goro Sato|Alumina sol, process for preparing the same, process for preparing alumina molding using the same, and alumina-based catalyst prepared thereby|
US6312619B1|1999-06-10|2001-11-06|Condea Vista Company|Method for producing water-dispersible alpha-alumina monohydrate|
JP4054183B2|2001-09-27|2008-02-27|触媒化成工業株式会社|Alumina production equipment|
US7422730B2|2003-04-02|2008-09-09|Saint-Gobain Ceramics & Plastics, Inc.|Nanoporous ultrafine α-alumina powders and sol-gel process of preparing same|
TW200846286A|2007-05-22|2008-12-01|Grace W R & Co|Alumina particles and methods of making the same|
RU2409519C1|2009-07-08|2011-01-20|Закрытое акционерное общество "Центр инновационных керамических нанотехнологий Нанокомпозит"|Method of producing nanopowder of alpha aluminium oxide with narrow particle size distribution|
JP5610842B2|2010-05-20|2014-10-22|日揮触媒化成株式会社|Alumina hydrate fine particles, method for producing alumina hydrate fine particles, binder and ceramic molded body|
CN101928029A|2010-09-08|2010-12-29|苏州创元投资发展有限公司|Method for preparing aluminum oxide sol|
CN102180497B|2011-03-15|2012-09-26|宣城晶瑞新材料有限公司|Non-hydrolytic sol-gel method for preparing high- dispersity nano alumina|
CN103288114A|2013-05-29|2013-09-11|如皋市乐恒化工有限公司|Preparation method of high-purity aluminum oxide|FR3047238B1|2016-01-29|2021-07-16|Ifp Energies Now|PROCESS FOR PREPARING AN ALUMINA GEL PRESENTING A HIGH DISPERSIBILITY AND A SPECIFIC CRYSTALLITE SIZE|
CN111320194A|2020-04-24|2020-06-23|山东中科天泽净水材料有限公司|Preparation method of aluminum glue and polyaluminium chloride|
FR3112540A1|2020-07-20|2022-01-21|IFP Energies Nouvelles|Process for the preparation of a high dispersibility alumina gel|
FR3112496A1|2020-07-20|2022-01-21|IFP Energies Nouvelles|Method for washing a suspension of metal oxides|
法律状态:
2015-06-02| PLFP| Fee payment|Year of fee payment: 2 |
2015-12-18| PLSC| Search report ready|Effective date: 20151218 |
2016-06-07| PLFP| Fee payment|Year of fee payment: 3 |
2017-06-22| PLFP| Fee payment|Year of fee payment: 4 |
2018-06-27| PLFP| Fee payment|Year of fee payment: 5 |
2020-06-26| PLFP| Fee payment|Year of fee payment: 7 |
2021-06-25| PLFP| Fee payment|Year of fee payment: 8 |
优先权:
申请号 | 申请日 | 专利标题
FR1455421A|FR3022235B1|2014-06-13|2014-06-13|HIGH DISPERSIBILITY GEL AND ITS PREPARATION PROCESS|FR1455421A| FR3022235B1|2014-06-13|2014-06-13|HIGH DISPERSIBILITY GEL AND ITS PREPARATION PROCESS|
RU2017100950A| RU2694751C2|2014-06-13|2015-06-09|Gel with high degree of dispersibility and method of its production|
US15/318,582| US20170121181A1|2014-06-13|2015-06-09|Gel with high dispersibility and method for preparing same|
PCT/EP2015/062829| WO2015189203A1|2014-06-13|2015-06-09|Gel with high dispersibility and method for preparing same|
EP15727663.5A| EP3154908B1|2014-06-13|2015-06-09|Method for preparing gel with high dispersibility|
CN201580031667.0A| CN106687412B|2014-06-13|2015-06-09|Gel with polymolecularity and preparation method thereof|
DK15727663.5T| DK3154908T3|2014-06-13|2015-06-09|PROCEDURE FOR THE GEL WITH HIGH DISPERSIBILITY|
BR112016028715A| BR112016028715A2|2014-06-13|2015-06-09|high dispersibility gel and its preparation process|
JP2016572481A| JP2017521343A|2014-06-13|2015-06-09|Highly dispersible gel and method for preparing the same|
US16/045,118| US10858262B2|2014-06-13|2018-07-25|Gel with high dispersibility and method for preparing same|
JP2019181423A| JP6789360B2|2014-06-13|2019-10-01|Highly dispersible gel and its preparation method|
[返回顶部]